Entec Hypel Pelld60 925 Lldpe

Entec Hypel® PELLD60/.925 LLDPE

    • Product Name: Entec Hypel® PELLD60/.925 LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 202404
    Product Name Entec Hypel PELLD60/.925 LLDPE
    Material Type Linear Low Density Polyethylene (LLDPE)
    Density 0.925 g/cm3
    Melt Index 60 g/10 min
    Melting Point 120 °C
    Vicat Softening Point 85 °C
    Tensile Strength At Yield 9 MPa
    Tensile Strength At Break 12 MPa
    Elongation At Break 700%
    Flexural Modulus 200 MPa
    Hardness Shore D 45
    Thermal Conductivity 0.35 W/m·K
    Specific Heat 2.3 J/g°C
    Dielectric Constant 2.3
    Volume Resistivity 1e16 ohm·cm
    Mold Shrinkage 0.020 cm/cm
    Processing Temperature 160-220 °C

    As an accredited Entec Hypel® PELLD60/.925 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Entec Hypel® PELLD60/.925 LLDPE is supplied in 25 kg (55 lb) polyethylene-lined paper bags, palletized and shrink-wrapped.
    Container Loading (20′ FCL) 20′ FCL loaded with Entec Hypel® PELLD60/.925 LLDPE pellets in 25 kg polyethylene bags, palletized and securely strapped for transport.
    Shipping Entec Hypel® PELLD60/.925 LLDPE is shipped as non-hazardous, non-regulated polyethylene pellets. Typical packaging includes 25 kg bags, octabins, or bulk containers. Transport cool, dry, and clean; avoid moisture, heat, and contamination. It is not classified as dangerous goods under DOT, IMDG, IATA, or ADR, so no UN number or hazard labels are required.
    Storage Store Entec Hypel® PELLD60/.925 LLDPE in a cool, dry, well-ventilated warehouse. Keep sealed bags or containers palletized, off the floor, away from direct sunlight, heat, flames, ignition sources, and strong oxidizers. Avoid moisture, contamination, and excessive stacking. Protect from UV light and weather. Inspect regularly for leaks or damage. Follow SDS and local regulations. Use appropriate PPE when handling.
    Shelf Life Typically 24 months when stored in original packaging, cool and dry, away from sunlight, heat, and ignition sources.
    Application of Entec Hypel® PELLD60/.925 LLDPE

    In heavy-duty industrial sack production, blown film extrusion of Entec Hypel® PELLD60/.925 at the specified 0.925 g/cm³ density and 0.60 g/10 min melt flow rate (determined per ISO 1133-1 at 190°C under 2.16 kg load) produces film in the 80–150 µm gauge range without the melt fracture surface defects common to narrow-die-gap LLDPE processing. The grade is differentiated from LDPE of equivalent melt index by a measurably higher shear viscosity at the die lip, which imposes specific machinery requirements. On a single-screw extruder with L/D 30:1 and a barrier screw containing a Maddock mixing section, barrel temperature zones are characteristically profiled from 150–160°C at the feed throat to 205–215°C at the die adapter. Published operating data for this density and melt index class places die melt pressure between 20 and 35 MPa at screw speeds of 70–100 rpm on a 90 mm extruder. Motor load for this LLDPE runs 15–25% higher than a comparable 0.60 g/10 min LDPE at identical throughput, because the linear molecular structure resists shear thinning less effectively than branched LDPE. Die gap selection is constrained at the lower end: gaps below 1.2 mm produce sharkskin melt fracture at wall shear rates above 400 s⁻¹. The recommended gap range of 1.8–2.4 mm permits melt stress relaxation before the die exit. A gear pump setup, where installed, should restrict inlet pressure to less than 12 MPa to avoid excessive shear heating that raises melt temperature by more than 5–8°C.

