Formosa Plastics Hdpe 8050

Formosa Plastics HDPE 8050

    • Product Name: Formosa Plastics HDPE 8050
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 737547
    Density 0.955 g/cm³
    Melt Flow Rate 0.35 g/10 min
    Tensile Strength At Yield 26 MPa
    Tensile Strength At Break 33 MPa
    Elongation At Break 600%
    Flexural Modulus 1170 MPa
    Notched Izod Impact Strength 100 J/m
    Vicat Softening Temperature 127 °C
    Heat Deflection Temperature 75 °C at 0.45 MPa
    Environmental Stress Crack Resistance >1000 h
    Hardness Shore D 65
    Melting Point 130 °C
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >10^16 ohm·cm

    As an accredited Formosa Plastics HDPE 8050 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Formosa Plastics HDPE 8050 is packaged in 25 kg polyethylene-lined paper bags, palletized, and may also be supplied in bulk.
    Container Loading (20′ FCL) 20′ FCL loaded with Formosa Plastics HDPE 8050, 25 kg bags on pallets, shrink-wrapped and strapped for secure export shipment.
    Shipping Formosa Plastics HDPE 8050 is shipped as a non-hazardous, solid polyethylene resin in pellet form. It is not regulated for DOT, IMDG, IATA, or ADR transport. Typical packaging includes 25-kg bags, jumbo bags, boxes, bulk trucks, or railcars. Keep containers closed, dry, and away from excessive heat.
    Storage Store Formosa Plastics HDPE 8050 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags sealed, off the floor on pallets, to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Use first-in, first-out stock rotation. Do not store near food or drinking water. Maintain normal industrial hygiene.
    Shelf Life Typically 24 months when stored sealed in original packaging in cool, dry, ventilated area away from sunlight, moisture, and contamination.
    Application of Formosa Plastics HDPE 8050

    Formosa Plastics HDPE 8050 is an injection-molding high-density polyethylene characterized by a nominal density of 0.950 g/cm³ using ASTM D792-20 and a melt flow index of 8.0 g/10 min under 2.16 kg load at 190 °C according to ASTM D1238-23. The grade is specified only in injection-molded downstream sectors where this melt-flow range supports thin-wall filling and high machine throughput. The following application segments exclude blow molding, film, pipe extrusion, and rotomolding because the melt-flow range and molecular design are not aligned with those processes. Continuous service temperatures above 65 °C are outside the recommended window, and direct contact with aromatic hydrocarbons, chlorinated solvents, or strong oxidizing agents is outside the resin compatibility range.

    Compliance matrix for HDPE 8050 injection-molded application segments
    Application segmentReferenced standardRepresentative condition
    Food-contact thin-wall containersFDA 21 CFR 177.1520, EU 10/2011, GB 4806.7-2016Overall migration ≤ 10 mg/dm²; olefin polymer density specifications
    Screw closuresASTM D2063-12, FDA 21 CFR 177.1520Removal torque after 24 h and 72 h; food-contact end-use conditions
    Open-head pailsUN 1H2, ASTM D1693-15Stack compression 48 h at 40 °C; cold drop 1.2 m at -18 °C
    Structural cratesASTM D1693-15, ISO 179-1:2010ESCR 100% Igepal CO-630 at 50 °C; Charpy notched impact at -20 °C
    Housewares and storage16 CFR 1303, ASTM F963-23Lead ≤ 90 mg/kg; mechanical use and abuse provisions for children's product positioning
    Refuse containersEN 840-1:2020, EN 840-5:2020Dynamic rolling, cold impact, and weathering test sequences

    Thin-wall dairy and deli containers are molded in hot-runner tools where the cavity fill time is controlled below 0.25 s to prevent premature freeze-off at the melt front. The formulation at the hopper is typically 96.0 wt% HDPE 8050, 3.0 wt% white TiO₂-pigmented masterbatch, 0.8 wt% processing aid, and 0.2 wt% hindered phenolic antioxidant; if opacity requirements increase, masterbatch content moves to 4–6 wt% while processing aid remains unchanged. Melt temperature at the nozzle is 210–230 °C, the mold cooling circuit is held at 15–25 °C, and transfer from injection to holding pressure occurs at 92–95% cavity filling. FDA 21 CFR 177.1520 and EU Regulation 10/2011 govern food-contact use; overall migration must not exceed 10 mg/dm² under the intended food simulant and time-temperature condition. GB 4806.7-2016 applies to China-bound food-contact articles. Hot-fill above 60 °C is outside the recommended processing window. Typical output includes 125 g to 500 g dairy tubs, deli containers, and matching lids produced in 16–32-cavity tools.

