Indorama Ventures Penstar Pen Copolyester 2389

Indorama Ventures PENSTAR® PEN Copolyester 2389

    • Product Name: Indorama Ventures PENSTAR® PEN Copolyester 2389
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 488925
    Density 1.36 g/cm³
    Intrinsic Viscosity 0.80 dL/g
    Water Absorption 0.10%
    Melting Point 240 °C
    Glass Transition Temperature 85 °C
    Heat Deflection Temperature At 1 8 Mpa 65 °C
    Vicat Softening Point 80 °C
    Tensile Strength At Yield 53 MPa
    Tensile Strength At Break 28 MPa
    Elongation At Break 250%
    Tensile Modulus 2.30 GPa
    Flexural Modulus 2.30 GPa

    As an accredited Indorama Ventures PENSTAR® PEN Copolyester 2389 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Indorama Ventures PENSTAR® PEN Copolyester 2389 is supplied in 25 kg moisture-resistant bags, with 1,000 kg per pallet.
    Container Loading (20′ FCL) Indorama Ventures PENSTAR® PEN Copolyester 2389 is loaded into 20′ FCL containers, properly secured for safe international chemical transport.
    Shipping Indorama Ventures PENSTAR® PEN Copolyester 2389 is shipped as solid copolyester pellets in moisture-barrier bags, drums, or octabins. It is non-hazardous and not regulated for transport. Keep packaging dry, avoid high heat and direct sunlight, and store in a cool, dry area.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, excessive heat, and ignition sources. Keep containers tightly closed to prevent moisture pickup and contamination. Protect from humidity and prolonged UV exposure. Use suitable stacking and handling to avoid package damage, and follow first-in, first-out inventory practices and local regulations.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in unopened original packaging under cool, dry, ambient conditions.
    Free Quote

    Competitive Indorama Ventures PENSTAR® PEN Copolyester 2389 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Indorama Ventures PENSTAR® PEN Copolyester 2389 is a pelletized naphthalate-containing copolyester supplied for injection molding, injection stretch-blow molding, extrusion blow molding, and sheet coextrusion. The grade designation 2389 identifies a specific comonomer balance and viscosity target within the producer’s PENSTAR® series; lot-level certificates are the source of exact intrinsic viscosity, density, color, and residual moisture values. Public literature for this exact grade remains limited, so processing boundaries described here are drawn from the behavior of naphthalate-containing copolyesters and should be verified against the lot-specific certificate from Indorama Ventures. The resin is selected where unmodified bottle-grade PET does not provide sufficient hot-fill stability, oxygen barrier, UV screening, or dimensional stability in rigid packaging and technical articles.

    Compared with PEN homopolymer, the copolyester grade is structured to be processed closer to PET conditions. PEN homopolymer typically requires melt temperatures above 310 °C and mold temperatures above 140 °C to develop full crystallinity; the copolyester lowers those thermal requirements while retaining a measurable improvement in barrier and glass transition temperature. Compared with PET/PEN dry blends, the pre-compounded copolyester reduces transesterification variability associated with pellet blending. Compared with EVOH, the PEN copolyester does not require tie layers and remains an oxygen barrier under high-humidity distribution; however, its oxygen barrier at 0% relative humidity is lower than that of EVOH, and its cost per kilogram is higher than that of PET. These comparisons define the specification window: the material is not a general-purpose PET substitute but a technical upgrade for an identified failure mode.

    What Thermal and Crystallization Boundaries Define PENSTAR 2389 versus PET?

    Thermal analysis under ASTM D3418-15 at 20 °C/min is used to identify glass transition, cold crystallization, and melting responses. PET homopolymer typically shows a glass transition near 78 °C and a melting peak near 245 °C. PEN homopolymer shows a glass transition near 120 °C and a melting point near 268 °C. PENSTAR® PEN Copolyester 2389 is a copolyester; its glass transition is intermediate and depends on the molar fraction of naphthalene-2,6-dicarboxylate in the polymer backbone. The practical result is that a preform or sheet made from the copolyester retains dimensional stability at filling temperatures that cause PET bottle sidewalls to deform. Hot-fill behavior must be confirmed on the finished container rather than inferred from resin-level DSC data. A typical hot-fill qualification fills dummy containers at 85–95 °C, holds the filled part for 5 min, and measures volume change after cooling.

    Crystallization kinetics are slower than PET under quiescent cooling. The cold crystallization peak is displaced upward in temperature, and the cooling rate required to suppress crystallinity in unstretched sections is correspondingly lower. In injection stretch-blow molding, the slower crystallization can reduce preform haze but may require longer conditioning time or a higher preform temperature setpoint. At cooling rates above 30 °C/min, the resin remains amorphous enough for stretch blow molding; at lower cooling rates, thick walls may develop spherulitic crystallinity that raises sidewall haze and lowers impact performance. Mold temperature control in injection molding should be validated with short-shot studies because the material’s slower crystallization changes the gate-freeze time and the packing-pressure decay curve.

