| HS Code | 127696 |
| Chemicalcomposition | Polylactic Acid (PLA) |
| Casnumber | 26100-51-6 |
| Appearance | White to off-white pellets |
| Form | Pellets |
| Density | 1.24 g/cm³ |
| Meltflowrate | 15-30 g/10 min at 210°C/2.16 kg |
| Meltingpoint | 165-180 °C |
| Glasstransitiontemperature | 55-60 °C |
| Crystallizationtemperature | 100-120 °C |
| Llactidecontent | ≥99% |
| Moisturecontent | ≤0.025% |
| Tensilestrength | 60-70 MPa |
| Tensileelongationatbreak | 3-5% |
| Tensilemodulus | 3.0-3.5 GPa |
| Flexuralmodulus | 3.0-3.5 GPa |
| Notchedizodimpactstrength | 20-30 J/m |
| Biobasedcontent | 100% |
| Biodegradability | Industrial compostable |
| Processingmethod | Melt spinning |
| Processingtemperature | 200-230 °C |
| Dryingtemperature | 80-100 °C |
| Dryingtime | 4-6 hours |
As an accredited Futerro PLA Fiber Melt Spinning Fiber-Grade Polylactic Acid Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Futerro PLA Fiber Melt Spinning Fiber-Grade Polylactic Acid Resin is supplied in 25 kg moisture-barrier bags, palletized for transport. |
| Container Loading (20′ FCL) | 20′ FCL loaded with palletized 25 kg bags of Futerro PLA fiber-grade polylactic acid resin, stretch-wrapped and secured for export. |
| Shipping | Futerro PLA Fiber Melt Spinning Fiber-Grade Polylactic Acid Resin is a non-hazardous, solid polymer shipped as pellets in moisture-barrier bags, FIBCs, or cartons. No UN number, hazard class, or special transport requirements apply. Store dry and cool, away from moisture, heat, and ignition sources, following local regulations. |
| Storage | Store Futerro PLA Fiber Melt Spinning Fiber-Grade Polylactic Acid Resin in original sealed packaging in a cool, dry, well-ventilated area. Protect from moisture, heat, direct sunlight, and ignition sources. Keep at 5–30°C and below 50% relative humidity. Avoid acids, bases, oxidizers. Reseal opened bags and follow FIFO. Use within recommended shelf life; avoid prolonged humidity exposure to prevent hydrolysis. |
| Shelf Life | Recommended shelf life is 12 months in unopened original packaging, stored cool and dry, away from moisture, heat, and sunlight. |
Competitive Futerro PLA Fiber Melt Spinning Fiber-Grade Polylactic Acid Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618136850665 or mail to admin@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618136850665
Email: admin@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!