Entec Hyboost 401 Masterbatch Lldpe

Entec HYBOOST® 401 Masterbatch, LLDPE

    • Product Name: Entec HYBOOST® 401 Masterbatch, LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 466269
    Product Name Entec HYBOOST® 401 Masterbatch, LLDPE
    Manufacturer Entec Polymers
    Material Type Maleic Anhydride Grafted LLDPE Masterbatch
    Carrier Resin Linear Low Density Polyethylene (LLDPE)
    Active Ingredient Maleic Anhydride Grafted Polyethylene
    Form Pellets
    Color Natural
    Density 0.920 g/cm³
    Melt Flow Rate 2.0 g/10 min at 190°C/2.16 kg
    Maleic Anhydride Content 0.9 wt%
    Melting Point 125°C
    Vicat Softening Point 105°C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 12 MPa
    Elongation At Break 500%
    Flexural Modulus 200 MPa
    Hardness Shore D 50
    Processing Method Extrusion, Injection Molding

    As an accredited Entec HYBOOST® 401 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Entec HYBOOST® 401 Masterbatch, LLDPE is typically packaged in 25 kg polyethylene-lined bags or 1,000 kg flexible intermediate bulk containers.
    Container Loading (20′ FCL) 20′ FCL container loading of Entec HYBOOST® 401 Masterbatch, LLDPE: palletized 25 kg bags, stretch-wrapped, securely stowed for ocean shipment.
    Shipping Entec HYBOOST® 401 Masterbatch, LLDPE is supplied in 25 kg moisture-resistant bags, FIBCs, or octabins, palletized and shrink-wrapped. Transport in clean, dry, covered vehicles by road, rail, sea, or air at ambient temperature. Keep dry and away from heat, sunlight, and strong oxidizers. Typically non-hazardous; follow SDS and local transport regulations.
    Storage Store Entec HYBOOST® 401 Masterbatch, LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep original containers tightly closed, upright, and protected from moisture, dust, and contamination. Avoid temperature extremes and prolonged storage above recommended limits. Follow good housekeeping practices and all local regulations. Use first-in, first-out inventory rotation.
    Shelf Life Shelf life is typically 12 months from manufacture when stored in original, unopened packaging in a cool, dry place.
    Application of Entec HYBOOST® 401 Masterbatch, LLDPE

    The application fields enumerated below are restricted to polyethylene-rich extrusion and moulding processes where LLDPE-carrier polymer processing aid masterbatches are used to suppress melt fracture, die-lip deposit formation and pressure-fluctuation instability. HYBOOST 401 Masterbatch is supplied as free-flowing pellets in an LLDPE carrier; published product-specific loading data for this configuration is limited, so the addition windows shown are derived from publicly documented processing-aid practice and require verification on the target extruder. Each scenario records regulatory status, typical addition ratio, downstream process sequence and terminal article classes. Product use in food-contact articles must be confirmed against the complete formulation including base resin, colorants and other additives.

    Application-specific processing window and primary standard mapping
    Application scenarioTypical continuous additionPrincipal process boundaryPrimary standard designation
    Blown film0.5 wt%–1.5 wt%Melt temperature 180°C–220°C; BUR 2.0:1–3.5:1ASTM D882 / ASTM D1922
    Cast stretch film0.5 wt%–1.2 wt%Line speed 500–900 m/min; chill roll 20°C–30°CASTM D5748 / ASTM D5458
    Pipe extrusion0.5 wt%–1.0 wt%Melt temperature 190°C–230°C; die-head pressure <350 barISO 9080 / ISO 4427
    Wire and cable jacketing0.8 wt%–1.5 wt%Cross-head pressure 80–150 bar; line speed 300–800 m/minIEC 60811-4 / IEC 60502
    Blow moulding1.0 wt%–2.0 wt%Clamp force 350–600 kN; mould temperature 10°C–30°CFDA 21 CFR 177.1520 / UN/DOT packaging certification
    Extrusion coating0.5 wt%–1.5 wt%Air gap speed 150–450 m/min; chill roll 15°C–25°CASTM D903 / ISO 11339

