Indorama Ventures Penstar Pen N1aa

Indorama Ventures PENSTAR® PEN N1AA

    • Product Name: Indorama Ventures PENSTAR® PEN N1AA
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 880548
    Materialtype Polyethylene naphthalate (PEN) homopolymer
    Density 1.36 g/cm³ (typical)
    Intrinsicviscosity 0.60-0.70 dL/g (typical)
    Meltingpoint 265 °C
    Glasstransitiontemperature 121 °C
    Tensilestrength 75-85 MPa
    Tensilemodulus 2.6-3.0 GPa
    Elongationatbreak 2-5%
    Flexuralmodulus 2.8-3.2 GPa
    Heatdeflectiontemperature 100 °C at 1.82 MPa
    Waterabsorption 0.2-0.4% (24 h)
    Oxygenpermeability Low; approximately 4 times lower than PET
    Coefficientoflinearthermalexpansion 20-30 ppm/K
    Uvresistance Good
    Hydrolyticstability Good

    As an accredited Indorama Ventures PENSTAR® PEN N1AA factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Indorama Ventures PENSTAR® PEN N1AA is supplied in 25 kg multiwall bags, palletized and stretch-wrapped for industrial handling.
    Container Loading (20′ FCL) Indorama Ventures PENSTAR® PEN N1AA is palletized, shrink-wrapped, and securely loaded into a clean 20′ FCL container for export.
    Shipping Indorama Ventures PENSTAR® PEN N1AA is shipped as solid polyethylene naphthalate resin pellets in moisture-barrier bags, octabins, or bulk containers. Keep dry and protected from heat and sunlight. It is not classified as dangerous goods; handle per SDS and local transport regulations.
    Storage Store Indorama Ventures PENSTAR® PEN N1AA in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep packages tightly sealed and palletized to prevent moisture, dust, and contamination. Avoid prolonged high-temperature or UV exposure. Segregate from incompatible materials and follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf Life: 2 years from date of manufacture when stored in original unopened packaging under dry, ambient conditions.
    Free Quote

    Competitive Indorama Ventures PENSTAR® PEN N1AA prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Indorama Ventures PENSTAR® PEN N1AA is a pelletized polyethylene naphthalate homopolymer supplied for high-barrier film, specialty monofilament, and high-temperature coated paperboard applications. The grade is specified primarily by intrinsic viscosity rather than melt flow rate; the producer’s technical data sheet indicates a nominal intrinsic viscosity of 0.62 dL/g when measured by ASTM D4603, and density of 1.36 g/cm³ when measured by ISO 1183-1. The 2,6-naphthalene dicarboxylic acid ethylene glycol backbone raises the glass transition to 120–125 °C and the melting point to 265–270 °C under ISO 11357-2 and ISO 11357-3, respectively. The N1AA designation denotes a standard film-grade formulation without intentionally added slip or antiblock; converters must confirm the additive package for printed, metallized, or adhesive-laminated surfaces. Lot-specific carboxyl end-group, color, and residual moisture data should be obtained from the supplier before high-speed conversion.

    The higher aromatic density of PEN N1AA distinguishes it from PET in three measurable ways: a higher glass transition, a lower oxygen diffusion coefficient, and a narrower thermal processing window. The resin is not a drop-in replacement for PET; screw profiles, barrel temperature settings, and downstream cooling must be re-engineered. Because the melt strength is higher and the crystallization rate is slower than PET, the resin tolerates biaxial orientation at higher temperatures but requires tighter control of moisture and residence time.

    How Does the Fused Naphthalene Ring Shift Oxygen Transport and Ultraviolet Shielding?

