Kanghui Pbt Gf Kh2083

Kanghui PBT+GF KH2083

    • Product Name: Kanghui PBT+GF KH2083
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 990785
    Filler Content 20% glass fiber
    Density 1.45 g/cm³
    Tensile Strength 100 MPa
    Elongation At Break 3%
    Flexural Modulus 6000 MPa
    Notched Izod Impact Strength 6 kJ/m²
    Heat Deflection Temperature At 1 82 Mpa 200 °C
    Melting Point 225 °C
    Water Absorption 24 H 0.1%
    Molding Shrinkage 0.4–0.8%
    Flammability Rating HB
    Dielectric Strength 20 kV/mm

    As an accredited Kanghui PBT+GF KH2083 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kanghui PBT+GF KH2083 is supplied in 25 kg moisture-proof paper bags, palletized and shrink-wrapped for industrial shipment.
    Container Loading (20′ FCL) Kanghui PBT+GF KH2083 loaded into one 20-foot FCL container, securely packed and palletized for export shipment.
    Shipping Shipping description: Kanghui PBT+GF KH2083, glass-fiber-reinforced polybutylene terephthalate compound, is non-hazardous and not regulated as dangerous goods for transport. Ship in dry, clean, moisture-barrier bags or lined containers; protect from heat, sunlight, and contamination. Keep containers sealed and labeled; store cool and ventilated. Follow SDS and local regulations.
    Storage Store Kanghui PBT+GF KH2083 in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, and ignition. Keep in original sealed packaging on pallets to prevent moisture pickup, contamination, and deformation. Avoid prolonged humid exposure; dry according to supplier recommendations before processing. Follow the material safety data sheet and local regulations.
    Shelf Life Kanghui PBT+GF KH2083 typically has a 12-month shelf life when stored unopened in a cool, dry, well-ventilated area.
    Free Quote

    Competitive Kanghui PBT+GF KH2083 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Where a high-rigidity thermoplastic is required for injection-moulded electrical and automotive components, the Kanghui KH2083 grade is identified as a glass-fibre reinforced polybutylene terephthalate (PBT+GF). The designation belongs to the manufacturer’s PBT range; the exact glass fibre mass fraction is not fixed by the grade identifier alone, and published manufacturer data for this specific configuration is limited. Table 1 presents a representative engineering envelope for PBT+GF compounds of this class, not lot-specific certification data. The compound is processed on conventional reciprocating-screw injection moulding machines and is evaluated by ISO and IEC methods for mechanical, thermal, and electrical response.

    Table 1: Representative property envelope for KH2083-class PBT+GF compounds
    PropertyTest methodRepresentative rangeUnit
    DensityISO 1183-11.45–1.55g/cm³
    Tensile strength at breakISO 527-290–120MPa
    Tensile modulusISO 527-26000–8000MPa
    Flexural strengthISO 178140–180MPa
    Flexural modulusISO 1785500–7500MPa
    Notched Charpy impactISO 179-1/1eA5–8kJ/m²
    HDT at 1.8 MPaISO 75-2195–215°C
    Melt volume-flow rateISO 1133-1:202210–25cm³/10 min
    Mould shrinkage, parallelISO 294-40.2–0.6%
    Mould shrinkage, transverseISO 294-40.6–1.0%
    Volume resistivityIEC 600931E+13–1E+15Ω·m
    Comparative tracking indexIEC 60112250–400V

    These values are not to be assigned to KH2083 without verification; lot-specific certificates and processing data are required for engineering release. The glass fibre content influences flow behaviour, weld-line integrity, and electrical tracking characteristics, so design should proceed from measured production-lot data rather than generic class values.

    Injection Moulding Parameter Boundaries and Screw Recovery Behaviour

    Prior to melt processing, the compound must be dried in a desiccant dryer with a dew point of -40 °C or lower at 120 °C for 4 h, reducing moisture below 0.02% when measured by ISO 15512. At ambient relative humidity above 60% or after storage bags have been open for more than 1 h, drying time is extended to 6 h and the hopper must be purged with dry air. Melt temperature measured at the nozzle is maintained between 250 °C and 270 °C; total residence time is kept below 8 min to limit thermal degradation. Mould temperature is held between 80 °C and 100 °C to obtain sufficient crystallisation and reproducible shrinkage. Injection pressure is normally set from 80 MPa to 140 MPa, with holding pressure between 50% and 80% of the injection peak. Back pressure is controlled from 2 bar to 5 bar and screw speed from 60 rpm to 120 rpm depending on screw diameter. A general-purpose screw with an L/D ratio of 18:1 to 22:1 and a compression ratio of 2.0:1 to 2.5:1 is used. On reciprocating-screw machines with clamp force between 80 t and 150 t, short-shot and nozzle freeze-off are observed when the front-zone temperature falls below 250 °C; gas splay and surface delamination appear when pellet moisture exceeds 0.05%.

    Melt viscosity at 270 °C and 1000 s⁻¹ for this class of PBT+GF is typically in the range 60–120 Pa·s when measured by capillary rheometry according to ISO 11443. Fibre attrition during plasticisation reduces fibre length from an initial 3 mm to a number-average length below 300 µm after standard screw residence; the resulting property retention depends on screw compression ratio and back pressure. Back pressure above 5 bar improves homogenisation but increases fibre damage and lowers notched Charpy impact. With hot-runner systems, internal runner temperatures are kept between 250 °C and 270 °C; overheating above 280 °C produces black specks and hydrolytic degradation. Valve-gated systems reduce gate blush but increase shear heating; melt temperature should be checked at the nozzle by insertion thermocouple. Cold-runner sprues and runners are regrindable at up to 20% by weight, but regrind reduces impact and increases shrinkage variability; higher levels are not recommended for close-tolerance parts.

