| HS Code | 747284 |
| Carrier Resin | LLDPE |
| Product Type | Masterbatch |
| Form | Pellets |
| Color | White |
| Additive Content | 40% |
| Density | 0.920 g/cm³ |
| Melt Flow Rate | 2.0 g/10 min (190 °C/2.16 kg) |
| Melting Point | 120 °C |
| Moisture Content | ≤0.10% |
| Pellet Size | 2.0-3.0 mm |
| Bulk Density | 0.55 g/cm³ |
| Recommended Loading | 1-5% |
| Processing Temperature | 180-220 °C |
| Shelf Life | 24 months |
| Storage Temperature | <30 °C |
| Packaging | 25 kg |
As an accredited Entec HYBOOST® 400 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Entec HYBOOST® 400 Masterbatch, LLDPE is supplied in 25 kg net polyethylene-lined bags, palletized and stretch-wrapped for shipment. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Entec HYBOOST® 400 Masterbatch, LLDPE, in palletized bags, evenly distributed and securely braced for transport. |
| Shipping | Entec HYBOOST® 400 Masterbatch, LLDPE is typically a non-hazardous solid masterbatch. It is not regulated for transport; no UN number, hazard class, packing group, labels, or placards are required. Ship in sealed bags or drums on pallets, store dry and cool, and verify with the current SDS. |
| Storage | Store Entec HYBOOST® 400 Masterbatch, LLDPE, in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, moisture, and strong oxidizers. Keep original containers tightly closed, off the floor, and protected from UV, dust, and physical damage. Maintain ambient temperature, avoid excessive stacking, and rotate stock using first-in, first-out. Do not store near food, drink, or animal feed. Clean spills promptly. |
| Shelf Life | Shelf life is 24 months from manufacture when stored in original, unopened packaging in a cool, dry, well-ventilated area. |
On a 350 mm annular die line running a 1.0 MI LLDPE-rich formulation for agricultural silage wrap, the observed failure mode without processing aid is sharkskin melt fracture on the bubble exterior and periodic draw oscillation above blow-up ratio 2.5:1. HYBOOST® 400 Masterbatch, LLDPE is gravimetrically dosed into the hopper at 0.5–1.5 wt%; the LLDPE carrier disperses in the feed section of a single-screw extruder with L/D 30:1 and a barrier screw, and the active components deposit at the die lip to reduce critical wall shear stress in the annular die gap. The downstream production process is tubular blown-film extrusion with internal bubble cooling, die gap 1.8 mm, blow-up ratio 2.5:1, frost line height 800 mm, and post-bubble corona treatment to 38–42 mN/m surface energy before slitting and center winding. Terminal finished articles are 25 µm and 30 µm silage stretch film, bale wrap, and greenhouse cover films. Compliance for agricultural stretch film is anchored to EN 13206:2017 for stretch retention and film integrity, ISO 527-3:2018 for tensile properties, and ASTM D1709-22 for dart impact; REACH Regulation (EC) No 1907/2006 applies to substance registration and Annex XVII restrictions. The operational boundary is set by a maximum let-down of 1.5 wt% in thin films to limit the influence of the carrier on seal initiation and haze; at addition levels above this, slip migration to the film surface can occur during aging at ambient warehouse temperatures.
Batch-to-batch variance in LLDPE base resin melt index across supplier lots—commonly ±0.3 MI—requires adjustment of masterbatch let-down within the stated range. A lower-MI lot at 0.8 MI may require the 1.5 wt% dose to maintain bubble stability, while a 1.2 MI lot may function at 0.5 wt%. This is a production-scale response, not a laboratory extruder artifact.