    What Limits Torque Retention in HDPE 8050 Screw Closures?

    In continuous-thread closure tools with 28 to 38 mm cavities, HDPE 8050 is processed under valve-gated hot-runner conditions where torque retention in the finished cap is governed by erucamide bloom kinetics rather than resin bulk strength alone. Processors run 0.05–0.15 wt% erucamide for initial removal torque control, 0.10–0.20 wt% behenamide when higher-temperature stability is required, 0.05–0.10 wt% antioxidant, and 1.5–2.5 wt% color masterbatch in 48- or 96-cavity valve-gated hot-runner molds. Melt temperature is maintained at 220–240 °C to avoid unmelts while limiting erucamide decomposition. Mold temperature is set to 10–20 °C to reduce cycle time; the closure is not annealed after ejection, so dimensional stabilization continues for 24–48 h as the slip additive migrates. ASTM D2063-12 removal torque is measured after 24 h and 72 h. For food-contact closures, FDA 21 CFR 177.1520 and EU 10/2011 apply; non-food detergent closures are evaluated under REACH. The grade is not recommended for carbonated soft drink closures where continuous internal pressure and cyclic ESCR loading create premature stress cracking at the tamper-evident band hinges. Terminal parts include snap-top lids, continuous-thread beverage caps for non-carbonated products, and household chemical closures.

    Stack Compression Testing Governs Open-Head Pail Cycle Parameters

    Open-head pail manufacturing in the 1 to 6 US gallon range runs wall thicknesses between 1.8 and 2.4 mm because thicker sections increase cycle time without improving cold drop performance. A production blend is 70–80 wt% virgin HDPE 8050, 20–30 wt% closed-loop regrind from trimmed sprues and rejected pails, 1.5–2.5 wt% color masterbatch, and 0.3–0.5 wt% hindered amine light stabilizer when outdoor storage is specified. The material is plasticated in a 1,000–1,600 metric ton clamp injection molding machine with screw L/D of 20:1–22:1 and compression ratio 2.5:1. Melt temperature is 230–250 °C, mold temperature 30–50 °C, and holding pressure is 700–800 bar for 8–12 s. UN 1H2 certification for removable-head plastic drums requires stack compression testing for 48 h at 40 °C and a cold drop at -18 °C; for food-ingredient pails, FDA 21 CFR 177.1520 applies. Handle boss weld lines are the primary failure locations when regrind content exceeds 30 wt%, because repeated extrusion shifts the molecular weight distribution and reduces environmental stress crack resistance. Terminal products include paint pails, metalworking fluid pails, food-ingredient pails with gasketed lids, and industrial powder-packaging pails.

    When Regrind Ratios Exceed 40% in Structural Crate Molding

    When internal return material exceeds 40 wt% in structural crate molding, the processing window shifts from virgin-dominated to regrind-dominated rheology. In mold designs with wall sections of 2.0–3.5 mm, a formulation of 60 wt% HDPE 8050 and 40 wt% closed-loop regrind still provides sufficient melt flow, but mold temperature is raised to 30–50 °C and melt temperature to 220–250 °C to maintain low-temperature chain entanglement after rapid cooling. Stack bosses, runner intersections, and side-latch undercuts are locations where weld lines reduce impact resistance; documented mold trials show brittle failure at -20 °C when boss-to-wall thickness ratio exceeds 0.8:1. For dairy crate applications, post-molding caustic washing at 60–70 °C with 2–3 wt% NaOH creates a stress-cracking environment screened by ASTM D1693-15 ESCR coupons; lot changes are accepted only when ESCR time exceeds an internal control limit established from HDPE 8050 production history. Compliance is process-driven; USDA dairy sanitation guidance and ISO 22000 hygienic facility requirements apply to the molding and distribution chain. Terminal parts include dairy transport crates, bread trays, beverage crate shells, and reusable produce totes.

