| HS Code | 522516 |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.955 g/cm³ |
| Melt Index 190 C 2 16 Kg | 0.35 g/10 min |
| Tensile Strength At Yield | 26.2 MPa |
| Tensile Strength At Break | 31.0 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 1.24 GPa |
| Vicat Softening Point | 127 °C |
| Brittleness Temperature | -70 °C |
| Environmental Stress Crack Resistance Escr | >1000 h |
| Hardness Shore D | 66 |
| Thermal Conductivity | 0.45 W/m·K |
| Water Absorption | <0.01% |
| Dielectric Constant | 2.3 |
| Dielectric Strength | 20 kV/mm |
| Volume Resistivity | 1e16 ohm·cm |
As an accredited Formosa Plastics HDPE AC5502 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Formosa Plastics HDPE AC5502 is packaged in 25 kg (55.1 lb) bags, palletized with 40 bags per pallet. |
| Container Loading (20′ FCL) | 20′ FCL loads 20 pallets; each pallet has 55 bags of 25 kg Formosa Plastics HDPE AC5502, shrink-wrapped and secured. |
| Shipping | Formosa Plastics HDPE AC5502 ships as a non-hazardous polyethylene resin in 25 kg polyethylene-lined bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks. Protect from moisture, heat, sunlight, and contamination. Standard dry-van or container shipment is suitable. No UN hazard class required. |
| Storage | Store Formosa Plastics HDPE AC5502 in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep in original unopened bags or containers, palletized off the floor, and protect from moisture, dust, oils, and other contaminants. Avoid prolonged UV exposure and extreme temperatures. Follow local regulations and the manufacturer’s SDS recommendations. |
| Shelf Life | Two years from manufacture when stored in original packaging in a cool, dry area away from direct sunlight and heat. |
For 220 L closed-head and open-head chemical drums, AC5502 is processed as a high-molecular-weight blow molding grade with a nominal melt index of 0.25 g/10 min under ASTM D1238-20 at 190 °C/2.16 kg and a density of 0.955 g/cm³ under ASTM D1505-18. The primary process conflict on accumulator-head machines arises from the combination of a parison mass of 6–9 kg and a low melt-flow index, which produces high parison swell and significant sag if melt temperature exceeds 205 °C. Production-scale observation on 80–120 mm screw diameters with 25:1–30:1 L/D barrier screws shows that rear barrel temperatures below 170 °C increase screw torque and reduce plasticating capacity, while front zones above 210 °C lower melt strength and create wall-thickness variation greater than ±5 % across the parison length. A 10–30 point parison programmer is therefore used to correct the radial wall profile, and the die gap is typically set between 2 mm and 5 mm depending on shot mass and swell ratio. Closed-loop mold temperatures of 10–25 °C are maintained to stabilize shrinkage; cooling time for a 220 L closed-head drum is generally 90–180 s, with longer cycles required when internal cooling air is not applied at 2–5 bar. Sustained melt temperatures above 230 °C initiate molecular weight reduction and an irreversible loss of environmental stress crack resistance. The formulation addition ratio for first-life UN packaging is 100 wt% AC5502 when the filling substance is in Packing Group I, while clean in-house regrind from the same drum line is often re-introduced at 20–30 wt% for Packing Group II and III products after re-qualification under UN drop and hydraulic pressure tests. Colour masterbatch is added at 1.5–2.5 wt%, and outdoor storage requires an ultraviolet stabilizer package at 0.15–0.35 wt%. Compliance for the finished container is set by UN 1H1/Y and 1H2/Y design-type approval under 49 CFR 178.504, ADR Chapter 6.1, and IMDG Code 6.1; the resin must also meet the chemical inventory obligations of REACH Regulation (EC) No 1907/2006 and the heavy-metal restrictions of RoHS Directive 2011/65/EU where applicable. Terminal product types include 120 L, 150 L, and 220 L open-head and closed-head drums for liquid and solid chemicals, as well as 20–30 L jerrycans designated under UN 3H1/Y and 3H2/Y.
