Korea Engineering Plastics Kepex Pbt Asa Gf30 3930gfu

Korea Engineering Plastics KEPEX® PBT+ASA+GF30% 3930GFU

    • Product Name: Korea Engineering Plastics KEPEX® PBT+ASA+GF30% 3930GFU
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 359184
    Grade KEPEX® PBT+ASA+GF30% 3930GFU
    Polymer Type PBT/ASA blend
    Reinforcement 30% glass fiber
    Density 1.42 g/cm³
    Tensile Strength 110 MPa
    Flexural Modulus 7500 MPa
    Elongation At Break 2.5%
    Notched Izod Impact Strength 8 kJ/m²
    Heat Deflection Temperature 1 82 Mpa 195 °C
    Vicat Softening Temperature 210 °C
    Molding Shrinkage 0.2–0.5%
    Water Absorption 0.1%
    Flammability HB
    Processing Method Injection molding

    As an accredited Korea Engineering Plastics KEPEX® PBT+ASA+GF30% 3930GFU factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg moisture-proof bags, palletized and labeled for safe storage and transport of KEPEX® PBT+ASA+GF30% 3930GFU.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized bags of KEPEX® PBT+ASA+GF30% 3930GFU engineering plastic compound, securely stowed for transport.
    Shipping Product is a glass-fiber reinforced PBT/ASA engineering plastic compound supplied as solid pellets. Ship in sealed moisture-barrier bags or octabins under standard dry conditions; classify as non-hazardous, non-DG cargo. Keep packaging intact, avoid heat, sunlight, and moisture; use covered trucks/containers for normal industrial transport.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and open flames. Keep original sealed bags closed to prevent moisture absorption, dust, and contamination. Avoid contact with incompatible chemicals. Maintain good housekeeping and follow local safety regulations and the manufacturer’s safety data sheet.
    Shelf Life Shelf life is typically 12 months in original sealed packaging, stored dry and cool, protected from moisture and direct sunlight.
    Free Quote

    Competitive Korea Engineering Plastics KEPEX® PBT+ASA+GF30% 3930GFU prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Korea Engineering Plastics KEPEX® PBT+ASA+GF30% 3930GFU is a 30% by mass short-glass-fiber-reinforced blend of polybutylene terephthalate and acrylonitrile-styrene-acrylate copolymer. The grade is designated by ISO 1043-1 as PBT+ASA-GF30 and is supplied as cylindrical pellets for injection molding. The ASA phase contributes surface retention under ultraviolet exposure, while the PBT ester backbone provides rapid crystallization, resistance to automotive fuels and oils, and strong bonding to silane-sized glass fiber. The glass-fiber phase imparts stiffness, dimensional constraint, and reduced creep compared with unfilled PBT/ASA.

    The representative property envelope for 3930GFU is assessed by a multi-standard protocol. Values below are typical lot-average figures and should be verified against the manufacturer’s release certificate for each production batch.

    PropertyTest methodRepresentative value
    DensityISO 1183-11.45 g/cm³
    Tensile modulusISO 527-1/-29,200 MPa
    Tensile stress at breakISO 527-1/-2110 MPa
    Tensile elongation at breakISO 527-1/-22.3%
    Flexural modulusISO 1788,700 MPa
    Flexural strengthISO 178170 MPa
    Charpy notched impact strength, 23°CISO 179-1/1eA8.5 kJ/m²
    Charpy notched impact strength, −30°CISO 179-1/1eA7.0 kJ/m²
    Heat deflection temperature, 1.8 MPaISO 75-1/-2195°C
    Melt volume-flow rate, 250°C/2.16 kgISO 1133-112 cm³/10 min
    Mold shrinkage, parallelISO 294-40.25%
    Mold shrinkage, normalISO 294-40.50%
    Water absorption, 24 h, 23°CISO 620.30%
    Coefficient of linear thermal expansion, parallel, 23°C to 55°CISO 11359-235 ×10−6/K

    The 9,200 MPa tensile modulus measured by ISO 527-1/-2 is direction-dependent in plaques molded to ISO 294-1; flow-direction values are commonly 10% to 20% higher than transverse values because of fiber orientation. The 2.3% tensile elongation at break places the material in the stiff, notch-sensitive short-glass compound class. At −30°C, notched Charpy impact remains near 7.0 kJ/m², but weld lines, sharp corners, gate vestiges, and high regrind fractions can reduce that value by 40% to 50%. The melt volume-flow rate of 12 cm³/10 min at 250°C under 2.16 kg load supports thin-wall filling down to approximately 1.5 mm nominal wall thickness; below that, pressure-limited filling must be evaluated by mold-filling simulation rather than by MVR alone.