    Bubble geometry for sack film is maintained at a blow-up ratio of 2.2:1 to 3.0:1. Published troubleshooting reports attribute gauge variation of ±2% at BUR 3.2:1 to incipient bubble flutter under ambient cross-flow velocities above 0.5 m/s. Above BUR 3.5:1, the bubble becomes unstable on unshielded lines without internal bubble cooling. Frost line height is set at 4–7 die diameters. Frost line positioning below 3 die diameters quenches molecular orientation prematurely and reduces dart impact by 25–40% relative to the optimum; positioning above 9 die diameters shifts the MD/TD tear balance by 15–20% toward TD tear and away from MD tensile modulus. Film property testing follows ASTM D882 for tensile, ASTM D1922 for Elmendorf tear, and ASTM D1709 Method A for dart impact. Published data for comparable grades reports MD tensile strength at break of 35–48 MPa and TD tensile strength at break of 30–42 MPa at 25 µm thickness. Elongation at break exceeds 700% in both axes. Elmendorf tear values show the characteristic LLDPE anisotropy, with TD tear exceeding MD tear by a factor of 3–5. Dart impact at 25 µm is reported in the range 180–280 g. Slip and antiblock packages are compounded at 500–1,000 ppm erucamide and 2,000–5,000 ppm synthetic silica. Blocking force measured per ASTM D3354 remains below 0.5 N/cm after 48 h of roll storage at 35°C when the silica loading is at the upper end of the range.

    Compliance for food-contact sack applications is assigned under FDA 21 CFR 177.1520(c) for olefin copolymers. At 0.925 g/cm³ density the applicable subdivision is 3.1b; a lot density falling below 0.925 g/cm³ shifts classification to 3.1c. EU compliance under Regulation (EU) No 10/2011 requires verification of overall migration at 10 mg/dm² using simulant D2 at 40°C for 10 days when the film is used for fatty dry foods. Non-food industrial sacks require only REACH SVHC absence documentation. Operationally, the polymer is non-hygroscopic and predrying is unnecessary under normal warehouse conditions. However, cold pellet transfer directly from outdoor silos into a heated mezzanine has been observed to produce surface condensation defects—pinhole rates up to 8 defects/m² at gauges below 50 µm—when ambient RH exceeds 85%. Blending with LDPE above 20 wt% improves bubble stability but reduces dart impact by approximately 30%. Blending with HDPE above 10 wt% raises heat seal initiation temperature by 8–12°C, which is incompatible with sack sealing lines operating at 120–140°C jaw temperature.

    ParameterRecommended RangeMeasurement BasisFailure Threshold / Note
    Die gap1.8–2.4 mmDie lip setting1.2 mm minimum; sharkskin above 400 s⁻¹ wall shear
    Barrel feed zone150–160°CThermocoupleBelow 140°C feed bridging risk
    Barrel metering zone195–205°CThermocoupleAbove 215°C gel formation begins
    Adapter / die temperature200–215°CThermocoupleMelt temperature above 230°C reduces dart impact
    Melt pressure at die20–35 MPaDruck sensor35 MPa exceeds gear pump inlet rating
    Blow-up ratio2.2:1–3.0:1Bubble measurement3.5:1 bubble instability threshold
    Frost line height4–7 die diametersVisual / IR pyrometerBelow 3 die diameters reduces dart impact 25–40%
    Motor load vs LDPE+15–25%Amperage comparisonEqual amperage loses throughput

    What Restricts Cast Film Throughput of a 0.60 g/10 min LLDPE at Melt Temperatures Below 210°C?

    Published processing data for this melt index class indicates that stable web formation on slot dies with 1.0–1.5 mm lip gap is achievable only up to 120–140 m/min. Above this speed, melt resonance sets in and produces thickness banding of ±5–8% across the web. Stretch hood film for automated pallet containment is therefore converted from PELLD60/.925 primarily on blown film lines in the 80–120 µm gauge range. High-stalk or low-stalk configurations are employed at BUR 2.5–4.0. The high-stalk geometry delivers higher MD tensile modulus, which contributes to holding force. High-stalk configuration also reduces TD gauge variation to ±3% at BUR 3.0–4.0 when internal bubble cooling is set to 2–4°C air temperature and external cooling air ring pressure 0.3–0.5 MPa. Holding force at 55% residual strain on 100 µm film is reported between 11 and 15 N/500 mm after 24 h relaxation at 23°C. Elastic recovery after 80% elongation is between 42% and 48% for monolayer LLDPE. Coextruded structures with metallocene LLDPE skin layers raise recovery above 55%.

