| HS Code | 582118 |
| Product Designation | Kingfa PBT+GF30% PBT-G30 |
| Material Type | Polybutylene terephthalate with 30% glass fiber reinforcement |
| Filler Content | 30% glass fiber |
| Density | 1.53 g/cm³ |
| Melt Flow Rate | 10 g/10 min at 250°C/2.16 kg |
| Tensile Strength | 135 MPa |
| Elongation At Break | 3% |
| Flexural Modulus | 9000 MPa |
| Flexural Strength | 200 MPa |
| Notched Izod Impact Strength | 8 kJ/m² |
| Heat Deflection Temperature | 205°C at 1.82 MPa |
| Melting Point | 225°C |
| Flammability | HB |
| Water Absorption | 0.03% |
| Molding Shrinkage | 0.2–0.5% |
| Volume Resistivity | 1×10^15 Ω·cm |
As an accredited Kingfa PBT+GF30% PBT-G30 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PBT+GF30% PBT-G30 is packaged in 25 kg moisture-proof bags, palletized and shrink-wrapped for safe transport. |
| Container Loading (20′ FCL) | 20′ FCL loading of Kingfa PBT+GF30% PBT-G30, packed in bags on pallets, securely stowed and labeled for export shipment. |
| Shipping | Kingfa PBT+GF30% PBT-G30 is shipped as non-hazardous thermoplastic pellets in moisture-barrier bags or boxes and is not regulated for transport. Store and ship dry, away from direct sunlight, heat, and moisture; keep containers closed and follow the SDS and supplier handling recommendations. |
| Storage | Store Kingfa PBT+GF30% PBT-G30 pellets in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and incompatible substances such as strong oxidizers, acids, and bases. Keep containers tightly closed to prevent contamination and moisture absorption. Avoid dust generation and static buildup; use grounded handling equipment. Follow local regulations and the safety data sheet. |
| Shelf Life | Shelf life: typically 24 months when stored in original sealed packaging under dry, cool conditions, protected from moisture, sunlight, and contamination. |
Competitive Kingfa PBT+GF30% PBT-G30 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PBT+GF30% PBT-G30 is a 30% glass-fibre-reinforced polybutylene terephthalate injection-moulding grade. The base polymer is semicrystalline PBT; the glass content is introduced as 30% by weight chopped strand, yielding a density typically reported between 1.52 g/cm³ and 1.56 g/cm³ when measured according to ISO 1183-1:2019. The melt volume-flow rate is batch-dependent and is commonly evaluated at 250°C under 2.16 kg using ISO 1133-1:2022; commercial 30% glass-filled PBT grades in this class often fall within 12 cm³/10 min to 20 cm³/10 min, but the value on the certificate of analysis governs. Pre-drying in a desiccant dryer at 120°C for 4 h to 6 h with a dew point not higher than -30°C is required before melt processing. Residual moisture above 0.02% by Karl Fischer titration or ISO 15512:2019 leads to hydrolytic molecular-weight loss, surface splay, and reduced weld-line strength. Processing is carried out on a three-zone screw with a length/diameter ratio of 20:1 to 22:1 and a compression ratio of 2.5:1 to 3.0:1; melt temperature is normally controlled between 250°C and 270°C, and mould temperature between 60°C and 100°C. The grade is not intended for processes requiring high extensional melt strength, such as thick-sheet extrusion.