Monolayer agricultural chemical containers based on AC5502 are typically produced with a virgin resin content of 95–98 wt%, with the balance comprising a polyethylene-compatible colour/UV masterbatch at 2–4 wt%; internal post-industrial regrind is limited to 10–15 wt% for solid formulations and is generally excluded for emulsifiable concentrates or solvent-based herbicides because cumulative heat history reduces environmental stress crack resistance. The governing compliance route is UN 3H1/Y for closed-neck plastic jerrycans and bottles through 49 CFR 178.509 and ADR 6.1, while single-use agricultural pesticide containers fall under 40 CFR 165.25 and refillable containers under 40 CFR 165.27 in the United States. Process conditions on continuous shuttle blow molding machines with 60–80 mm extruders and 24:1 barrel length typically place melt temperatures at 180–200 °C, with die heads held 10–15 °C below the melt temperature to raise viscosity and control parison elongation. Parison swell for this high-molecular-weight grade ranges from 25–40 %; without a parison programmer, the pinch-off seams of a 10 L bottle can show wall-thickness deviation greater than ±10 % and fail the drop test at -18 °C. The production process uses blow pins at 4–7 bar and mold cooling water at 10–20 °C. ESCR acceptance is normally benchmarked through ASTM D1693-15 Condition B with an F50 requirement above 600 h for solvent contact, while tensile yield strength is verified by ASTM D638-14 and notched Izod impact by ASTM D256-23. Terminal product types include 1 L, 5 L, 10 L, and 20 L pesticide bottles, closed-neck jerrycans, and graduated dispensing containers for agricultural adjuvants. Where the active ingredient contains high-permeation solvents, AC5502 serves as the structural layer in multi-layer constructions and not as the monolayer barrier; published data for AC5502 as a monolayer barrier against xylene or toluene is limited and replacement with a polyamide or EVOH interlayer is required.
| Application segment | Primary compliance framework | Critical test or method | Typical AC5502 addition | Terminal article class |
|---|---|---|---|---|
| UN chemical drums and jerrycans | UN 1H1/Y, 1H2/Y, 3H1/Y, 3H2/Y; 49 CFR 178.504; ADR 6.1 | ASTM D1693-15 ESCR, UN drop and hydraulic pressure | 100 wt% first-life; 20–30 wt% clean regrind for PG II/III | 120–220 L drums; 20–30 L jerrycans |
| Agricultural chemical containers | UN 3H1/Y; 49 CFR 178.509; 40 CFR 165.25/165.27 | ASTM D1693-15 Condition B; ASTM D638-14 | 95–98 wt% virgin; 10–15 wt% regrind for solids only | 1–20 L bottles and jerrycans |
| Water and chemical dosing tanks | NSF/ANSI 61; EN 13575:2012; DVS 2205 | EN 13575 hydrostatic and chemical compatibility; ASTM D1693-15 | 100 wt% potable; 10–25 wt% regrind industrial | 200–5,000 L vertical tanks, brine tanks |
| DEF reservoirs and automotive fluid tanks | ISO 22241-3:2017; ISO 16750-3:2012 | ASTM D1693-15; ISO 527-2:2012; hot-plate weld burst test | 90–95 wt% virgin; 15–20 wt% regrind | 10–30 L DEF reservoirs, washer reservoirs |
| IBC inner receptacles | UN 31HA1/Y; IMDG Code 6.5; 49 CFR 178.703 | UN bottom lift, top lift, stacking, vibration; ASTM D1693-15 | 100 wt% first-life; ≤20 wt% clean regrind | 820 L, 1,000 L, 1,250 L liners |
| Stationary chemical storage tanks | EN 13575:2012; DVS 2205; REACH Regulation (EC) No 1907/2006 | EN 13575 leakage; weld-line hydrostatic test | 100 wt% hazardous service; ≤20 wt% regrind non-hazardous | 500–5,000 L vertical tanks |
In large water and chemical dosing tank production, AC5502 is fed as a pre-compounded base resin into single-station accumulator-head machines with 100–150 mm screw diameters and 30:1 L/D grooved-barrel extruders; the low melt index imposes a high pumping pressure of 180–250 bar behind the accumulator head, and screw speed is restricted below 60 rpm to prevent excessive shear heating. For potable water applications, the resin addition ratio remains 100 wt% virgin AC5502 unless the finished tank has separate national approval for regrind; industrial chemical dosing and brine tank production commonly uses 10–25 wt% clean in-house regrind, while outdoor UV resistance is obtained with 2–2.5 wt% carbon