Entec Hypel Pelld5 935 Lldpe

Entec Hypel® PELLD5/.935 LLDPE

    • Product Name: Entec Hypel® PELLD5/.935 LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 151938
    Density 0.935 g/cm3
    Melt Flow Rate 5.0 g/10 min (190 °C/2.16 kg)
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 17.2 MPa
    Elongation At Break 800 %
    Flexural Modulus 0.345 GPa
    Hardness Shore D 55
    Vicat Softening Point 100 °C
    Melting Point 125 °C
    Brittleness Temperature < -70 °C
    Thermal Conductivity 0.33 W/m·K
    Specific Heat 2.3 J/g·°C
    Coefficient Of Linear Thermal Expansion 1.5E-4 1/°C
    Water Absorption 0.010 %
    Dielectric Constant 2.3
    Dielectric Strength 20 kV/mm
    Volume Resistivity 1E16 ohm·cm
    Dissipation Factor 0.0003

    As an accredited Entec Hypel® PELLD5/.935 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Entec Hypel® PELLD5/.935 LLDPE is packaged in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped for transport and storage.
    Container Loading (20′ FCL) 20′ FCL loading for Entec Hypel® PELLD5/.935 LLDPE: 25 kg bags, palletized, stretch-wrapped, securely loaded into a standard 20-foot container.
    Shipping Entec Hypel® PELLD5/.935 LLDPE is a non-hazardous polyethylene resin. Ship in sealed, moisture-resistant bags, bulk bags, or octabins. Store and transport dry at ambient temperature, away from heat, sunlight, and ignition sources. Not DOT/IMDG/IATA regulated. Use normal industrial hygiene; avoid dust and static buildup.
    Storage Store Entec Hypel® PELLD5/.935 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture and contamination. Store separately from strong oxidizers. Control dust and static; protect from physical damage; use grounding/bonding where required. Ensure containers are labeled and inspected regularly. Follow the manufacturer’s SDS and local storage regulations.
    Shelf Life Entec Hypel® PELLD5/.935 LLDPE shelf life is typically 24 months when stored sealed in original packaging, cool, dry, away from heat and sunlight.
    Application of Entec Hypel® PELLD5/.935 LLDPE

    Heavy-Duty Agricultural Silage Film and Stretch Hood via Three-Layer Blown Coextrusion

    Entec Hypel® PELLD5/.935 possesses a density of 0.935 g/cm³ under ISO 1183-1 and a nominal melt flow rate of 0.5 g/10 min under ISO 1133-1:2022 at 190°C with 2.16 kg load. When compounded for agricultural silage applications, the resin is loaded at 70–85 wt% as the primary structural polymer, with 15–30 wt% of a metallocene LLDPE having density 0.918 g/cm³ to elevate machine-direction Elmendorf tear values, 2–5 wt% of a silica anti-block masterbatch, and 0.5–1.5 wt% of a UV stabilization masterbatch that provides 0.2–0.5 wt% HALS and 0.1–0.3 wt% ultraviolet absorber in the final film. Compliance documentation for cross-border shipments commonly includes EN 13206:2017 for thermoplastic films used in agriculture, FDA 21 CFR 177.1520(c) where incidental contact with animal feed occurs, and REACH SVHC screening; mechanical acceptance is verified through ASTM D1709-16a for dart impact, ASTM D1922-09 for Elmendorf tear, and ISO 527-3/2/500 for film tensile properties.

    On production-scale three-layer blown film lines equipped with L/D 30:1 barrier screws, die gap 2.0–2.4 mm, blow-up ratio 2.8:1, and internal bubble cooling, setting the frost line height at 1.2–1.5 m is necessary to stabilize the higher-density bubble; barrel temperatures are held between 195°C and 210°C, with the adapter and die at 210°C. A bottleneck observed when converting this grade on LDPE-designed equipment is a rise in melt pressure at the screen changer; widening the die gap from 1.6 mm to 2.2 mm and increasing screw speed to 75–95 min⁻¹ usually restores line throughput without sacrificing film gauge uniformity. Terminal articles produced under this process include silage bags at 150–250 µm, stretch hood films at 120–180 µm, and flat agricultural covers; ambient temperature below 5°C during field deployment is addressed by increasing the metallocene content toward the upper bound rather than by reducing film thickness.