    For non-contact housewares and storage-tote components, HDPE 8050 is specified in family tools where granule weight ranges from 0.3 to 1.2 kg and wall thickness varies from 1.2 to 3.5 mm. The blend is 97.0–98.0 wt% HDPE 8050, 2.0–3.0 wt% color masterbatch, and 0.1 wt% processing lubricant; no drying is required below 60% ambient relative humidity. Melt temperature is 200–230 °C, mold temperature 20–30 °C, and holding pressure 400–550 bar. Compliance for consumer-accessible components requires conformance with 16 CFR 1303 lead ≤ 90 mg/kg in accessible substrate; if promoted for children's use, ASTM F963-23 mechanical safety testing is added. Published data specific to HDPE 8050 in family tool housewares is limited; this segment is based on standard high-flow HDPE injection practice rather than published application-specific engineering data. Terminal products include drawer organizers, storage totes, shelf supports, and modular closet bins.

    Rib-Base Weld Line Cracking in Refuse Container Shells

    Rib-base weld line cracking in refuse container shells is observed when sidewall ribs are filled at high injection speed in tools for 80 to 240 L bin bodies. The blend is 96.0 wt% HDPE 8050, 2.5 wt% UV-stabilized black masterbatch, 1.3 wt% processing aid/antioxidant, and 0.2 wt% acid scavenger. Large-format injection molding machines with 2,000–2,500 metric tons clamp force operate at melt temperature 230–250 °C, mold temperature 25–40 °C, holding pressure 600–800 bar, and final cushion 3–5 mm. EN 840-1:2020 and EN 840-5:2020 govern mobile waste containers; cold impact at -20 °C and dynamic rolling tests are required. If injection speed exceeds 150 mm/s at the rib base transition, cold slug formation and oriented skin layers create crack initiation sites; mold trials indicate that reducing speed to 80–120 mm/s at the last 15% of fill lowers reject rate by eliminating rib-base tearing. Terminal products include 80 to 240 L two-wheeled refuse bin bodies and smaller janitorial bins.

    Free Quote

    Competitive Formosa Plastics HDPE 8050 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Formosa Plastics HDPE 8050 is a high-density polyethylene injection-moulding resin supplied by Formosa Plastics Corporation. The grade is characterised by a nominal melt flow rate of 50 g/10 min when tested under ASTM D1238 at 190 °C with a 2.16 kg load and a nominal density of 0.953 g/cm³ determined by ASTM D1505. These two values place the product in the low-viscosity HDPE segment for high-cavitation, thin-wall, and short-cycle injection moulding. Published typical values include a tensile yield strength of approximately 26 MPa under ASTM D638, a flexural modulus near 1,310 MPa under ASTM D790, and a Shore D hardness of 68 under ASTM D2240. The material is not intended for extrusion blow moulding or cast film; its low melt strength and high fluidity are optimised for injection filling rather than parison stability or bubble stability. End users must confirm batch-specific properties against the supplier’s certificate of analysis because typical values are not specification limits.

    How Does a 50 g/10 min Melt Flow Rate Redistribute Moulding Stresses?

    At 50 g/10 min, the shear viscosity under injection conditions is substantially lower than that of conventional injection HDPE grades with melt flow rates below 20 g/10 min. In hot-runner multi-cavity tools, this viscosity reduction lowers the pressure drop per unit flow length and permits filling of wall sections below 0.8 mm without exceeding hydraulic pressure limits. On a 1,200 kN clamp force injection moulding machine with a 24:1 L/D general-purpose screw, the grade is typically processed at melt temperatures from 190 °C to 230 °C; lower temperatures increase filling pressure and frozen-layer formation, while higher temperatures extend cooling time and increase cycle-energy input. The practical injection pressure depends on flow length, gate diameter, and cavity thickness, but the high melt flow rate allows pressure-limited tools to fill with lower specific pressure than a 12 g/10 min grade. However, the same low molecular weight that reduces viscosity also lowers tensile elongation at break and environmental stress crack resistance under ASTM D1693 conditions. Therefore, the grade is not a drop-in replacement for tough, slow-flow grades in living hinges or load-bearing snap fits without evaluating impact requirements.