black masterbatch and 0.2–0.4 wt% hindered amine light stabilizer. The governing standards are NSF/ANSI 61 for drinking-water contact and EN 13575:2012 for above-ground thermoplastic storage tanks, with design and welding verification handled under DVS 2205 where installed in the European Economic Area; finished part certification must be confirmed against the current resin listing because published data for AC5502 under some mandatory water approvals is limited. The blow molding process uses melt temperatures of 190–205 °C, mold temperatures of 12–20 °C, and cooling fixtures that hold the part for 180–300 s to control post-mold shrinkage. Typical terminal products are vertical cylindrical water tanks from 200 L to 5,000 L, conical-bottom chemical dosing tanks, brine tanks for water softeners, and underground septic tanks where structural loads are managed by external support. Constant internal pressure beyond 0.1 MPa is outside the design envelope unless the cylindrical geometry is reinforced and the weld seams are re-calculated according to DVS 2205.
Under ISO 22241-3:2017 and OEM thermal cycling from -40 °C to 80 °C, diesel exhaust fluid reservoirs made from AC5502 are validated as welded assemblies rather than as raw resin alone; the resin is formulated at 90–95 wt%, with a heat stabilizer and carbon black masterbatch at 5–8 wt% and clean post-industrial regrind limited to 15–20 wt%. The governing material test set includes ISO 527-2:2012 for tensile yield, ISO 178:2019 for flexural modulus, ASTM D1693-15 Condition B for environmental stress crack resistance, and ISO 16750-3:2012 for mechanical vibration on the complete reservoir. Production equipment is typically a 80 mm accumulator head with 24:1–30:1 L/D screw geometry and a suction blow molding or three-dimensional parison manipulation system for complex underhood envelopes; melt temperature is held at 190–205 °C, mold temperature at 10–20 °C, and pinch-weld sections are cooled locally to reduce post-weld stress. Hot plate welding of bracket bosses and inlet fittings is performed at 200–230 °C with welding pressure below 0.15 MPa; the process bottleneck is weld-line ESCR retention, because the weld zone can lose 10–20 % of the base ESCR value if the melt film is overheated or if the joining force is applied too early. Terminal products include 10–30 L DEF reservoirs, coolant expansion tanks, and windshield washer reservoirs for commercial vehicles and agricultural tractors. This grade is not considered a validated monolayer replacement for pressurized fuel tanks under ECE R34 or SAE J2587 unless fluorination or multi-layer permeation barriers are introduced.
Intermediate bulk container inner receptacles are blown from AC5502 when the filled substance is assigned to UN Packing Group II or III and the transport configuration requires a rigid plastics inner receptacle inside a welded steel cage, designated for shipment as UN 31HA1/Y. The formulation addition ratio for the 1,000 L liner is normally 100 wt% virgin AC5502 at the first manufacturing step; clean in-house regrind from rejected liners or pinch-off flash can be incorporated up to 20 wt% only after the outer cage and the bottle pass the UN bottom lift test, top lift test, and stacking test required under 49 CFR 178.703 and IMDG Code 6.5. The production process uses accumulator-head extrusion blow molding with a shot capacity of 15–25 kg, a 120–150 mm screw, and a 30:1 L/D grooved barrel; melt temperature is maintained at 190–205 °C, and the die gap is widened to 5–8 mm to produce the thick preform needed for a 9–14 kg bottle. Cooling time is 180–300 s with mold water at 10–18 °C, and leak testing is performed at 0.1–0.3 bar before assembly into the steel cage. The largest process failure mode is vertical wall-thickness variation along the parison caused by gravity-driven sag; without a parison programmer, a 1,000 L liner can show bottom corners thinner than 1.5 mm while the top sidewall exceeds 5 mm, creating a low-cycle fatigue crack in the UN vibration test. Terminal product types include 820 L, 1,000 L, and 1,250 L IBC inner bottles for liquid fertilizers, industrial cleaners, water-treatment chemicals, and non-solvent process fluids.