    On vertical form-fill-seal equipment, frozen food packaging requires a sealant polymer that resists puncture at temperatures down to -40°C and still initiates a seal below 105°C on high-speed sealing jaws. PELLD5/.935, at density 0.935 g/cm³ and MFR 0.5 g/10 min, is formulated as the sealant and toughness layer at 75–90 wt% of the total film structure, with 10–25 wt% metallocene LLDPE or plastomer at density 0.902–0.912 g/cm³ to suppress seal initiation temperature; slip and antiblock masterbatch loads of 0.3–1.0 wt% yield an erucamide concentration of 500–1000 ppm in the final film. Food-contact status is established under EU Regulation (EU) No 10/2011 with overall migration testing per EN 1186-1, and under FDA 21 CFR 177.1520(c) with extractives limits in 21 CFR 177.1520(d)(3)(i); low-temperature puncture retention is evaluated by ASTM D1709-16a and seal initiation by ASTM F1921-12. On a three-layer blown or cast coextrusion line with die gap 1.8–2.2 mm and chill roll temperature 18–22°C for cast processes, the addition of plastomer above 20 wt% can create melt destabilization on polished chill rolls, requiring an air knife and reduced line speed. Hot tack strength is evaluated by ASTM F1921-12 at dwell times below 0.5 s and sealing pressure 0.4–0.8 MPa; ethylene bis-stearamide is avoided because it can plate out on the die lip and cause web defects. Finished products include frozen vegetable bags, IQF seafood pouches, and barrier-overwrap films for frozen prepared foods, typically at total thickness 40–90 µm.

    When Geomembrane Sheet Extrusion Requires a 0.935 g/cm³ Density Fraction

    Landfill and liquid-containment projects specify smooth or textured geomembrane in 1.0–2.5 mm thickness, and PELLD5/.935 is compounded at 95–98 wt% with 2–3 wt% carbon black masterbatch and 0.3–0.8 wt% antioxidant package for long-term oxidative resistance. Compliance for engineered containment uses ASTM D6693-20 for tensile properties, ASTM D1603-14 for carbon black dispersion, and the GRI GM13 specification for LLDPE geomembranes; where welding is specified, destructive shear tests follow ASTM D6392-12 for geomembrane seams. Process on flat die sheet extrusion uses a 120 mm single-screw extruder with L/D 33:1, grooved feed section, and screen pack 40/80/40 mesh, operated at melt temperature 205–230°C, die gap 2.5–3.0 mm, and roll stack temperatures from 60°C to 90°C on the textured embossing roll. Because the MFR is 0.5 g/10 min, the melt viscosity at 200°C and 100 s⁻¹ is higher than that of film-grade LLDPE, increasing motor torque and limiting line speed for 2.0 mm sheet to approximately 4–6 m/min on a 90 mm extruder; published data for this exact grade on flat die geomembrane lines is limited, so commissioning trials typically verify head pressure and sheet gauge before full-rate production. Edge tear during trimming is minimized by maintaining a die lip temperature within 5°C of center. Terminal products include landfill liners, raw-earth reservoir liners, aquaculture pond liners, and tailings impoundment panels; hot-wedge seam welding at 360–420°C with a travel speed of 2.5–4.0 m/min is used to join panels after deployment.

    In beverage multipack converting, shrink collation film is subjected to a narrow window between free shrink and burn-through during tunnel exit; PELLD5/.935 is introduced into the cast film at 80–95 wt%, with 5–20 wt% LDPE to raise shrink force and prevent web sag during machine-direction orientation. Erucamide slip is controlled at 500–1000 ppm to maintain film-to-film slip after shrinkage. Compliance testing uses ASTM D2732-14 for free shrink and ISO 14616:1997 for shrink tension; mechanical strength is validated by ASTM D882-18 for thin sheeting. The conversion sequence begins with cast film at 200–400 µm, followed by machine-direction orientation through a short-gap MDO unit at draw ratios 4:1 to 7:1 and annealing temperature 100–120°C; the final film thickness is 40–60 µm. Field data from MDO lines show that draw resonance begins when the draw ratio exceeds 7:1, creating transverse thickness variation above ±5%; reducing the die bolts and increasing annealing roll temperature to 120°C reduces neck-in but lowers shrink tension. Terminal articles are collation shrink film for cans, bottles, and multi-pack bundling.

