    HS Code 302140
    Density 1.36 g/cm³
    Intrinsic Viscosity 0.60 dL/g
    Melting Point 265 °C
    Glass Transition Temperature 121 °C
    Tensile Strength 80 MPa
    Tensile Elongation At Break 4%
    Flexural Modulus 2500 MPa
    Notched Izod Impact Strength 30 J/m
    Heat Deflection Temperature At 1 82 Mpa 100 °C
    Water Absorption 24 H 0.3%
    Mold Shrinkage 0.6%
    Processing Temperature 280–300 °C

    As an accredited Indorama Ventures PENSTAR® PEN N1S6 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Indorama Ventures PENSTAR® PEN N1S6 is supplied in 25 kg moisture-resistant bags, palletized for secure storage and transport.
    Container Loading (20′ FCL) Indorama Ventures PENSTAR® PEN N1S6 is loaded in a 20′ FCL container using dry, secure, labeled packaging for safe transport.
    Shipping Indorama Ventures PENSTAR® PEN N1S6 is shipped as solid resin pellets in moisture-barrier PE-lined 25 kg bags or 1,000 kg supersacks on pallets. It is non-hazardous for transport and should be kept dry, cool, and away from direct sunlight/UV and heat during storage and shipment.
    Storage Store PENSTAR® PEN N1S6 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep in tightly sealed original packaging or suitable containers, palletized and off the floor. Prevent exposure to UV, dust, and incompatible chemicals. Avoid prolonged high humidity; dry resin before processing as recommended. Follow supplier guidance and local regulations.
    Shelf Life Typically 24 months from manufacture when stored unopened in a cool, dry place, protected from moisture, heat, and sunlight.
    Free Quote

    Competitive Indorama Ventures PENSTAR® PEN N1S6 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Indorama Ventures PENSTAR® PEN N1S6 is introduced for melt-phase conversion operations that exceed the thermal and oxygen-barrier limits of commodity polyethylene terephthalate. The grade belongs to the polyethylene naphthalate family, in which the aromatic diacid component is naphthalene-2,6-dicarboxylic acid rather than terephthalic acid. This substitution creates a fused bicyclic aromatic repeat unit in the polyester backbone, reducing segmental mobility and free volume. The N1S6 designation identifies a specific molecular-weight and additive configuration within the PENSTAR portfolio. Lot-specific intrinsic viscosity, color coordinates, residual moisture, and melt stability should be taken from the certificate of analysis before process validation.

    Unlike standard PET bottle resins, the naphthalate repeat unit shifts the thermal transitions of the resin class. Differential scanning calorimetry under ASTM D3418 places the glass transition temperature near 120 °C, compared with 76–80 °C for PET. The melting endotherm is commonly observed at 265–268 °C. Unfilled resin density measured by ISO 1183-1 is approximately 1.36 g/cm³. These values are characteristic of the PEN class rather than lot-specific N1S6 specifications; published data for this specific configuration is limited, and incoming resin lots are therefore screened against the intended conversion process.

    What Shifts When Naphthalene-2,6-Dicarboxylate Replaces Terephthalate in the Polyester Backbone?

    Gas permeation is the most significant property shift. In biaxially oriented 25 µm film, oxygen transmission measured under ASTM D3985 at 23 °C and 0% relative humidity typically falls between 15 cm³/(m²·day·atm) and 25 cm³/(m²·day·atm) for PEN, while oriented PET film of the same gauge commonly registers 90–110 cm³/(m²·day·atm). Water vapour transmission under ASTM F1249 at 38 °C and 90% RH is also reduced by a factor of three to four. The improvement originates from the greater aromatic density of the naphthalene ring and from the higher activation energy for diffusion through the amorphous phase. Unlike ethylene-vinyl alcohol copolymers, PEN does not suffer a severe barrier collapse at high relative humidity because the polyester backbone contains no strongly hydrophilic hydroxyl groups capable of plasticizing the amorphous phase.

    Ultraviolet absorption in the 320–380 nm band is stronger than PET. This characteristic is useful for UV-screening primary packaging and for capacitor film that must resist ultraviolet-assisted oxidation, but it also accelerates yellowing and surface embrittlement in unpigmented outdoor articles unless an ultraviolet stabilizer package is added. The base N1S6 grade should not be specified as inherently weatherable. Chemical resistance resembles PET in many solvents, but the higher aromatic density of PEN improves resistance to dilute acids and many aliphatic hydrocarbons. Strong bases, hot phenol/tetrachloroethane solutions, and certain chlorinated solvents degrade or dissolve the polymer and should not be used for cleaning process equipment without verification.

    Extrusion-Grade Processing Limits and Drying Envelope

    Processing of N1S6 starts with desiccant-bed drying at an air inlet temperature of 160–180 °C, a dew point at or below −40 °C, and a residence time of 4–6 h. Residual moisture must be reduced to ≤50 ppm when checked by ISO 15512 or ASTM D6869. Feedstock stored at relative humidity above 60% without sealed hopper blanketing will exceed the safe moisture threshold and undergo hydrolytic chain scission in the barrel. The failure signature is a drop in intrinsic viscosity, increased die-lip deposits, and film gel counts concentrated near the die edges. Drying below 160 °C leaves moisture that hydrolyzes the ester linkage; drying above 180 °C for more than 8 h can oxidatively yellow the pellet surface and shift the color coordinates of the final film or preform.