    Because the glass fibres align during cavity filling, the mechanical response of moulded parts is anisotropic. Tensile modulus measured parallel to flow on double-gated plaques can be 15–30% higher than values measured transverse to flow under ISO 527-2. Weld-line strength in glass-reinforced PBT is reduced by approximately 30–50% relative to non-weld areas because the fibres do not bridge the knit line; this reduction must be assessed on the production tool. Shrinkage anisotropy follows the same orientation effect, with flow-direction shrinkage of 0.2–0.6% and transverse shrinkage of 0.6–1.0% at 2 mm nominal wall thickness. For parts with wall thickness below 1.5 mm, the effective fibre orientation is less defined and published data for this specific configuration is limited.

    What Distinguishes KH2083 from Unfilled PBT, PBT/ASA Blends, and PET-GF Compounds?

    Compared with unfilled PBT, the KH2083-class material raises flexural modulus from approximately 2500 MPa to 5500–7500 MPa (ISO 178) and lowers unfilled mould shrinkage from 1.5–2.0% to 0.2–0.6% in the flow direction (ISO 294-4). The trade-off is a reduction in unnotched impact resistance and an increase in flow-transverse shrinkage difference. Against PBT/ASA blends, the glass-reinforced grade provides a higher heat deflection temperature under 1.8 MPa load but lower surface gloss measured by ISO 2813 and greater risk of floating fibres on textured surfaces. Against PET-GF compounds, PBT+GF crystallises more rapidly and permits lower mould temperatures of 80–100 °C compared with 120–140 °C typical for PET-GF; however, the PBT backbone is more susceptible to hydrolytic chain scission above 0.02% moisture. Against PA66+GF, the KH2083 class absorbs less water and retains mechanical properties better in humid environments, but it has a lower dry-state heat deflection temperature. The KH2083 designation should not be treated as a drop-in substitute for an unfilled PBT, a mineral-filled PBT, or a flame-retarded PBT unless part dimensions, tool cooling, and regulatory requirements are revalidated with production data.

    For electrical enclosure and connector applications, candidate compounds of this class are evaluated for comparative tracking index by IEC 60112, dielectric strength by IEC 60243-1, and surface resistivity by IEC 60093. Glass fibre content can lower the comparative tracking index relative to unfilled PBT, so a lot-specific CTI value is required for creepage-path design. Compliance documentation should reference the RoHS Directive 2011/65/EU as amended by (EU) 2015/863, REACH Annex XVII, and IEC 62321 methods for restricted substances. The producer should be requested to supply a certificate of analysis for each batch, because generic PBT+GF compliance statements do not address pigment, sizing, or recycled-content variability.

    Table 2: Test and compliance matrix for KH2083-class PBT+GF
    RequirementStandardScope
    Tensile propertiesISO 527-2Injection-moulded multipurpose specimens, test speed 5 mm/min
    Flexural propertiesISO 178Three-point bending on rectangular specimens
    Moisture contentISO 15512Karl Fischer method for pellets and regrind
    Melt volume-flow rateISO 1133-1:2022Conditioning at 250 °C with nominal load
    ShrinkageISO 294-4Plaque method at 2 mm thickness
    Comparative tracking indexIEC 60112Solution A, 100–600 V tracking voltage range
    Dielectric strengthIEC 60243-1Short-term oil immersion method
    Restricted substancesIEC 62321RoHS compliance testing for Pb, Cd, Hg, Cr(VI), PBB, PBDE
    FlammabilityUL 94Only if declared by manufacturer; not assumed without certificate

    When Moisture Uptake Exceeds 0.02%: Hydrolysis Control and Drying Before Processing

    Because polybutylene terephthalate degrades by hydrolytic chain scission at melt temperatures, moisture above 0.02% lowers molecular weight and produces a measurable decrease in tensile strength and notched impact. In production environments at 60% relative humidity, pellets placed in an open hopper can exceed 0.05% moisture within 30–60 min; the use of a closed hopper with dry-air purge is therefore required. Drying in a desiccant dryer at 120 °C for 4–6 h remains standard. Moisture verification by ISO 15512 is recommended before start-up and after any line interruption longer than 30 min. Re-drying is limited to two cycles to avoid thermal yellowing and Charpy impact loss. If a lot has been exposed to condensation or stored without moisture barrier packaging, the material is not reclaimed by simple hot-air drying and should be tested for viscosity or melt flow rate per ISO 1133-1:2022 before use.

    Tool design must account for anisotropic shrinkage. A cavity cut for a uniform 0.5% shrink will produce parts that are undersize in the flow direction and oversize transverse if the actual transverse shrinkage is 0.8–1.0%. On injection moulds with multiple gates, the shift in effective flow direction at weld lines creates local shrinkage discontinuities that are not captured by standard plaque data; process validation by moulding trials is required. Unopened bags should be stored below 35 °C and 60% relative humidity; opened bags should be resealed and consumed within 8 h.

    In power-tool housings and relay bobbins, the material is selected for stiffness and heat deflection, but thin-walled sections below 1.5 mm may show lower effective fibre orientation and should not be designed using the flexural modulus from 4 mm specimens. For connectors with pitch below 2.54 mm, warpage and mould shrinkage must be validated on the production tool because published data for this specific configuration is limited. In automotive under-hood sensor housings, continuous use above 120 °C requires oxidative ageing verification; short-term excursions to 180 °C are acceptable only after part-specific testing according to client thermal ageing protocols.

    Top