In high-speed cast film extrusion of linear-low-density polyethylene stretch films, the limiting defect is not bubble instability but die lip build-up and draw resonance at line speeds above 400 m/min. HYBOOST® 400 Masterbatch, LLDPE is added at 0.8–2.0 wt% in this process. The equipment configuration is a 90 mm single-screw extruder with L/D 30:1, a barrier feed section, a screen pack of 20/40/60/80 mesh, an automatic gravimetric dosing system, and a slot die with lip gap 0.5 mm and width 2000 mm. The melt curtain is pinned by an air knife, edge pinners, and a vacuum box onto a chill roll held at 15–20°C. Terminal finished articles are 12–17 µm machine-grade pallet stretch film, hand stretch film, and hygiene backsheet laminating films. Compliance for food-contact versions follows EU No 10/2011 with overall migration testing into food simulants A, B, and D2 according to Annex III and Annex IV; olefin polymer status is evaluated under FDA 21 CFR 177.1520(c). Mechanical performance is assessed by ASTM D882-18 for tensile modulus and elongation at break, and ASTM D1922-23 for propagation tear. In this process, the LLDPE carrier masterbatch reduces die lip deposit caused by low-molecular-weight oxidized species; field observations on cast lines show die-cleaning intervals extended from 8 h to 24 h when the masterbatch is maintained in the feed, though published data for this specific configuration is limited. The upper addition boundary is 2.0 wt% because excess processing aid can produce chill-roll deposition and transfer to film surfaces under high-speed winding tension.
Melt pump operation in cast film lines is affected by the viscosity reduction effect at the die wall rather than by bulk melt temperature changes. When the masterbatch is omitted, die pressure measured before the melt pump commonly exhibits short-cycle fluctuation of ±5–8 bar; after addition, the fluctuation band narrows to ±2–3 bar in the same line configuration. This is the practical signal used by operators to confirm that the active component has established a stable coating at the die lip.
Heavy-duty shipping sacks produced from LLDPE/HDPE blends often exhibit melt fracture bands at the die lip, especially when the melt index of the LLDPE component falls below 0.7 MI. For tubular film extrusion using a 250 mm die with a 2.0 mm die gap, a blow-up ratio of 2.0:1, and an internal bubble cooling system, HYBOOST® 400 Masterbatch, LLDPE is introduced at 0.6–1.2 wt%. The downstream production process is low-stalk bubble extrusion, where the bubble is kept below the die face by 1.0–1.5 m to improve molecular orientation and yield strength; this is followed by gusseting, surface treatment if printing is required, and flat or center-surface winding. Terminal finished articles are 80–120 µm heavy-duty shipping sacks, FIBC liner film, and industrial drum liners. Compliance for mechanical suitability is evaluated by ASTM D1709-22 for dart impact and ISO 527-3:2018 for tensile strength at break; the final sack article is often qualified under the customer's transport packaging protocol rather than a single ISO sack standard. The relevant food-contact framework, if the liner is used for contact with dry food, is FDA 21 CFR 177.1520 and EU No 10/2011. Processing observations show that head pressure on a 75 mm extruder running 350 kg/h is reduced by 12–20% after masterbatch introduction, with the disappearance of sharkskin bands on the film surface. Pre-drying is not required for the masterbatch; moisture uptake of the LLDPE carrier at 60% RH remains below 0.01 wt%.
The operational limitation is the interaction with high levels of recycled content: calcium carbonate and other fillers can adsorb the processing aid and delay the onset of die coating, so the dose should be increased only after verifying filler content and melt filtration through a screen changer. Avoid combination with high-surface-area mineral fillers in the same layer where a stable die coating must be formed within 15–30 min of production start-up.
| Conversion method | HYBOOST® 400 Masterbatch, LLDPE let-down range | Processing equipment configuration | Observed processing modification |
|---|---|---|---|
| High-stalk blown film | 0.5–1.5 wt% | single-screw L/D 30:1, die gap 1.8 mm, blow-up ratio 2.5:1 | die pressure reduction, reduced sharkskin |
| High-speed cast film | 0.8–2.0 wt% | slot die 0.5 mm, line speed >400 m/min | delayed die lip build-up, improved edge pinning |
| Heavy-duty sack tubular film | 0.6–1.2 wt% | die gap 2.0 mm, blow-up ratio 2.0:1, output 350 kg/h | lower head pressure, fewer melt fracture bands |
Extrusion lamination coating of paperboard and aluminium foil with low-melt-index LLDPE often generates significant die lip oxidation and neck-in variation at speeds above 150 m/min. In this process, HYBOOST® 400 Masterbatch, LLDPE is dosed at 1.0–2.5 wt% into a 120 mm single-screw extruder feeding a T-die with a width of 1200 mm and an air gap of 150 mm. The melt web is drawn onto a primed substrate and pressed against a chill roll at 15–20°C, with corona or flame treatment before the pressure roll. Terminal finished articles are 15–30 g/m² extrusion coating layers on liquid packaging board, aseptic cartons, coffee bag laminates, and coated paper for food service. Compliance for food-contact articles is governed by EU No 10/2011 Annex I and Annex II for overall and specific migration, and FDA 21 CFR 177.1520 for the olefin polymer layer. The addition ratio must not exceed 2.5 wt% in this process because higher levels have been observed to interfere with substrate adhesion after flame treatment; the LLDPE carrier can alter the surface polarity development at the melt-web-to-substrate interface. Unlike tubular film extrusion, no internal bubble stability issue exists; the critical variables are melt web edge pinning and oxidized-LLDPE byproduct formation, both of which are mitigated by maintaining the die lip deposit control provided by the masterbatch.