    In blown film extrusion of linear-low-density polyethylene-rich formulations, sharkskin melt fracture appears at the die land when wall shear stress exceeds approximately 0.14 MPa at melt temperatures between 180°C and 220°C. HYBOOST 401 Masterbatch is metered into the main throat at a continuous dose of 0.5 wt% to 1.5 wt% using a gravimetric screw feeder; start-up purges of 2.0 wt% to 3.0 wt% are stopped when die pressure variation falls below ±0.5 bar over 20 min. The downstream conversion process runs on single-screw extruders with L/D ratios from 24:1 to 30:1, screw diameters from 50 mm to 90 mm, die gaps from 0.8 mm to 2.0 mm, blow-up ratios from 2.0:1 to 3.5:1, and frost line heights between 600 mm and 1200 mm; the active phase collects at the metal-polymer interface under high shear and suppresses melt fracture without destabilizing the frost line. Food-contact applications where the finished article falls under Regulation (EU) No 10/2011 or FDA 21 CFR 177.1520 require migration testing according to EN 1186-1 or the applicable FDA condition-of-use matrix; REACH Regulation (EC) No 1907/2006 applies to all industrial exports. Terminal film types produced under these conditions include 25 µm to 150 µm collation shrink film, agricultural silage cover, lamination film for flexible packaging, and heavy-duty industrial liners. Tensile property verification uses ASTM D882; tear resistance uses ASTM D1922; dart impact uses ASTM D1709. Addition above 2.0 wt% should be validated for haze according to ASTM D1003, because increasing interfacial slip can raise surface haze in thin gauges.

    Why Does Cast Stretch Film Processing Require Interfacial Slip Additives Above 700 m/min?

    Because die-lip build-up removes the stable contact line between melt curtain and die exit—leading to edge weave and gauge variation—cast film lines running above 700 m/min often operate with 0.5 wt% to 1.2 wt% HYBOOST 401 Masterbatch in polyethylene-rich machine and cling layers. On a typical cast line with a 2500 mm-wide flat die, die gap from 0.4 mm to 0.8 mm, vacuum box and air knife positioned prior to the primary chill roll at 20°C to 30°C, and line speeds from 500 m/min to 900 m/min, the LLDPE carrier melts completely before the active phase deposits at the die land; the effect is measured as a reduction in die pressure standard deviation and a more stable neck-in distance. Downstream coextrusion combines linear low-density polyethylene, metallocene polyethylene and low-density polyethylene in an A/B/C structure, where the processing aid is generally placed in the skin or core layer at 0.5 wt% to 1.2 wt%; the finished film is then corona-treated for cling or pre-stretch use. For regulatory compliance, the product used in machine stretch film for industrial pallet wrapping must meet REACH Regulation (EC) No 1907/2006 and, where applicable, RoHS Directive 2011/65/EU; food-contact stretch film should be evaluated under Regulation (EU) No 10/2011 and any national positive list. Terminal articles include 12 µm to 23 µm machine pallet wrap, 25 µm agricultural stretch film, and hand-wrap film; performance tests include ASTM D5748 for puncture resistance, ASTM D5458 for peel cling, and ISO 527-3 for tensile modulus of film. Doses above 2.0 wt% are not recommended unless surface coefficient of friction is re-qualified via ISO 8295, because the slip-promoting active phase can change cling performance.

    Pipe extrusion of PE100 and PE100-RC compounds through 38D grooved-feed single-screw extruders presents two convergent constraints: molecular-weight distribution is broad enough to generate die-line shark skin, and the pipe calibration stage cannot remove surface irregularities formed in the die. HYBOOST 401 Masterbatch is added at 0.5 wt% to 1.0 wt% via the main hopper or a side feeder before the compression zone; in this range it lowers die-head pressure oscillation and allows extruder motor load to be managed without altering the MRS classification of the base resin. The process runs at melt temperatures from 190°C to 230°C through a spiral mandrel die for pipe diameters from 32 mm to 630 mm, followed by vacuum sizing, spray cooling, haul-off, and cut-to-length; the LLDPE carrier is consumed within the polyethylene pipe matrix and is not intended to function as a separate phase. Regulatory status for pressure pipe applications includes ISO 12162 for material classification, ISO 9080 for long-term hydrostatic strength prediction, ISO 4427 and EN 12201 for PE water and gas pipes, and ISO 1167 for hydrostatic testing; industrial exports are covered by REACH Regulation (EC) No 1907/2006. Terminal product classes include PE100 drinking-water mains, gas distribution pipe, industrial slurry lines, and cable protection conduits made from high-density polyethylene. The processing aid is not a substitute for correct die design: if die-head pressure exceeds 350 bar or melt temperature exceeds 240°C, localized gel formation may occur and line purging with an HDPE purge compound at 250°C is required before restart.