The following ranges are representative of commercial polybutylene terephthalate compounds processed under supplier-recommended conditions; exact Kingfa certificate values should not be inferred from this table. The comparison shows the directional effect of glass loading, not a substitute for grade-specific datasheets.
| Property | Test standard | PBT-G0 (unfilled) | PBT-G15 | PBT-G30 | PBT-G45 |
|---|---|---|---|---|---|
| Tensile stress at break, MPa | ISO 527-2:2012 | 55–60 | 90–110 | 120–140 | 150–170 |
| Tensile modulus, MPa | ISO 527-2:2012 | 2500–2700 | 4500–5500 | 8000–9500 | 10500–12500 |
| Flexural modulus, MPa | ISO 178:2019 | 2300–2500 | 4200–5200 | 7500–9000 | 10000–12000 |
| Notched Charpy impact, kJ/m² | ISO 179-1/1eA:2023 | 4–6 | 5–7 | 6–8 | 7–9 |
| Heat deflection temperature, °C | ISO 75-2/Af:2013 | 55–65 | 185–195 | 205–215 | 210–220 |
| Mould shrinkage parallel, % | ISO 294-4:2018 | 1.6–2.0 | 0.4–0.7 | 0.3–0.5 | 0.2–0.4 |
The tensile stress at break of PBT-G30 is approximately twice that of unfilled PBT-G0 because glass fibre transfers load from the matrix to the fibre under tensile testing at 23°C and 50% relative humidity. Elongation at break, however, drops from unfilled PBT values commonly above 50% to 2.0%–3.5% for the 30% glass-filled grade. This reduction in ductility is measurable in tensile bars but is not necessarily predictive of impact behaviour in complex snap-fit geometries. Compared with PBT-G45, PBT-G30 provides lower stiffness but better flow, lower tool abrasion, and more uniform colour dispersion because the fibre loading places less shear demand on colour masterbatch distribution. Compared with PBT-G15, PBT-G30 raises heat deflection temperature and flexural modulus while reducing parallel mould shrinkage, but it also shortens the available flow length for thin-wall filling.
When a multi-cavity connector tool originally qualified for PBT-G15 is converted to PBT-G30, the reduction in mould shrinkage and the increase in melt viscosity change both part dimensions and cavity-filling behaviour. Parallel mould shrinkage measured by ISO 294-4:2018 typically decreases from 0.4%–0.7% for PBT-G15 to 0.3%–0.5% for PBT-G30; perpendicular shrinkage can remain at 0.8%–1.2% because of flow-induced fibre orientation. Packing pressure may need to be increased by 10%–20% to compensate for reduced melt compressibility and faster gate freeze-off. In a 48-cavity hot-runner arrangement, the higher glass loading increases shear heating; melt temperature across drops should be held within 5°C of the set point, and hot-runner balance should be verified with in-mould pressure sensors rather than short-shot weight alone. Gate diameter for a 0.8 mm wall should not be reduced below 0.6 mm; smaller gates promote fibre breakage and early freeze-off. Injection speed is typically set in the range 60 mm/s to 120 mm/s for medium to large parts, while screw speed is held at 60 rpm to 120 rpm with back pressure from 0.3 MPa to 0.7 MPa. A shut-off nozzle or spring needle nozzle is preferred to prevent drool.
Fibre-rich weld lines are a documented failure mode in PBT-G30 mouldings. At knit lines, glass fibre alignment is disrupted; tensile strength at a weld line may be only 40%–60% of the bulk value depending on melt temperature and fibre length, as evaluated by ISO 527-2:2012 after direct-gated comparison moulding. Increasing melt temperature to 270°C improves weld-line strength by promoting polymer diffusion, but excessive residence time above 270°C causes matrix decomposition and surface yellowing. Vacuum venting and adequate cold slug wells are required because volatile degradation products from hydrolysis can produce silver streaks at the gate. Production-scale failure modes also include hopper bridging caused by glass fibre compaction; insulated hoppers with fast refill cycles reduce this risk. Screw and barrel wear from 30% glass requires a bimetallic barrel and hard-coated screw; nitrided steel alone is insufficient for sustained runs above 500,000 cycles. Shot-to-shot variance in melt cushion should be less than 0.5 mm to maintain dimensional repeatability of critical connector pitch features.
