Entec Hypel Pelld20 925 Lldpe

Entec Hypel® PELLD20/.925 LLDPE

    • Product Name: Entec Hypel® PELLD20/.925 LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 257025
    Material Linear Low Density Polyethylene (LLDPE)
    Density 0.925 g/cm³
    Melt Index 190 C 2 16 Kg 20 g/10 min
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 13.8 MPa
    Elongation At Break 800%
    Flexural Modulus 207 MPa
    Vicat Softening Temperature 88 °C
    Melting Point 121 °C
    Hardness Shore D 50
    Water Absorption <0.01%
    Volume Resistivity >10^15 ohm·cm
    Dielectric Constant 1 Mhz 2.3
    Thermal Conductivity 0.2 W/m·K
    Coefficient Of Linear Thermal Expansion 1.5E-4 /°C
    Processing Temperature Range 180-220 °C

    As an accredited Entec Hypel® PELLD20/.925 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Entec Hypel® PELLD20/.925 LLDPE is supplied in 25 kg polyethylene-lined bags, with 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL container loaded with Entec Hypel® PELLD20/.925 LLDPE in 25 kg bags, palletized, stretch-wrapped, and secured for ocean transport.
    Shipping Shipping Description: Entec Hypel® PELLD20/.925 LLDPE is a non-hazardous LLDPE resin, not regulated as dangerous goods for transport. Ship in original sealed bags or octabins on clean, covered vehicles. Protect from moisture, contamination, heat, and direct sunlight. No UN number, hazard class, or packing group required.
    Storage Store Entec Hypel® PELLD20/.925 LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep original bags or containers tightly closed on pallets to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and temperatures exceeding recommended limits. Maintain good housekeeping; prevent spills that create slipping hazards. Follow local regulations and supplier SDS.
    Shelf Life Entec Hypel® PELLD20/.925 LLDPE typically has a 24-month shelf life when stored unopened in a cool, dry place away from sunlight.
    Application of Entec Hypel® PELLD20/.925 LLDPE

    What Processing Limits Govern a 0.925 g/cm³ LLDPE Carrier Resin at 45% Carbon Black Loading?

    Entec Hypel® PELLD20/.925 LLDPE is a linear low-density polyethylene with a melt mass-flow rate of 20 g/10 min measured under ISO 1133-1:2022, Method A, at 190°C and 2.16 kg, and a base density of 0.925 g/cm³ determined by ISO 1183-1:2019. In carbon black masterbatch production, the grade is used as the primary carrier resin at 55–65 wt% when carbon black loading is set between 40–45 wt%, with a low-molecular-weight polyethylene wax at 1–3 wt% and a phenolic antioxidant masterbatch at 0.2–0.5 wt%. The 20 g/10 min melt mass-flow rate reduces torque during filler wetting, while the 0.925 g/cm³ density reduces pellet-cutting energy and strand breakage in underwater pelletizing. The resulting masterbatch is let down in polyolefin film or injection-molding compounds at 2–6 wt%; for articles with wall thickness below 0.8 mm, the letdown ratio is reduced or a finer carbon black grade is selected because agglomerates above 10 µm can initiate environmental stress-crack sites when tested under ASTM D1693-15. If the carbon black has a DBP absorption value above 100 cm³/100 g under ASTM D2414-22, the melt-pressure increase in the mixing zone requires a 20 g/10 min carrier rather than a fractional-melt film grade.

    Compounding is carried out on a co-rotating twin-screw extruder with an L/D ratio of 44:1–52:1 and segmented screw elements. The solids-conveying zone is kept at 40–60°C; the plastification zone is ramped from 180°C to 220°C; the mixing zone is controlled at 220–240°C; and the die plate is held at 200–220°C. Carbon black is introduced through a side feeder downstream of the primary melting zone when the filler surface area exceeds 250 m²/g. Screw speed is set at 500–800 rpm, and specific mechanical energy input typically falls between 0.20 kWh/kg and 0.30 kWh/kg. A vacuum vent at -0.06 MPa to -0.08 MPa removes moisture and low-molecular-weight volatiles; loss of vacuum produces microvoids in the pellet that become visible as pinholes in film at letdown levels as low as 3 wt%. The melt is filtered through a screen changer before an underwater pelletizer; water temperature is maintained at 40–60°C. Water temperature below 40°C creates rough pellet surfaces that influence bulk density and feeding uniformity, while water temperature above 60°C causes pellets to agglomerate in the discharge chute. Melt-pressure fluctuation across the screen changer exceeding ±0.5 MPa indicates filler accumulation on the screen pack; the screens are replaced within 20–30 min to limit thermal degradation of the carrier resin.

