Entec Hyboost 329 Masterbatch Lldpe

Entec HYBOOST® 329 Masterbatch, LLDPE

    • Product Name: Entec HYBOOST® 329 Masterbatch, LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 281584
    Productname Entec HYBOOST® 329 Masterbatch, LLDPE
    Manufacturer Entec
    Additivetype Nucleating agent
    Carrierresin LLDPE
    Physicalform Pellets
    Color White
    Specificgravity 0.92 g/cm³
    Meltflowrate 20 g/10 min
    Moisturecontent ≤0.1%
    Activecontent Proprietary
    Recommendeddosage 1-5%
    Processingtemperature 180-260°C
    Packaging 25 kg bags
    Shelflife 12 months
    Storageconditions Cool, dry place

    As an accredited Entec HYBOOST® 329 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Entec HYBOOST® 329 Masterbatch, LLDPE comes in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped for secure storage and transport.
    Container Loading (20′ FCL) Entec HYBOOST® 329 Masterbatch, LLDPE, loaded in a 20′ FCL dry container; palletized, ambient, secured per applicable transport regulations.
    Shipping Entec HYBOOST® 329 Masterbatch, LLDPE typically ships as non-hazardous industrial material in sealed bags or pails, palletized and shrink-wrapped. Transport in cool, dry, ventilated conditions away from moisture, heat, direct sunlight, and physical damage. Ensure packages remain closed, labeled, and handled with standard PPE.
    Storage Store Entec HYBOOST® 329 Masterbatch, LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep original containers tightly closed and palletized, avoiding excessive stacking or contamination. Maintain ambient storage temperatures, ideally below 40°C. Follow good inventory practice (FIFO) and use within the recommended shelf life. Avoid contact with incompatible materials.
    Shelf Life Shelf life is 12 months from date of manufacture when stored in original, unopened packaging in a cool, dry place.
    Application of Entec HYBOOST® 329 Masterbatch, LLDPE

    In three-layer LLDPE blown film lines producing 80–220 µm heavy-duty liners, sharkskin melt fracture typically begins at die land shear rates above 500 s⁻¹ when the melt is held below 200 °C at the die exit. HYBOOST 329 is introduced at 0.5–1.5 wt% by gravimetric pellet blending before the extruder throat; feeding into the hopper throat rather than into a secondary mixing port prevents concentration stratification in the barrier screw channel. The process runs a 24:1–30:1 L/D single-screw extruder, die gap 1.6–2.0 mm, die land length 2.0–3.0 mm, blow-up ratio 2.2:1–3.0:1, and bubble cooling by dual-lip air ring. The film formulation must comply with the LLDPE carrier provisions of FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011 for food-contact migration; industrial non-food articles require REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU assessment. Tensile properties are benchmarked to ASTM D882-18. Terminal articles are heavy-duty sacks, industrial bin liners, and protective packaging for bulk chemicals.

    What Controls Die-Lip Deposit Accumulation in High-Rate Cast Film Extrusion?

    Cast film lines converting LLDPE stretch film at line speeds above 250 m/min develop die-lip deposit at the slot exit when the polymer fraction contains short-chain branches that migrate under shear. The masterbatch is added at 0.3–1.0 wt% in the pellet blend before the extruder, not injected into the melt stream; pellet blender residence time must be at least 3 min to avoid local additive imbalance. Process configuration: single-screw extruder 30:1–36:1 L/D, barrier flight geometry, slot die gap 0.8–1.2 mm, air knife and vacuum-edge pinning, chill roll at 18–24 °C. The regulatory basis for food-grade cast film is FDA 21 CFR 177.1520 for the LLDPE fraction and EU Regulation (EU) No 10/2011; migration is verified according to the intended food-contact surface. Film mechanical properties are measured according to ASTM D882-18 and ISO 527-3:2018. Terminal products include hand-wrap stretch film, machine-wrap silage film, and food overwrap where the masterbatch is kept below the food-contact migration threshold established in the end-use formulation.

