| HS Code | 685042 |
| Product Name | Jiangsu Hengli PBT+GF15%-FR PBT-2110 |
| Manufacturer | Jiangsu Hengli |
| Grade | PBT-2110 |
| Base Polymer | Polybutylene terephthalate (PBT) |
| Glass Fiber Content | 15% |
| Flame Retardant | Yes |
| Density | 1.45 g/cm³ (typical) |
| Tensile Strength | 80 MPa (typical) |
| Flexural Modulus | 5000 MPa (typical) |
| Notched Izod Impact Strength | 6 kJ/m² (typical) |
| Heat Deflection Temperature | 200 °C (typical) |
| Flammability Rating | UL94 V-0 (typical) |
| Molding Shrinkage | 0.3–0.8% (typical) |
| Dielectric Strength | 20 kV/mm (typical) |
| Volume Resistivity | 1E15 Ω·cm (typical) |
| Water Absorption | 0.05% (typical) |
| Processing Method | Injection molding |
As an accredited Jiangsu Hengli PBT+GF15%-FR PBT-2110 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packed in 25 kg moisture-proof bags, 40 bags per pallet (1,000 kg pallet), for Jiangsu Hengli PBT+GF15%-FR PBT-2110. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Jiangsu Hengli PBT+GF15%-FR PBT-2110 chemical in packaged form, palletized, secured, and stowed for ocean freight. |
| Shipping | Jiangsu Hengli PBT+GF15%-FR PBT-2110 is shipped as flame-retardant, glass-fiber-reinforced PBT resin pellets, usually in moisture-proof 25 kg bags or jumbo bags. It is generally non-hazardous for transport. Keep dry, ventilated, away from heat, sunlight, and contamination; handle with care and avoid bag damage. |
| Storage | Store Jiangsu Hengli PBT+GF15%-FR PBT-2110 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original containers tightly closed and palletized, protecting them from moisture, rain, and physical damage. Avoid strong acids, bases, and oxidizers; follow SDS and local regulations, using first-in, first-out rotation. |
| Shelf Life | Typically 12 months when stored dry, cool, in original unopened packaging, protected from moisture and direct sunlight. |
Competitive Jiangsu Hengli PBT+GF15%-FR PBT-2110 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The injection-moulding compound designated Jiangsu Hengli PBT+GF15%-FR PBT-2110 is a flame-retardant polybutylene terephthalate grade containing a nominal 15% by weight E-glass fibre reinforcement. The supplier code PBT-2110 identifies a specific formulation of base resin, sizing, thermal stabiliser and flame-retardant chemistry, but publicly available grade-specific datasheets for this exact designation are limited. The following technical description therefore uses the established property envelope for the 15 wt% glass-fibre-reinforced flame-retardant PBT class and identifies where supplier verification is mandatory. Representative class data include density 1.55–1.62 g/cm³ under ISO 1183-1, melt volume-flow rate 8–18 cm³/10 min at 250°C and 2.16 kg per ISO 1133-1, and tensile strength 85–110 MPa under ISO 527-2.
A nominal 15 wt% glass loading corresponds to approximately 8.3 vol% fibre when calculated by the rule of mixtures from a PBT matrix density of 1.31 g/cm³ and an E-glass density of 2.54 g/cm³. The glass content is normally verified by calcination under ISO 1172. The fibre–matrix interface is controlled by silane coupling agents applied to the glass surface; the resulting interfacial adhesion raises tensile strength from the 50–60 MPa typical of unfilled flame-retardant PBT to 85–110 MPa in the reinforced grade. Flexural modulus for this class is typically 6,500–8,500 MPa under ISO 178, while notched Charpy impact at 23°C is 5–7 kJ/m² under ISO 179-1/1eA. Heat deflection temperature at 1.8 MPa is 195–205°C under ISO 75-2. The flame-retardant package may be brominated with an antimony trioxide synergist or halogen-free, and the PBT-2110 supplier datasheet must state the chemistry because it controls smoke density, corrosion during processing and comparative tracking index.
| Property | Test method | Class range |
|---|---|---|
| Density | ISO 1183-1 | 1.55–1.62 g/cm³ |
| Melt volume-flow rate | ISO 1133-1, 250°C/2.16 kg | 8–18 cm³/10 min |
| Tensile stress at break | ISO 527-2 | 85–110 MPa |
| Tensile modulus | ISO 527-2 | 5,500–7,500 MPa |
| Flexural strength | ISO 178 | 130–165 MPa |
| Flexural modulus | ISO 178 | 6,500–8,500 MPa |
| Notched Charpy impact, 23°C | ISO 179-1/1eA | 5–7 kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-2 | 195–205°C |
| Mould shrinkage, flow direction | ISO 294-4 | 0.40–0.80% |
| Mould shrinkage, transverse direction | ISO 294-4 | 0.70–1.20% |
| Flammability | IEC 60695-11-10 | V-0 at 1.5 mm or 3.0 mm, package dependent |
| Comparative tracking index | IEC 60112 | 200–400 V, FR-chemistry dependent |
When the compound is plasticated on a conventional injection-moulding machine with a 25:1 L/D screw and compression ratio 2.0:1 to 3.0:1, pre-drying is mandatory. Desiccant drying at 120–130°C for 3–4 h to residual moisture below 0.02% is required because PBT undergoes hydrolytic chain scission at melt temperature if moisture exceeds 0.03%. The resulting splay and reduction in notched impact are common failure modes on production lines using undried regrind. Barrel settings are typically rear 230–240°C, centre 240–250°C, front 250–260°C and nozzle 250–265°C; mould temperature should be held at 80–100°C to develop crystallinity and achieve the class HDT/A range. Back pressure of 0.3–0.7 MPa and screw speed of 80–120 rpm for a 40 mm screw limit fibre attrition, while injection pressure is generally 80–140 MPa. Because glass fibre is abrasive, bimetallic screw and barrel assemblies are standard for continuous glass-filled production.
