| HS Code | 831408 |
| Density | 1.41 g/cm³ |
| Glass Fiber Content | 15 wt% |
| Tensile Strength | 90 MPa |
| Tensile Elongation At Break | 3.0% |
| Flexural Modulus | 4500 MPa |
| Flexural Strength | 140 MPa |
| Notched Izod Impact Strength | 50 J/m |
| Heat Deflection Temperature At 1 82 Mpa | 195 °C |
| Melting Point | 225 °C |
| Water Absorption 24h | 0.05% |
| Molding Shrinkage Flow | 0.4% |
| Molding Shrinkage Cross Flow | 0.8% |
| Ul94 Flammability | HB |
| Dielectric Strength | 20 kV/mm |
| Volume Resistivity | 1E15 ohm·cm |
As an accredited Korea Engineering Plastics KEPEX® PBT+GF15% 3315GF factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg moisture-proof bags, 40 bags per 1,000 kg pallet, labeled KEPEX® PBT+GF15% 3315GF for safe storage and transport. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized 25 kg bags of KEPEX® PBT+GF15% 3315GF, shrink-wrapped and secured for export shipment. |
| Shipping | Korea Engineering Plastics KEPEX® PBT+GF15% 3315GF is shipped as non-hazardous, glass-fiber-reinforced PBT pellets, typically packed in 25 kg moisture-barrier bags or 1,000 kg jumbo bags. Transport in dry, clean, closed containers, avoiding moisture, direct sunlight, and excessive heat. Store cool and dry before use; no special dangerous-goods classification is indicated. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and ignition sources. Keep containers tightly closed to prevent moisture absorption and contamination. Avoid dust generation and static buildup. Use proper grounding during handling. Protect from physical damage and store separately from incompatible chemicals. Observe local regulations and material safety data sheet recommendations. |
| Shelf Life | Shelf life: 12 months in original unopened packaging, stored dry and cool, protected from moisture and direct sunlight. |
Competitive Korea Engineering Plastics KEPEX® PBT+GF15% 3315GF prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Korea Engineering Plastics KEPEX® PBT+GF15% 3315GF is a 15% by mass short-glass-fibre-reinforced polybutylene terephthalate injection-molding grade. The designation “3315GF” identifies the glass-filled variant within the KEPEX PBT series, with nominal glass content retained as specified by ISO 3451-1 Method A. The material is positioned between unfilled PBT and 30% glass-filled PBT for moulded components that require higher flexural modulus than unfilled PBT but lower anisotropic shrinkage and improved surface uniformity compared with 30% glass-filled systems. Representative values consolidated from manufacturer technical data are provided in the table. These values are not specification limits and may shift with colour, regrind content, moisture condition, and sampling lot. Verification against the current KEPEX datasheet is required before tooling release.
| Property | 3315GF | Unfilled PBT | PBT+GF30 | Test standard |
|---|---|---|---|---|
| Glass fibre content | 15% | 0% | 30% | ISO 3451-1 |
| Density | 1.42 g/cm³ | 1.31 g/cm³ | 1.53 g/cm³ | ISO 1183-1 |
| Tensile strength at break | 88 MPa | 55 MPa | 120 MPa | ISO 527-1/2 |
| Flexural modulus | 4,700 MPa | 2,500 MPa | 7,500 MPa | ISO 178 |
| Charpy notched impact strength, 23 °C | 4.5 kJ/m² | 4.0 kJ/m² | 7.0 kJ/m² | ISO 179-1/1eA |
| Heat deflection temperature, 1.8 MPa | 185 °C | 60 °C | 200 °C | ISO 75-1/2 |
| Mould shrinkage, flow direction / transverse | 0.4–0.9% / 0.6–1.1% | 1.5–2.0% / 1.5–2.0% | 0.3–0.7% / 0.5–0.9% | ISO 294-4 |
At 15% fibre loading, the tensile strength-to-flexural modulus ratio places the grade in the lower stiffness region of reinforced PBT, while the retained notched impact strength and melt-flow behaviour support thin-wall filling and ejection-warp control. The anisotropic shrinkage shown in the table follows glass-fibre orientation. The flow-direction and transverse-direction shrinkage differential is smaller for 3315GF than for 30% glass-filled PBT, which reduces arching and twist in flat parts. This shrinkage behaviour is measured by ISO 294-4 plaque testing and is influenced by fibre length retention during compounding. On production-scale co-rotating twin-screw compounding equipment with a length-to-diameter ratio of 40:1, excessive side-feeder shear can reduce mean glass-fibre length below 200 µm and lower flexural modulus by more than 10%.