    Tensile properties are characterized by ASTM D638-14. Naphthalate-containing copolyesters tend to exhibit higher tensile modulus than PET in oriented and unoriented states, but exact yield stress and elongation at break depend on draw ratio and thermal history. Oriented film property retention is evaluated by ASTM D882; birefringence measurements can indicate orientation level in a transparent preform. Instrumented impact testing under ISO 6603-2 is preferred for comparing container drop performance, because conventional Izod or Charpy data from injection-molded bars do not translate reliably to blow-molded wall sections.

    Chemical resistance and UV screening differ from PET. The naphthalene ring absorbs UV below 380 nm more strongly than PET, reducing photochemical degradation of light-sensitive contents. This also means outdoor weathering of unstabilized naphthalate-containing copolyester may produce more yellowing than PET unless a UV stabilizer package is included. In contact with aggressive fluids, the copolyester shows lower solubility of non-polar aroma compounds; flavor scalping of d-limonene and other citrus terpenes is generally lower than PET but not as low as polyamide or EVOH in certain beverage systems. Organoleptic evaluation under ASTM E1870 or equivalent taste-transfer protocols should be performed because the higher processing temperature can introduce trace volatiles that are absent at lower PET melt temperatures.

    Drying, Melt Residence, and Regrind Control on Twin-Screw Extruders

    Moisture is the primary source of hydrolytic degradation. Naphthalate-containing copolyesters hydrolyze when wet pellets are melted above 260 °C, causing intrinsic-viscosity loss and brittle container sidewalls. A desiccant dryer with a dew point of −40 °C or lower and an inlet air temperature of 150–160 °C should be used. For cold-start pellets, drying time is 4–6 h; when ambient relative humidity exceeds 60%, the drying time should be extended by 2 h. The target moisture content after drying is below 50 ppm when measured by ASTM D6869 or Karl Fischer titration. Pellets left in an open hopper at floor conditions for more than 30 min may pick up enough surface moisture to raise the moisture content above 150 ppm, producing an intrinsic-viscosity drop of 0.03–0.05 dL/g during the first barrel residence.

    Melt delivery settings are higher than PET but below PEN homopolymer. A nozzle melt temperature of 285–305 °C is used for thin-wall packaging; barrel zones are typically set from 260–270 °C in the feed, 275–290 °C in compression, and 285–300 °C in metering. Exceeding 305 °C at the nozzle increases acetaldehyde-like volatiles and shifts color. The screw should have an L/D of 24:1 to 32:1 and a compression ratio of 2.5:1 to 3.0:1; high-shear mixing sections with compression ratios above 3.5:1 can overheat the melt at recovery speeds above 80 min⁻¹. Shot size should be 60–75% of barrel capacity. On a 300-ton injection molding machine with a 16-cavity hot runner tool, residence time above 8 min at 300 °C can generate black specks and gel accumulation in the manifold. Purging with a PET-based purge compound is required when changing from higher-temperature materials because dead spots in the hot runner retain degraded resin.

    Post-industrial regrind from multilayer sheet or preforms must be segregated by naphthalate content. When edge trim containing PENSTAR 2389 is ground together with PET and fed to the PET layer, the mixture contains two polymers with different melting points and crystallization rates. The maximum mixed regrind level commonly accepted in carbonated soft-drink preforms is 5 wt%; in non-critical opaque applications, up to 10 wt% may be used if the preform is tested for delamination under ISO 6603-2. Above 10 wt%, sidewall haze increases and interlayer adhesion may drop, leading to base-cracking after storage. A dedicated grinder and separate storage bin prevent cross-contamination.

    When Layer Ratios in Co-Injected Preforms Drop Below 10 Percent

    Co-injection of PENSTAR 2389 as a barrier layer in PET preforms follows series-resistance permeation. A barrier layer that is 10% of the total wall thickness and has an oxygen permeability coefficient one-fourth that of PET reduces oxygen flux only by a small amount; the benefit is proportional to the layer’s fractional contribution to total permeance. In practice, oxygen-sensitive beverage preforms specify the naphthalate-containing layer at 15–25% of the nominal wall thickness. At layer ratios below 10%, the barrier benefit may be too small to justify the additional drying and higher processing temperature unless the purpose is UV blocking rather than oxygen shelf-life extension. Published permeability data for this exact grade in a multimaterial structure are limited; the actual oxygen permeability coefficient should be obtained from the lot certificate and used in a finite-element diffusion calculation.

