| HS Code | 501698 |
| Product | Formosa Plastics HDPE E924 |
| Material Type | High-Density Polyethylene (HDPE) |
| Melt Mass Flow Rate | 4.0 g/10 min (190°C/2.16 kg) |
| Density | 0.953 g/cm3 |
| Tensile Strength At Yield | 27 MPa (3900 psi) |
| Tensile Strength At Break | 22 MPa (3200 psi) |
| Elongation At Break | 600% |
| Flexural Modulus | 1240 MPa (180,000 psi) |
| Notched Izod Impact | 107 J/m (2.0 ft-lb/in) |
| Vicat Softening Temperature | 127°C (261°F) |
| Heat Deflection Temperature | 82°C (180°F) at 0.45 MPa |
| Hardness Shore D | 65 |
| Environmental Stress Crack Resistance | 1000 h |
| Brittleness Temperature | -70°C (-94°F) |
| Melting Temperature | 134°C (273°F) |
| Water Absorption | <0.01% |
| Dielectric Strength | 500 V/mil (20 kV/mm) |
| Volume Resistivity | >10^16 ohm-cm |
As an accredited Formosa Plastics HDPE E924 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Formosa Plastics HDPE E924 is supplied in 25 kg polyethylene-lined paper bags, securely palletized 40 bags per pallet. |
| Container Loading (20′ FCL) | Formosa Plastics HDPE E924 loaded in 20′ FCL: 25 kg bags on pallets, shrink-wrapped, floor-loaded or palletized to maximize weight. |
| Shipping | Formosa Plastics HDPE E924 is a non-hazardous high-density polyethylene resin, typically shipped as pellets in 25-kg bags, 1,000-kg jumbo bags, or bulk trucks/railcars. Transport and store in clean, dry conditions, away from heat, moisture, sunlight, and contamination. Standard industrial packaging applies; no special transport hazard classification. |
| Storage | Store Formosa Plastics HDPE E924 in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed, palletized, and off the floor to prevent moisture and contamination. Avoid dust generation and prolonged UV exposure. Use first-in, first-out stock rotation. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Formosa Plastics HDPE E924 shelf life: typically indefinite under cool, dry, unopened storage away from sunlight, heat, moisture, and contaminants. |
In multi-cavity thin-wall injection moulding cells producing 250 mL to 500 mL spreadable-fat tubs, dip cups, and press-fit lids, Formosa Plastics HDPE E924 is processed at a nozzle temperature of 210 °C to 230 °C. The mould cooling water is fed at 8 °C to 14 °C with turbulent flow through conformal channels; steel surface temperatures below 10 °C shrink the pin-gate freeze time below 0.8 s and produce rim-side short shots, while surface temperatures above 28 °C create sink marks deeper than 0.05 mm at the central hub. With wall thickness of 0.8 mm to 1.2 mm and flow length of 120 mm to 180 mm, injection velocity is set from 180 mm/s to 350 mm/s and fill time is held at 0.10 s to 0.18 s. Peak cavity pressure is measured with piezoelectric cavity-pressure sensors at 45 MPa to 60 MPa; the holding phase uses 50 MPa to 60 MPa for 1.5 s to 3.0 s. If the integral of cavity pressure over time falls below 18 MPa·s, top-load wall stiffness measured under ISO 12048 drops below the customer minimum of 250 N on a 0.9 mm wall. White dairy tubs are produced with titanium dioxide-based masterbatch at 2 wt% to 4 wt%; at loadings above 5 wt%, the melt viscosity rises and the cavity-pressure integral must be increased by 5 MPa to maintain top load. EVA carrier masterbatch is avoided because it reduces crystallinity and can increase lid warpage. Pre-drying is not normally required; only when silo storage at relative humidity above 60% leads to surface moisture above 0.05 wt% is dehumidified-air drying at 70 °C for 2 h applied. The food-contact status for this segment is verified under FDA 21 CFR 177.1520(c) 3.1a and 3.2a; for EU markets the finished article must meet Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm², using simulant D2 and the Annex III reduction factors for fatty contact. Final articles are single-portion dairy tubs, margarine containers, deli lids, and meal-prep bowls.
