| HS Code | 493093 |
| Polymertype | Polyethylene naphthalate (PEN) |
| Intrinsicviscosity | 0.90 dL/g |
| Density | 1.36 g/cm3 |
| Meltingpoint | 265 °C |
| Glasstransitiontemperature | 121 °C |
| Waterabsorption | 0.30 % |
| Tensilestrength | 85 MPa |
| Tensilemodulus | 2.50 GPa |
| Elongationatbreak | 15 % |
| Flexuralmodulus | 2.80 GPa |
| Heatdeflectiontemperature | 100 °C at 1.82 MPa |
| Dielectricconstant | 3.0 |
| Dissipationfactor | 0.005 |
| Refractiveindex | 1.64 |
As an accredited Indorama Ventures PENSTAR® PEN N9AA factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Indorama Ventures PENSTAR® PEN N9AA is packaged in 25 kg net bags or 1,000 kg bulk bags, palletized for shipment. |
| Container Loading (20′ FCL) | Indorama Ventures PENSTAR® PEN N9AA is loaded into a 20′ FCL container, palletized, secured, and labeled for safe ocean shipment. |
| Shipping | Indorama Ventures PENSTAR® PEN N9AA is typically shipped as dry resin pellets in moisture-barrier-lined bags, drums, octabins, or bulk containers. Use clean, covered transport; avoid heat, moisture, UV, and contamination. Keep containers sealed and follow the SDS and applicable transport regulations. |
| Storage | Store PENSTAR® PEN N9AA in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, moisture, and incompatible oxidizing materials. Keep original containers tightly closed and protect them from physical damage. Avoid dust generation and static buildup. Use first-in, first-out stock rotation, prevent excessive temperature exposure, and follow the manufacturer’s safety data sheet and local regulations. |
| Shelf Life | Shelf life is two years from manufacture in unopened original packaging, stored dry at ambient temperature away from direct sunlight. |
Competitive Indorama Ventures PENSTAR® PEN N9AA prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Indorama Ventures PENSTAR® PEN N9AA is a thermoplastic polyethylene terephthalate resin supplied for injection stretch blow molding, preform injection, and downstream container conversion. The grade sits within the PENSTAR bottle-resin series and is typically positioned for applications where the release specification controls residual acetaldehyde, intrinsic viscosity, carboxyl end groups, and pellet-to-pellet melt viscosity distribution. Published data for this exact commercial designation is limited; therefore, process and application decisions should be based on the seller’s certificate of analysis rather than on generalized polyester literature. The resin is supplied as pellets and must be handled as a hygroscopic condensation polymer.
Specification testing for bottle-grade PET commonly includes intrinsic viscosity by ASTM D4603, density by ASTM D792, melting and crystallization behavior by ISO 11357-3, carboxyl end groups by ASTM D7409, and residual acetaldehyde by ASTM F2013. Color coordinates are reported in CIE L*a*b* units, and diethylene glycol content may be reported where process control requires it. The typical solid-state density of polyethylene terephthalate bottle resin is 1.38–1.40 g/cm³; the melting peak for bottle-grade material generally falls between 245°C and 255°C. The specific limits assigned to N9AA must be read from the lot-specific certificate of analysis.
Pre-drying is the first process boundary. Polyethylene terephthalate undergoes hydrolytic chain scission during melting when residual moisture is present. The resin should be dried in a desiccant-bed dryer with a dew point below -40°C and sufficient airflow to hold the pellet bed at 160–180°C for 4–6 h. Target residual moisture is below 0.005% by weight, measured by ASTM D4019 or equivalent coulometric Karl Fischer titration. Material stored at relative humidity above 60% must be re-dried before processing. Hopper residence time beyond 2 h without an inert gas blanket can allow moisture regain at the feed throat.
During injection, melt temperature is normally maintained at 270–290°C. The barrel profile should be flat through the compression zone, with a maximum melt temperature no higher than 295°C to suppress thermal degradation. A reciprocating screw with an L/D ratio of 24:1 to 25:1 and a low-shear metering profile is typical for preform molding. The compression ratio should generally fall between 2.0:1 and 3.0:1. Barrel residence time should be minimized; production-scale experience indicates that exposure beyond 5 min at the upper melt temperature promotes thermal and hydrolytic degradation, shifting molecular weight distribution downward and increasing acetaldehyde generation.
Intrinsic viscosity of bottle-grade PET is commonly specified in the range of 0.80–0.85 dL/g for carbonated soft drink applications, but the exact N9AA setpoint is controlled by the certificate of analysis. Carboxyl end group content for fresh bottle-grade material is often specified below 30 meq/kg; elevated values indicate hydrolysis or thermal degradation. These values are general bottle-grade PET typicals, not N9AA-specific, unless listed on the lot certificate.
At production-scale preform injection, hot-runner balance and gate freeze-off are commonly the dominant sources of cavity-to-cavity variation. Multi-cavity tools with valve-gated hot runners require uniform melt residence time across all drops. Accumulation of degraded material in dead zones can release periodic high-acetaldehyde slugs into adjacent cavities. The resulting spread may exceed the product specification even when the average value is acceptable. Field data from preform lines shows that melt-cushion consistency and screw recovery time stability correlate with lower acetaldehyde variation. Processors should monitor shot weight, cushion position, and decompression distance as indirect indicators of residence-time disruption.
Shot capacity utilization should be maintained between 40% and 70% of barrel capacity where practical. Operation below 20% of shot capacity can extend residence time and increase degradation; operation above 80% can cause recovery-time extension and melt temperature variation. Desiccant dryers should be sized for the resin throughput, with return-air dew point remaining below -30°C as a warning threshold. These limits are standard for bottle PET, not N9AA-specific.
