Kanghui Pbt Gf Khbt2130 Bk921

Kanghui PBT+GF KHBT2130 BK921

    • Product Name: Kanghui PBT+GF KHBT2130 BK921
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 792302
    Product Name Kanghui PBT+GF KHBT2130 BK921
    Polymer Base Polybutylene terephthalate (PBT)
    Reinforcement Glass fiber
    Glass Fiber Content 30%
    Color Black (BK921)
    Density 1.53 g/cm³
    Tensile Strength 120 MPa
    Elongation At Break 2.5%
    Flexural Modulus 8500 MPa
    Notched Izod Impact Strength 8 kJ/m²
    Heat Deflection Temperature At 1 82 Mpa 205 °C
    Melting Point 225 °C
    Molding Shrinkage 0.2-0.5%
    Water Absorption At 24 H 0.1%
    Flammability Rating UL94 HB
    Processing Method Injection molding

    As an accredited Kanghui PBT+GF KHBT2130 BK921 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kanghui PBT+GF KHBT2130 BK921 packaging: 25 kg moisture-proof bags on pallets, suitable for bulk industrial handling and storage.
    Container Loading (20′ FCL) Container loading: Kanghui PBT+GF KHBT2130 BK921 black glass-filled PBT resin, palletized and secured in a 20′ FCL for export.
    Shipping Shipping description: Kanghui PBT+GF KHBT2130 BK921 is a black, glass-fiber-reinforced polybutylene terephthalate compound supplied as pellets. Pack in sealed moisture-barrier bags or boxes. Keep dry, cool, ventilated, and protected from sunlight. Store away from contaminants and ignition sources. Typically not classified as dangerous goods for transport.
    Storage Store in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, moisture, and incompatible chemicals. Keep in original tightly closed packaging, palletized off the floor, and protect from dust, contamination, and physical damage. Avoid prolonged high humidity; rotate stock FIFO, follow the supplier’s SDS, and do not store near food, drink, or feed.
    Shelf Life Shelf life: 12 months from production date when stored dry, sealed in original packaging, away from sunlight, below 30°C.
    Free Quote

    Competitive Kanghui PBT+GF KHBT2130 BK921 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kanghui PBT+GF KHBT2130 BK921 is a black, glass-fibre reinforced polybutylene terephthalate injection moulding compound. The model designation KHBT2130 identifies the resin series and the nominal glass-fibre mass fraction as stated on the lot-specific certificate of analysis; BK921 is the manufacturer’s colour code for black. Published product-specific data for this grade are limited; therefore, numerical values in the following sections refer to class-typical data for PBT+GF compounds with comparable glass-fibre loading, conditioned and tested under the cited ISO and ASTM methods. The content is intended for tooling engineers and injection moulding process planners, not for direct substitution without certificate verification.

    Which Processing Boundaries Govern KHBT2130 BK921?

    Residual moisture is the first boundary. PBT is subject to hydrolytic degradation when melt temperature exceeds 250 °C and moisture is above 0.02 wt%. The compound is dried in a desiccant dryer with a dew point of −30 °C or lower. Drying at 120 °C for 4 h typically achieves the threshold; when plant relative humidity is above 60 %, the residence time is extended to 6 h. Moisture content is verified by ISO 15512:2019. Melt temperature is controlled between 245 °C and 265 °C; excursions above 270 °C for more than 5 min produce surface carbon-black migration and yellowing. Mould temperature is set in the range 70 °C–100 °C. Back pressure between 0.1 MPa and 0.3 MPa maintains glass-fibre length; higher back pressure accelerates fibre breakage and lowers tensile modulus.

    Moisture gradients in granulate are not corrected by rising barrel temperature alone. A hopper dryer that maintains inlet air dew point below −30 °C removes surface water quickly, but diffusion of moisture from the centre of a 4 mm granule requires the full 4 h residence period. Dry-air units with desiccant beds that are not regenerated within 8 h produce load-to-load moisture variation above 0.03 wt%, measured by ISO 15512:2019. This variation manifests as splay and reduced weld-line strength in multi-cavity connector housings.