Open-head 25 L pails are moulded from E924 on 3800 kN to 5200 kN hydraulic presses with shot weights of 850 g to 1100 g and a sidewall thickness of 2.8 mm to 3.5 mm. The melt temperature is 220 °C to 235 °C, and mould temperature is held between 15 °C and 25 °C; lower coolant temperatures produce cold weld lines at the bail ears and lid lugs. The injection profile uses a screw velocity of 60 mm/s to 100 mm/s for the body and a secondary increase to 120 mm/s when the melt front crosses the handle boss. Back pressure is limited to 0.5 MPa to 1.0 MPa, holding pressure is 55 MPa to 65 MPa, and holding time is 5 s to 8 s per 3.0 mm wall. The pail body and lid are certified as UN 1H2 for packaging group II/III liquids; drop testing is conducted after conditioning at -18 °C for 48 h with a water/antifreeze fill, using a drop height of 1.2 m for PGII. The critical failure location is the vertical weld line at the bail ear because orientation there reduces the frozen stress-bearing cross-section. To move weld lines away from stress concentrations, the gate is located so that the flow front meets at low-stress zones, and radii at the handle boss are maintained at 5 mm minimum. Sidewall thickness variation across the pail of more than ±0.2 mm creates uneven cooling and can shift top-load deformation by more than 15%. Notched impact is verified under ASTM D256-23 at 23 °C; stress crack resistance is measured under ASTM D1693-15 Condition B in 10% Igepal CO-630 at 50 °C. If pigment masterbatch loading exceeds 1.5 wt%, or if regrind tails are used above 15 wt%, low-temperature drop performance must be revalidated because wax-based carriers and shear-modified molecular chains can lower interlamellar strength.
Tamper-evident closures for bottled water, isotonic drinks, and edible oil are moulded from E924 in 48- and 64-cavity valve-gated tools with cycle times under 5 s. The closure shell weight is 2.5 g to 5.0 g, the tamper-band hinge thickness is 0.35 mm to 0.50 mm, and the tamper-evident fracture line is scored to 0.12 mm to 0.18 mm. Melt temperature is 210 °C to 225 °C, mould temperature is 12 °C to 20 °C, and injection velocity is 150 mm/s to 400 mm/s. The gate diameter is 0.8 mm to 1.2 mm; gate land shear rate is calculated to remain below 1.0 × 10⁴ s⁻¹ to avoid high molecular orientation that causes uneven tamper-band breakage. Holding pressure is 40 MPa to 50 MPa for 1.0 s to 1.5 s, and ejection is performed when the band surface temperature is below 60 °C. Removal torque on a 28 mm water closure is typically in the range of 0.8 N·m to 2.0 N·m after 48 h at 40 °C, but the target is closure-design specific and is validated with a digital torque meter under ASTM D3474-19. Stress crack resistance for edible-oil closures is evaluated by immersion in 10% Igepal CO-630 at 50 °C for 48 h under ASTM D1693-15 Condition B; acceptance requires no visual cracking at 5× magnification. The base resin food-contact status is documented under FDA 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011; organoleptic testing on the filled package is required for bottled-water closures because taste and odour transfer depends on the complete cap, liner, and masterbatch system.
In beverage crates, dairy crates, and warehouse totes, E924 is blended with plant regrind tails and sometimes clean post-consumer HDPE. The blend is gravimetrically controlled at the feed throat of a 4000 kN to 8000 kN injection machine. At regrind fractions up to 20 wt%, the melt temperature is raised by 5 °C to 8 °C to compensate for shear-history-induced viscosity shift. Above 20 wt%, low-temperature notched Izod impact under ISO 180/A or ASTM D256-23 at -20 °C may decrease by more than 15% relative to virgin pellets; published data for this specific E924-regrind configuration are limited, so line trials are required. Top-load stiffness is tested under ISO 12048 or ASTM D642-20 at 23 °C and 40 °C; when stacking height exceeds 6 units, hot top load is the governing factor. A typical crate design with 2.5 mm to 3.0 mm sidewalls and 1.0 mm to 1.5 mm rib roots is used. Moisture contamination in regrind above 0.05 wt% creates surface splay; regrind is dried at 80 °C for 3 h when bulk handling has exposed it to ambient humidity. Carbon black masterbatch at 2 wt% to 4 wt% is used for UV-stabilised crates; carbon black loading changes shrinkage, and mould shrinkage in the flow direction is expected to shift from roughly 1.5% to 2.0% in thick sections. Dimensions are validated after 48 h conditioning at 23 °C ± 2 °C and 50% ± 5% RH.