    Single-screw extrusion lines with an L/D of at least 24:1 and a barrier screw with compression ratio 2.5:1 to 3.5:1 are typical for melt-phase conversion. Barrel set points from rear zone to die are set between 280 °C and 305 °C, with melt temperature controlled at 295–310 °C. Above 315 °C, thermal degradation accelerates sharply; gel formation and color shift become visible after 5 min of static hold-up. Adapter and die residence time is therefore kept below 3 min where possible. Vacuum venting at −0.08 MPa or lower reduces volatile oligomers but cannot compensate for wet feedstock. Melt filtration through a screen pack with 20–40 µm nominal retention is used on cast film and extrusion coating lines to remove gel particles and agglomerated additives.

    For injection molding and preform conversion, melt temperature is maintained at 295–305 °C and mold temperature at 120–150 °C. Elevated mold temperature is necessary because PEN crystallization is significantly slower than PET. At mold temperatures below 120 °C, thin-wall parts retain an amorphous skin and can distort during downstream hot-fill exposure or annealing. Cycle time may increase by 15–30% relative to PET unless the tool is designed with heated sprues, valve gates, and hot-runner drops held above 295 °C. Unheated nozzle tips can freeze because the melt solidifies near 120 °C, which is well above the solidification point of commodity PET. Hot-runner systems must be purged thoroughly during shutdown, because retained PEN in dead spots can crosslink into gels when reheated.

    Biaxially oriented film conversion on a tenter frame uses machine-direction draw ratios of 3.0–3.5 and transverse-direction draw ratios of 3.5–4.0. Preheat temperatures are commonly set at 135–150 °C, with stretching at 145–155 °C and heat-setting at 180–210 °C. Insufficient heat-setting leaves residual shrink above 2% when the film is later exposed to 150 °C air for 30 min, a common screening condition for capacitor and flexible-circuit carriers. Balanced BOPEN film tensile strength under ASTM D882 is typically in the range of 250–300 MPa in the machine direction, with elongation at break of 80–120% depending on draw ratio and heat-set temperature. These values are class benchmarks and must be validated for the specific N1S6 lot and line configuration.

    Comparative polyester class benchmarks for orientable barrier resins
    PropertyTest methodPEN N1S6 target classPET bottle/film resin
    Glass transition temperatureASTM D3418118–122 °C76–80 °C
    Melting temperatureASTM D3418265–268 °C245–255 °C
    DensityISO 1183-11.36 g/cm³1.34 g/cm³
    Oxygen transmission, 25 µm oriented filmASTM D398515–25 cm³/(m²·day·atm)90–110 cm³/(m²·day·atm)

    The values in the table are comparative class benchmarks drawn from published polyester literature and should not be read as lot-specific N1S6 specifications. Certificate-of-analysis data, orientation level, heat-setting history, and test humidity all move the measured result. Users should establish internal control limits from a statistically valid set of production lots rather than relying on single-point datasheet values.

    Differentiation from standard Indorama PET grades appears most sharply at the equipment level. A bottle-grade PET line operating at 270–285 °C melt temperature and 10–20 °C mold temperature cannot directly process N1S6 without overhauls to drying, hot runners, mold cooling circuits, and screw temperature profiling. Conversely, a PEN N1S6 film line can often process PET after derating temperatures, but purge time must be sufficient to avoid naphthalate ring residues in high-clarity PET. The higher aromatic density of PEN also raises melt elasticity, which improves melt strength during tentering but increases die swell in profile extrusion and can narrow the stable draw resonance window on cast film lines.

    Compared with polybutylene terephthalate, PEN N1S6 provides a higher aromatic density, superior oxygen barrier, and a service-temperature advantage, but it crystallizes more slowly and generally exhibits lower elongation at break in unoriented molded articles. The material is not a drop-in replacement for PBT in thin-wall electrical connectors where rapid crystallization controls cycle time. Unoriented tensile bars tested under ASTM D638 at 23 °C typically show tensile strength in the 80–100 MPa range and elongation at break of 20–40% for the PEN class; specific N1S6 values depend on thermal history, gate orientation, and moisture content before molding.

    Regulatory evaluation depends on the final article and condition of use. In the United States, 21 CFR 177.1630 addresses polyethylene phthalate polymers, but naphthalate-based articles may require a Food Contact Notification because the regulation is historically oriented toward terephthalic acid-based polyesters. In the European Union, compliance with Regulation (EU) No 10/2011 is established by migration testing under EN 1186-1 and specific migration methods; the overall migration limit for plastic food-contact materials is 10 mg/dm². For electronic applications, RoHS Directive 2011/65/EU requires verification of lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE at the homogeneous-material level. Under REACH, the polymer may be exempt from registration under Article 2(9), but deliberately released substances and residual monomers above 0.1% w/w can carry separate obligations.

    Operational boundaries for N1S6 include avoiding combination with amine-based additives or colorants that catalyze ester aminolysis, avoiding melt contact with strong bases and hot phenol/chlorinated solvent mixtures during cleaning, and avoiding storage of unopened gaylords in direct sunlight for more than 6 months without sealed foil liners. The resin is not recommended for applications requiring long-term outdoor weatherability without additional stabilization, nor for direct extrusion coating onto unprimed aluminum foil where acidic copolymers are required for adhesion. For hot-fill container preforms, the main process conflict is between barrier and crystallinity. Increasing mold temperature to 150 °C raises sidewall crystallinity and reduces oxygen permeation, but it extends cooling time and can create gate crystallinity if the hot-runner tip is not thermally isolated.

    Typical conversion uses include biaxially oriented capacitor films that must survive 150 °C thermal excursions, high-barrier medical device trays exposed to hydrogen peroxide plasma sterilization, hot-fill container preforms that require low oxygen ingress across the sidewall, and industrial monofilament for paper machine clothing where dimensional stability under wet tension is mandatory. In each application, the converter shall validate lot-specific intrinsic viscosity, color, gel count, thermal shrinkage, and final-article migration before production release.