    When a Wire and Cable Jacketing Line Starts Shedding Die Deposits

    If a crosshead die used for HDPE or LLDPE jacketing starts accumulating oxidized material at the die exit, the first visible failure is specking at the conductor surface and short-term line stops for die lip cleaning. HYBOOST 401 Masterbatch is dosed at 0.8 wt% to 1.5 wt% into the main extruder throat; on a 65 mm single-screw extruder with a barrier screw, L/D 24:1 to 30:1, and cross-head pressures from 80 bar to 150 bar, the LLDPE carrier assimilates during plastication and the active phase concentrates at the die wall. The downstream cabling process runs with conductor preheating at 40°C to 60°C, a crosshead die for jacket thickness 0.5 mm to 2.0 mm, water trough cooling in stages from 60°C to 25°C, and haul-off speeds from 300 m/min to 800 m/min; the masterbatch does not replace an on-line spark tester or diameter gauge but reduces melt-fracture-induced diameter variation. For compliance, wire and cable grades are generally evaluated under IEC 60811-4 for low-temperature mechanical tests, IEC 60502 for low-voltage power cable insulation and sheathing, and ASTM D4568 for polymeric materials used in wire and cable; REACH Regulation (EC) No 1907/2006 applies to the finished sheath material. Terminal products include low-voltage power cable jackets, control cable sheathing, HDPE duct sleeves, and drop-cable insulation skins. Melt temperatures above 250°C or residence times beyond 10 min should be avoided because the LLDPE carrier may begin chain-branching and generate measurable gel content.

    Accumulator-Head Blow Moulding of High-Molecular-Weight HDPE

    In high-molecular-weight HDPE blow moulding, parison surface defects are not recoverable once the mould closes; HYBOOST 401 Masterbatch is therefore added at 1.0 wt% to 2.0 wt% because high-melt-viscosity grades generate visible die-lip flow marks when wall shear stress exceeds the critical slip threshold. The LLDPE carrier melts in the extruder, and the active phase shifts the apparent wall shear stress in the parison die; the result is a stable parison diameter and lower rejected-part rate. The downstream blow moulding sequence includes 50 mm to 80 mm extruders with L/D 24:1 to 30:1, a grooved feed section for HDPE, an accumulator head, a converging die gap, mould close and blowing, flash removal, post-cooling, and leak testing. Clamp force is typically 350 kN to 600 kN, parison drop time is 2 s to 5 s, and mould temperature is held at 10°C to 30°C. Regulatory alignment for industrial packaging includes UN/DOT dangerous goods packaging certification where applicable, FDA 21 CFR 177.1520 for food-grade containers, and REACH Regulation (EC) No 1907/2006; the masterbatch does not supersede organoleptic testing when containers are used for food or pharmaceutical powders. Terminal product classes are 20 L to 60 L tight-head and open-head drums, 5 L jerry cans, and intermediate bulk container liners. The additive must be mixed uniformly in the extruder because short residence time in accumulator heads can cause local concentration variation; pre-drying is not necessary below 60% RH, but material stored above 80% RH for more than 2 h should be dried at 60°C for 2 h before processing.

    Extrusion Coating Uses Interfacial Slip to Control Edge Neck-In on Aluminium and Board

    Whenever line speed exceeds 150 m/min on an extrusion-coating line, the melt curtain exhibits edge neck-in and draw resonance unless the polymer-metal interface is modified. HYBOOST 401 Masterbatch is mixed at 0.5 wt% to 1.5 wt% into the coating resin, which is typically LLDPE or LDPE with melt index between 4 g/10 min and 8 g/10 min; the LLDPE carrier in the masterbatch does not change the coating rheology beyond the intended slip effect. The downstream process uses a 75 mm to 120 mm single-screw extruder, flat die widths from 1200 mm to 2800 mm, die gap 0.5 mm to 0.8 mm, line speeds from 150 m/min to 450 m/min, and a polished chill roll at 15°C to 25°C; the melt is extruded through an air gap onto corona-treated paper, board or aluminium foil and immediately quenched. The processing aid reduces die-lip build-up and stabilizes the melt curtain at the die exit; it does not improve adhesion, so substrate surface tension must be verified at 40 mN/m to 46 mN/m for polyolefin adhesion. For regulatory compliance, extrusion coating for food packaging must comply with Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520 for olefin polymers; REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU apply to industrial laminates. Terminal product classes are liquid packaging board coatings, aluminium foil lamination for pouches, sachet film, and release paper coating. Peel strength is tested by ASTM D903 or ISO 11339; melt index for incoming coating resin is measured by ISO 1133-1:2022.