    Compliance for masterbatch intended for food-contact end uses is determined at the final article level under Commission Regulation (EU) No 10/2011, Annex I and Annex II, and under FDA 21 CFR 177.1520(c) for the olefin polymer carrier. REACH registration and Article 33 information obligations apply to any substance of very high concern in the masterbatch formulation, and carbon black grades intended for food-contact use are assessed for PAH content under the relevant food-contact additive specifications. Terminal products produced from this carrier-resin masterbatch include carbon black-loaded agricultural film, black industrial injection-molded containers, cable jacket concentrates, and non-food packaging regrind colorants. The upper practical loading limit is 50 wt% carbon black; above this concentration, melt filtration area requirements increase disproportionately and pellet integrity deteriorates during underwater pelletization.

    In thin-wall injection molding of flexible anti-tamper closures and overcaps, the 0.925 g/cm³ density and 20 g/10 min melt mass-flow rate of Entec Hypel® PELLD20/.925 LLDPE reduce peak hydraulic pressure relative to fractional-melt film grades and permit filling of wall sections between 0.8 mm and 1.5 mm without excessive shear heating. The grade is processed neat or with a polyolefin-based color concentrate added at 2–4 wt%; when surface slip is required, erucamide is incorporated at 500–1,000 ppm and synthetic silica anti-block at 1,000–2,000 ppm, with total additive content kept below 5 wt% to avoid measurable loss in elongation at break under ASTM D638-22 or environmental stress-crack resistance under ASTM D1693-15. For food-contact closures, compliance is evaluated under FDA 21 CFR 177.1520(c) and Commission Regulation (EU) No 10/2011 Annex I; closure integrity is additionally verified by ASTM D3078-02 because the molded geometry must remain dimensionally stable under top-load and vacuum conditions. Processing on a reciprocating-screw injection molding machine with a 22–30 mm screw and 20:1–25:1 L/D ratio uses barrel temperatures of 180–230°C, nozzle temperature of 210–230°C, mold temperature of 10–30°C, injection speed of 150–300 mm/s, and hold pressure of 35–60 MPa. Hold pressure below 35 MPa produces sink marks at the gate, while hold pressure above 60 MPa increases molded-in stress at the undercut and can cause demolding deformation. Post-mold shrinkage is 1.5–2.5% after 48 h; cooling time for a 1.0 mm wall is 3–8 s, and cycle time must account for the low thermal conductivity of polyethylene at 0.33 W/(m·K). Terminal parts include beverage cup overcaps, dairy container snap lids, pail covers, and flexible closures with integral pull-tabs. Below a wall thickness of 0.6 mm, flow hesitation at the weld line becomes the limiting factor, and the mold requires additional venting or injection velocity above 300 mm/s; published data for this grade below 0.6 mm wall thickness is limited, and tool-release trials should include short-shot analysis and weld-line tensile testing under ASTM D638-22.

    Extrusion Coating Parameters for a 20 g/10 min Linear Low Density Polyethylene on Paperboard

    Extrusion coating of paperboard and flexible laminates uses the 20 g/10 min melt mass-flow rate of Entec Hypel® PELLD20/.925 LLDPE to achieve low coating weights without excessive melt temperature or screw backpressure. The resin is processed as a neat coating layer or as a blend with 10–30 wt% low-density polyethylene having a melt index of 4–8 g/10 min; the LDPE fraction reduces neck-in and improves chill-roll adhesion. For foil-laminated structures, anhydride-modified LLDPE or ethylene-acrylic acid tie resin is added at 2–5 wt%. Coating weight for paperboard is maintained at 15–40 g/m²; for foil-laminated sachet structures, the coating layer may be reduced to 8–15 g/m² when the substrate is pre-primed. Compliance is evaluated under FDA 21 CFR 176.170 for paper and paperboard components and Commission Regulation (EU) No 10/2011 Annex I for the plastic coating layer. The extrusion coating line uses a single-screw extruder with 90–120 mm screw diameter, 28:1–32:1 L/D ratio, and a coat-hanger die maintained at 270–310°C. The air gap is set at 150–250 mm, and the chill roll is held at 15–20°C. Line speed is typically 100–300 m/min; above 300 m/min, the onset of melt fracture produces transverse bands across the web unless a fluoropolymer processing aid is added at 300–500 ppm. Die temperature below 270°C increases melt pressure and edge instability, while sustained operation above 310°C promotes oxidative gel formation in the die lip; the preferred operating window is therefore constrained to a ±5°C band around the selected set point. Terminal products include liquid packaging board for dairy cartons, paper cups, food-service wrappers, and sachet laminates for dry beverage powders. For structures requiring heat-seal strength above 8 N/15 mm, an additional sealant layer is usually required because this grade alone provides limited seal-initiation temperature control under ASTM F88/F88M-21 conditions.

