| HS Code | 248553 |
| Density | 1.52 g/cm³ |
| Glass Bead Content | 30% |
| Tensile Strength | 60 MPa |
| Elongation At Break | 3% |
| Flexural Modulus | 5000 MPa |
| Flexural Strength | 95 MPa |
| Charpy Notched Impact Strength | 4 kJ/m² |
| Hdt At 0 45 Mpa | 200 °C |
| Hdt At 1 82 Mpa | 70 °C |
| Melting Point | 225 °C |
| Molding Shrinkage | 0.9-1.1% |
| Water Absorption After 24 H | 0.08% |
| Flammability Rating | UL94 HB |
| Coefficient Of Linear Thermal Expansion | 7×10⁻⁵ /°C |
| Dielectric Strength | 20 kV/mm |
As an accredited Korea Engineering Plastics KEPEX® PBT+GB30% 3330GB factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packed in 25 kg moisture-resistant paper sacks, 40 sacks per pallet, totaling 1,000 kg per pallet. |
| Container Loading (20′ FCL) | Korea Engineering Plastics KEPEX® PBT+GB30% 3330GB is palletized and securely loaded into 20′ FCL containers for ocean shipment. |
| Shipping | KEPEX® PBT+GB30% 3330GB is supplied as non-hazardous thermoplastic pellets, typically in 25 kg moisture-barrier bags or octabins on pallets. Ship under dry, ventilated conditions, protected from moisture, direct sunlight, and excessive heat; no UN dangerous-goods classification normally applies. |
| Storage | Store KEPEX® PBT+GB30% 3330GB in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, moisture, and strong oxidizers. Keep original packaging sealed and intact to prevent contamination, moisture pickup, and physical damage. Do not store outdoors or near incompatible chemicals. Ensure containers remain closed when not in use. Use first-in, first-out rotation and maintain clean, dry, normal room-temperature conditions. |
| Shelf Life | Shelf life is typically 24 months when stored dry, cool, and in unopened original packaging, away from moisture and direct sunlight. |
Competitive Korea Engineering Plastics KEPEX® PBT+GB30% 3330GB prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Within the KEPEX® thermoplastic polyester range supplied by Korea Engineering Plastics, the designation PBT+GB30% 3330GB identifies a polybutylene terephthalate injection-moulding compound reinforced with 30% by weight spherical glass beads. The grade code 3330GB is the manufacturer’s internal series identifier and should be cross-referenced with the lot-specific certificate of analysis before tooling dimensions are released. Base-resin characterisation is governed by ISO 1133-1:2022 for melt mass-flow rate, ISO 1183-1:2019 for density, and ISO 3451-1:2019 for glass-content verification. Because the designation expresses reinforcement content by weight, the filler fraction by volume is lower than an equivalent mass fraction of high-aspect-ratio fibre and must be calculated from the density of the matrix and the glass phase. Published data for this specific 3330GB configuration is limited outside supplier-controlled channels; the technical datasheet issued by Korea Engineering Plastics therefore remains the definitive source.
Published class data for polybutylene terephthalate compounds containing 30% glass beads place density in the range of 1.52 g/cm³ to 1.56 g/cm³, compared with 1.30 g/cm³ to 1.31 g/cm³ for unfilled PBT. The density increase is approximately linear with glass addition, and the exact value depends on bead size distribution, surface treatment, and void content. Two production-relevant implications follow. First, the material weight per part increases relative to unfilled PBT by roughly 15% to 18% for identical part volume, which affects piece-price and energy calculations. Second, the presence of the glass phase alters melt thermal diffusivity and viscosity, so barrel temperature profiles may require slightly higher rear-zone inputs than unfilled PBT to achieve uniform melt temperature without exceeding the degradation boundary.
In semi-crystalline PBT, mould shrinkage after solidification is driven by crystallite formation and thermal contraction. A 30% spherical glass-bead loading reduces the volume fraction of crystallizable polymer and restricts local matrix contraction, so the linear mould shrinkage measured according to ISO 294-4 is lower than that of unfilled PBT. More importantly, the spherical reinforcement does not align strongly in the flow direction. Short-glass fibres orient along flow and generate pronounced anisotropic shrinkage: published class values for 30% glass-fibre PBT commonly show flow-direction shrinkage of 0.2% to 0.5% and transverse shrinkage of 0.8% to 1.2%. Glass-bead-filled PBT, by contrast, typically exhibits a more balanced shrinkage envelope near 0.8% to 1.2% in both flow and transverse directions. This balance is the primary reason the KEPEX 3330GB grade is positioned for flatness-sensitive mouldings where fibre-induced warpage is unacceptable.