    The base grade contains no tackifier. Pallet grip requires either an embossed nip roller surface or post-extrusion corona treatment at 2–4 kW/m width. Corona treatment above 8 kW/m raises surface energy above 38 dyn/cm and induces blocking on rolls stored beyond 60 days at ambient temperature above 30°C. For indirect food contact pallet wrap, FDA 21 CFR 177.1520 compliance is accepted only when the film is separated from food by a functional barrier. UV exposure during warehouse storage does not compromise holding force within the first 12 months. Film stored outdoors loses 30–50% of MD tensile strength after 6 months unless a UV inhibition package is compounded into the resin.

    Dart Impact Retention After 12-Month UV Exposure Depends on HALS Loading, Not Base Resin

    Because the base resin is supplied without UV stabilization, agricultural silage wrap converted from PELLD60/.925 at 25–38 µm thickness requires additive compounding before extrusion. The film is pre-stretched 55–70% on baling equipment before spiral wrapping. Gauge increase alone does not correct the UV deficiency: an unstabilized 38 µm film loses more than 80% of initial dart impact within 3 months of continuous outdoor exposure in temperate latitudes. The converter must compound hindered amine light stabilizers at 0.5–1.2 wt% and a benzotriazole UV absorber at 0.2–0.4 wt% to satisfy the 12-month service requirement under EN 13207:2018. Published field data for LLDPE silage wrap indicates that a 1.0 wt% HALS package retains 70–80% of original ASTM D1709 dart impact after 12 months. Below 0.4 wt% HALS, retention falls below 50% over the same period.

    Tack performance is not intrinsic to the 0.925 g/cm³ LLDPE surface. Silage wrap self-adhesion requires a coextruded EVA-based tack skin or migratory polyisobutylene at 3–7 wt% in the surface layer. Without this modification, unwind tension on bale wrappers exceeds 12 N/25 mm and causes pre-stretch roller slippage. Peel force under ASTM D3330 for the unmodified LLDPE surface remains below 0.5 N/25 mm, which is insufficient for reliable overlap at 60% pre-stretch. Blown film extrusion for silage wrap operates at die melt temperature 190–210°C, die gap 1.6–2.2 mm, and BUR 2.0–3.0. Lowering die temperature to 185°C protects the dispersed HALS package from thermal degradation but raises melt pressure to the upper end of the 20–35 MPa window and increases motor load by 10–15%. Mulch film claims under EN 17033:2018 are excluded because the grade is not biodegradable. REACH Annex XVII documentation must confirm absence of intentional microplastic release where the film is sold into the EU agricultural market. The pigment masterbatch must demonstrate absence of listed phthalates and heavy metals.

    To achieve a heat seal initiation temperature below 100°C on vertical form-fill-seal lines running frozen vegetables at 90–100 cycles/min, a sealant layer of PELLD60/.925 is positioned in a three-layer frozen food bag structure. The sealant layer thickness ranges from 15 to 25 µm and is coextruded between a tie layer and the food contact surface. Heat seal initiation temperature, measured per ASTM F2029 as the temperature at which seal strength reaches 4.4 N/25 mm, is reported at 92–98°C for comparable grades. Plateau seal strength at 115–130°C jaw temperature is between 18 and 25 N/25 mm for a 20 µm sealant layer sealed at 0.3 MPa for 0.5 s. The low sealing threshold permits packaging lines to maintain throughput without exceeding heat exposure limits for IQF vegetables. The sealant layer is coextruded with an EVOH barrier layer in a three-layer or five-layer structure. The sealant layer melt flow rate must be matched to the adjacent tie layer within 10% to prevent interfacial instability in the coextrusion feedback. Published line data attributes encapsulated layer break-up to viscosity mismatch exceeding 15%. No recycled content may be placed in the sealant layer without full migration testing under Regulation (EU) No 10/2011, because the barrier is positioned behind the sealant rather than between the food and the sealant. Odor threshold testing per ASTM E1870 is recommended for frozen food contact because low-molecular-weight fractions migrate at measurable rates even at freezer temperatures when the food fat content exceeds 25%. Direct contact with aqueous foods at refrigeration temperatures above 50 µm sealant thickness requires specific migration testing for the α-olefin comonomer. Published migration data for 1-hexene and 1-octene comonomers indicates compliance below this thickness.