    When post-industrial LLDPE scrap with degraded melt strength is converted into non-food transport packaging, addition of virgin Entec Hypel® PELLD20/.925 LLDPE at 10–30 wt% compensates the viscosity loss of the recyclate and reduces injection pressure variability during production. The blend uses 70–90 wt% washed LLDPE/HDPE regrind, 10–30 wt% virgin PELLD20/.925, and a phosphite antioxidant masterbatch at 0.1–0.3 wt%; above 30 wt% virgin addition, the flexural modulus of the final part under ISO 178:2019 can fall below typical crate specifications, while below 10 wt%, the change in melt mass-flow rate under ISO 1133-1:2022 is insufficient to offset batch-to-batch viscosity variation in the recyclate. Compliance is governed by EU Packaging and Packaging Waste Directive 94/62/EC for packaging material recycling and by REACH Article 33 communication duties for substances of very high concern in recycled feedstock; the compound is not intended for direct food contact without a functional barrier because migration of unknown contaminants from recyclate cannot be excluded. Processing is performed on a co-rotating twin-screw extruder with 36:1 L/D ratio, melt temperature 190–210°C, vacuum degassing at -0.08 MPa, and a screen changer equipped with 80–120 mesh screens. Terminal products include industrial pails, crates, storage bins, drainage fittings, and non-food closures. If residual moisture in the regrind exceeds 0.05 wt%, vacuum venting becomes unstable and pellet porosity increases; a drying step at 60°C for 2 h is required before extrusion.

    When a High-Flow LLDPE Is Compounded with EVA for Chemically Foamed Cap Liners

    Chemically foamed cap liners and gaskets are produced from a compound in which Entec Hypel® PELLD20/.925 LLDPE contributes processability and flexibility, while ethylene-vinyl acetate copolymer provides compression set and sealability. Based on 100 parts total polymer, the starting-point formulation contains 65–80 wt% EVA with vinyl acetate content between 9–28%, 20–35 wt% LLDPE, plus 0.5–2.0 phr azodicarbonamide chemical blowing agent, 0.5–1.0 phr slip/lubricant, and 0.1–0.3 phr antioxidant. When the LLDPE fraction exceeds 35 wt%, gas retention during foaming becomes inconsistent because the polyolefin phase cannot maintain sufficient melt strength at the decomposition temperature; below 20 wt%, the compound becomes too soft for automated liner insertion. Compliance for food-contact closures is evaluated under FDA 21 CFR 177.1520(c) for the olefin portion and FDA 21 CFR 177.1350 for ethylene-vinyl acetate copolymers, along with Commission Regulation (EU) No 10/2011 Annex I migration limits for decomposition residues. Processing is carried out on a reciprocating-screw injection molding machine with a melt temperature of 180–210°C, mold temperature of 20–40°C, and short-shot volume of 70–85% of the full cavity. The blowing agent decomposition window is narrow: below 200°C gas yield is incomplete, and above 210°C cell coalescence and surface blistering occur; the processing window is therefore controlled to ±5°C at the nozzle. Terminal products include foamed cap liners for metal and plastic closures, gaskets for beverage caps, and tamper-evident liner structures. Published data for this specific grade and VA ratio combination is limited; the ranges above represent starting-point formulations that require closure-specific compression-set testing under ASTM D395-18 before production release.