Stationary above-ground chemical storage tanks in the 500 L to 5,000 L range use AC5502 only after the stored medium is classified as non-flammable, non-oxidizing, and compatible with high-density polyethylene through an immersion test matrix under EN 13575:2012 and DVS 2205. The addition ratio for large outdoor tanks is 100 wt% AC5502 when the stored chemical is classified as hazardous to water; non-hazardous service permits up to 20 wt% in-house regrind. Ultraviolet stabilization is achieved with 2–2.5 wt% carbon black masterbatch compounded with the resin, giving a minimum wall thickness of 3 mm for non-structural service and 6 mm where hydrostatic stress increases. Processing occurs on a large accumulator-head blow molder with 150 mm screw diameter, 30:1 L/D barrier screw, melt temperature 195–210 °C, and mold temperature 10–18 °C; because the part is cooled unevenly in thick-wall flange regions, a post-mold cooling fixture is required for 240–360 s to prevent radial shrinkage. The critical defect mode in this segment is weld-line separation at the bottom skirt and nozzle weld zones, which is why the pinch area is blown at a local die gap 15–20 % larger than the nominal wall and the mold is run cold at 10 °C to increase weld strength. Finished tanks are tested under EN 13575 for hydrostatic deformation and chemical compatibility, and leak testing is carried out at 0.05–0.1 bar for 30 min. Terminal products include 500–5,000 L vertical storage tanks for waste oil, detergents, agricultural adjuvants, and water-treatment chemicals. Strong oxidizing acids, aromatic solvents, and flammable liquids are outside the safe operating envelope of this construction unless secondary containment and additional barrier liners are used.
Competitive Formosa Plastics HDPE AC5502 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Formosa Plastics HDPE AC5502 is a high-density polyethylene resin supplied as cylindrical pellets for extrusion and molding operations where a combination of moderate stiffness, melt strength, and environmental stress-cracking resistance is required. The grade is produced by a low-pressure catalytic polymerization process and is characterized by a nominal density near 0.955 g/cm³ and a melt flow index of 0.30 g/10 min under ASTM D1238 / ISO 1133-1:2022 conditions at 190 °C with a 2.16 kg load. The product designation AC5502 is a supplier-specific identifier; the numeric segment is commonly understood in the industry as identifying the density and flow class, but the engineering performance of the grade is defined by the full technical bulletin rather than by the designation alone.
Unlike high-flow HDPE injection molding grades with melt indices between 5 g/10 min and 20 g/10 min, AC5502 is intended for high-molecular-weight processing regimes: sheet, profile, conduit, thermoforming, and non-pressure pipe service. Its difference from general-purpose blow molding and injection molding resins lies in the balance of molecular parameters that control sag resistance, slow crack growth, and long-term creep. The paragraphs below compile specification data, processing boundary conditions, comparative performance, and material incompatibilities that appear in supplier literature and standard test methodologies.
Representative values for Formosa Plastics HDPE AC5502 are reported against the following test designations. These values are not a substitute for a batch-specific certificate of analysis; density and flow rate can vary within the supplier’s release limits. All values below are taken from standard equilibrium or room-temperature conditioning protocols.