    On single-stage reciprocating-screw injection machines, the screw recovery time for HDPE 8050 is typically shorter than that of a 8 g/10 min HDPE grade under the same screw speed and back pressure. This permits reduced cycle time in high-cavitation tools, but the screw can over-dosage if the shot size is small relative to the barrel capacity. Barrel residence time should be kept below 5 min at melt temperatures above 220 °C to avoid thermal oxidative degradation. For thin-wall parts, high injection acceleration and velocity are more critical than high hold pressure; the flow front must traverse the cavity before the surface layer solidifies. Processors should record the actual melt temperature by air-shot pyrometer, not rely solely on barrel set-point, because shear heating can raise melt temperature by 10–20 °C at high screw speeds.

    Typical mechanical data reported for HDPE 8050 are summarised in Table 1. The property set reflects rapid crystallisation from the melt and a moderately high density. Because the resin is formulated for stiffness and processability, resistance to slow crack growth is lower than high-molecular-weight HDPE grades with melt flow rates below 1.0 g/10 min. The tensile yield stress and flexural modulus provide dimensional stability in rigid containers; impact behaviour in thin walls is highly dependent on gate geometry and mould temperature.

    PropertyTest methodTypical published value
    Melt flow rateASTM D123850 g/10 min
    DensityASTM D15050.953 g/cm³
    Tensile strength at yieldASTM D63826 MPa
    Flexural modulusASTM D7901,310 MPa
    Notched Izod impact, 23 °CASTM D25637 J/m
    Shore D hardnessASTM D224068
    Deflection temperature under load, 0.455 MPaASTM D64870 °C
    Vicat softening temperatureASTM D1525120 °C

    Processing of HDPE 8050 on production-scale injection moulding lines is characterised by short hold-pressure requirements because the high melt flow rate reduces gate-seal time. The screw recovery rate increases relative to lower-MFR grades, but back pressure should be minimised to avoid excessive shear heating and screw slippage. If the melt temperature exceeds 245 °C, the risk of odour generation and discolouration rises, particularly in hot runner channels with dead spots. Mould cooling uniformity controls shrinkage more strongly than melt temperature; non-uniform cooling in multi-cavity tools produces part-to-part weight variation and roundness deviation in closures.

    Thin-Wall Container Tooling and Gate Freeze Constraints

    In thin-wall food packaging and disposable containers, wall sections commonly range from 0.4 mm to 1.2 mm. The fill time must be shorter than the time required for the flow front to freeze, which for HDPE occurs when the melt temperature falls below the crystallisation onset near 120 °C. HDPE 8050 at 50 g/10 min permits injection speeds above 150 mm/s in cold-runner tools without excessive pressure spikes, but gate diameter must be at least 60% of the nominal wall thickness to prevent jetting and flow marks. Pin gates smaller than 0.5 mm can freeze prematurely and produce sink marks or voids. Rapid filling increases molecular orientation in the flow direction; this raises tensile strength along the flow path but reduces transverse impact resistance. Therefore, gate placement should orient flow along the part’s principal stress direction. Cooling time is governed by the square of wall thickness; a 0.8 mm wall may reach ejection temperature in 4–8 s depending on mould temperature and coolant turbulence.

    Compared with a 20 g/10 min HDPE injection grade, HDPE 8050 reduces fill pressure but may exhibit lower notched Izod impact and ESCR. Mould shrinkage for high-density polyethylene typically ranges from 1.5% to 2.5% along the flow direction and 1.0% to 2.0% transverse, depending on packing pressure and mould temperature. The high fluidity allows lower packing pressures to be used, but under-packing often produces higher shrinkage variation and vacuum voids in bosses and ribs. On hydraulic machines with closed-loop process control, cavity pressure transducers are recommended to maintain a cavity pressure of at least 25–40 MPa during packing for rigid containers.

    The Density of 0.953 g/cm³ Establishes a Permeation and Stiffness Threshold

    A density of 0.953 g/cm³ places HDPE 8050 near the upper range for HDPE injection grades. The crystallinity associated with this density yields a flexural modulus sufficient for stackable containers and caps, but it also reduces low-temperature impact relative to linear low-density polyethylene or lower-density HDPE copolymers. Water vapour transmission rate and oxygen permeability are lower than for lower-density polyethylenes, but HDPE is not a high-barrier resin; oxygen transmission rates for HDPE are typically three to four orders of magnitude higher than for EVOH or PVDC. Consequently, the resin is suitable for short-shelf-life food packaging but not for oxygen-sensitive products requiring a barrier layer. Chemical resistance to dilute acids, alkalis, and polar solvents is typical of high-density polyethylene. The product should not be exposed to strong oxidising acids, chlorinated solvents, or aromatic hydrocarbons at elevated temperature, because swelling and environmental stress cracking may occur. For outdoor use, UV stabilisation is required; unpigmented or unstabilised grades exhibit surface chalking and embrittlement under prolonged UV exposure.

