| HS Code | 363611 |
| Productname | Huacheng New Material HuaCheng PEN PEN Resin HC-PEN-1000 |
| Manufacturer | Huacheng New Material |
| Materialtype | Polyethylene naphthalate (PEN) resin |
| Grade | HC-PEN-1000 |
| Form | Pellets |
| Color | Natural/amber |
| Density | 1.36 g/cm3 |
| Meltingpoint | 265-270 °C |
| Glasstransitiontemperature | 120-125 °C |
| Intrinsicviscosity | 0.90-1.00 dL/g |
| Tensilestrength | 80-90 MPa |
| Elongationatbreak | 3-10% |
| Flexuralmodulus | 3.0-3.5 GPa |
| Heatdeflectiontemperature | 100-110 °C |
| Waterabsorption | <0.1% |
| Moldshrinkage | 0.2-0.5% |
| Dielectricconstant | 3.0-3.2 at 1 MHz |
| Volumeresistivity | >1E15 ohm·cm |
As an accredited Huacheng New Material HuaCheng PEN PEN Resin HC-PEN-1000 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | HC-PEN-1000 resin is supplied in 25 kg sealed, moisture-proof fiber drums with inner liners and batch labels. |
| Container Loading (20′ FCL) | Huacheng New Material HuaCheng PEN Resin HC-PEN-1000 is securely loaded into a 20′ FCL container for export, with proper packing and handling. |
| Shipping | Ship Huacheng PEN Resin HC-PEN-1000 in sealed, moisture-resistant bags or drums. Transport in a cool, dry, ventilated area, protected from sunlight, heat, moisture, and contamination. Label clearly, include SDS and shipping documents, and verify UN/transport classification and local regulations before dispatch. |
| Storage | Store Huacheng New Material HuaCheng PEN PEN Resin HC-PEN-1000 in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed in original packaging, protect from moisture and physical damage, and separate from incompatible materials. Use appropriate PPE and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Typically 12 months in original sealed packaging under cool, dry conditions, away from sunlight and moisture; confirm with supplier. |
Competitive Huacheng New Material HuaCheng PEN PEN Resin HC-PEN-1000 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Huacheng New Material HuaCheng PEN PEN Resin HC-PEN-1000 is a thermoplastic polyethylene naphthalate supplied in pellet form. The grade is designated for injection moulding, extrusion, and blow-moulding applications in which thermal rigidity, low gas transmission, and resistance to hydrolytic ageing after correct drying are required. Product-specific values for HC-PEN-1000 are not fully published in this summary; therefore, the physical and rheological data provided below are representative polyethylene naphthalate resin-class values that should be confirmed against producer certificates of analysis and technical datasheets. The principal differentiation of HC-PEN-1000 is its combination of higher glass transition temperature, ultraviolet filtration, and gas barrier relative to conventional PET and PBT polyesters.
Oxygen permeability coefficient of the polyethylene naphthalate resin class is commonly reported at 1.0–1.5 cm³·mm/(m²·day·atm) under dry conditions at 23°C and 0% relative humidity when measured according to ISO 15105-2:2014. Under the same test atmosphere, PET homopolymer references typically fall in the range of 3.0–5.0 cm³·mm/(m²·day·atm). The barrier advantage narrows at elevated relative humidity because polyester oxygen transmission increases with matrix plasticization, but published polyethylene naphthalate film data still show lower oxygen flux than PET at 85% relative humidity. Carbon dioxide and water-vapour transmission coefficients for the PEN class follow the same permeability ranking, although HC-PEN-1000-specific values are limited and should be obtained from the producer. Water-vapour transmission rate of the PEN class is lower than PET, but product-specific values at 38°C and 90% relative humidity should be measured by ISO 15106-2. Ultraviolet transmission measurements show a sharp absorption edge near 380 nm, which reduces 320–380 nm UV-A flux through package walls. This characteristic differentiates HC-PEN-1000 from standard PET, whose absorption edge is near 320 nm; the effect should not be interpreted as complete ultraviolet protection unless the finished wall thickness and additive package are tested by spectroradiometric methods such as ASTM E903.