    For extrusion coating and LLDPE lamination lines operating at 250–450 m/min, the melt is drawn from a coat-hanger die at a melt temperature of 290–315 °C; the concentrate is dosed at 0.5–1.2 wt% to stabilize the film edge and reduce neck-in during drawdown. The process is a single-screw coater-laminator with 28:1–32:1 L/D extruder, a 0.6–0.9 mm die gap, and an air gap of 100–250 mm before the nip. Compliance for board and liquid packaging applications requires the LLDPE carrier to be covered by FDA 21 CFR 177.1520 and the finished laminate to be tested under EU Regulation (EU) No 10/2011 for overall migration. Melt flow consistency is verified by ISO 1133-1:2022; substrate adhesion is tested according to ASTM D1876-08(2015)e1 for peel strength. Terminal end products include paperboard cupstock, liquid carton board, and barrier laminating webs for flexible packaging.

    Compliance matrix applied across LLDPE-carrier processing aid masterbatch applications
    Standard/regulationDesignationScopeVerification point
    FDA 21 CFR177.1520Olefin polymers in food-contact article componentsCarrier resin in film, coating, and molded closures
    EURegulation (EU) No 10/2011Plastic materials and articles intended to contact foodOverall migration testing of finished articles
    ISO1133-1:2022Melt mass-flow rate and melt volume-flow rateIncoming batch and dilution verification
    ASTMD882-18Tensile properties of thin plastic sheetingCast and blown film property retention
    ASTMD638-14Tensile properties of plasticsMolded and rigid extruded articles
    REACHRegulation (EC) No 1907/2006Registration, evaluation, authorisation and restriction of chemicalsSubstances in the masterbatch formulation
    RoHSDirective 2011/65/EURestriction of hazardous substancesElectrical and electronic cable/component jacketing

    Blow Molding Parison Wall Stability and Die Pressure Response in LLDPE-Rich Container Formulations

    In extrusion blow molding of LLDPE-rich containers of 5–30 L, parison drawdown and wall thinning are governed by the elongational viscosity of the melt leaving the die bushing. The masterbatch is dosed at 0.5–1.5 wt% and mixed with the container compound before the hopper. Process configuration: single-screw extruder 24:1–30:1 L/D, grooved feed throat, die head temperature 195–215 °C, blow pressure 0.6–0.8 MPa, and mold clamp force 800–1,500 kN. Compliance for industrial packaging is covered by FDA 21 CFR 177.1520 for the carrier resin; hazardous goods packaging requires UN 6.1.5 stack and drop certification for the finished jerrycan. Mechanical property validation is performed according to ASTM D638-14 and ASTM D1238-20 for melt consistency. Terminal articles include agricultural chemical drums, industrial liquid containers, and small-volume jerry cans where die pressure drift on multi-cavity heads must remain below 5% across shift-running conditions.

    When LLDPE-Rich Compounding Appears in Monofilament and Tape Extrusion for Industrial Fabrics

    The high-shear slot die used for LLDPE-rich monofilament and tape extrusion produces gel-like deposits at the die edge when the melt is run above 220 °C for prolonged campaigns. HYBOOST 329 is added at 0.3–1.0 wt% to the pellet blend; dosing above 1.2 wt% is not recommended because the additional carrier fraction can reduce tape tensile modulus. Process configuration: single-screw extruder 28:1–32:1 L/D, flat slot die, water bath at 28–35 °C, primary draw ratio 1.5:1–3.5:1, hot-air annealing tunnel at 90–110 °C. Pre-drying is not routinely required; however, if the masterbatch bag is opened above 60% relative humidity for more than 4 h, purge 2 kg through the feeder before start-up. Regulatory compliance for industrial fabrics falls under REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU; food-contact woven sacks require LLDPE carrier compliance with FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011. Tensile properties are measured according to ISO 527-3:2018 and ASTM D638-14. Terminal articles are geotextile tapes, artificial grass fibre, and woven sack fabric for industrial and agricultural use.