| Property | Test method | Nominal value |
|---|---|---|
| Density | ASTM D1505 | 0.955 g/cm³ |
| Melt flow index at 190 °C, 2.16 kg | ASTM D1238 / ISO 1133-1:2022 | 0.30 g/10 min |
| Tensile strength at yield | ASTM D638-14 | 27 MPa |
| Elongation at break | ASTM D638-14 | >800% |
| Flexural modulus, secant 1% | ASTM D790 | 1,100 MPa |
| Notched Izod impact strength at 23 °C | ASTM D256 | 12 kJ/m² |
| Vicat softening temperature, 10 N load | ASTM D1525 | 127 °C |
| Hardness | ASTM D2240 | 64 Shore D |
| Environmental stress-cracking resistance, F50, 100% Igepal | ASTM D1693 | >1,000 h |
| Oxidation induction time at 200 °C | ASTM D3895 | >40 min |
The 0.30 g/10 min melt flow index is low relative to standard blow molding grades and indicates a high molecular weight. The combination of 1,100 MPa flexural modulus and >1,000 h ESCR places AC5502 in a stiffness class that is useful for load-bearing extruded profiles and chemical-resistant sheet. The oxidation induction time of >40 min is a quality-control indicator for antioxidant package retention after pelletization; it is not a continuous-use temperature rating.
Processing of AC5502 follows the thermal profile typical of high-molecular-weight HDPE with a grooved-barrel feed section. Melt temperature is controlled between 190 °C and 220 °C; sustained operation above 230 °C accelerates oxidative chain scission and can reduce the oxidation induction time below the specification floor of 40 min when tested by ASTM D3895. The feed throat is kept below 70 °C to prevent pellet agglomeration in the grooved feed bushing. Screws with an L/D of 24:1 to 30:1 and a compression ratio of 3.0:1 to 3.5:1 are used in sheet and pipe profile lines. Screens of 20/40/60 mesh are installed ahead of the breaker plate to remove gels; pressure drop across a clean screen pack typically remains below 20 MPa. In blown film operations, a die gap of 1.2–1.6 mm and a blow-up ratio between 2.0:1 and 3.0:1 are employed to balance transverse and machine direction tear properties. Pre-drying is not required for virgin resin stored below 60% relative humidity; condensation on pellets stored in unheated silos above 60% relative humidity requires drying at 80 °C for 2 h before extrusion.
Thermoforming sheet made from AC5502 requires high melt stiffness during the sag phase. On single-station shuttle thermoforming machines, the sheet core temperature is held between 130 °C and 145 °C and the pre-stretch rate is limited by the grade’s strain-hardening behavior. The forming window is narrower than that of a random copolymer polypropylene because the onset of sagging and the onset of crystallization occur closer together in the heating curve. Operators report that the usable forming window is approximately 5–8 °C when measured at the sheet surface; published data for this specific configuration is limited, and infrared pyrometer calibration should be verified against a contact thermocouple before establishing the production recipe.
The distinction between AC5502 and a certified PE100 pipe material is defined by long-term hydrostatic strength evaluation under ISO 9080 and classification under ISO 12162. The presence of high ESCR and density near 0.955 g/cm³ does not, by itself, establish the minimum required strength for pressure service. Formosa Plastics application literature for AC5502 identifies non-pressure conduit, profile, sheet, and thermoforming as target sectors; pressure-pipe qualification must be confirmed separately under ISO 4427 or EN 12201 before use.
| Resin category | Melt index (ASTM D1238) | Density (ASTM D1505) | ESCR (ASTM D1693 F50, 100% Igepal) | Typical processing sector |
|---|---|---|---|---|
| HDPE AC5502 | 0.30 g/10 min | 0.955 g/cm³ | >1,000 h | sheet, profile, non-pressure conduit |
| General-purpose HDPE blow molding resin | 0.3–0.8 g/10 min | 0.954–0.958 g/cm³ | 50–200 h | bottles, containers, large-part blow molding |
| PE100 pressure-pipe resin | 0.2–0.4 g/10 min | 0.959–0.963 g/cm³ | >1,000 h | water and gas pressure pipe |
The ESCR of AC5502 is comparable to PE100 grades in the Igepal test, but this does not confer equivalent slow crack growth resistance under sustained internal pressure. PE100 resins are formulated with bimodal or multi-modal molecular weight distributions and specific comonomer placement to resist slow crack growth under hoop stress; AC5502 does not carry the same hydrostatic design basis. For pressure service, the pipe must be qualified under the relevant national standard such as ISO 4427 or EN 12201, and the resin must have a validated minimum required strength. Users must not infer pressure-pipe suitability from ESCR data alone.