Residual acetaldehyde is a critical release property for water and soft-drink containers. It forms as a thermal degradation by-product and partitions between the polymer matrix and the container headspace. Measurement is commonly performed by gas chromatography according to ASTM F2013, typically using cryogenic grinding of preforms followed by headspace analysis. Water-grade preforms commonly require less than 3 µg/L acetaldehyde in the bottle headspace; carbonated soft drink applications may permit higher values, but supplier specifications vary by contract and region.
Intrinsic viscosity is measured by ASTM D4603 in a 60/40 phenol/1,1,2,2-tetrachloroethane solvent at 30°C. Carboxyl end group titration according to ASTM D7409 indicates the extent of hydrolytic and thermal chain scission. A drop in intrinsic viscosity below 0.72 dL/g often corresponds to measurable loss of preform burst strength and should trigger an audit of the drying system and melt residence time. These relationships are characteristic of bottle-grade PET; the specific limits for N9AA are source-controlled.
Stretch blow molding conditions affect container crystallinity, residual stresses, and acetaldehyde migration. Preform surface temperature should be uniform in the 95–115°C range before stretching. Blow mold temperature of 8–14°C is typical for still-water containers, while higher mold temperatures can increase crystallinity and modify barrier and thermal stability. Excessive reheat energy can create surface crystallinity gradients that appear as haze or affect material distribution. These conditions are equipment-specific and should be optimized on the intended platform rather than transferred from generic PET guidelines.
Hot-fill packaging requires heat-setting of the stretch blow mold. If the grade is used in hot-fill formats, the blow mold temperature may need to be raised above 120°C to induce thermal crystallization and stabilize the container against shrinkage at fill temperatures of 85–95°C. This is a processing-route issue, not inherently grade-specific, and the suitability of N9AA for hot-fill must be confirmed through container qualification.
Because the N9AA designation is often compared with fast-reheat bottle grades and general-purpose PET resins, the differentiation must be established from the certificate of analysis. Fast-reheat grades contain controlled levels of infrared-absorbing reheat agents that increase preform surface temperature for a given lamp exposure. If N9AA is not formulated with such additives, its reheat response will differ and the cycle time on the blow molder may need adjustment. If it is formulated with reheat agents, the concentration and chemical identity are lot-specific and are not fully disclosed in public literature. Published data for this specific configuration is limited, and side-by-side molding trials on the intended platform are the only reliable method to determine relative cycle-time differences.
Differences from PET film and fiber grades are more pronounced. Film grades are frequently designed with higher comonomer content or lower intrinsic viscosity, whereas bottle resins balance stretchability, molecular weight retention, and acetaldehyde control. N9AA should not be assumed interchangeable with polyethylene naphthalate or glycol-modified PET unless the certificate of analysis explicitly identifies such chemistry. Modification with isophthalic acid or diethylene glycol lowers crystallinity and permits lower preform temperatures in many bottle resins; the exact comonomer chemistry of N9AA is not disclosed in public literature.
Post-industrial preform and bottle regrind is commonly reintroduced into the material stream. The proportion should be limited to typical food-contact bottle-grade levels, often 25% by weight, unless the supplier’s letter of no objection or national legislation allows otherwise. Every additional heat history reduces intrinsic viscosity and increases carboxyl end groups. The resulting virgin-regrind blend must still satisfy the same release specifications as virgin resin.
Regrind particle size distribution requires control. Fines below 500 µm can trap moisture and degrade more rapidly during drying. The bulk density of regrind differs from virgin pellets and affects gravimetric feeder calibration. A gravimetric blender with batch weighing is preferred over volumetric metering when regrind is introduced. Production-scale experience shows that excessive fines increase variation in screw recovery time and shot weight, which then appears as cavity-to-cavity inconsistency in preform weight and acetaldehyde.
Regulatory compliance for food-contact use is specific to the market and to the grade formulation. In the United States, polyethylene terephthalate resins intended for food contact are generally covered by 21 CFR 177.1630 and applicable good manufacturing practices. European Union food-contact compliance is addressed under Commission Regulation (EU) No 10/2011, including overall migration and specific migration limits for additives. The supplier should provide a compliance statement linking the specific lot to the applicable regulation.
| Requirement | Standard or Regulation | Test or Clause |
|---|---|---|
| U.S. PET food-contact resin | 21 CFR 177.1630 | Polyethylene terephthalate polymers |
| EU food-contact compliance | Regulation (EU) No 10/2011 | Annex I authorized substances; overall migration 10 mg/dm² |
| REACH compliance | Regulation (EC) No 1907/2006 | SVHC candidate list |
| RoHS restricted substances | Directive 2011/65/EU | Annex II |
| Intrinsic viscosity | ASTM D4603 | 60/40 phenol/tetrachloroethane, 30°C |
| Residual acetaldehyde | ASTM F2013 | Gas chromatography headspace |
Amine-based additives, including certain colorants and nucleating agents, should be excluded from the blend unless the resin supplier has explicitly approved the formulation. Amines can react with the polyester ester linkage under melt conditions, accelerating chain scission and acetaldehyde generation. Polyvinyl chloride contamination must also be avoided because thermal decomposition of PVC releases hydrogen chloride, which catalyzes polyester degradation. High-moisture bio-based fillers should not be blended without pre-drying and stabilizer evaluation.
Pellet handling should avoid open flame, dust, and prolonged direct sunlight. Silos and feed hoppers should be cleaned between polymer campaigns to prevent cross-contamination from other polymer families. The resin should be used within the supplier’s recommended shelf life when stored in unopened bags at ambient temperature and low humidity. Material that has been exposed to roof condensation or warehouse flooding should be quarantined and tested before use.