    Production-scale operation of three-zone single-screw injection units with L/D ratios of 20:1 and clamp force between 1,500 kN and 3,500 kN shows that shot-to-shot mass variation increases when barrel zone temperatures differ by more than 8 °C. Fibre-length degradation is observed when screw surface speed exceeds 75 m/min or when check-ring clearance exceeds 0.2 mm. Melt residence time at 260 °C should not exceed 10 min. Hot-runner systems with externally heated manifolds are preferred over internally heated systems because glass fibre can accumulate at dead spots. If a hot runner is used, manifold and nozzle temperatures are maintained within 5 °C of the barrel front zone to prevent fibre-matrix separation. Valve-gate sequencing should be adjusted to avoid filling two flow fronts of dissimilar glass orientation, which lowers weld-line tensile strength by 25 %–40 % compared with the base material.

    Glass-Fibre Retention, Melt Viscosity, and Dimensional Stability

    Glass-fibre retention separates KHBT2130 BK921 from unfilled PBT and from competing high-glass PBT grades. In a 30 wt% glass-fibre PBT compound, fibre length after plastication typically averages 0.25 mm–0.45 mm when a general-purpose screw is used; a low-compression screw with a longer feed zone retains fibres closer to 0.5 mm. Melt viscosity at shear rates of 1000 s⁻¹ and 260 °C is higher than unfilled PBT by a factor of 2–3; this raises injection pressure demand in thin-wall sections. Dimensional stability improves because glass fibre lowers isotropic mould shrinkage from 1.5 %–2.0 % for unfilled PBT to 0.2 %–0.6 % in the flow direction, while transverse shrinkage may remain 0.7 %–1.0 %. The resulting anisotropy must be addressed through gate placement.

    Table 1. Class-typical property ranges for a 30 wt% glass-fibre reinforced PBT compound after ISO 291:2008 conditioning.
    PropertyTest methodTypical range
    DensityISO 1183-1:20191.50–1.54 g/cm³
    Tensile stress at breakISO 527-1:2019 / ISO 527-2:2012110–130 MPa
    Tensile modulusISO 527-1:2019 / ISO 527-2:20128000–10000 MPa
    Flexural modulusISO 178:20197500–9500 MPa
    Elongation at breakISO 527-2:20122–4 %
    Notched Izod impact at 23 °CISO 180:20197–11 kJ/m²
    Notched Izod impact at −30 °CISO 180:20195–8 kJ/m²
    Heat deflection temperature at 1.8 MPaISO 75-2:2013200–210 °C
    Melt flow rate at 250 °C/2.16 kgISO 1133-1:202210–25 g/10 min
    Mould shrinkage, flow directionISO 294-4:20180.2–0.6 %
    Moisture at injectionISO 15512:2019≤ 0.02 wt%

    For electrical connector housings that replace metal bracketry, the attraction of KHBT2130 BK921 is not weight reduction alone. Compared with unfilled PBT tested according to ISO 527, the glass-fibre reinforced grade raises tensile stress at break from 50–60 MPa to 110–130 MPa and flexural modulus from approximately 2500 MPa to 7500–9500 MPa. This shifts failure mode away from snap-fit deflection and allows thinner latch arms only when the design is recalculated for reduced elongation at break, which falls from 50–200 % for unfilled PBT to 2–4 % for the glass-filled grade.

    When Black Colourant Loading Changes Tracking Resistance

    When carbon black is added at loadings required for the BK921 black specification, the comparative tracking index can fall relative to natural PBT because conductive carbon black increases surface leakage current. IEC 60112:2020 testing on PBT+GF30 black grades commonly returns CTI values between 250 V and 400 V; grades with additional inert mineral fillers may reach 600 V. Surface resistivity measured under IEC 62631-3-2:2019 is typically between 1012 Ω and 1015 Ω, which is below the antistatic threshold but sufficient for most insulation coordination applications. This is a measurable difference from natural glass-filled PBT and should be checked against the UL Yellow Card for the exact KHBT2130 BK921 listing.

    Designers who require a guaranteed CTI above 600 V under IEC 60112:2020 should not rely on the black colourant package alone; an additive-modified high-CTI grade may be required. Conductive paths in closely spaced terminal cavities have been observed when mould-release agents or external hydrocarbon films reduce surface cleanliness. Tooling trials should avoid excessive mould-release spray and should clean cavities with deionised water rather than silicone-based cleaners.