When AC5502 is considered for replacement of a general-purpose blow molding resin, the lower melt index and higher molecular weight produce measurable changes in parison behavior and extruder load. The parison hang time increases relative to a resin with a melt index of 0.8 g/10 min, but shear heating in the screw and die also rises. In a grooved-barrel extruder with an L/D of 30:1, head pressure at constant screw speed is commonly 25–35 MPa for high-molecular-weight HDPE of this density class. Drive amperage is therefore expected to be higher than for a lower-viscosity blow molding grade; a definitive substitution trial should monitor melt temperature at the die entry and confirm that the output rate remains within the downstream cooling capacity.
In blow molding, the die swell of AC5502 is greater than that of high-flow injection grades, which affects die gap settings and flash removal. Parison thickness programming may require a different profile than a 0.8 g/10 min resin because the higher melt strength resists sag but also restricts the drawing of the parison. The recommended die gap for large-part blow molding with this viscosity class is typically 1.5–2.5 mm, with a blow air pressure of 0.6–0.8 MPa and mold temperature held at 10–20 °C for rapid solidification. Published data for this specific substitution is limited; the values given here are processing windows commonly cited for high-molecular-weight HDPE blow molding grades.
The substitution of AC5502 into an existing blow molding or sheet line should not proceed without an audit of downstream cooling, screen-pack configuration, and screw geometry. A resin with 0.30 g/10 min melt index generates lower melt flow than typical household and industrial container resins, so thin-wall sections below 2 mm may exhibit incomplete filling or excessive orientation. Injection molding of AC5502 is generally not recommended for thin-wall packaging because the melt index is too low for acceptable cycle times; if injection molding is attempted, gates smaller than 2.0 mm may cause shear-induced melt fracture and delamination at the gate. Melt temperature at the nozzle should be held at 215–230 °C, and mold temperature should be maintained at 20–40 °C for dimensional stability.
The grade differs from a conventional HDPE blow molding resin not only in flow but also in stiffness and environmental stress-cracking performance. Containers made from AC5502 can withstand stress-cracking agents better than many general-purpose blow molding resins, but the higher viscosity may reduce surface gloss and can produce weld lines with lower burst strength unless the die head and mandrel are polished and maintained. Weld-line integrity should be verified by burst testing under ASTM F2057 or an equivalent internal pressure test, and by drop testing at -20 °C when the article is intended for cold-temperature service.
Chemical compatibility and long-term exposure boundaries complete the technical profile. AC5502 is a nonpolar hydrocarbon polymer and is not recommended for continuous immersion in strong oxidizing acids, aromatic hydrocarbons, chlorinated solvents, or fuels containing high concentrations of aromatic compounds. Stress cracking can be accelerated by polar surfactants, alcohols, and certain ester plasticizers, particularly at tensile stress levels above 4 MPa. Contact with ozone, chlorine dioxide, or permanganate solutions at temperatures above 40 °C can initiate oxidative attack and reduce the oxidation induction time below the value observed on virgin pellets. For outdoor service, ultraviolet stabilizers must be added through a compounding step or a selected UV-stabilized concentrate; natural resin does not contain sufficient UV protection for prolonged direct sunlight.
For butt-fusion joining of AC5502 conduit, the interfacial melt bead temperature is controlled at 200–220 °C and the joining force is adjusted to produce a double-rib bead of uniform width. The cooling time in the fusion machine is based on pipe wall thickness and is generally 8–12 min for a wall thickness of 20 mm; pressure data should follow DVS 2207-1 or the equipment manufacturer’s verified parameters. Published data for this specific configuration is limited, so procedure qualification is required.
For food-contact applications, compliance with FDA 21 CFR 177.1520 requires end-use testing of the finished article because processing additives, colorants, and potential contaminants can affect migration performance. The resin supplier may provide a declaration that the virgin grade is suitable for food-contact applications when processed under specified conditions, but this declaration does not cover downstream changes. For European Union applications, the finished article must comply with Regulation (EU) No 10/2011 and its amendments, including overall migration limits and specific migration limits for any additives used. REACH and RoHS compliance applies to the finished component after addition of masterbatch, not to the base resin alone.