| Application segment | Standard or regulation | Test method / numerical criterion |
|---|---|---|
| Thin-wall dairy packaging | FDA 21 CFR 177.1520(c) 3.1a/3.2a, EU 10/2011 | OML ≤ 10 mg/dm²; top load ≥ 250 N at 0.9 mm |
| UN open-head pails | UN 1H2, ADR/RID/IMDG | Drop at -18 °C from 1.2 m; ASTM D1693-15 Condition B in 10% Igepal CO-630 |
| Tamper-evident closures | FDA 21 CFR 177.1520, EU 10/2011 | ASTM D1693-15 Condition B 48 h; torque retention under ASTM D3474-19 |
| Crates and totes | ISO 12048, ASTM D256-23, ISO 180/A | Notched Izod at -20 °C; stacking deformation at 23 °C and 40 °C |
| Toys and housewares | EN 71-3:2019, ASTM F963-23, CPSIA Section 108 | Soluble element migration; phthalates ≤ 0.1% |
| Structural foam pallet feet | ASTM D1622, ISO 844, ISO 8611-1 | Density reduction 15% to 30%; compressive strength at 10% strain |
Moulded toy blocks, storage bins, food-scoop handles, and appliance housings are processed from E924 on 800 kN to 1600 kN presses with polished or SPI A2 textured cavities. The wall thickness is 1.8 mm to 2.5 mm; rib roots are limited to 50% of adjacent wall thickness to avoid sink marks visible after painting or printing. Melt temperature is 190 °C to 210 °C; mould temperature is kept at 25 °C to 35 °C to improve surface replication. Cooling time is 8 s to 12 s for a 2.0 mm wall; ejection is delayed until the surface temperature is below the heat deflection temperature measured at 0.45 MPa under ASTM D648-18, which for HDPE is in the range of 70 °C to 80 °C. Toy-grade E924 is checked against EN 71-3:2019 for migration of soluble elements; as an unpigmented base polymer it does not contribute regulated heavy metals above background, but masterbatch and mould-release agents must also pass. ASTM F963-23 and CPSIA Section 108 phthalate limits of 0.1% per listed phthalate apply to the finished article. The resin supplier should provide a statement of composition for FDA 21 CFR 177.1520 when the item is intended as a mouthed toy; this statement covers only the base resin, not the finished article.
Low-pressure structural foam moulding of E924 into pallet feet, dunnage trays, and collapsible bulk bins uses 0.5 wt% to 1.5 wt% endothermic chemical foaming agent, typically sodium bicarbonate/citric acid pelletized in a polyolefin carrier. The melt is kept at 190 °C to 205 °C to prevent premature gas evolution in the feed zone; the screw is a 24:1 L/D low-shear mixing design. The shot size is set to 70% to 90% of the solid-mould shot weight; expansion packs out wall sections of 10 mm to 15 mm. Foam density reduction is 15% to 30% measured by ASTM D1622; compressive strength of the cellular core is tested under ISO 844 at 10% strain. The swirl surface generated by low-pressure foaming limits this application to non-appearance, non-food-contact parts. Load-bearing components are validated under ISO 8611-1 for pallet systems; E924 in structural foam is not suitable for food contact because chemical foaming agent residues and the open-cell surface are not cleared under FDA 21 CFR 177.1520 unless the converter obtains specific end-article testing.
Competitive Formosa Plastics HDPE E924 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Formosa Plastics HDPE E924 is a high-molecular-weight high-density polyethylene supplied for extrusion blow moulding of large, thick-walled parts in which parison hang time, environmental stress-crack resistance, and wall-thickness control determine process viability. The grade is polymerised as an ethylene-hexene-1 copolymer; the short-chain branch population reduces crystalline density and lamellar thickness relative to an ethylene homopolymer, shifting solid-state behaviour toward slow-crack-growth resistance rather than maximum flexural stiffness. The nominal density is 0.953 g/cm³ measured by ASTM D1505 or ISO 1183-1. The melt mass-flow rate is 0.30 g/10 min at 190 °C under 2.16 kg load in ASTM D1238 or ISO 1133-1. The corresponding high-load melt index is approximately 10 g/10 min at 21.6 kg, producing a shear-thinning ratio near 33:1. This ratio indicates that E924 has high low-shear viscosity for parison stability and considerably lower apparent viscosity at die-wall shear rates.