    Chemical Exposure Limits Are as Critical as Mechanical Load

    PBT and its glass-fibre reinforced variants resist many automotive fluids, but the resistance is not universal. Immersion testing under ISO 175:2010 shows that dilute mineral acids, petrol, diesel, and ethylene glycol at 60 °C produce small mass changes below 0.5 % after 72 h. Strong alkaline solutions, especially at pH above 13, cause surface etching and fibre blooming. Hot aqueous glycol above 85 °C accelerates hydrolysis and should be treated with the same caution as wet moulding. Stress-crack resistance under fixed strain is evaluated by ISO 22088-2:2006; carbon-black-filled PBT can develop microcracks in contact with zinc-chloride road de-icing brine at concentrations above 5 wt%.

    Compared with PBT+GF50 grades, KHBT2130 BK921 at a 30 wt% glass-fibre loading provides lower tensile modulus and lower melt viscosity, which allows filling of flow lengths beyond 150 mm with lower injection pressure. Where a PBT+GF50 grade might require injection pressure above 120 MPa in a 2 mm-thick wall, a 30 wt% glass-fibre class typically fills at 80–100 MPa under the same gate geometry. The penalty is higher mould shrinkage and lower HDT; PBT+GF50 can reach HDT values near 215 °C, while PBT+GF30 remains between 200 °C and 210 °C.

    Table 2. Comparative typical ranges for unfilled PBT, PBT+GF30 class, and PBT+GF50 class.
    PropertyTest methodUnfilled PBTPBT+GF30 classPBT+GF50 class
    DensityISO 1183-1:20191.30–1.32 g/cm³1.50–1.54 g/cm³1.70–1.76 g/cm³
    Tensile stress at breakISO 527-1:2019 / ISO 527-2:201250–60 MPa110–130 MPa160–190 MPa
    Flexural modulusISO 178:20192200–2800 MPa7500–9500 MPa12000–15000 MPa
    Heat deflection temperature at 1.8 MPaISO 75-2:201350–60 °C200–210 °C210–220 °C
    Mould shrinkage, flow directionISO 294-4:20181.5–2.0 %0.2–0.6 %0.1–0.3 %
    Notched Izod impact at 23 °CISO 180:20194–6 kJ/m²7–11 kJ/m²8–13 kJ/m²

    Under-bonnet sensor housings use PBT+GF30 black because heat deflection temperature under load remains above 200 °C and continuous use temperature is typically rated at 140 °C–150 °C for electrically insulating parts under IEC 60216-1:2013 long-term thermal evaluation. The BK921 black colour provides ultraviolet opacity but does not alone guarantee UV stabilisation; outdoor use requires an additional UV package. Warpage after ageing is assessed by dimensional change after thermal cycling from −40 °C to 150 °C, with soak periods of 60 min per chamber, and should remain below 0.3 % in the flow direction for connector bodies.

    RoHS compliance under Directive 2011/65/EU Annex II and REACH Regulation 1907/2006/EC should be confirmed from the supplier’s material declaration for the specific BK921 colour masterbatch. Carbon black and E-glass fibre are not themselves restricted, but antimony oxide synergists sometimes present in flame-retarded PBT grades are not assumed. If a flame-retarded variant is required, testing under UL 94 must be performed on the final part at the end-use wall thickness. Lot-specific documentation remains the controlling reference because colour concentrates, stabiliser packages, and glass sizing can shift the property envelope even within the same grade designation.

    Tooling trials on hydraulic injection machines with clamp force above 2,000 kN for multi-cavity moulds show that the KHBT2130 BK921 flow length depends on gate diameter and wall thickness. With a 2.5 mm-thick housing and a gate diameter of 1.2 mm, flow length-to-wall thickness ratios of 120:1 are achievable before short-shot begins at melt temperature 260 °C and mould temperature 80 °C. Lower mould temperatures reduce achievable flow length and increase skin-core orientation difference. These process windows are not product-specific but are derived from industrial PBT+GF30 black moulding data.

    Top