Stress transfer differs fundamentally. A short glass fibre has an aspect ratio above 10:1, allowing axial load transfer along the length of the filament. A glass bead has an aspect ratio close to 1:1, which limits the maximum modulus and tensile strength achievable at the same filler content. Under ISO 527-1/-2, class-level tensile strength for 30% glass-bead-filled PBT is generally reported in the 55 MPa to 65 MPa band, overlapping many unfilled PBT grades, whereas 30% short-glass-fibre PBT is commonly reported above 110 MPa. Thus, 3330GB is not a drop-in replacement for a high-aspect-ratio fibre grade in structural ribs, snap-fit beams, or under-hood brackets where tensile strength is the design driver.
The benefit of the bead geometry appears in creep and thermal expansion. Rigid glass spheres constrain the matrix at multiple points, reduce overall thermal expansion, and improve resistance to progressive strain under sustained load when compared with unfilled PBT. However, notched impact may remain similar to or lower than unfilled PBT because the spherical particles do not bridge cracks as effectively as fibres. Charpy notched impact according to ISO 179-1/1eA should therefore be treated as a limitation, not a selection feature. Weld lines also require explicit validation: where two flow fronts meet, glass beads do not orient across the weld plane, and local strength may fall below the surrounding matrix even when the rest of the part shows acceptable dimensional stability.
PBT is susceptible to hydrolytic degradation when residual moisture is present in the melt. For glass-bead-filled PBT grades, the same boundary condition applies: the pellets should be dried in a desiccant dryer at 120 °C for 4 h to 6 h, with a dryer dew point of -30 °C or lower. The target residual moisture content by Karl Fischer titration is 0.02% or less. Moisture above this threshold reduces molecular weight at melt temperature and produces surface defects such as splay, silver streaking, and visible porosity at the flow-front edges. On production injection lines, moisture-related failures are often misread as mould temperature problems because the visible symptoms appear as local roughness rather than as overall brittleness.
The melt temperature window is relatively narrow. Class-level processing guidance for PBT compounds is 240 °C to 260 °C at the nozzle, with a maximum safe melt temperature near 270 °C. Residence time above 5 min at temperatures beyond 270 °C accelerates thermal degradation, shifting the melt viscosity downward and reducing tensile elongation. When hot-runner systems are used, the manifold and drop temperatures should be profiled to avoid local overheating. Screw rotation should be selected to avoid excessive shear; a general-purpose screw with an L/D of 20:1 to 24:1 and a compression ratio of 2.3:1 to 2.8:1 is acceptable for initial trials. Back pressure between 0.3 MPa and 0.6 MPa assists homogeneous melt formation without introducing excessive frictional heat.
Mould temperature influences final crystallinity and shrinkage. A mould temperature between 60 °C and 90 °C is normally specified for dimensionally stable PBT mouldings. Lower mould temperatures reduce cycle time but freeze the surface prematurely, increasing the risk of sink marks opposite thick sections and producing lower crystallinity that may drift on later annealing. Higher mould temperatures above 90 °C improve crystallinity and long-term dimensional stability but extend cooling time. For glass-bead-filled PBT, excessive injection speed can generate jetting, in which the melt front enters the cavity as a narrow stream and cools before filling is complete. Bead-filled melts are less prone to fibre agglomeration than glass-fibre PBT but still require gate placement that avoids unrestricted filling paths from small sprue diameters.
On a corotating twin-screw compounding line with L/D of 40:1 or higher, spherical glass beads are typically side-fed downstream of the polymer melting zone to minimise bead fracture and limit barrel abrasion in the main feed section. The same abrasion concern applies downstream at the injection machine, though at lower severity than short-glass fibre. Nitrided barrels, bimetallic cylinders, and hardened screw flights are advisable for sustained high-volume production. Clamp force requirements are broadly comparable to unfilled PBT because cavity pressure is not dominated by the filler-bed stiffness of fibre-reinforced grades; however, the higher filled-melt viscosity may raise injection pressure by 10% to 20% relative to unfilled PBT in thin-wall tools.