At 23 °C, representative tensile yield strength for E924 is approximately 28 MPa under ASTM D638, elongation at break exceeds 600 %, and flexural modulus is near 1,100 MPa under ASTM D790. The grade exhibits a Vicat softening temperature of approximately 126 °C under ASTM D1525 and a brittleness temperature below -75 °C under ASTM D746. Environmental stress-crack resistance under ASTM D1693 Condition B, 100 % Igepal CO-630 at 50 °C commonly exceeds 1,000 h for high-molecular-weight HDPE of this density; lot-specific values for E924 should be obtained from the certificate of analysis. These values are not specification limits and are sensitive to specimen preparation, conditioning according to ASTM D618, and test speed.
Parison programming for E924 differs from programming for a 0.70–1.0 g/10 min medium-molecular-weight HDPE grade because low-shear viscosity is larger and molecular relaxation time is longer. In accumulator-head blow moulding, melt is discharged through the die during a shot, and the unsupported parison sags between die and mould. Sag rate is inversely related to zero-shear viscosity and extensional viscosity; E924 reduces sag, allowing longer parison length for large containers and deeper draw ratios. The compensating effect is an increase in die swell. At the same die gap and melt temperature, E924 exits the die with greater annular wall thickness and larger diameter than a lower-molecular-weight HDPE. If the die gap is not corrected, the parison becomes over-thick at the pinch-off region, increasing pinch-weld mass, entrapped air, and flash. The die gap is often widened by 10–20 % relative to a 0.70 g/10 min grade to maintain the same target part weight, although the exact correction is tooling-dependent.
The long relaxation time of E924 also delays the parison response to mandrel movement. Transients in die gap position do not produce instantaneous changes in local wall thickness. The programmer curve is therefore shifted earlier in the shot so that wall-thickness reductions intended for the lower part or shoulder occur before the corresponding parison section exits the die. Short-shot studies and parison weight mapping are required to calibrate the programmer for new tooling. This behaviour is more pronounced than with low-density polyethylene or medium-molecular-weight HDPE.
The product difference extends to solid-state performance. Compared with a 0.957 g/cm³ HDPE blow moulding grade of 0.70 g/10 min melt index, E924 has lower density and lower crystallinity. The lower density reduces flexural modulus but increases environmental stress-crack resistance in the presence of surfactants, oils, and agricultural chemicals. Under ASTM D1693 Condition B, 100 % Igepal CO-630 at 50 °C, high-molecular-weight HDPE of this density often exceeds 1,000 h; lower-molecular-weight grades can fail earlier, though exact values vary with notching, orientation, and residual stress. This difference is the primary reason E924 is selected for large industrial containers and chemical packaging rather than small thin-wall bottles.
E924 is processed on single-screw extruders with length-to-diameter ratios of 24:1 to 32:1. A barrier screw with a Maddock or spiral mixing section is preferred because the high viscosity of the resin can leave unmelted polymer in the metering zone when a general-purpose screw is used. Barrel temperature profiles are ramped from 170–190 °C in the feed zone to 210–220 °C in the metering zone. Head and die temperatures are normally set at 200–220 °C. The measured melt temperature at the die exit should remain between 200 °C and 230 °C. Melt temperatures above 230 °C for prolonged hold-up cause oxidative chain scission and reduce extensional viscosity; the resin then exhibits increased sag and lower ESCR in the finished part. Melt temperatures below 190 °C raise die-head pressure, promote surface melt fracture or sharkskin, and weaken pinch-weld strength.
The accumulator fill rate controls shear rate and melt pressure. On a 90 mm extruder with 30:1 L/D, high-viscosity charge can limit screw speed through motor amperage rather than screw rpm. Melt pressure at the die entrance is commonly maintained within 15–30 MPa; fluctuations above 5 % of setpoint indicate pressure-drop changes at the screen pack or inconsistent feed. A screen pack of 40–80 mesh is typical for clean, unpigmented E924; finer packs can create excessive shear and pressure. When the machine reaches torque limit before the required shot weight, the die gap is widened or the melt temperature is increased within the permitted window. If the problem persists, a screw with a lower compression ratio or deeper metering channel is used.