    The fused aromatic naphthalene ring restricts segmental rotation and reduces the amorphous free-volume fraction available for gas diffusion. Oxygen transport through a 25 µm biaxially oriented PEN film is therefore reported at 5–8 cm³/(m²·day·atm) when measured under ASTM D3985 at 23 °C and 50 % RH, whereas an equivalent PET film commonly transmits 25–35 cm³/(m²·day·atm) under identical conditions. The barrier advantage is smaller at elevated relative humidity because water plasticizes the amorphous phase and weakens the naphthalene ring packing effect. Carbon dioxide transmission is similarly reduced by a factor of 3–4, but moisture vapor transmission remains close to PET values because water transport depends more strongly on hydrogen bonding than on aromatic ring volume. Ultraviolet absorption below 380 nm is substantially higher than PET, which protects riboflavin and carotenoid-containing products from photo-oxidation but limits the use of UV-cured inks and adhesives where through-cure is required. In laminated retort pouches, the distinguishing performance of PEN N1AA appears as a measurable reduction in oxygen ingress after 90 minutes at 121 °C, although published data for this specific grade under retort conditions is limited.

    Thermal Transitions and Crystallization Half-Time Create a Higher Orientation Threshold

    The elevated glass transition of 120–125 °C forces orientation stretching to occur at surface temperatures 15–25 °C higher than PET. In sequential biaxial film production, transverse stretching of PEN is typically conducted at 130–150 °C, compared with 90–115 °C for PET. The slower crystallization half-time of the naphthalate permits stable bubble formation in double-bubble film lines, but the processing window between crystallization onset and melt instability narrows when residual moisture exceeds 0.02 %. Production-scale film lines have demonstrated that cast sheet temperature deviations greater than ±5 °C create skin-core crystallization mismatch, which later appears as thermal haze and uneven thickness after stretching. On a 50 mm twin-screw extruder with 30:1 L/D, the melt temperature is usually held between 290 °C and 310 °C. At 310 °C, a residence time above 5 minutes produces gel particles from ester cleavage and oxidation; the screw speed must be reduced if back-pressure exceeds 180 bar in the metering zone.

    Pre-drying is the dominant process control for PEN N1AA. The pellet is supplied at moisture content ≤ 0.40 % by Karl Fischer titration, but hydrolysis during plastication becomes measurable at moisture contents above 0.02 %. A desiccant bed dryer with a dew point of -40 °C or lower and air flow of 0.5 m/s should reduce moisture to ≤ 50 ppm in 4–6 hours at 150–170 °C. Drying above 175 °C causes pellet sticking and color body formation; drying below 140 °C does not reduce moisture to a safe level within normal hopper residence times. The resin should not be dried in uninsulated hoppers exposed to ambient relative humidity above 60 %, because re-adsorption at the hopper inlet can raise the melt moisture to 120–150 ppm within 20 minutes. Hydrolytic degradation in the barrel then follows zero-order kinetics with respect to water concentration, and produces intrinsic viscosity loss of approximately 0.02–0.03 dL/g per 5 minutes at 300 °C. The released naphthalene dicarboxylic acid can plate out on vacuum pump seals and causes compressor maintenance intervals to shorten by 30–40 % compared with PET extrusion.

    When Melt Residence Exceeds Five Minutes at 315 °C

    Thermal degradation of PEN N1AA proceeds through random ester chain scission and naphthalene ring oxidation. At barrel temperatures exceeding 315 °C, melt viscosity decreases independently of shear history, and the intrinsic viscosity drops by approximately 0.02–0.03 dL/g per 5 minutes of residence time. Acetaldehyde, carbon dioxide, and gel particles are the primary decomposition products. Injection molders must size the shot so that total residence time remains below 5 minutes, preferably 2–3 minutes, and must purge with a high-viscosity PET transition after interruptions longer than 10 minutes. The decomposition pathway is accelerated by moisture above 50 ppm; therefore, the desiccant bed dryer must remain connected to the feed throat rather than relying on pre-dried gaylord boxes. Compatibility with hot runner systems is limited to externally heated manifolds with melt channel diameters above 4 mm; narrow gates below 1.5 mm can generate shear heating that locally exceeds 320 °C and black speck defects in transparent parts.

    In biaxially oriented film conversion, PEN N1AA requires higher heat settings than PET without a corresponding increase in line speed. The film is cast at a melt temperature of 285–300 °C, quenched on a chill roll held at 30–50 °C, and reheated to 130–150 °C before stretching. Machine-direction draw ratios of 2.5–3.5 and transverse draw ratios of 3.0–4.0 are used to achieve tensile modulus near 2.5 GPa under ISO 527-2 and heat shrinkage below 1.5 % after crystallization at 200 °C for 30 seconds. The higher winding tension of PEN film, typically 15–25 % above PET at equal thickness, requires heavier core shafts and driven lay-on rollers. Differences from PET become visible as reduced sag in high-temperature lamination and a sharper thermal haze transition at the edge of the tenter frame where temperature control is less uniform.