Neck-in behavior on a 1200 mm T-die is typically measured as the difference between die width and coated substrate width. On lines without processing aid, neck-in values of 70–90 mm per edge are observed; with the masterbatch in the feed, neck-in stabilizes at the lower end of this range and the melt web edge remains continuous at 180 m/min. This is a direct downstream-processing variable affecting trim waste and substrate coverage.
Shrink hood and stretch hood films for pallet containment are produced on three-layer coextrusion blown film lines with annular dies of 300–400 mm and die gaps of 1.2–1.5 mm. HYBOOST® 400 Masterbatch, LLDPE is added to the outer layers at 0.4–1.0 wt% of layer mass; the core layer contains no processing aid in this configuration to preserve interlayer adhesion. The downstream production process is coextruded blown film with internal bubble cooling, blow-up ratio 3.0:1, frost line height 1200 mm, and collapsing frames with gusseting before wind-up. Terminal finished articles are 100–200 µm shrink hood film and stretch hood film for pallet wrapping, typically printed with flexographic inks after corona treatment to 45–50 mN/m. Compliance for these films is anchored to ASTM D2732-23 for unrestrained linear thermal shrinkage, ISO 14616:2019 for shrinkage stress in polyethylene heatshrink film, and RoHS Directive 2011/65/EU Annex II for restricted substances in packaging components. The lower addition limit of 0.4 wt% is set by the need to prevent die-lip deposit during extended production runs of mixed scrap-containing resin batches, while the 1.0 wt% upper limit is set by the requirement to maintain strong gusset welds during shrink installation. Processing experience shows that die pressure fluctuations are reduced when the masterbatch is fed through a side-port gravimetric feeder rather than tumble-mixed, because tumble-mixing can segregate the masterbatch particles from the base resin pellets at hopper discharge.
Gauge uniformity in this process is controlled by an automatic capacitance or near-infrared gauge system interfaced with the air ring. When die pressure is unstable, the gauge loop compensates by changing air ring pressure rather than correcting melt distribution; this leads to film thickness variation of ±5–8% across the web. Stable die pressure after masterbatch addition keeps the gauge loop within ±3% on lines where the collapsing frame is correctly aligned.
| Application zone | Standard or regulation | Test method / clause |
|---|---|---|
| Agricultural silage film | EN 13206:2017 | thickness, stretch retention, UV stabilization retention |
| Food-contact cast film | EU No 10/2011 | overall migration into food simulants A, B, D2 |
| Olefin polymer articles | FDA 21 CFR 177.1520 | density, melt index, extractable fraction |
| Shrink hood film | ASTM D2732-23 | unrestrained linear thermal shrinkage |
| Heatshrink polyethylene film | ISO 14616:2019 | shrinkage stress and contraction stress |
When HYBOOST® 400 Masterbatch, LLDPE is introduced into a five-layer blown film coextrusion line producing barrier packaging films, the processing aid is confined to the two outer layers at 1.0–1.5 wt% of the skin layer mass. The production process uses a five-layer annular die with spiral mandrel distribution, die diameter 400 mm, die gap 1.0 mm, internal bubble cooling, and oscillating haul-off; layer distribution is controlled by gravimetric dosing at each extruder. Terminal finished articles are 35–70 µm barrier films for dairy packaging, meat vacuum pouches, and stand-up pouch laminates, where the core contains EVOH or polyamide and the tie layers are maleic anhydride-grafted polyolefin. Compliance for food contact is evaluated under EU No 10/2011 Annex IV for overall migration into simulants A, B, and D2, and FDA 21 CFR 177.1520 for the polyolefin skin layers. Mechanical and optical quality are tested under ASTM D882-18 and ASTM D1003-13 for haze and total transmittance. The specific operational boundary is that the masterbatch must not be placed in the tie or barrier layers; the LLDPE carrier is not compatible with EVOH melt flow at the interface and can cause layer thickness variation. Published data for this specific configuration is limited, but production-scale observations indicate that skin-layer addition reduces die-lip deposit around the die outer circumference and improves bubble stability at blow-up ratio 2.8:1.
