Indorama Ventures Penstar Pen N1s7

Indorama Ventures PENSTAR® PEN N1S7

    • Product Name: Indorama Ventures PENSTAR® PEN N1S7
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 118046
    Material Type Polyethylene naphthalate (PEN) homopolymer
    Density 1.36 g/cm3
    Melting Point 265 C
    Glass Transition Temperature 120 C
    Intrinsic Viscosity 0.70 dL/g
    Tensile Strength 80 MPa
    Tensile Elongation At Break 3%
    Flexural Modulus 2.8 GPa
    Heat Deflection Temperature At 1 8 Mpa 100 C
    Water Absorption 0.3%
    Mold Shrinkage 0.2-0.5%
    Processing Melt Temperature 280-300 C

    As an accredited Indorama Ventures PENSTAR® PEN N1S7 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Indorama Ventures PENSTAR® PEN N1S7 is packaged in 25 kg moisture-resistant bags, palletized for safe industrial storage and transport.
    Container Loading (20′ FCL) Indorama Ventures PENSTAR® PEN N1S7 is palletized, moisture-protected, and securely loaded into a 20-foot FCL container for transport.
    Shipping PENSTAR® PEN N1S7 is shipped as non-hazardous polyethylene naphthalate resin pellets, typically in 25 kg bags, big bags, or octabins. Use clean, dry, covered transport at ambient temperature; avoid moisture, direct sunlight, heat, and contamination. No special dangerous-goods placarding is required under normal shipping conditions.
    Storage Store **PENSTAR® PEN N1S7** in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers closed and use original packaging to prevent moisture and contamination. Avoid prolonged UV exposure and excessive stacking. Follow the supplier’s SDS and local regulations for safe handling and storage.
    Shelf Life Indorama Ventures PENSTAR® PEN N1S7 typically has a two-year shelf life when stored dry, cool, and sealed in original packaging.
    Free Quote

    Competitive Indorama Ventures PENSTAR® PEN N1S7 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Indorama Ventures PENSTAR® PEN N1S7 is a naphthalate-based polyester resin in which dimethyl 2,6-naphthalenedicarboxylate replaces a portion of the terephthalate moiety present in standard bottle-grade polyethylene terephthalate. The N1S7 model designation identifies a polyethylene naphthalate grade with a medium-to-high intrinsic-viscosity window and a crystallization rate suited to injection stretch-blow molding, barrier film extrusion, and elevated-temperature packaging. Representative resin values from available technical literature place intrinsic viscosity between 0.65 dL/g and 0.75 dL/g when measured in 60:40 w/w phenol/1,2-dichlorobenzene at 25 °C according to ISO 1628-5:2015. The glass transition temperature is approximately 120 °C and the melt endotherm is approximately 265 °C by ISO 11357-2. Density is 1.36 g/cm³ per ISO 1183-1:2019. These values distinguish PEN N1S7 from conventional PET grades, which typically exhibit a glass transition near 78 °C and a melt peak near 245 °C under the same test methods. The difference originates from the stiffness and polarity of the naphthalene ring, which reduces amorphous-phase segmental mobility and increases chain packing density relative to terephthalate-based polyesters.

    What process parameters constrain melt stability during screw recovery and preform injection?

    PEN N1S7 requires moisture removal before melt processing because ester linkages are susceptible to hydrolysis at processing temperatures. Desiccant drying with a supply-air dew point no higher than -40 °C and pellet moisture below 50 ppm by Karl Fischer titration is required. Drying temperature set points between 160 °C and 170 °C for 4 h to 6 h are typical. Hopper residence beyond 8 h at temperature risks intrinsic-viscosity loss and should be avoided in continuous operations where line stoppages exceed the drying interval.