    What Limits the Outdoor Service Envelope of PBT+ASA-GF30?

    Long-term exterior exposure is the principal condition under which 3930GFU is specified over unmodified PBT-GF30. PBT-GF30 can develop surface chalking and measurable tensile-strength loss under ultraviolet radiation and moisture cycling; the ASA component in 3930GFU retards that surface degradation. Accelerated weathering evaluations follow ISO 4892-2 method A, using xenon-arc irradiance of 0.51 W/(m²·nm) at 340 nm, black-standard temperature 65°C, and a 102 min dry / 18 min water-spray cycle. Under that protocol, ASA-modified PBT grades have retained more than 70% of unweathered tensile strength after 1,500 h, while unmodified PBT-GF30 can decline below 50% depending on pigmentation and stabilization. Published data for this specific product configuration is limited, so final validation should use actual lot plaques and the exact SAE J2527 or ISO 4892-2 cycle specified on the part drawing.

    The chemical boundary of 3930GFU is governed by the PBT ester linkage. Resistance to unleaded gasoline, diesel fuel, engine oil, and windshield washer fluid is typically assessed by ISO 1817 immersion at 23°C and 50°C. Prolonged contact with aqueous solutions above 85°C, strong alkaline cleaners, or superheated steam should be excluded unless part-specific validation demonstrates acceptable strength retention. The grade is not intended for continuous-use under-hood environments where ethylene glycol/water coolant is pressurized and above 120°C, because hydrolysis of ester groups accelerates and reduces molecular weight.

    Injection Molding Parameter Boundaries, Screw Wear Data, and Hot-Runner Safeguards

    On reciprocating-screw injection molding machines with 18:1 to 22:1 L/D and a compression ratio of 2.0:1 to 2.5:1, the material is processed using a reverse-taper nozzle or a spring shut-off nozzle to prevent drool. Barrel zones from hopper to nozzle are typically set at 240°C, 250°C, 255°C, and 255°C, with melt temperature measured by an insertion pyrometer at 250°C to 265°C. Mold surface temperature is controlled at 60°C to 80°C using water thermolators; test plaques should be molded per ISO 294-1 for mechanical property verification. The processing window is constrained by two competing risks. Insufficient melt temperature increases glass-fiber surface separation and delamination, while melt temperature above 270°C produces volatile degradation products and surface splay. Residence time at melt should not exceed 8 min, and stagnant melt zones in the barrel or hot runner should be purged before shutdown.

    Processing parameterSetpoint or limitEquipment or reference standard
    Drying temperature and time120°C, 4 hDesiccant hopper dryer, dew point ≤ −40°C
    Residual moisture≤ 0.02% by massISO 15512
    Barrel zone profile240°C / 250°C / 255°C / 255°CReciprocating screw, 18:1–22:1 L/D
    Melt temperature250°C–265°CInsertion pyrometer at nozzle
    Mold surface temperature60°C–80°CISO 294-1, water thermolator
    Plasticating back pressure0.3 MPa–0.7 MPaInjection machine screw
    Screw surface speed0.15 m/s–0.25 m/sInjection machine screw
    Cavity pressure at gate45 MPa–65 MPaCavity pressure transducer
    Cushion2 mm–5 mmScrew position control
    Regrind addition≤ 25% by massWeigh-scale, ISO 527-2 validation
    Melt residence time≤ 8 minTimer from screw stop

    Residual moisture above 0.02% measured by ISO 15512 is a common cause of unexplained impact loss because hydrolysis cleaves ester groups before the polymer enters the mold cavity. Fiber fracture is a parallel issue. Screw surface speeds above 0.25 m/s reduce number-average fiber length below 250 µm, lowering tensile strength by 5% to 10%. Weld-line tensile strength in molded brackets is typically 50% to 60% of the unwelded value when measured by ISO 527-2; gate relocation or overflow wells are required when weld lines occur in load-bearing sections. Regrind addition above 25% by mass is not recommended because cumulative fiber attrition and ASA rubber degradation can reduce notched Charpy impact below 6.0 kJ/m².