    In pipe and profile extrusion of LLDPE-based chemically resistant industrial tubing, the use of the masterbatch at 0.5–1.5 wt% is concentrated in the skin layer in coextruded multilayer configurations; in monolayer configurations it is preblended with the pellet stream. Process configuration: single-screw extruder 30:1–36:1 L/D with grooved feed zone, die head pressure 12–18 MPa, melt temperature 190–210 °C, vacuum calibration tank water at 15–25 °C, and haul-off speed controlled by wall thickness measurement. Industrial pipe systems are validated to ISO 1167-1:2006 for hydrostatic strength and ISO 178:2019 for flexural properties; chemical resistance is screened according to ISO 175:2010. Compliance under REACH and RoHS applies; no potable water approval is implied. The LLDPE carrier is covered by FDA 21 CFR 177.1520 only for article components, not for potable water contact. Terminal articles include drainage pipes, protective cable ducts, and industrial effluent tubing.

    Injection molding of thin-wall closures benefits from controlled masterbatch dosing only under high-shear gate geometries

    The shear rate at the gate in thin-wall injection molding of LLDPE-based closures routinely exceeds 50,000 s⁻¹; at such shear rates the masterbatch addition must be limited to 0.2–0.8 wt% to avoid excessive melt slip that produces gate blush. Process configuration: high-speed injection molding machine with clamp force 1,500–3,000 kN, barrel temperature profile 180–210 °C, mold wall temperature 25–35 °C, injection speed 150–300 mm/s, and back pressure 5–10 bar. Compliance for molded articles is benchmarked to ASTM D638-14, ISO 1133-1:2022, and, for food-contact closure systems, FDA 21 CFR 177.1520 plus EU Regulation (EU) No 10/2011 overall migration testing. Published comparative shear-rate data for this specific masterbatch under >50,000 s⁻¹ gate flow is limited; molders should qualify on the target hot-runner tool. Terminal end products include pail lids, closure caps, and dispensing fitments where the gate mark is hidden or removed.

    Free Quote

    Competitive Entec HYBOOST® 329 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Entec HYBOOST® 329 Masterbatch, LLDPE is a pelletised additive masterbatch supplied in a linear low-density polyethylene carrier. The grade identifier 329 is a manufacturer-specific model code; it does not encode additive concentration, melt flow rate, or regulatory clearance status. The material is intended for let-down into polyolefin film, sheet, and extrusion coating operations, where the LLDPE carrier is selected to reduce differential melting and compatibility errors sometimes observed with LDPE-based or HDPE-based concentrates. Because the carrier is LLDPE, its crystallinity, feed-zone softening behaviour, and melt rheology differ from those of a conventional low-density polyethylene carrier.

    The product is a delivery system for an active additive package, not a final compound. No end-use performance claim is made without reference to that active package. Supplied as free-flowing pellets, the material is typically handled through gravimetric feeders and should be protected from prolonged exposure to high humidity. Lot-specific certificates of analysis are required before setting let-down ratios, because the carrier resin alone does not define the additive concentration or thermal stability limit.

    How Is HYBOOST® 329 Introduced on a Single-Screw Film Line Without Causing Feed Bridging?

    On a 65 mm single-screw extruder with a 30:1 L/D ratio and a grooved feed section, LLDPE-based masterbatch pellets can be dry blended with the main resin at the throat. Gravimetric feeding is preferred over volumetric feeding because pellet shape, bulk density, and surface hardness differences can produce feed-rate drift even when the nominal feeder setpoint is unchanged. The hopper throat should be maintained below 40 °C using water-cooled feed-zone jackets; otherwise, LLDPE pellets may soften at the throat and form a cohesive mass that disrupts solids conveying. The resulting screw-speed to output relationship becomes nonlinear, and melt pressure may oscillate at the die by more than ±5 bar.

    No universal addition rate can be derived from the carrier resin alone. The manufacturer’s lot-specific let-down recommendation must be applied. Industrial practice for additive masterbatches in polyolefin film extrusion often operates between 2 wt% and 10 wt%, but published data for this specific configuration is limited. In thin-wall injection moulding of LLDPE-rich compounds, the masterbatch is more commonly added at 1 wt% to 3 wt% to avoid shifting the compounded melt flow rate outside the moulding window. Processors should measure the compounded melt mass-flow rate according to ASTM D1238-20 or ISO 1133-1:2022 before setting injection pressure profiles.