| Property | Test method | PEN resin class | PET reference | PBT reference |
|---|---|---|---|---|
| Specific gravity | ISO 1183-1:2019 | 1.36 g/cm³ | 1.34 g/cm³ | 1.31 g/cm³ |
| Glass transition temperature | ISO 11357-2:2020 | 118–125°C | 78–82°C | 45–60°C |
| Melting temperature | ISO 11357-3:2018 | 265–270°C | 245–255°C | 220–225°C |
| Tensile modulus | ISO 527-2:2012 | 2.0–2.5 GPa | 2.0–2.3 GPa | 1.5–2.0 GPa |
| Oxygen permeability coefficient | ISO 15105-2:2014 | 1.0–1.5 cm³·mm/(m²·day·atm) | 3.0–5.0 cm³·mm/(m²·day·atm) | 5.0–8.0 cm³·mm/(m²·day·atm) |
| Heat deflection temperature at 0.45 MPa | ISO 75-2:2013 | 120–150°C | 115–120°C | 115–130°C |
In comparison with polybutylene terephthalate, the polyethylene naphthalate backbone gives HC-PEN-1000 class a higher glass transition temperature and lower gas permeability but also slower melt crystallization. A direct drop-in substitution of HC-PEN-1000 into a PBT tool is therefore not supported without re-evaluating mould temperatures, gate size, and cycle-time limits. Against PET, the primary differences are a shift of glass transition temperature by approximately 40°C, a longer melt crystallization half-time, and a reduction of oxygen permeability by a factor of 3–5. These differences translate into higher hot-fill resistance and longer flavour-retention potential, but require higher processing temperatures and stricter drying control.
Because melt viscosity and molecular weight control downstream process stability, the producer certificate of analysis for HC-PEN-1000 should report intrinsic viscosity measured in 60/40 phenol/1,1,2,2-tetrachloroethane according to ISO 1628-5:2015, carboxyl end-group concentration, pellet moisture, and colour coordinates. Melt mass-flow rate may be reported under a specified load and temperature according to ISO 1133-1:2022; the exact parameters must be shown on the certificate because a single MFR value without test temperature is not comparable. Batch-to-batch melt viscosity variation should be monitored by intrinsic viscosity and MFR because small shifts in polyester molecular weight alter injection pressure and film gauge. Published data for HC-PEN-1000-specific melt density and extensional rheology are limited.
Glass transition temperature of the PEN class is measured by differential scanning calorimetry according to ISO 11357-2:2020 and typically lies between 118°C and 125°C. This property supports dimensional stability in hot-fill containers where wall sections are subjected to 85°C to 95°C filling media, provided that part crystallinity and wall thickness are validated by finished-article burst and vacuum testing. Tensile modulus measured by ISO 527-2:2012 is in the range of 2.0–2.5 GPa for the resin class; creep and stress relaxation under load should be evaluated for specific part geometries. Because polyethylene naphthalate crystallizes more slowly than PET, thermal crystallization of injection-moulded parts depends strongly on mould temperature and cooling rate. Published literature indicates that lower mould temperatures below 80°C produce largely amorphous parts with lower short-term heat deflection temperature, while mould temperatures above 120°C increase crystallinity and improve dimensional stability but extend cycle time. HC-PEN-1000-specific crystallization kinetics must be obtained from producer differential scanning calorimetry data.