The die-lip deposit in five-layer barrier film production is frequently concentrated at the outer skin layer because the outer extruder operates at higher melt temperatures to improve surface gloss. As the active component migrates to the die surface, the outer layer melt stream maintains a continuous slip boundary while the EVOH core remains isolated from the die metal. This is the rationale for excluding the masterbatch from the tie layers, where interfacial residence time would delay the formation of a stable die coating.
Competitive Entec HYBOOST® 400 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Entec HYBOOST® 400 Masterbatch, LLDPE is a pelletized additive concentrate supplied in a linear low-density polyethylene carrier matrix. The product is handled as a free-flowing solid for direct gravimetric addition to polyethylene film, sheet, and extrusion coating operations. The trade designation identifies a specific additive loading and carrier resin combination; however the supplier does not publish the complete additive chemistry or the exact active concentration in this technical overview. Lot-specific certificates of analysis should be requested before equipment settings are fixed.
The material is intended for LLDPE-rich systems. It is not offered as a universal masterbatch for polar resins, plasticized polyvinyl chloride, polyamide, or polycarbonate melt streams. In polyolefin film operations, it can be introduced at the feed throat with a separate gravimetric feeder or preblended with the main LLDPE resin in a tumble mixer at the converter’s site. Long-distance preblend transfer should be controlled to prevent pellet segregation.
Production experience on LLDPE blown film lines with single-screw extruders at L/D 24:1 to 30:1 indicates that a masterbatch approach allows additive dispersion during transition-section melting. The effect is most visible when die pressure reductions are monitored. Before installation, a baseline extrusion run should be recorded with virgin resin to document die pressure, motor load, melt temperature, and bubble stability.
Melt fracture is typically observed as matte, angular surface defects near the die exit. On high-speed LLDPE blown film lines, the defect is governed by wall shear stress at the die lip. Capillary rheometry conducted according to ISO 11443:2021 is used to determine the critical shear rate. When a process-aid masterbatch is added, the measured apparent shear viscosity at a given shear rate may decrease only slightly in the capillary; the main commercial benefit appears as a delay of melt fracture onset in the die itself. This discrepancy means that capillary data alone should not be used to define the optimum addition level.
The product should be metered at the resin inlet using a gravimetric dosing device. Single-screw volumetric augers may be insufficient because pellet bulk density variations can change the let-down ratio. Feed throat bridging, inconsistent pellet flow, or static charge at the hopper often indicates moisture uptake or low ambient humidity. A calibrated loss-in-weight feeder is preferred for consistent addition in thin-film lines operating with tight haze and gel specifications.
When the product is first introduced, die-lip build-up may transiently increase before the new additive package stabilizes. Operators have noted that the transition period can be shortened by maintaining a constant die temperature and by avoiding rapid screw-speed adjustments. If the line is stopped, the die gap should be purged with virgin LLDPE before restart. The product does not eliminate the need for purging; it only changes the time required to reach steady surface quality.
In cast film lines with flat dies, the same principle applies, but the absence of bubble stretching means surface roughness at the chill-roll contact is more visible. The masterbatch may be evaluated by measuring haze per ASTM D1003 and gloss at 60° per ASTM D2457. Published data for this specific configuration is limited; therefore acceptance criteria must be established by the converter.
Storage of the masterbatch should occur in a closed container below 30°C and below 60% relative humidity. Exposure to higher humidity can produce surface moisture. If pellet bridging or feed throat condensation is observed, dehumidified-air drying at 60°C to 70°C for 2 h to 4 h is usually sufficient. Moisture content can be checked by ISO 15512 Method B. Thermal stability in the carrier resin can be monitored by thermogravimetric analysis under nitrogen according to ISO 11358-1. Lot-specific degradation onset values are not substituted here because the supplier’s certificate of analysis is the controlling document.