Mechanical response under load differs by failure mode. Unfilled PBT yields at low stress and fails by ductile drawing, while 30% glass-filled PBT often fails by fibre pullout and matrix microcracking, with higher tensile strength but reduced practical flow in ribs below 1.0 mm thickness. 3315GF produces a mixed failure mode: short glass fibres bridge incipient crazes and increase load-bearing capacity without the marked embrittlement associated with 30% fibre loading. Under ISO 527-1/2 Type 1A tensile testing, the 15% grade typically shows elongation at break of 3–5%, compared with 5–10% for unfilled PBT and 2–3% for 30% glass-filled PBT. The result is a component that can tolerate occasional snap-fit deflection while remaining stiffer than unfilled PBT under creep at room temperature. Creep modulus under a 1,000 h load and 0.5% strain follows ISO 899-2; published data for this specific configuration is limited, and long-term design should use coupon-level flexural creep testing on production-colour specimens.
Drying residual moisture to below 0.02% is the first processing constraint. Hydrolysis of PBT is autocatalytic when wet pellets are exposed to melt temperatures above 240 °C. On a 25 mm diameter three-zone screw with L/D 22:1, a barrel temperature profile of 240/245/250/255/260 °C from rear to nozzle and a screw speed of 60–120 min⁻¹ produce stable melt. Dehumidified hopper drying at 120 °C for 4 h with a dew point not higher than −40 °C is recommended. Target residual moisture, measured by ISO 15512, must remain below 0.02% by mass. At melt temperatures above 250 °C, apparent melt viscosity may fall by 10–20% within 5 min of residence time due to hydrolytic chain scission. The non-return valve should be inspected after every 2,000 shots; valve leakage increases cushion variation and causes short shots, gas burns, and fibre clumping at the gate. Back pressure of 0.3–0.7 MPa and injection velocity of 80–120 mm/s are typical starting parameters. Clamp force requirement at a projected-area pressure of 0.5–0.7 kN/cm² is usually satisfied by a 60–80 t toggle press for parts up to 300 cm² projected area. For hot-runner systems, externally heated manifolds with independent nozzle control at 250–260 °C are preferred; internal heater failures create cold slugs and fibre-orientation defects at the gate.
Underhood sensor housings require long-term heat aging, dimensional stability, and resistance to automotive fluids. The grade’s heat deflection temperature of 185 °C at 1.8 MPa under ISO 75-1/2 supports short-term paint-bake cycle exposure, but continuous use above 150 °C requires confirmation because PBT retained properties after thermal aging depend on antioxidant protection. Immersion in SAE 10W-40 oil at 120 °C for 500 h typically reduces tensile strength by less than 15%; however, published data for this specific configuration is limited, and validation should follow ISO 175. For electrical connectors, the grade can be moulded in wall thicknesses from 0.5 mm to 2.0 mm with a melt flow length that permits filling of 0.8 mm wall sections at 80–100 MPa injection pressure. Flammability classification is grade-specific; a natural PBT+GF15 product is typically classified UL 94 HB at 1.5 mm thickness when tested in accordance with Underwriters Laboratories UL 94, but the current yellow card must be verified for production-colour and lot-specific data. The same balance of dimensional stability and flow is used for relay bobbins, cooling fan shrouds, and motor end caps. In relay bobbins, the 15% glass loading reduces post-mould creep under coil winding stress, while the lower fibre concentration than 30% glass-filled PBT reduces coil breakage from brittle edge chipping. In cooling fan shrouds, the shrinkage difference between flow and transverse directions is low enough to maintain circularity within 0.4% after 24 h at 23 °C and 50% relative humidity.
Unlike unfilled PBT, tooling for 15% glass-filled PBT requires positive ventilation and revised shrink factors. Vent depth is limited to 0.01–0.03 mm because melt viscosity at 250 °C is higher than unfilled PBT and glass fibres can obstruct deep vents. Vent width is increased to 5–8 mm at intervals of 25–40 mm along the parting line. Runner diameter should be 6–8 mm for full-round runners or 7–10 mm equivalent for trapezoidal runners; subgates of 0.8–1.5 mm diameter are effective for automatic degating. Weld-line strength in glass-filled PBT is orientation-dependent. When two flow fronts meet, fibres align parallel to the weld plane, and tensile strength across the weld may be only 50–70% of the nominal value. Gate placement should force the weld line away from snap-fit features and press-fit bores. Shrink factor for tooling is normally 1.005–1.009 in the flow direction and 1.008–1.012 in the transverse direction; mould-making should use ISO 294-4 plaque data from the same colour and regrind level because regrind above 25% increases glass-fibre length degradation and can lower tensile modulus by up to 15%. If the part includes threaded inserts, the insert should be preheated to 80–100 °C before placement to reduce differential shrinkage cracking around the insert boss.