    Extrusion Blow Molded Container Wall Distribution and Parison Sag Metrics

    A 350 mm parison drop on a continuous shuttle blow molder demonstrates why 0.60 g/10 min melt flow is selected for flexible squeeze containers. Parison sag is lower than that of a 1.0–2.0 g/10 min LLDPE at equivalent melt temperature. Melt temperature at the die head is held at 180–195°C. Above 205°C, parison drawdown increases by 20–30% over a 350 mm drop length and produces wall thickness variation exceeding ±12% in the finished container. Die swell ranges from 35–50% over the die diameter under these conditions and must be compensated in die head machining to achieve the target parison diameter. Blow air pressure is set at 0.55–0.75 MPa (5.5–7.5 bar), and mold temperature is maintained at 10–20°C. Cooling cycle time for a 500 mL bottle at 0.8 mm nominal wall thickness ranges from 8–14 s. The finished container exhibits elongation at break above 700%. Low-temperature drop impact failure per ASTM D2463 at -40°C and 1.2 m height is below 5% for bottles with uniform wall distribution.

    For pharmaceutical dropper bottles, USP 〈661.1〉 testing for plastic packaging systems is mandatory. Published compliance data for comparable LLDPE grades reports passing values for nonvolatile residue and heavy metals under the specified extraction ratio. The converter must validate each bottle geometry because surface-to-volume ratio changes extraction severity. Haze measured per ASTM D1003 at 0.8 mm wall thickness is 25–40%. Where transparency is a market requirement, this grade is unsuitable and an HDPE or clarified random copolymer PP should be substituted. Compatibility testing with the intended liquid fill is mandatory for squeezable dispensers because stress cracking at the pinch-off weld can occur with surfactant-based formulations when molded-in residual stress exceeds 2.5 MPa.

    When Seam Peel Strength Falls Below 60% of Sheet Yield Strength, Welding Parameters Are Non-Conforming

    Hot wedge welding of 1.5 mm flexible geomembrane sheet proceeds at wedge temperatures 260–320°C, travel speed 1.0–2.5 m/min, and nip pressure 0.25–0.40 MPa. The geomembrane is extruded from PELLD60/.925 at 0.75–2.0 mm thickness through a 1,200 mm flat die with 0.8–1.5 mm lip gap at melt temperatures 190–215°C. Tensile yield strength per ASTM D6693 is reported between 8 and 12 MPa, and elongation at break exceeds 800%. The lower yield strength relative to 0.940 g/cm³ HDPE geomembrane (15–20 MPa yield) is intentional: it permits deformation without strain-softening under differential settlement. Puncture resistance per ASTM D4833 is reported at 200–350 N for 1.0 mm sheet, depending on surface texturing. Seam peel strength measured per ASTM D6392 must exceed 60% of the sheet tensile yield strength for acceptance under GRI-GM17 for LLDPE geomembranes. At wedge temperatures below 240°C, peel strength falls below the acceptance threshold because insufficient interdiffusion occurs across the weld interface. Above 350°C, oxidative degradation at the seam edge reduces elongation at break in the heat-affected zone by more than 50% and produces brittle cracking. Published failure investigations from containment installations associate low-pressure cold welding with seam peel values below 5.5 N/mm and attribute premature liner leakage to this mechanism.