Polyethylene carrier oxidation can be assessed by oxidative induction time using ISO 11357-6. A reduced oxidative induction time relative to virgin resin indicates antioxidant consumption or surface contamination. The masterbatch should not be stored near copper-based heat stabilizers or open amine-containing additives. Combination with certain amine-based additives may cause acid-base interactions that neutralize the processing-aid chemistry and reduce melt stability. Compatibility testing on the actual production formulation is required.
Prolonged exposure to ultraviolet radiation should be prevented because the carrier resin may undergo chain scission, producing low-molecular-weight oxidation products that influence film seal strength. The product is supplied in packaging that should remain sealed until immediately before use. Partially used containers should be reclosed and stored under the same controlled conditions.
Compared with conventional fluoroelastomer-based polymer processing aid masterbatches supplied in high-density polyethylene carriers, the LLDPE carrier in HYBOOST® 400 is mechanically miscible with LLDPE film resins over a broad melt-index range. In contrast, high-density polyethylene-carrier processing aids may require additional melt-temperature adjustment to avoid carrier-induced gel specks in films below 25 µm. Ethylene-vinyl acetate carrier systems can introduce polar comonomer residues that affect seal initiation temperature and coefficient of friction. These class-level differences are derived from general polymer compatibility principles; no direct comparative study of HYBOOST® 400 against specific commercial grades is published in this technical overview.
| Parameter or Compliance Scope | Reference Method or Standard | Verification Requirement |
|---|---|---|
| Melt mass-flow rate of carrier resin | ISO 1133-1:2022 | Lot certificate of analysis |
| Density of carrier resin | ISO 1183-1 | Lot certificate of analysis |
| Moisture content after storage | ISO 15512 Method B | Internal dryness check above 60% RH exposure |
| Oxidative stability of carrier | ISO 11357-6 | Comparative oxidative induction time against virgin LLDPE |
| Food-contact migration evaluation | EU 10/2011, FDA 21 CFR 177.1520 | Supplier confirmation on final film at intended worst-case time-temperature conditions |
| Heavy metals restrictions | Directive 2011/65/EU RoHS | Supplier declaration for homogeneous material |
| REACH SVHC status | Regulation EC 1907/2006 | Safety data sheet Section 15 reference |
Conduct experimental confirmation on the target film structure before full-scale conversion. The first production trial should be limited to one extruder, with continuous monitoring of die pressure, motor load, melt temperature, and bubble stability. Samples should be collected every 15 min during the transition period to establish when surface quality reaches steady state. For food-contact packaging, migration testing under the intended worst-case time-temperature conditions is required using the final film, not the masterbatch alone, because dilution and processing alter the additive distribution.
Because the exact additive chemistry is not disclosed in this overview, analytical verification of the final film by Fourier-transform infrared spectroscopy or gas chromatography–mass spectrometry should be developed using the supplier’s reference spectra. A lot-specific certificate of analysis, safety data sheet Sections 1 through 16, and migration compliance statement are required documents before use in FDA 21 CFR or EU 10/2011 applications.
Addition-rate optimisation requires stepwise trials from a supplier-confirmed starting point. The concentrate is not intended as a filler. Over-addition beyond the supplier’s maximum recommended loading may cause film clarity loss and potential die-lip deposit accumulation. Published data for this specific configuration is limited; the processing boundaries described here are based on general behaviour of LLDPE-carrier masterbatches and should be verified for each converter’s resin blend, die geometry, and output rate.
Die pressure transducers should be installed upstream of the die entrance to quantify pressure reduction. Operators should record melt temperature at the adapter and die body. A stable reduction in die pressure without a corresponding increase in motor load indicates that the masterbatch is acting at the die wall rather than simply diluting the LLDPE viscosity. If motor load increases while die pressure remains unchanged, the addition level may exceed the useful range or the additive may not be fully dispersed.
For coex film structures, the masterbatch is generally added to the layer that exhibits surface melt fracture. In high-speed five-layer lines, the addition point is often the skin layer hopper. However, the choice of layer should be confirmed by measuring defect density on the finished web. Published data for this specific configuration is limited, so a single-layer pilot trial is recommended before multidie commercial qualification.
The product is not a substitute for correct die design. It will not correct severe melt-temperature maldistribution, damaged die lips, or improperly designed spiral mandrels. If the die gap is severely worn or uneven, surface defects may persist even after effective additive dispersion. Operators should verify die lip flatness and concentricity before attributing residual melt fracture to formulation limitations.