    What Limits Emitter Punching Precision in LLDPE Drip Irrigation Tape?

    Drip irrigation tape production demands a resin that holds a precise wall thickness of 0.15–0.40 mm while withstanding inline emitter placement without splitting. The formulation uses PELLD5/.935 at 97–99 wt%, carbon black masterbatch at 1–2 wt% to supply UV resistance, and a fluoropolymer processing aid at 0.02–0.05 wt% to reduce melt fracture at high line speed. Product requirements are specified under ISO 9261:2004 for emitters and emitting pipe, including dimensional tolerance and burst pressure classes; carbon black dispersion is checked by ASTM D1603-14. Downstream processing uses a 45–75 mm single-screw extruder with a vacuum calibration tank and inline emitter insertion; the melt temperature is held at 200–220°C and die pressure is typically 250–350 bar depending on emitter geometry. A production bottleneck occurs during emitter insertion when the tube wall is thinner than 0.15 mm; the probability of pinhole leakage increases as the melt exits the die with any melt fracture, which is why the processing aid is maintained at the upper limit. Drip tape producers evaluate the coefficient of variation of wall thickness at ±0.02 mm using laser gauges; batch-to-batch variation in carbon black masterbatch dispersion affects both UV resistance and abrasive wear on the emitter punch. Terminal products include drip irrigation tapes, microirrigation lateral pipes, and flat emitter tubing for row crops and greenhouse irrigation.

    Extrusion Blow Molding of 5–25 L High-ESCR Industrial Containers

    For industrial containers requiring resistance to stress cracking and stacking loads, PELLD5/.935 is compounded at 85–95 wt% with 5–15 wt% high-density polyethylene to improve top-load stiffness and surface hardness. ESCR is verified under ASTM D1693-15b Condition B; containers intended for dangerous goods transport are tested according to UN Model Regulations 6.1.6 with stack and drop tests. Extrusion blow molding on a shuttle machine with accumulator head and parison programmer uses a die gap of 2.5–3.5 mm, melt temperature 190–210°C, mold temperature 10–20°C, and blow air at 6–8 bar. At mold temperatures below 10°C the low-density fraction can freeze prematurely, shifting the weld-line geometry and reducing top-load performance; at melt temperatures above 210°C surface shark skin may develop if the die land length is less than 15 times the die gap. Terminal articles include 5–25 L jerrycans for lubricants, agricultural chemical containers, and industrial liquid liners; the higher molecular weight of the 0.935 g/cm³ fraction improves weld line ESCR but may reduce surface gloss, which is addressed by mold venting rather than formulation change.

    Free Quote

    Competitive Entec Hypel® PELLD5/.935 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Entec Hypell® PELLD5/.935 LLDPE is a linear low-density polyethylene supplied for rotational molding and related powder processing. The designation encodes two primary setpoints: nominal density 0.935 g/cm³ and nominal melt flow rate 5 g/10 min measured under ISO 1133-1:2022 at 190 °C/2.16 kg. Density is normally determined by ISO 1183-1 or ASTM D1505 on conditioned compression-molded plaques. The linear backbone, copolymerized with an alpha-olefin, contains fewer long-chain branches than conventional low-density polyethylene and therefore retains a higher population of tie chains bridging crystalline lamellae. In service, that structure increases slow crack growth resistance and low-temperature impact capacity relative to branched LDPE at comparable melt flow.

    Table 1 provides the property envelope commonly associated with a 0.935 g/cm³ LLDPE rotomolding powder. The values are representative of the material class and are not a substitute for lot-specific certificate-of-analysis data from the supplier.