Comparative property envelopes for unfilled PBT, glass-bead-filled PBT class, and short-glass-fibre-filled PBT class are summarised below using ISO test methods. The table is not a certificate of analysis for KEPEX 3330GB; it is a design-orientation matrix compiled from public class data, and final design values must be taken from the lot-specific technical data sheet issued by Korea Engineering Plastics.
| Property and test method | Unfilled PBT | PBT + 30% glass bead | PBT + 30% short glass fibre |
|---|---|---|---|
| Density, ISO 1183-1:2019 | 1.30–1.31 g/cm³ | 1.52–1.56 g/cm³ | 1.53–1.58 g/cm³ |
| Tensile strength, ISO 527-1/-2 | 50–60 MPa | 55–65 MPa | 110–130 MPa |
| Tensile modulus, ISO 527-1/-2 | 2.5–2.8 GPa | 4.5–5.5 GPa | 9.0–10.0 GPa |
| Flexural modulus, ISO 178 | 2.2–2.5 GPa | 4.0–5.0 GPa | 8.0–10.0 GPa |
| Notched Charpy impact, ISO 179-1/1eA | 3–5 kJ/m² | 3–5 kJ/m² | 8–10 kJ/m² |
| Mould shrinkage, ISO 294-4 | 1.5–2.0% isotropic | 0.8–1.2% isotropic | 0.2–0.5% flow / 0.8–1.2% transverse |
The tabulated comparison identifies the core trade-off. The KEPEX 3330GB grade, when it follows the general PBT+GB30 class, sacrifices at least 40% of the tensile modulus available from a short-glass-fibre alternative while recovering nearly isotropic shrinkage and lower warpage. Therefore, design groups that replace a GF30 PBT with a GB30 PBT solely on equal filler mass without adjusting section thickness will encounter either higher deformation under load or lower safety margins in snap-fit maximum strain. Conversely, replacing unfilled PBT with the same glass bead grade reduces shrinkage and improves stiffness without imposing the pronounced flow-to-transverse shrinkage differential that glass fibre introduces. The difference is therefore not one of simple property enhancement but of selecting the reinforcement shape most compatible with the geometry, gate map, and load environment.
Regulatory status is formulation-specific, not generic. The supplier declaration for Korea Engineering Plastics KEPEX PBT+GB30% 3330GB should be obtained for EU RoHS Directive 2011/65/EU, REACH Regulation (EC) No 1907/2006 SVHC content, and any customer-specific packaging or automotive substance restrictions. Flammability classification must be verified against the UL Yellow Card; unfilled and glass-filled PBT compounds without flame-retardant additives commonly fall into UL 94 HB at 1.5 mm, but no V-0 claim should be inferred for a non-flame-retardant grade unless certified. Electrical insulation requirements such as comparative tracking index under IEC 60112 or dielectric strength under IEC 60243-1 should be tested on moulded plaques from the specific lot, not transferred from general PBT literature.
Batch-to-batch variance in glass-bead-filled compounds is frequently smaller than that of fibre-reinforced compounds because the spherical filler creates less anisotropic orientation; nevertheless, incoming inspection should monitor filler content by ISO 3451-1:2019, melt flow rate by ISO 1133-1:2022, and density by ISO 1183-1:2019. A shift in melt flow rate above the datasheet band can indicate either hydrolytic damage during drying or a change in the base PBT resin’s intrinsic viscosity. If the compound is stored in unsealed bags at relative humidity above 60%, drying before moulding is mandatory, and vacuum or desiccant drying should be preferred over hot-air drying because hot-air systems may not reach the 0.02% moisture target under high-humidity plant conditions.
The abrasiveness of glass beads is lower than that of short glass fibres but higher than unfilled PBT. Screw and barrel wear should be monitored when the material is run in high-volume production. Use of separate material-handling lines for glass-filled and unfilled PBT prevents cross-contamination that would otherwise shift the glass content and alter cavity fill behaviour. Reground glass-bead-filled PBT can often be incorporated at low percentages in non-appearance parts, but only after drying and only within limits established by the manufacturer for the specific lot.
On existing multi-cavity tools originally sampled with unfilled PBT, the switch to KEPEX PBT+GB30% 3330GB usually requires rebalancing of the runner system because the filled melt has a steeper viscosity response and reduced thermal shrinkage. On tools originally sampled with PBT GF30, the 3330GB grade may improve post-mould flatness but may also require a thicker wall section in structural features to compensate for the lower tensile modulus. Part validation for dimensional precision parts should include a capability study using mould shrinkage measured to ISO 294-4 and, where the part functions as an electrical housing, tracking resistance or dielectric strength data generated from moulded plaques rather than from pellet samples alone.