    This grade is not suitable for primary hazardous waste containment where HDPE geomembranes certified under GRI-GM13 are specified. The lower crystallinity of 0.925 g/cm³ LLDPE raises permeation rates of benzene, toluene, and xylene by a factor of 2–4× relative to 0.940 g/cm³ HDPE at 23°C. The 0.75 mm minimum thickness is also incompatible with specifications requiring 1.5 mm minimum for hazardous chemical secondary containment. Oxidative induction time is specified per ASTM D3895 at 200°C by the project engineer. Published values for stabilized LLDPE geomembrane grades are available from resin producers and should be incorporated into the project specification before liner installation. Seam peel testing must be performed on every field weld because ambient wind speed above 3 m/s during welding has been documented to cool the wedge surface non-uniformly and produce intermittent peel values between 4 and 6 N/mm that pass visual inspection but fail the 60% yield criterion.

    Application SegmentStandard / ClauseTest MethodCondition / Limit
    Food contact sack filmFDA 21 CFR 177.1520(c) 3.1b/3.1cExtractables per §177.1520(d)Density boundary at 0.925 g/cm³
    EU food packagingRegulation (EU) No 10/2011Overall migration10 mg/dm² / simulant D2 / 40°C / 10 days
    Pharmaceutical bottlesUSP 〈661.1〉Plastic packaging systemGeometry-specific extraction ratio
    LLDPE geomembraneGRI-GM17ASTM D6693, ASTM D4833, ASTM D6392Seam peel ≥ 60% sheet yield
    Agricultural silage filmEN 13207:2018ASTM D1709 after UV exposure12-month field service
    Irrigation tubingISO 9261Dimensional / hydrostaticWall ±0.05 mm
    Melt flow rate determinationISO 1133-1Extrusion plastometer190°C / 2.16 kg

    For non-potable agricultural water distribution, low-pressure drip irrigation layflat tubing of 0.3–0.6 mm wall thickness is extruded at melt temperature 180–205°C without the torque penalty observed in film extrusion because the annular die imposes lower shear rates. Finished tubing conforms to ISO 9261 dimensional requirements for agricultural drip tape when wall thickness is held within ±0.05 mm. The material is not recommended for potable water distribution above 0.6 MPa without chlorinated water resistance testing per ISO 1167.

    As a masterbatch carrier resin, the 0.60 g/10 min melt index provides adequate pigment wetting at 40–50% carbon black loading in a co-rotating twin-screw extruder with L/D 44:1, but torque remains high and a higher-MI LLDPE is preferred above 50% filler loading.

    Free Quote

    Competitive Entec Hypel® PELLD60/.925 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Entec Hypel® PELLD60/.925 LLDPE is a linear low-density polyethylene injection molding grade whose designation carries three operational parameters. The prefix PELLD identifies polyethylene linear low density, the value 60 denotes a nominal melt flow rate of 60 g/10 min under ASTM D1238 at 190 °C/2.16 kg, and .925 denotes a nominal density of 0.925 g/cm³ by ASTM D1505. That combination places the grade at the high-fluidity end of the injection molding LLDPE spectrum while retaining the lower crystallinity and flexibility associated with a density below 0.930 g/cm³. The material is normally supplied as natural pellets with an antioxidant stabilizer package intended to protect the polymer during melt processing and service. End-use suitability must be confirmed against the supplier certificate of analysis, because nominal values do not establish lot-specific compliance with food-contact, medical, or performance specifications.

    What Distinguishes a 60 g/10 min Melt Flow Rate from Standard LLDPE Grades?