    Representative property envelope for a 0.935 g/cm³ LLDPE rotomolding powder
    PropertyTest methodRepresentative range
    Nominal densityISO 1183-10.933–0.937 g/cm³
    Melt flow rate, 190 °C/2.16 kgISO 1133-1:20224.5–5.5 g/10 min
    Tensile yield stressISO 527-218–21 MPa
    Tensile elongation at breakISO 527-2500–900%
    Flexural modulusISO 178450–600 MPa
    Environmental stress crack resistance, 100% Igepal CO-630, condition BASTM D1693F50 > 1,000 h typical for the class
    Vicat softening temperatureASTM D1525112–120 °C

    Food-contact suitability, portable water certification, and regulatory status must be confirmed against the supplier safety data sheet and end-use extraction testing. Olefin polymers of this type may fall under FDA 21 CFR 177.1520, but end-use compliance depends on migration testing under the applicable conditions of use. Lot-specific density, melt flow rate, additive package, particle size distribution, and bulk density are the controlling purchase specifications.

    What Limits the Processing Window for 0.935 g/cm³ LLDPE Rotational Molding Powders?

    Rotational molding of this grade is conduction-limited rather than shear-activated. The powder densifies against a heated mold wall, and the cycle is governed primarily by peak internal air temperature, oven air temperature, and cooling rate. Oven set temperatures for 0.935 g/cm³ LLDPE rotomolding powders typically fall between 260 °C and 315 °C. Peak internal air temperature is generally controlled between 190 °C and 220 °C; lower peak internal air temperature can leave unconsolidated bubbles at the inner surface, while higher peak internal air temperature may accelerate oxidative degradation and produce discoloration. Infrared pyrometry or internal Rotowave sensing is recommended for closed-loop control.

    The powder must have sufficient dry flow and particle size distribution to fill mold contours and densify without trapped air. A 35-mesh grind with a narrow particle size distribution is common in rotomolding; excessive fines can reduce bulk density and create microporosity, while coarse particles may not sinter completely at thin-wall sections. Bulk density for rotomolding polyethylene powders typically ranges from 0.38 to 0.44 g/cm³, but the supplier value for this specific product should be verified.

    Rotational speed ratio between primary and secondary axes is normally held between 4:1 and 6:1. Lower ratios can produce wall-thickness variation on deep draw vertical surfaces. The absence of shear means that melt flow rate is not a direct processing analogue to injection molding; 5 g/10 min balances powder particle coalescence and melt elongation without excessive sag.

    Chemical storage applications for 0.935 g/cm³ LLDPE are specified where tanks and liners must tolerate intermittent hydrostatic loading and contact with surfactants, mild acids, alkalis, or agricultural chemicals. Slow crack growth in polyethylene proceeds by disentanglement of tie chains in the amorphous phase. A linear low-density grade at this density has a lower crystallinity than high-density polyethylene, which increases the amorphous fraction available for stress redistribution and extends failure times under notched constant-load tests such as ASTM F1473. Environmental stress crack resistance is commonly ranked by ASTM D1693, condition B, in 100% Igepal CO-630 at 50 °C; typical 0.935 g/cm³ LLDPE rotomolding materials exhibit F50 values exceeding 1,000 h. However, published data for this specific configuration is limited, and lot-specific values should be obtained from the supplier. For oxidizing media or chlorinated water, the stabilizer package must be evaluated separately by immersion testing under ISO 175, and continuous service above 60 °C should not be assumed without validated chemical resistance data.

    Differences from HDPE, LDPE, and MDPE in Slow Crack Growth Service

    Relative to high-density polyethylene with density between 0.950 and 0.965 g/cm³, the 0.935 g/cm³ LLDPE has lower crystallinity, lower flexural modulus, and higher resistance to brittle slow crack growth at equal wall thickness. Compared with branched low-density polyethylene, the linear architecture increases tensile yield stress and strain hardening modulus while reducing long-chain branching. Compared with medium-density polyethylene, the resin sits at the upper density boundary but retains a high tie-chain density because of the linear comonomer distribution. Table 2 summarizes the positioning.