Blow air pressure of 0.5–0.8 MPa and mould temperatures of 10–20 °C are suitable for large parts. Chilled water at 5–10 °C maintains mould surface temperature under continuous cycling. Cooling time is heat-transfer limited and increases with wall thickness; for wall thickness above 6 mm, cycle time rises approximately with the square of wall thickness. Mould cooling circuits must be balanced to avoid hot spots above 25 °C, which can cause sink marks, post-mould shrinkage, and warpage in thick sections.
Start-up purging uses a lower-viscosity LDPE or HDPE until the barrel, head, and die are thermally stable. PVC or strongly acid-generating purging compounds should not be used because hydrogen chloride released from PVC degradation accelerates polymer oxidation and corrodes tooling. The grade does not require pre-drying when stored in dry conditions; if moisture condensation is present or relative humidity exceeds 60 %, the resin should be dried at 70–80 °C for 2–4 h to prevent splay and pinholes.
Substitution into existing tooling designed for a lower-viscosity 0.70 g/10 min HDPE is not a direct drop-in. The first difference observed on the production line is parison weight increase at unchanged die gap because E924 swells more and sags less. This changes the parison programming baseline; flash may increase at the parting line and the pinch weld may become thicker. The die gap is usually widened by 10–20 %, but the value is established by weighing the parison at several programmed points across the shot.
The second difference is pressure response. E924 has higher viscosity at low shear, so the extruder can draw more motor current and generate higher melt pressure at the same screw speed. Older machines with fixed-speed AC motors may not reach the screw speed required for the target shot size. Excessive backpressure above 35 MPa is generally unnecessary and can degrade the stabiliser package. If melt pressure is too high, raising melt temperature within the 200–230 °C window is safer than increasing screw speed until torque limit is reached.
The cooling load increases when a thicker-walled E924 part is produced in the same mould. Mould cooling circuits may be insufficient because E924 is selected for applications requiring greater wall thickness or improved ESCR, both of which often result in more retained heat. Cycle-time increases are not unique to E924 but follow heat-transfer scaling. Reducing mould temperature below the dew point can create condensation and surface defects, so the mould temperature should remain at 10–20 °C rather than overcooling the cavity.
Compared with lower-molecular-weight HDPE grades used for small containers, E924 offers higher environmental stress-crack resistance and greater parison melt strength, but with lower screw output, higher die-head pressure, and longer cooling cycles. Compared with homopolymer HDPE of similar melt index, the hexene-1 copolymer composition of E924 reduces density and flexural modulus while increasing crack resistance. Published data for this specific configuration is limited for direct substitution; production-scale trials with shot-weight mapping and ESCR verification are therefore required before locking the process.
Compliance of HDPE E924 with regulatory standards depends on the finished article, not only on the pellet. The table summarises the typical boundaries to be verified for blow moulded articles.
| Regulation or standard | Clause or test method | Boundary condition |
|---|---|---|
| U.S. FDA olefin polymers | 21 CFR 177.1520 | Applies to articles made from olefin polymers when extractives and density specifications of paragraph (d) are met; resin lot must be evaluated for the intended temperature and food type. |
| EU food-contact framework | Regulation (EC) No 1935/2004 | Finished article must not transfer constituents above migration limits in EU 10/2011; compliance is not conferred by resin composition alone. |
| EU REACH SVHC screening | Regulation (EC) No 1907/2006 | Resin as supplied is typically below 0.1 % w/w for listed substances of very high concern; downstream formulations must be re-screened. |
| RoHS restricted substances | Directive 2011/65/EU as amended by (EU) 2015/863 | Unmodified HDPE typically falls below homogeneous-material thresholds for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE; flame-retardant or conductive modifiers require verification. |
| Migration testing protocols | EN 1186 series / EU 10/2011 | Overall migration and specific migration limits depend on food simulant, contact time, temperature, and article surface-to-volume ratio. |
Operational boundaries for E924 are primarily thermal and moisture-related. Avoid holding the resin above 230 °C for more than 15–20 min in the head and accumulator; unavoidable shutdowns should be followed by purging. Regrind from clean, unpigmented production can be reused, but the percentage must be validated by ASTM D1238, ASTM D1693, and part drop-impact or wall-thickness capability, because repeated heat history reduces molecular weight and ESCR. Avoid blending with low-molecular-weight polyethylene waxes at concentrations that reduce parison strength; these additives may be present in processing aids and should be evaluated separately.