    Melt flow rate is an inverted indicator of average molecular weight: a linear polyethylene with a nominal MFR of 60 g/10 min has a substantially lower melt viscosity than a 20 g/10 min LLDPE of equivalent density. At low shear rates, the viscosity difference between the two grades can approach the inverse ratio of their MFR values, but at the apparent shear rates typical of injection mold filling—roughly 103 to 105 s−1—shear-thinning narrows the observed gap without eliminating it. Capillary rheometry according to ASTM D3835 at 190 °C is the preferred method for establishing a comparative viscosity curve across the shear rate range encountered in a specific tool. On a high-speed packaging line using a 100-ton reciprocating screw machine and a 24-cavity hot-runner thin-wall container mold, the practical effect is lower peak hydraulic pressure demand and the ability to fill wall sections of 0.8 to 1.2 mm at lower melt temperatures than would be required for a 20 g/10 min control grade. The same molecular weight reduction also lowers melt strength, which is why this grade is not suitable for blown film, blow molding, or extrusion processes requiring bubble or parison stability. Tensile yield stress, creep resistance, and environmental stress crack resistance are typically lower than those of a 1.0 g/10 min film-grade LLDPE, and load-bearing closures or snap-fit designs should be evaluated using ASTM D638 tensile data and ASTM D1693 ESCR data from the production lot rather than from generic grade comparisons.

    Processing of Entec Hypel® PELLD60/.925 LLDPE on reciprocating-screw injection molding machines should begin with a general-purpose polyethylene screw having an L/D ratio of 20:1 to 24:1 and a compression ratio of 2.5:1 to 3.0:1. Barrel profile settings from rear to nozzle commonly fall between 160 °C and 220 °C, with the nozzle held at 190 °C to 220 °C; actual settings depend on shot size, screw recovery time, gate geometry, and the residence-time distribution of the specific machine. Mold temperatures of 15 °C to 35 °C are typical for fast-cycle packaging, but low mold surface temperatures increase frozen-in orientation and can increase post-mold shrinkage in thicker sections. Because polyethylene is not hygroscopic, desiccant drying is generally unnecessary unless condensation from storage or handling at relative humidity above 60% is present; in such cases a 65 °C to 80 °C drying step for approximately 2 h reduces surface moisture before extrusion. Venting is critical in high-speed thin-wall tooling because the low melt viscosity and high injection velocity can trap air at flow-front convergence points. Vents of 0.02 to 0.03 mm depth are commonly required at the end of fill, and vacuum-assist venting may be necessary for parts with wall sections below 1.0 mm.

    Thermal, Mechanical, and Regulatory Specification Matrix

    The values in the following table are nominal design values read directly from the grade designation. Lot-specific certificate-of-analysis data may vary within supplier specification limits and must control release decisions.

    Specification item Nominal value Test method
    Melt flow rate 60 g/10 min ASTM D1238, 190 °C/2.16 kg; ISO 1133-1:2022
    Density 0.925 g/cm³ ASTM D1505; ISO 1183-1:2019
    Polymer class Linear low-density polyethylene Designation prefix PELLD

    The density of 0.925 g/cm³ corresponds to a semicrystalline morphology that generally produces a peak melting endotherm near 122 °C to 124 °C by ASTM D3418. Vicat softening temperatures for similar density LLDPE grades often fall near 95 °C to 105 °C by ASTM D1525, but the exact value for this grade must be obtained from the supplier datasheet because comonomer type and molecular weight distribution shift thermal response independently of density. Published data for this specific configuration is limited outside the controlled datasheet. Food-contact suitability, if claimed, should be verified under FDA 21 CFR 177.1520 for olefin polymers and, for European Union applications, under Regulation (EU) No 10/2011 with overall migration testing according to the EN 1186 series. Unfilled polyethylene grades are not typically affected by heavy metal restrictions under RoHS Directive 2011/65/EU, but supply-chain documentation should confirm that no prohibited additive has been introduced during compounding or pelletizing.

    High-fluidity LLDPE is selected for injection molded articles where wall thickness is below 1.5 mm, flow length is long relative to part thickness, and cycle-time reduction is a primary manufacturing objective. Typical applications include thin-wall disposable containers, pails with integral handles, flexible living-hinge closures, and overcaps that must snap over rigid sealing surfaces. In such parts, the 60 g/10 min MFR reduces the pressure required to fill multi-cavity hot-runner molds, allowing the use of smaller clamp tonnage or lower hydraulic pressure settings. The grade should not be specified for applications requiring sustained load-bearing creep resistance or high ESCR in the presence of polar surfactants, because the lower average molecular weight reduces the tie-molecule population associated with slow crack growth resistance. Chemical resistance must be confirmed by immersion testing under the intended service fluid according to ASTM D543; published data for this specific configuration is limited, and no single grade can be assumed resistant across solvents, oils, and aqueous surfactant systems.