    Positioning of PELLD5/.935 relative to conventional polyethylene classes
    ClassDensity rangeMelt flow rangeCrystallinityESCR tendencyLow-temperature impact tendency
    PELLD5/.935 LLDPE0.935 g/cm³ nominal5 g/10 minmoderatehighhigh
    LDPE0.915–0.925 g/cm³variablelowmoderatehigh
    MDPE0.926–0.940 g/cm³variablemoderatemoderate to highhigh
    HDPE0.945–0.965 g/cm³variablehighlower than LLDPE at equivalent MIlower than LLDPE at equivalent wall

    Unlike crosslinked HDPE rotomolding grades, PELLD5/.935 remains thermoplastic and can be reground in plant scrap recovery. It does not, however, provide the same upper-use temperature or creep resistance as a crosslinked high-density network. Flexural modulus is governed by crystallinity; at 0.935 g/cm³, the material is less stiff than HDPE but stiffer than most LDPE grades. The melt flow rate of 5 g/10 min removes the need for the low melt flow rates often required in pipe and blow molding grades, while still avoiding the excessive sag observed in higher-MI linear resins.

    Rotational molding equipment and powder handling boundaries require specific controls. Pulverized powder is produced by high-intensity attrition milling, and heat generated during grinding must be controlled to prevent particle surface melting, which can lower bulk density and reduce dry flow. Powders should be kept dry; although polyethylene is not hygroscopic, surface condensation at relative humidity above 60% can introduce steam bubbles during heating. Pre-drying at 60–80 °C for 2–4 h is prudent when storage conditions are humid or when cold powder is charged into a warm mold. Static charge on fines can create non-uniform layer formation on the mold surface; grounding and humidity control are required. Finely divided polyethylene powders can form combustible dust, so dust concentration should be managed in accordance with NFPA 654.

    Contamination by incompatible polymers must be avoided. Polypropylene or PVC contamination at levels as low as 2–5 wt% can form discrete low-cohesion domains that weaken weld lines and reduce impact strength. Additive packages for rotomolding grades typically include a hindered phenol primary antioxidant, a phosphite secondary antioxidant, and an acid scavenger. Outdoor service grades require additional ultraviolet stabilization.

    When Wall Thickness Uniformity Dictates Mold Temperature and Cooling Rate

    Wall thickness uniformity in rotomolding is controlled by mold design, rotation ratio, and the thermal history of the mold. Differential cooling between thick and thin sections creates residual stress and warpage after demolding. Air-cooled parts develop higher crystallinity and may show greater shrinkage but lower frozen-in stress; water mist cooling accelerates solidification and can reduce warpage in flat panels, but too rapid a quench can produce microcracking or inner-surface porosity. The melting peak of a 0.935 g/cm³ LLDPE by differential scanning calorimetry is typically between 122 °C and 128 °C. Demolding should occur only after the internal air temperature has fallen below approximately 80–90 °C for most structural parts, because early demolding can cause puncture or distortion at thin ribs.

    Venting is critical with internal air expansion. In rotomolding, internal air pressure rises during heating and can prevent complete powder coalescence if not vented through a properly sized vent tube. The vent must remain open without admitting moisture or foreign material. If the mold is heated too rapidly, the powder may stick irregularly and create a “cobblestone” inner surface. If the oven air temperature is too low, cycle time increases and peak internal air temperature may be insufficient for bubble removal. Production-scale carousel machines, shuttle machines, and rock-and-roll machines can all process this grade, provided multi-axis speed control and mold temperature monitoring are available.

    Ultraviolet stabilization is mandatory for outdoor service. Hindered amine light stabilizers at 0.2–0.5 wt% suppress free-radical degradation at exposed surfaces, and carbon black at 2–2.5 wt% is used for long-term sunlight resistance in agricultural tanks and outdoor containers. Oxidation induction time testing under ASTM D3895 provides a check on retained antioxidant activity after accelerated oven aging. For transparent or light-colored parts, UV absorber systems replace carbon black, but weathering resistance must be confirmed by ASTM G154 or ISO 4892-3 using the buyer’s thickness and exposure geography.