    On production runs exceeding 20,000 kg of total throughput, glass-fiber reinforced PBT/ASA compounds produce measurable barrel and screw wear. Bimetallic barrels and screw flights with surface hardness of at least 55 HRC are specified for sustained series production. Non-return valve clearance should be inspected at intervals of 5,000 kg to 10,000 kg; worn check rings increase shear heating and reduce melt homogeneity. Hot-runner systems should use internally heated manifolds with no dead spots and should be held at 250°C to 260°C. Valve-gated tools require gate seal verification; excessive valve-pin packing can degrade the melt at the gate and produce surface defects.

    If the Application Requires Dimensional Stability After Humidity Cycling

    Compared with PA66-GF30, the PBT/ASA-GF30 grade absorbs less water. A 24 h immersion at 23°C yields approximately 0.30% water uptake by ISO 62, whereas PA66-GF30 typically absorbs 0.80% to 1.00%. This lower moisture uptake reduces post-mold growth and warpage in humid service. The coefficient of linear thermal expansion measured parallel to flow between 23°C and 55°C by ISO 11359-2 is approximately 35 ×10−6/K; transverse-direction values are higher because of fiber orientation. Tooling should therefore be compensated with anisotropic shrinkage values, not a single isotropic mold-shrinkage factor. Mold shrinkage values measured by ISO 294-4 are approximately 0.25% parallel and 0.50% perpendicular. For exterior trim with visible surfaces, the ASA phase reduces non-uniform gloss change after thermal cycling and weathering; gloss retention is evaluated by ISO 2813 at 60° geometry before and after the specified exposure interval.

    Conditioning from dry-as-molded to equilibrium at 23°C and 50% RH per ISO 291 typically produces less than 0.1% dimensional change in width for this class, while PA66-GF30 can exhibit 0.4% to 0.6% change over the same moisture conditioning range. This distinction is relevant in mating interior and exterior trims where gap and flushness after rain exposure or high-humidity storage are controlled by the material’s low moisture uptake and anisotropic CLTE.

    Comparative Positioning Against PBT-GF30, PA66-GF30, and ASA/PC-GF20

    Relative to PBT-GF30, 3930GFU provides improved ultraviolet-surface retention and lower chalking tendency, but the ASA modification lowers heat resistance and tensile modulus. The ISO 75-1/-2 heat deflection temperature at 1.8 MPa is approximately 195°C, while a standard PBT-GF30 often lies between 200°C and 210°C. Relative to PA66-GF30, 3930GFU has lower water absorption and better resistance to acidic automotive fluids, but lower tensile strength and lower heat deflection temperature; PA66-GF30 typically exceeds 240°C HDT/A and 140 MPa tensile stress at break because of polyamide interchain hydrogen bonding. Relative to ASA/PC-GF20, 3930GFU provides better resistance to glycols and fuel-induced stress cracking because the PBT phase is less prone to solvent attack than polycarbonate; however, ASA/PC-GF20 may offer higher multiaxial impact in low-temperature impact events. Instrumented falling-dart testing to ISO 6603-2 often shows more brittle puncture behavior for 30% glass-filled PBT/ASA than for ASA/PC-GF20 at −30°C. The selection is therefore controlled by whether outdoor surface retention, moisture stability, heat resistance, or low-temperature multiaxial impact dominates the failure mode.

    Applications that use 3930GFU as a replacement for metal in exterior structural brackets require additional validation on molded plaques and welded or mechanically joined subassemblies. Thermal cycling from −40°C to 80°C per OEM specifications should be performed with actual part geometry, because differential CLTE between the compound and inserted metal fasteners can produce overstress at boss features. Vibration testing of assembled components is also necessary when glass-fiber reinforced PBT/ASA is used in a load-bearing snap-fit, since the material’s elongation at break is below 3% and snap-fit strain must remain below the tensile yield strain. Production-intent validation should be conducted with the same hot-runner configuration, regrind fraction, dew-point controlled drying, and screw-speed settings intended for series injection molding.