Prior to melt processing, HC-PEN-1000 pellets should be dried in a desiccant dryer to a moisture content of 50 ppm or lower, measured by an in-line moisture analyzer or Karl Fischer titration. The resin class usually requires a hopper air temperature of 150°C to 160°C for 5–6 h, with a regeneration dew point of -40°C or lower. In a twin-screw extruder with an L/D ratio between 32:1 and 40:1, barrel settings for polyethylene naphthalate are generally ramped from 270°C at the feed zone to 290–310°C at the metering zone; HC-PEN-1000 melt temperature must follow producer guidance because melt viscosity and shear heating vary by lot. Residence time above 310°C should be limited because polyester degradation can reduce intrinsic viscosity and generate volatile by-products. On injection moulding machines, barrel temperatures in the upper range are used with a mould temperature of 120°C to 160°C when dimensional stability is critical. Clamp force requirements should be calculated from part projected area; for high-Tg polyester grades, a reference range of 0.6–0.8 t/cm² of projected area is often used, but this does not replace cavity-specific pressure analysis. Gate size should be increased relative to PET because the higher melt viscosity of polyethylene naphthalate creates greater pressure drop. Hot-runner tips and valve gates should have thermocouple control capable of 320°C continuous operation; open nozzle designs may cause stringing or drool if the melt temperature exceeds 310°C. Screw recovery speed should be set to avoid adiabatic shear heating that drives melt temperature beyond the producer maximum. Failure modes caused by insufficient drying in polyester processing lines include surface splay, screw surging, and reduced intrinsic viscosity in purged melt; these observations indicate moisture exposure during melt conversion rather than an off-specification material.
On biaxial film lines, sequential stretching at longitudinal draw ratios of 2.5–3.5 and transverse draw ratios of 3.0–4.0 is typical for polyethylene naphthalate films, but HC-PEN-1000-specific drawability must be verified on cast roll and tenter equipment. Cast roll temperatures below 25°C may produce quasi-amorphous film that tears during transverse stretching if molecular orientation is insufficient. Film and sheet converters should measure final crystallinity and oxygen transmission on a finished-article basis because orientation and heat setting alter permeability relative to resin pellet data.
Masterbatches and processing aids formulated for PET may be thermally unsuitable for HC-PEN-1000 because the processing window of polyethylene naphthalate is higher by approximately 20–30°C. Additive systems containing free amine groups should be screened for melt-phase aminolysis reactions that can reduce molecular weight during compounding. Flame-retardant packages tested on PBT should not be assumed to transfer without changes in melt viscosity and tensile elongation. The producer should be consulted for approved slip, antistatic, and colorant packages compatible with HC-PEN-1000 melt temperature and residual moisture sensitivity.
For food-contact applications, HC-PEN-1000 may be subject to FDA 21 CFR 177.1630 for polyester resins if the producer has supporting compositional and migration data; conditions of use and food types must be set out in a specific declaration. European compliance should be supported by migration testing according to EN 1186-1 and EN 13130-1, together with the final article’s overall migration limit of 10 mg/dm² or 60 mg/kg depending on packaging form. Electrical and electronic applications require RoHS Directive 2011/65/EU Annex II review for lead, mercury, cadmium, and hexavalent chromium restrictions. REACH registration status for the substance or article must be verified with Huacheng New Material before import. The absence of a producer declaration for a specific use should be treated as a documentation gap, not a technical failure.
HC-PEN-1000 is intended for evaluation in hot-fill rigid containers, retortable trays, technical films, and electronic films where polyester-grade heat resistance and gas barrier are required. Retortable trays made from HC-PEN-1000 should be evaluated after retorting at 121°C for 30 min; the test protocol should measure tensile impact retention, top-load at 85°C, and barrier retention after retort. Printed and laminated structures should be tested for ink adhesion under ASTM D3359-17 and heat-seal strength under ASTM F88/F88M-21. Dimensional stability after hot filling must be confirmed by thermoforming trials with cavity temperature control and by top-load testing on filled containers. Published data for long-term hydrolysis resistance of HC-PEN-1000-specific finished articles are limited; accelerated ageing conditions should be designed according to the intended sterilization or retort cycle and validated on production tooling.