    Twin-screw extrusion with 25:1 to 40:1 L/D and vacuum venting at approximately -0.08 MPa gauge pressure should maintain melt temperature between 290 °C and 310 °C. Screw speed and throughput should be balanced to keep residence time below 10 min at melt temperature. Residence above 10 min at 310 °C promotes chain scission, intrinsic-viscosity loss above 0.05 dL/g, and an increase in crystallization half-time that can alter preform transparency. Barrel purge compounds containing amine-functional additives are incompatible; aminolysis of the ester backbone accelerates molecular weight reduction and produces surface defects on molded articles.

    Injection stretch-blow molding of preforms typically uses barrel profiles between 280 °C and 300 °C, hot-runner manifolds between 290 °C and 305 °C, and mold cooling water at 8 °C to 12 °C for amorphous preform production. Crystallized preforms or hot-fill articles require conditioned mold temperatures between 130 °C and 150 °C to avoid brittle skin formation and warpage. Clamp force requirements generally fall between 5.0 kN/cm² and 7.0 kN/cm² of projected area depending on flow length and wall thickness. Scrap rates above 30 wt% require an edge-trim or flake crystallizer and a dryer system rated for PEN-grade material because regrind particle geometry differs from virgin pellet feed and alters melting behavior in single-screw compression zones.

    Oxygen and carbon dioxide permeation differentials in monolayer and multilayer preforms

    Published oxygen transmission observations for PEN N1S7 indicate oxygen permeability approximately 5 to 6 times lower than PET at 23 °C, 50% RH, when measured according to ASTM D3985. Carbon dioxide permeability is approximately 4 to 5 times lower under comparable conditions using ASTM D1434. The reduction is attributed to restricted segmental motion and tighter amorphous packing in the naphthalene-containing backbone. Moisture vapor transmission is approximately 3 to 4 times lower than PET, which reduces package deformation during retort cycles and limits water uptake in oxygen-sensitive dry formulations.

    The barrier advantage is orientation-dependent. Blow-stretch orientation in the sidewall must exceed axial stretch ratios of 2.5 to 3.0 and hoop stretch ratios of 3.0 to 3.5 to approach the published sheet barrier values. Preform injection and blow mold temperatures must be controlled to avoid fractional crystallinity above approximately 2% in barrier regions, because spherulitic growth scatters light and introduces localized permeation paths. In multilayer preforms, PEN N1S7 can serve as the core or barrier layer in co-injection with PET or virgin copolyester skins; tie-layer incompatibility is generally not required when the skin and core are polyester-based, but interfacial viscosity matching at the co-injection manifold must be verified on the production line to prevent layer thickness variation above 10% of nominal.

    Tensile stress at break for unoriented samples of PEN N1S7 tested according to ISO 527-1/-2 at 23 °C falls between 75 MPa and 85 MPa. Tensile modulus is approximately 3.4 GPa to 3.6 GPa. Flexural modulus according to ISO 178 is between 4.5 GPa and 5.0 GPa. Notched Izod impact according to ISO 180/A at 23 °C is approximately 2.0 kJ/m² to 3.0 kJ/m², indicating notch-sensitive behavior in thick sections. Heat deflection temperature at 1.82 MPa according to ISO 75-2 is approximately 100 °C to 105 °C. The resin therefore tolerates short-term contact with 121 °C retort steam only when wall thickness, crystallinity, and package headspace are optimized. Continuous service above 150 °C is outside the intended operating boundary; thermotropic liquid crystal polymers or polyimides should be used where sustained exposure exceeds that threshold.

    Representative property comparison: unmodified PEN N1S7 versus PET bottle-grade homopolymer
    PropertyTest standardPEN N1S7PET reference
    Glass transition temperatureISO 11357-2120 °C78 °C
    Melt endothermISO 11357-2265 °C245 °C
    DensityISO 1183-1:20191.36 g/cm³1.34 g/cm³
    Tensile stress at breakISO 527-1/-275–85 MPa50–60 MPa
    Flexural modulusISO 1784.5–5.0 GPa2.5–3.0 GPa
    Heat deflection temperature at 1.82 MPaISO 75-2100–105 °C65–70 °C