    Free Quote

    Competitive Entec HYBOOST® 401 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Entec HYBOOST® 401 Masterbatch is a pelletized additive concentrate carried in linear low-density polyethylene. The 401 grade designation identifies a specific carrier-additive pairing within the HYBOOST product family; it should not be interchanged with LDPE-carrier or EVA-carrier grades without verification of target additive concentration, melt flow ratio, and critical film values specified by the converter. The masterbatch is intended for meter-in blending into polyethylene extrusion and molding operations where the LLDPE carrier is compatible with the host resin. Because LLDPE exhibits a linear chain structure with limited long-chain branching relative to LDPE, the carrier contributes different shear-thinning behavior and extensional viscosity in film blowing and cast-film processing. The converter must obtain the supplier certificate of analysis for lot-specific values including melt mass-flow rate determined according to ISO 1133-1:2022 at 190 °C with 2.16 kg load, ash content by ISO 3451-1, and additive concentration by the manufacturer’s validated method. Where no certificate value is cited in this document, the parameter is treated as product-specific and must not be inferred from generic LLDPE datasheets.

    What Processing Parameters Govern LLDPE-Based Masterbatch Letdown in Single-Screw Extrusion?

    Letdown accuracy is governed by feeder calibration against the masterbatch bulk density and pellet geometry. Single-screw extrusion lines with a barrier screw of length-to-diameter ratio 24:1 to 30:1 and compression ratio 2.5:1 to 3.5:1 are suitable when the host polyethylene and masterbatch are dry-blended at the hopper. Metering by a gravimetric or volumetric side feeder at the feed throat is recommended for additive loadings below 2 wt% because hopper stratification can alter concentration. The melt temperature measured at the die should be maintained within the standard LLDPE processing range of 190 °C to 230 °C; sustained operation above 240 °C may initiate thermal degradation of the carrier unless the masterbatch datasheet permits a higher ceiling. Backpressure from the screen pack should be recorded at startup. An increase greater than 30 % over the initial value at constant output when processing a 1000 kg lot can indicate additive agglomeration or inadequate dispersion. The pressure profile across a breaker plate fitted with 100 µm and 200 µm screens provides an early indication of undispersed additive.

    On co-rotating twin-screw compounding lines, the use of a side feeder at barrel five of a 40:1 L/D extruder prevents premature melting of the LLDPE carrier in the main feed and reduces motor load fluctuations. A screw profile combining forward conveying elements, two kneading block zones, and a vacuum devolatilization port at −0.08 MPa has been used to incorporate LLDPE-based masterbatches into polyethylene compounds. Specific mechanical energy input must be recorded and compared against the supplier’s dispersion curve; published data for this specific grade is limited. Batch-to-batch variation in pellet size distribution is controlled by screening the masterbatch through a 6.3 mm sieve before automatic conveying; carryover particles greater than 8.0 mm can bridge in hopper loaders and cause mass flow interruption. For processes that add the masterbatch via an unheated side feeder, screw speed may be adjusted to maintain a feed factor of 0.90 to 1.10 relative to the host resin; the exact factor must be derived from the feed calibration curve rather than nominal bulk density.

    Thermal Stability and Devolatilization Boundaries Above 220 °C

    Thermal stability in LLDPE-carrier masterbatches is evaluated by dynamic thermogravimetric analysis under nitrogen according to ISO 11358-1. A 5 % mass-loss temperature above 320 °C is a typical lower acceptance boundary for LLDPE carrier compounds, but the value for Entec HYBOOST® 401 must be measured on the specific lot because the additive package may lower the onset of degradation. In extrusion, residence time at melt temperatures above 220 °C should be kept below 300 s wherever possible. If a process stops for longer than 15 min, the die and screw should be purged with low-melt-index polyethylene before restart. The masterbatch is not classified as hygroscopic, but surface moisture may accumulate on pellets stored in unheated silos at relative humidity above 60 %. Pellets should be pre-dried at 60–80 °C for 2–4 h using a desiccant dryer with a dew point of −20 °C or lower when moisture-induced surface defects are observed. Water content measured by Karl Fischer titration according to ISO 15512 should be below 0.05 wt% before processing in cast film or extrusion coating.