    When Thin-Wall Packaging Demands High Flow Without Excessive Shrinkage

    Control of shrinkage in high-flow LLDPE requires attention to packing pressure and gate geometry because the low melt viscosity accelerates gate freeze-off if gates are undersized. For thin-wall containers with wall sections of 0.8 to 1.2 mm, the packing phase must be completed before the gate freezes; gate diameters below 0.8 mm can reduce pack effectiveness and increase post-mold shrinkage variability. Mold shrinkage in the flow direction and transverse direction are not equal, and high filling velocity tends to increase shrinkage anisotropy through molecular orientation. Tool designers should apply mold shrinkage factors derived from ASTM D955 measurements on a flat plaque of equivalent thickness, not from generic datasheet values. Because density is 0.925 g/cm³, the semicrystalline shrinkage is lower than that of lower-density LLDPE film grades but higher than that of high-density polyethylene. Hot-runner systems with valve gates provide more consistent packing pressure control than open hot sprue bushings when part-to-part weight variation must remain below 0.5%. Processing trials on stack molds or high-cavitation tooling should record shot-to-shot cushion, peak cavity pressure, and gate seal time to separate machine variability from material shrinkage behavior.

    The comparative class data below illustrate the position of Entec Hypel® PELLD60/.925 LLDPE relative to typical blown-film LLDPE and injection HDPE grades. Class-typical ranges are not substitutes for lot-specific testing and are provided to clarify application selection boundaries.

    Parameter Entec Hypel® PELLD60/.925 LLDPE Typical blown-film LLDPE Typical injection HDPE
    Nominal melt flow rate 60 g/10 min 0.5–2.0 g/10 min 20–60 g/10 min
    Nominal density 0.925 g/cm³ 0.918–0.922 g/cm³ 0.950–0.960 g/cm³
    Primary process suitability High-speed injection molding Blown film extrusion Injection molding and blow molding
    Melt strength class Low High Moderate to high
    Flexural modulus class Lower than HDPE Low 900–1400 MPa

    LLDPE grades are polymerized with butene, hexene, or octene comonomers, and the comonomer type influences impact strength, tear strength, and environmental stress crack resistance at equivalent density and MFR. Hexene and octene copolymers generally provide greater tie-molecule continuity and better puncture resistance than butene copolymers at similar density. Consequently, a 60 g/10 min, 0.925 g/cm³ grade produced with butene will not automatically match the ESCR or instrumented impact behavior of a hexene-based LLDPE at the same density and lower MFR. The grade designation does not specify comonomer type, and the supplier should provide this information when cold-temperature impact or detergent resistance is critical. Comparative testing under ASTM D3763 instrumented puncture and ASTM D256 Izod impact is required before substituting this high-fluid product into an application currently served by a lower-MFR hexene LLDPE or a higher-density HDPE.

    Entec Hypel® PELLD60/.925 LLDPE should not be blended with high levels of regrind unless the regrind is from the same grade and is free of contamination. Excessive residence time at melt temperatures above 240 °C can cause chain degradation, yellowing, and the formation of low-molecular-weight species that affect odor and taste in food-contact applications. The material is incompatible with strong oxidizing agents and should not be stored adjacent to volatile organic solvents that can be absorbed and later desorbed during processing. If flame retardancy is required, the effect of additive loading on melt flow rate and density must be re-evaluated because the nominal 60 g/10 min MFR and 0.925 g/cm³ density apply to the unfilled base resin, not to compounded formulations. No conclusion or forward-looking statement is made regarding fitness for use in any particular medical device or food-contact article without application-specific validation under the relevant regulation.

    Top