Below 0.02% residual moisture, PBT-G30 pellet feed remains chemically stable; above this threshold, melt hydrolysis accelerates with temperature and residence time. In production lines with relative humidity above 60%, open air exposure of dried pellets should not exceed 30 min; otherwise drying must be repeated. Molten material held above 270°C for more than 10 min shows a measurable reduction in melt viscosity, resulting in short-shot instability and reduced Charpy impact values. These operational boundaries are critical because glass fibre increases shear heating but does not raise the polymer decomposition temperature.
Electrical connector applications require comparative tracking index proof through IEC 60112:2020. For 30% glass-filled PBT without flame retardant, CTI values are often reported between 250 V and 400 V; the actual value is influenced by mould-release residues, pigment package, and moisture condition. Conditioning at 23°C and 50% relative humidity before electrical testing is standard. The base PBT-G30 datasheet does not list an inherently UL 94 V-0 classification; parts requiring flame retardance at 0.8 mm or 1.6 mm must be reviewed against Kingfa’s FR PBT portfolio or tested under the exact final colour. High-voltage connectors should be evaluated for dry arc resistance and tracking; published data for this specific configuration is limited, so end-use testing is required. The grade is suitable for coil formers, relay bobbins, sensor housings, and EV charging connector structural components only when the final part passes the relevant insulation coordination standard such as IEC 60664-1.
| Requirement | Test or reference | Typical status for PBT-G30 |
|---|---|---|
| RoHS restrictions | RoHS 2011/65/EU + (EU) 2015/863, screened by IEC 62321 | Pass for natural and black base grade; coloured variants require re-confirmation |
| REACH SVHC | Regulation (EC) No 1907/2006 | Declaration required per article as supplied |
| Flammability | UL 94:2023 | Base grade often HB at 1.6 mm; final colour and thickness control yellow card |
| Tracking resistance | IEC 60112:2020 | Typically 250–400 V; product-specific |
| Melt mass-flow rate | ISO 1133-1:2022 | Indicative 12–20 cm³/10 min at 250°C/2.16 kg |
Hot-runner balance in multi-cavity PBT-G30 moulds is limited by shear-induced fibre migration, not by simple polymer flow length. Capillary rheometry at 260°C and 1000 s⁻¹ for 30% glass-filled PBT often shows viscosity between 40 Pa·s and 80 Pa·s; direct measurement according to ISO 11443:2021 is recommended for each lot. Pressure drop per gate varies with glass orientation in the runner; therefore, artificial balancing with equal runner lengths is insufficient. Melt rotation devices or valve gates with independent temperature control improve cavity-to-cavity consistency. For a 0.8 mm to 1.0 mm wall, gate freeze time is commonly 1.0 s to 1.5 s, after which packing compensation ceases. This makes in-mould shrinkage prediction software calibrated with fibre-orientation tensors preferable to isotropic shrinkage equations. When short-shots are observed in the last cavities, increasing barrel temperature should be limited to 5°C increments because fibre-matrix separation worsens above 270°C.
Compared with PA66-GF30, PBT-G30 absorbs less water and therefore retains electrical and mechanical properties more consistently in humid environments. Water absorption after 24 h at 23°C according to ISO 62:2008 is typically below 0.2% for PBT-G30; saturation values remain below about 0.5%, whereas PA66-GF30 can absorb several percent by equilibrium. This difference matters in sealed connectors exposed to condensation or underhood environments. Compared with PBT/ASA blends, PBT-G30 has higher stiffness but lower low-temperature impact; when snap-fit arms or retaining clips experience repeated deflection, a notched impact test alone may not capture performance. The glass-fibre reinforcement lowers melt flow length; therefore, PBT-G30 is not a direct substitute for high-flow unfilled PBT in very thin-wall fuse housings or micro-connectors with wall stock below 0.4 mm. For parts requiring chemical resistance to hot oil, PBT-G30 is preferred over polycarbonate/ABS, but fuel immersion may cause stress cracking; compatibility should be confirmed under the actual service fluid.