    In blown-film conversion, the host polyethylene and masterbatch are tumble-blended for 20 min before transfer to hopper loaders. A grooved-barrel extruder with spiral mandrel die gap of 1.6 mm to 2.4 mm and blow-up ratio of 2.0:1 to 2.5:1 is typical for LLDPE-rich formulations. Chill air temperature and frost line height are set to control bubble stability because the LLDPE carrier can have lower melt strength than a branched LDPE carrier. The bubble is monitored for draw resonance and edge weave; deviation in layflat width greater than ±3 mm at constant line speed indicates feed concentration drift or uneven blending. For cast film lines, die temperatures are maintained at 220–240 °C with an air gap of 15–25 cm and a chill roll temperature of 20–35 °C. Tear propagation by ASTM D1922 and dart impact by ASTM D1709 are used to compare the masterbatch’s effect on film toughness relative to the neat host resin. No performance claim for Entec HYBOOST® 401 is made without comparison to the converter’s reference formulation.

    When the Masterbatch Is Substituted for an EVA-Carrier or LDPE-Carrier Grade

    An LLDPE carrier differs from LDPE and EVA carriers in chain architecture, crystallinity, and seal response. LDPE-carried masterbatches generally show broader molecular weight distribution and higher melt strength, which can stabilize the bubble in blown film but can also produce higher gel counts under high-shear processing. EVA carriers exhibit higher polarity and are often used for slipping or antifog additives; however, EVA introduces vinyl acetate groups that can increase moisture affinity and may contribute to plate-out on die lips at temperatures above 220 °C. LLDPE carriers reduce the vinyl acetate input and provide closer compatibility with metallocene or Ziegler-Natta LLDPE host films. Differential scanning calorimetry according to ISO 11357-3 can be used to confirm the melting peak of the carrier and to detect crystallinity changes when the masterbatch is used at high letdown. In applications requiring low seal initiation temperature, the 401 grade may not be interchangeable with an EVA-carried product; the converter should compare heat seal strength via ASTM F88 and hot-tack via ASTM F1921 on the complete film structure.

    Regulatory Documentation and Standard Test Designations

    Documentation topicStandard or referenceEvidence required from supplier
    Melt mass-flow rateISO 1133-1:2022Certificate of analysis value per lot
    Density of LLDPE carrierISO 1183-1:2019Value at 23 °C
    Ash contentISO 3451-1:2019Percent residue after calcination
    Heavy metals and RoHS screeningIEC 62321-5:2013, IEC 62321-7-1:2015Supplier statement or test report
    Food-contact suitabilityFDA 21 CFR 177.1520, EU 10/2011Written confirmation for the final article
    REACH registrationRegulation (EC) No 1907/2006 Annex IISDS in current EU format

    This documentation matrix does not establish compliance; it identifies the documents demanded from the masterbatch supplier before use in regulated packaging. The final article manufacturer remains responsible for overall migration tests according to EU 10/2011 or FDA 21 CFR 177.1520.

    In injection molding of polyethylene compounds containing the masterbatch, a machine with a general-purpose polyolefin screw of L/D 20:1 to 24:1 and check ring is used. The clamp force is selected from the projected area; for a 2 mm wall thickness part, injection velocity should be set to fill in 1.0–2.0 s to prevent flow lines. Mold temperature is held at 20–45 °C. Back pressure at plastication should not exceed 5 bar to avoid intense shear on temperature-sensitive additives in the masterbatch, unless the supplier’s datasheet permits higher energy input. Tensile bars are molded per ISO 294-1 and tested per ISO 527-2; notched Izod impact is measured per ISO 180. Batch-to-batch consistency can be assessed by the standard deviation of molded plaque colorimeter readings; a ΔE shift greater than 1.0 under D65/10° illumination suggests concentration drift after feeder cleaning.

    Hopper loading systems for the masterbatch should avoid long pneumatic conveying distances above 60 m unless the conveying air is dried and pellet fracture is monitored. Attrition can generate fines that separate from the host resin in the feed throat and create localized additive spikes. A fines content below 0.5 wt% through a 500 µm sieve is a practical acceptance limit for uniform feeding; the value for Entec HYBOOST® 401 should be confirmed on the delivered lot. In storage, the product should be kept in sealed containers at temperatures not exceeding 40 °C. Containers exposed to direct sunlight for more than 14 days should be inspected for surface tack before use. These boundaries are derived from industrial handling practice for LLDPE-based masterbatches; published data specific to the 401 grade is limited and must be verified through supplier documentation.

    Top