    Food-contact status must be verified for each production campaign. High-density polyethylene olefin polymers may be cleared under FDA 21 CFR 177.1520 for specific conditions of use, provided the resin meets extraction limits and end-use restrictions. European Union compliance is typically assessed under EU Regulation 10/2011 and its amendments, with overall migration limits of 10 mg/dm² for food contact materials. Formosa Plastics can provide regulatory assurance documentation for the grade as supplied, but converters are responsible for compliance of the finished article after colourants, additives, and processing aids are added. Heavy metal restrictions under EU Directive 94/62/EC and CONEG model legislation may apply to packaging; the grade is typically formulated without intentionally added lead, cadmium, mercury, or hexavalent chromium, but batch-to-batch verification against IEC 62321 test methods is required where full compliance documentation is needed.

    Regulatory referenceScopeVerification requirement
    FDA 21 CFR 177.1520Olefin polymers for food contactSupplier clearance letter and extraction limits
    EU Regulation 10/2011Plastic food contact materialsOverall migration 10 mg/dm² on finished article
    EU Directive 94/62/ECPackaging heavy metal limitsSum of Pb, Cd, Hg, Cr(VI) ≤ 100 mg/kg
    CONEG model legislationPackaging toxicity reductionSame 100 mg/kg threshold
    IEC 62321Determination of regulated substancesAnalytical verification on coloured or printed articles

    When 8050 Is Substituted for a 20 g/10 min Grade in an Existing Multi-Cavity Mould

    Replacement of a 20 g/10 min HDPE with 8050 in an existing tool frequently reduces injection pressure and clamp force, but the change also alters the gate-freeze time and packing behaviour. The lower-molecular-weight resin reaches a lower steady shear viscosity, so the pressure trace at switch-over from velocity to pressure control may shift downward. If the process control system maintains the original pressure limits, the mould may overfill or flash at the parting line. Conversely, if the switch-over point is not adjusted, the lower viscosity can result in excessive screw travel and cavity overpacking. The practical remedy is to reduce hold pressure and shorten hold time, then verify part weight against the established baseline. Dimensional changes arise from altered shrinkage; conversion from a 20 g/10 min grade to 8050 can reduce the necessary hold pressure by 10–30% depending on wall thickness and flow length, but the exact adjustment must be determined experimentally on the production tool. Published data for this specific substitution is limited, so a conservative start-up with rheometer characterisation and short-shot study is recommended before full production.

    Pre-drying is generally unnecessary for HDPE 8050 if storage has been dry and the resin is not exposed to condensation. At relative humidity above 60% or after outdoor storage, surface moisture can produce splay and bubbles; hopper drying at 70–80 °C for 1–2 h may be applied, but the manufacturer’s processing guidance should be consulted. Avoid contamination with PVC or acetal residues at high temperature; degradation of halogenated polymers generates acidic by-products that corrode mould surfaces and accelerate polymer chain scission. Incompatibility with strong oxidising agents and long-term exposure to hot surfactant solutions limits use in industrial containers for concentrated detergents without specific ESCR validation under ASTM D1693 or equivalent.

    Compared with extrusion blow-moulding HDPE grades of melt flow rate 0.2–1.0 g/10 min, HDPE 8050 has insufficient melt strength to maintain parison shape and is unsuitable for continuous or accumulator blow moulding. Compared with high-molecular-weight film grades, the narrow molecular weight distribution and high melt flow rate do not provide the strain-hardening behaviour required for stable bubble expansion. Within the injection-moulding HDPE family, the 50 g/10 min grade is intended for thin-wall and high-cavitation production; it trades impact and ESCR for shorter cycle time and lower filling pressure. This trade-off must be matched to the end-use load case rather than treated as a universal property improvement.

    Top