The upper melt temperature is limited by the flame-retardant package. In brominated systems, thermal decomposition above 270°C may release hydrogen bromide and cause corrosion of mould surfaces and hot-runner components; in halogen-free phosphinate systems, thermal stability can be higher, but melt viscosity may require temperatures near the upper end of the 245–270°C range. Residence time at melt temperature should be kept below 5 min per shot, and cumulative hold-up time in hot runners below 10 min, to prevent discoloration and loss of UL 94 V-0 performance. The lower processing boundary is set by melt and mould temperature: mould temperatures below 70°C produce rapid solidification, poor weld-line integrity and reduced crystallinity, while melt temperatures below 245°C increase screw torque and may cause incomplete fibre dispersion. The addition of 15% glass fibre reduces melt flow relative to unfilled PBT; injection pressure can therefore rise by 20–40% compared with unfilled FR PBT of the same base viscosity.
The main difference between PBT-2110 and an unfilled flame-retardant PBT is the 15 wt% E-glass reinforcement, which raises tensile modulus and HDT but reduces flow length. Compared with a 30% glass-fibre FR PBT, the 15% grade typically operates with a flexural modulus lower by 2,000–3,000 MPa, a density lower by 0.10–0.20 g/cm³, and lower moulded-in anisotropy. That lower anisotropy reduces warpage in flat connector bodies and terminal carriers because fibre orientation produces less differential mould shrinkage between flow and transverse directions. Compared with a non-flame-retardant 15% GF PBT, the FR package commonly reduces tensile strength by 5–10% and may lower comparative tracking index, but raises the compound to UL 94 V-0 at the same wall thickness. These differences are class-level and must be confirmed from the PBT-2110 certificate because flame-retardant chemistry and sizing can shift the balance.
When the compound is used to replace die-cast aluminium in a connector bracket or sensor carrier, the design must account for the difference in elastic modulus: aluminium is approximately 70 GPa, whereas this PBT class exhibits a flexural modulus of 6,500–8,500 MPa under ISO 178. For a metal-to-plastic conversion, ribs and boss reinforcements are required to compensate for the lower modulus, and creep behaviour should be evaluated under ISO 899-2 at the maximum service temperature. Compared with thermoset moulding compounds, PBT-2110 offers faster cycle time because wall sections of 1.5–2.5 mm can solidify in injection cycles under 20 s, but the polymer is thermoplastic and cannot match the thermo-oxidative resistance of phenolic or unsaturated polyester above 180°C continuous use. Weld-line tensile strength in glass-filled FR PBT can be 40–60% of the parent material value, so gate locations should be selected to position weld lines away from snap-fit features; weld-line validation should follow ISO 527-2 with specimens cut across the weld plane.
Electrical connector housings, relay bases, terminal blocks, bobbins and low-voltage switchgear components are typical uses for this material class because the combination of UL 94 V-0 at 1.5 mm under IEC 60695-11-10 and a comparative tracking index between 200 V and 400 V under IEC 60112 supports insulation coordination. Glow-wire testing at 750°C according to IEC 60695-2-12 is relevant for unattended appliance components, but the specific glow-wire ignition temperature for PBT-2110 must be stated on the supplier safety data sheet. Mould shrinkage in the flow direction is typically 0.40–0.80% and in the transverse direction 0.70–1.20% under ISO 294-4; tooling should be cut after verifying shrinkage on the actual gate configuration. The flexural modulus of 6,500–8,500 MPa under ISO 178 in the 15% glass-filled grade supports pin retention and terminal alignment in multi-pin designs while retaining shorter flow paths than 30% glass-filled grades.
Brominated aromatic flame retardants used in PBT typically decompose in the 370–390°C range in nitrogen, as measured by thermogravimetric analysis; the decomposition releases acidic species that accelerate PBT hydrolysis if moisture is present. Phosphinate-based systems show different degradation chemistry, with phosphorus volatilisation and char formation, and often retain higher CTI values. PBT-2110 should be protected from moisture before processing because residual acids from FR decomposition or hydrolysis products lower molecular weight and reduce notched impact. Incompatibilities include strong alkaline and amine-based additives, which can attack the ester linkage and, in brominated systems, disrupt the antimony-halogen synergism required for UL 94 V-0. The specific thermal stability and decomposition products of the PBT-2110 flame-retardant package must be obtained from the supplier; TGA onset should not be used as the sole processing limit because residence time and shear heating lower the practical melt-temperature ceiling.
For multi-cavity connector tools, gate dimensions of 0.8–1.0 mm and vent depths of 0.02–0.03 mm are common for this filler level. Regrind levels above 20–25% are not recommended for thin-wall UL 94 V-0 parts unless the supplier has validated the flame-retardant performance after multiple heat histories, because brominated or phosphinate FR efficacy can decline with repeated extrusion. Storage in sealed containers at relative humidity below 60% is standard. The exact PBT-2110 grade may differ from class data; material qualification should include tensile testing under ISO 527-2, flammability testing under IEC 60695-11-10, and tracking index measurement under IEC 60112 on production-representative mouldings.