    Dielectric strength measured on 1 mm plaques according to IEC 60243-1 is approximately 17 kV/mm to 20 kV/mm. Dielectric constant at 1 MHz according to IEC 60250 is approximately 3.0 to 3.2. These values support use in electrical insulation films, flexible printed-circuit carrier films, and motor slot liners where thermal class and dimensional stability are specified. Film extrusion thickness from 12 µm to 100 µm can be produced with sequential or simultaneous draw ratios up to approximately 3.5 in both machine and transverse directions. Surface treatment is required before metallization or lamination; corona or plasma treatment to a wetting tension above 42 mN/m as measured by ASTM D2578 is typical.

    When retort packaging replaces PET with PEN N1S7 in dual-ovenable tray applications

    Injection-molded dual-ovenable trays and hot-fill sauce containers are candidate applications for PEN N1S7 because the material combines thermal resistance with oxygen and carbon dioxide barrier at comparable wall thickness. In monolayer trays, the resin reduces oxygen ingress and carbon dioxide loss relative to PET. However, published data for this specific configuration is limited; converters must validate migration, organoleptic transfer, thermal shock, and seal performance in the finished article according to EU Regulation 10/2011, FDA 21 CFR 174.5, or applicable national food-contact provisions. Crystallinity distribution in injection-molded trays must be controlled by mold temperature and cooling time; uncontrolled quench-free orientation can produce warpage after retort exposure above 100 °C.

    For high-acid retort applications, adhesion to lidding films requires corona or plasma treatment and may require a tie-coating or extrusion lamination layer if the sealant is olefin-based. The resin also differs from PET and polypropylene in thermal conductivity and shrinkage; tooling shrinkage allowances of approximately 0.4% to 0.8% are typical for unfilled PEN injection-molded parts, depending on flow direction and mold temperature. In co-injection with PET, the higher melt viscosity of N1S7 can cause asymmetric layer distribution if manifold temperatures are not independently controlled; layer-thickness verification by cross-sectional microscopy is required at startup and after every tool change.

    PEN N1S7 is not recommended for continuous contact with aggressive alkaline detergents at elevated temperature or with amine-containing processing aids. In industrial monofilament and strap extrusion, oven temperatures and quench bath conditions must be adjusted to avoid brittle surface orientation. The resin’s processing window is narrower than PET; melt temperature variation beyond ±5 °C at the die or hot-runner tip can produce measurable intrinsic-viscosity drift and fluctuation in crystallization half-time. Production lines without independent hot-runner zone control should not be used for N1S7 preform molding.

    Compared with poly(butylene terephthalate) and polycarbonate, N1S7 provides a higher glass transition temperature than poly(butylene terephthalate) and lower moisture sensitivity than polycarbonate in barrier-oriented structures. Against standard PET grades in the PENSTAR® portfolio, N1S7 requires elevated drying and melt temperatures and offers improved retort tolerance and gas barrier. The material is not a direct drop-in substitute on PET lines without dryer and mold-temperature upgrades. Processors should verify melt-pressure transducers, heater wattage, and dryer regeneration capacity before conversion because the higher melt temperature increases heater duty and the higher mold temperature raises chiller load. Published data for this specific configuration is limited for high-speed rotary stretch-blow molding above 2,000 bottles per cavity per hour; pilot-scale trials are required to establish the reheat profile and preform temperature mapping.

    The compliance profile for PEN N1S7 in food-contact use is tied to the converted article. The base resin is expected to be evaluated under the framework of EU Regulation 10/2011 for overall migration and specific migration of naphthalene-2,6-dicarboxylic acid and ethylene glycol. For the United States, food-contact status should be confirmed under 21 CFR 177.1630 or an applicable food-contact notification. Electrical and electronic applications require conformity assessment for RoHS 2011/65/EU and REACH 1907/2006/EC substance restrictions. No claim of compliance for the final article is valid without converter-specific testing because monomers, processing aids, and print layers can alter extractive profiles.