    Compliance referenceScopeRelevant limit or test
    Commission Regulation (EU) No 10/2011Plastic food-contact materialsAnnex I overall migration limit 10 mg/dm²
    FDA 21 CFR 177.1520(c)Olefin polymersFood-contact use conditions
    FDA 21 CFR 177.1350Ethylene-vinyl acetate copolymersFood-contact use conditions
    ASTM D395-18Compression set of closures22 h at 70°C
    Free Quote

    Competitive Entec Hypel® PELLD20/.925 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Entec Hypel® PELLD20/.925 LLDPE is an injection-molding-grade linear low-density polyethylene whose identifier encodes a nominal density of 0.925 g/cm³ and a nominal melt flow rate of 20 g/10 min when determined at 190 °C under 2.16 kg load in accordance with ISO 1133-1:2022. The model designation indicates a high-flow rheology that reduces injection pressure and increases flow-length-to-wall-thickness capability in thin-wall packaging, closures, and technical mouldings. Compared with fractional-melt LLDPE film or rotomoulding grades, the 20 g/10 min flow class shifts the conversion envelope toward shorter cycles, lower clamp-force demand per projected area, and thinner nominal wall sections. The same flow class also narrows the molecular weight distribution around a lower average chain length, which reduces melt strength and accelerates gate freeze relative to a 7 g/10 min LLDPE.

    The PELLD20/.925 identifier does not specify the comonomer architecture. In linear low-density polyethylene, 1-butene introduces ethyl branches, 1-hexene introduces butyl branches, and 1-octene introduces hexyl branches. These branch-length differences control tie-molecule concentration between lamellae and therefore control environmental stress-crack resistance, low-temperature impact, and flexural modulus at fixed density and melt flow rate. Published data for this specific configuration is limited; the following benchmarks are class-level values reported for 0.925 g/cm³ LLDPE with 20 g/10 min MFR, not guaranteed product minima.

    Class-level property anchors for 0.925 g/cm³ LLDPE with 20 g/10 min MFR
    PropertyMethodClass-level range
    DensityISO 1183-1:20190.923–0.927 g/cm³
    Melt flow rateISO 1133-1:202218–22 g/10 min
    Tensile yield stressISO 527-2:201211–14 MPa
    Tensile elongation at breakISO 527-2:2012600–900%
    Flexural modulusISO 178:2019220–320 MPa
    Notched Izod impact at 23 °CISO 180/A:2023No break or >50 kJ/m²
    Vicat softening temperature A50ISO 306:202288–100 °C
    Mould shrinkageASTM D955-211.5–2.5%

    How Does the 0.925 g/cm³ Density Influence Solid-State Performance?

    Density is not merely a classification parameter; it is an indirect measure of crystalline volume fraction. A linear low-density polyethylene with 0.925 g/cm³ density contains a lower crystalline fraction than HDPE grades at 0.945–0.965 g/cm³ and a higher crystalline fraction than very-low-density PE at 0.900–0.915 g/cm³. The consequence is an intermediate flexural modulus, reported in the class range 220–320 MPa under ISO 178:2019, with sufficient compliance to resist cracking during part ejection and assembly. Tensile yield stress for this class falls between 11 MPa and 14 MPa under ISO 527-2:2012, while elongation at break remains above 600%. These values indicate ductile yielding followed by extensive cold drawing before failure.

    Impact resistance is the strongest functional distinction against high-density polyethylene. At 23 °C, notched Izod specimens typically exhibit no break under ISO 180/A:2023, and the ductile-to-brittle transition is displaced to temperatures substantially below 0 °C relative to HDPE. Low-temperature impact in a 20 g/10 min grade is more sensitive to comonomer type than in a low-MFR grade. A butene-based resin at 0.925 g/cm³ can lose impact sharply below -10 °C because shorter ethyl branches generate fewer load-bearing tie molecules than butyl or hexyl branches from hexene or octene comonomers. Converters must therefore request notched Izod or instrumented puncture data at the actual service temperature rather than assuming density alone predicts toughness.

    When High MFR Reshapes Filling, Packing, and Cooling

    A melt flow rate of 20 g/10 min under ISO 1133-1:2022 is a low-shear-rate index. Under injection-moulding shear rates between 10³ s⁻¹ and 10⁵ s⁻¹, linear low-density polyethylene is shear-thinning but generally remains higher in viscosity than LDPE at equivalent MFR. The high-flow designation should therefore be interpreted as improved filling at constant injection pressure, not as unrestricted melt extension. On a spiral-flow mould with 1.5 mm channel depth, a 20 g/10 min LLDPE typically achieves flow-length increases of approximately 20–35% relative to a 7 g/10 min LLDPE at identical melt temperature and injection pressure; published data for this specific grade is limited.