    Comparative processing and property values for PENSTAR PEN N1AA, PET, and PBT references
    Property or parameterPENSTAR PEN N1AA / PEN homopolymer typicalPET bottle-grade referencePBT general-purpose referenceTest method or equipment
    Glass transition (°C)120–12575–8045–50ISO 11357-2
    Melting point (°C)265–270245–255223–228ISO 11357-3
    Drying temperature (°C)150–170160–180120–140Desiccant bed dryer, dew point -40 °C
    Melt temperature (°C)290–310270–290240–260Melt thermocouple, screw tip
    Mold surface temperature (°C)120–15010–3060–90Water/oil mold temperature control unit
    Oxygen transmission relative to PET4–5× lowerBaseline 1×Not applicableASTM D3985, 23 °C, 50 % RH

    Compared with higher-IV PEN grades used for tire cord and stretch blow molded containers, PEN N1AA is positioned for film and monofilament with nominal intrinsic viscosity of 0.62 dL/g. High-IV PEN grades may exceed 0.80 dL/g, which increases melt pressure and orientation stress but does not necessarily improve oxygen barrier. The lower IV of N1AA reduces screw torque and permits higher throughput on 50 mm to 75 mm extruders, but high-speed film lines should still limit screw speed to 150–180 min⁻¹ to avoid shear heating. Published data for this specific configuration is limited; converters should generate a viscosity curve by ASTM D3835 before specifying extruder drive power. Compared with PBT, PEN N1AA offers a 70–80 °C higher glass transition and better oxygen barrier, but it requires higher melt temperature and longer drying. PBT is often selected for low-temperature electrical housings because of its faster crystallization and lower mold temperature; PEN is selected when the part must retain modulus above 100 °C or resist hot oil exposure.

    PEN N1AA Monofilament Quench Stability and Spinline Stress

    Fiber and monofilament processes exploit the high glass transition to produce heat-resistant yarns and industrial cords. Spinning temperatures are set at 300–320 °C, with a spinneret exit velocity of 10–15 m/min and quench air temperature of 20–30 °C at 0.4–0.6 m/s. The filament requires draw ratios of 4.0–6.0 across a hot plate at 140–160 °C to achieve tensile strengths above 700 MPa under ISO 527-2. Differences from PET include a higher spinline stress and lower necking stability. Production experience on monofilament lines has shown that quench air turbulence above 0.8 m/s causes periodic diameter variation, while insufficient quench below 0.3 m/s produces internal voids. The higher spinline stress also increases filter pack pressure. Screen packs with filtration ratings coarser than 20 µm are recommended to avoid rapid pressure rise; finer filtration is associated with shear heating and molecular weight loss. The resulting fiber retains dimensional stability at 150 °C, which is outside the continuous-use range of conventional PET fiber.

    Chemical resistance of PEN N1AA is greater than PET toward dilute acids, aliphatic hydrocarbons, and chlorinated solvents at 23 °C. The resin is attacked by concentrated sulfuric acid, hot alkaline solutions above pH 12, and phenolic compounds. Environmental stress-cracking resistance in surfactant-containing environments is measurable by ASTM D1693; PEN homopolymer typically survives longer than PET at 50 °C, but the exact failure time depends on molded-in stress and comonomer content. Food-contact suitability must be established for the finished article under EU 10/2011 or FDA 21 CFR 177.1630 after migration testing. Compliance with RoHS Directive 2011/65/EU and REACH Regulation (EC) No 1907/2006 is declared by the producer for the pellet form; downstream additives, printing inks, and adhesives may alter the final article status. The grade should not be blended with amine-based nucleating agents or certain organophosphite stabilizers without pre-screening, because ester exchange with the naphthalate backbone can shift crystallization kinetics and produce off-odor at melt temperatures above 300 °C.

    Top