    Layer uniformity is governed by melt-viscosity ratio. The naphthalate-containing stream has a higher viscosity than PET at equivalent melt temperature. Capillary rheometry under ISO 11443 at 280 °C and 1000 s⁻¹ is used to compare melts. If the viscosity ratio of the PENSTAR 2389 stream to PET exceeds 1.5:1, the barrier layer may wander toward the inner or outer surface in the preform sidewall; below 1.1:1, the layer may become discontinuous near the gate. Hot runner manifold temperatures are therefore set asymmetrically: 290–300 °C for the barrier channel and 265–275 °C for the PET channel. The two melts are kept in separate channels until the last possible point to reduce residence time in the higher-temperature stream.

    In monolayer extrusion, the higher melt temperature and slower crystallization of PENSTAR 2389 require different downstream handling than PET. Chill-roll temperatures for sheet are typically maintained at 15–30 °C to quench an amorphous sheet. If roll temperature exceeds 30 °C, the sheet may develop crystallization-induced haze and uneven gauge due to sticking. In blow molding, preform reheat oven power must be increased relative to PET because the resin has lower infrared absorption in certain wavelength bands; preform surface temperature is set 2–4 °C higher than PET for the same stretch ratio. The exact reheat profile is machine-dependent and must be developed with a thermal camera.

    Sheet coextrusion with PENSTAR 2389 as a cap or core layer requires attention to melt-temperature differences at the die. The higher melt viscosity can create edge encapsulation defects if the die exit melt temperatures differ by more than 10 °C. The extruder screw for the naphthalate layer should have a lower compression ratio than the PET extruder, and a gear pump is recommended to stabilize output at layer percentages below 10%. At high line speeds above 80 m·min⁻¹, the sheet edge may show draw resonance; raising the barrier layer die temperature to 300 °C can reduce the instability but increases monomer formation.

    For injection-molded articles, the mold surface temperature influences crystallinity. With a mold temperature below 20 °C, the part remains substantially amorphous and transparent; with a mold temperature of 120–130 °C and holding times of 15–30 s, the part develops crystallinity and improved heat resistance. Gates should be located to avoid jetting because the higher melt viscosity can produce flow marks in thin sections. A valve-gated hot runner with a gate diameter of 0.8–1.2 mm is used for transparent parts.

    Common failure modes on production lines include brittle gate regions from moisture or excessive residence, off-center barrier layers from viscosity mismatch, preform base splay from excessive hot runner decompression, and yellowing from hot spots above 300 °C. Each failure is diagnosed by measuring moisture, intrinsic viscosity, layer distribution, and color; process adjustments are made against the production record rather than inferred from laboratory samples alone.

    Quality-control methods for naphthalate-containing copolyester conversion
    Property or process variableMethod or standardApplication link
    Intrinsic viscosityASTM D4603Controls molecular weight retention and mechanical strength
    Melt viscosity ratioISO 11443Determines co-injection layer uniformity
    Residual moisture after dryingASTM D6869Defines hydrolytic degradation threshold
    Oxygen permeability coefficientASTM D3985Sets shelf-life and barrier-layer thickness
    Carbon dioxide permeability coefficientASTM D1434Retains carbonation in beverage containers
    Heat deflection temperatureASTM D648Evaluates hot-fill and service temperature limits
    DensityASTM D1505Used for crystallinity calculation and feed blending
    Tensile properties at breakASTM D638-14Confirms oriented and unoriented structural strength
    Instrumented impactISO 6603-2Characterizes drop impact and delamination failure

    Food-contact use of PENSTAR 2389 requires a written compliance statement from the resin producer and a migration assessment under Regulation (EU) No 10/2011 using the intended contact simulant and time-temperature conditions. The resin should not be assumed to be automatically equivalent to PET under 21 CFR 177.1630; naphthalate-containing polyesters may be covered by distinct food-contact notifications or authorizations in the United States. For pharmaceutical and diagnostic packaging, extractables testing under USP <661> and USP <665> may apply depending on dosage form. Final container manufacturers bear responsibility for migration testing and for volatile or color transfer to the packaged product.

    The grade is not compatible with certain oxygen-scavenging additives that release formaldehyde or with amine-based additives that can attack the ester linkage at melt temperature. Steam sterilization above 121 °C should be validated on the finished part, because post-mold crystallization and stress relaxation can reduce retained burst strength. For technical articles outside packaging, the material may be injection molded in tools heated to 120–130 °C to develop crystallinity; sections thicker than 3 mm require packing times of at least 6 s to avoid surface sinks. Thermal annealing at 150–160 °C for 30 min under nitrogen can improve heat deflection but may increase haze depending on wall thickness and cycle parameters.

    Top