    In production-scale injection moulding, a thin-wall container lid with 0.8 mm nominal wall thickness can be filled on a 1,500 kN hydraulic injection moulding machine at melt temperatures between 190 °C and 220 °C. Increasing melt temperature to 230 °C is typically unnecessary and may extend cooling time without proportional gain in flow length. Melt residence time above 240 °C should not exceed 10 min to avoid oxidative chain scission and gel formation. For outdoor-stored material exposed to condensation, pre-drying at 70–80 °C for 1–2 h is sufficient; polyethylene is not hygroscopic, so drying is generally not required when relative humidity is below 60%.

    Gate freeze time is shorter for high-MFR grades because the low-molecular-weight fraction crystallizes and solidifies rapidly after shear ceases. With a gate diameter below 1.0 mm, pack pressure transfer may be effective for only 0.2–0.8 s. Moulders must therefore set velocity-to-pressure switchover earlier than for a 7 g/10 min LLDPE to avoid short shots or surface sinks. Shrinkage anisotropy is higher than in HDPE, and post-mould dimensional change can occur over 24–48 h at 23 °C. Dimensional checks should follow conditioning periods specified in ISO 294-4:2018 or ASTM D955-21.

    Thin-wall closures and dispensing fitments manufactured from this grade are evaluated for sealability under ASTM D2463-15 drop impact, for torque retention in closure systems under ASTM D3475-18, and for environmental stress-crack resistance under ASTM D1693-15. In closures, a resin at 0.925 g/cm³ density is selected when the part must survive hinge flexing and child-resistant cap actuation at low temperature; the high MFR permits filling of narrow hinge bridges without excessive orientation. The same flow class is used as a carrier resin in polyolefin masterbatch because it disperses pigment and additive concentrates under high-shear compounding while retaining acceptable pellet hardness.

    Comparative Boundaries Against Butene, Octene, and Metallocene LLDPE

    The product occupies a position between conventional autoclave LDPE, high-density PE, and metallocene-catalysed LLDPE. At equal density and melt flow rate, LLDPE has higher tensile yield stress and puncture resistance than LDPE because the linear backbone with short-chain branches forms a more regular lamellar structure. LDPE has stronger melt extension and better optical clarity due to long-chain branching; PELLD20/.925 is not a direct substitute for LDPE in extrusion coating or high-clarity film where draw resonance resistance is required.

    Qualitative comparison at 0.925 g/cm³ and 20 g/10 min unless noted
    Comparison attributeButene LLDPE classHexene/octene LLDPE classMetallocene LLDPE class
    Short-chain branch lengthethylbutyl or hexylcontrolled butyl or hexyl distribution
    Environmental stress-crack resistance at constant density and MFRlowest among the threeintermediate to highhigh due to more uniform tie-molecule placement
    Low-temperature impactmost brittle below -10 °Cductile at -20 °C in many gradesgenerally superior at -30 °C if MFR allows
    Melt strengthmoderate; lower than LDPEmoderate; lower than LDPElow to moderate; narrow MWD reduces recoverable shear
    Shear thinningmoderatemoderateless pronounced; higher viscosity at high shear than broad-MWD LLDPE at equal MFR
    Screw torque in compoundinglowerslightly higher at same melt temperaturehighest among LLDPE classes when processed on 40:1 L/D twin-screw equipment

    In metallocene-catalysed LLDPE of equal MFR, narrower molecular weight distribution reduces long-chain branching and can produce sharkskin surface defects at lower output rates than broad-MWD Ziegler-Natta LLDPE. The PELLD20/.925 grade is therefore evaluated on the basis of shear viscosity under capillary rheometry, not solely on MFR. Processors running hot-runner closure moulds with 0.8 mm wall thickness and 12 cavities should maintain barrel temperature control within ±3 °C to limit shot-to-shot weight variation below 0.4%; this control is more critical for high-MFR LLDPE than for fractional-melt grades because small viscosity changes translate directly into cavity filling variation. Environmental stress-crack resistance is formulation-specific, and converters should avoid exposure to polar organic solvents, aggressive detergents, and oxidizing acids at elevated temperature unless full chemical compatibility testing is performed.

    Top