    For film lines without an additional mixing element, dispersive mixing may be insufficient when the masterbatch is introduced at high let-down ratios. A Maddock mixing section or a barrier screw with an intensive mixing tip is preferable to avoid additive-rich streaks. If only a general-purpose single-thread screw is available, screw speed should be limited to a range that maintains melt temperature at the die adapter below 230 °C. At equivalent output, LLDPE-based masterbatch may produce a slightly higher melt pressure than an LDPE-based masterbatch at low screw speeds, but the pressure differential tends to narrow as screw speed increases because LLDPE shear-thins more strongly than LDPE. Capillary rheology data measured under ASTM D3835 can quantify this difference for a given lot.

    Where the active package is heat-sensitive, a processing window of ±5 °C around the recommended melt temperature should be treated as a controlled process boundary. A temperature deviation beyond that window may produce measurable changes in film appearance, odour, or additive retention. Lot-specific thermal stability data should be requested from the supplier before establishing production setpoints.

    Because the active chemistry in HYBOOST® 329 is proprietary, published data for this specific configuration is limited. The matrix below separates carrier-dependent parameters, which are constrained by LLDPE resin-class behaviour, from additive-dependent parameters, which require lot-specific documentation. The values listed are representative of LLDPE carrier masterbatch behaviour and must not be used as lot-specific acceptance criteria.

    ParameterTest designationTechnical note
    Carrier melt mass-flow rate at 190 °C/2.16 kgASTM D1238-20 / ISO 1133-1:2022Report from certificate of analysis; no generic melt flow rate applies to the fully compounded masterbatch.
    Carrier density at 23 °CASTM D792-20 / ISO 1183-1:2019LLDPE film resin carriers commonly fall within 0.918–0.925 g/cm³; grade-specific confirmation is required.
    Melting peakASTM D3418 / ISO 11357-3Typically 120–126 °C for LLDPE carrier on second heating; melting peak is not a processing target.
    Moisture contentASTM D6869 / ISO 15512:2019Unopened bags typically below 0.10 wt%; pre-drying may be required after exposure to high humidity.
    Bulk densityASTM D1895Pellet bulk density typically 0.48–0.54 g/cm³; feeder calibration is required for accurate let-down.
    Additive concentrationNot applicableMust be verified from the lot-specific certificate of analysis; no generic specification is valid.

    Where the product is used in moisture-sensitive operations, lot-specific Karl Fischer data should be requested. If opened bags show visible condensation or storage relative humidity exceeds 60%, pre-drying with dry air at 70–80 °C for 2–4 h may be applied. The supplier should confirm whether the active package tolerates temperatures above 80 °C before any drying step is performed.

    Thermal and Rheological Boundaries Are Not Set by the Carrier Resin Alone

    For blown film lines, the die adapter melt temperature should be kept below the decomposition threshold of the active package, not merely below the carrier resin degradation point. LLDPE carriers can generally be processed at 190–230 °C; however, the active additive chemistry may be more heat-sensitive than the carrier. A lower melt temperature not only protects the active chemistry but also reduces die lip build-up on 90 mm spiral mandrel dies. At die temperatures above 225 °C, low-molecular-weight carrier fractions may volatilise and condense on the air ring, producing surface defects on the bubble.

    Rheologically, LLDPE exhibits higher low-shear viscosity than LDPE at the same melt index, but it may show stronger shear-thinning. Replacing an LDPE-based masterbatch with HYBOOST® 329 may therefore require a slight reduction in screw speed if the extruder is operating near its maximum motor load. The melt pressure difference is machine-dependent; direct machine trials are required because published data for this specific comparison is limited. On a 65 mm extruder running at 120 kg/h, a switch from LDPE carrier to LLDPE carrier may alter specific drive power, but no universal percentage can be assigned without lot-specific capillary rheology data.

    Bubble stability in blown film can also be affected by the carrier resin fraction. LLDPE has a different extensional viscosity and melt strength behaviour than LDPE. When the masterbatch is used at high let-down ratios, bubble height, frost line position, and blow-up ratio should be re-optimised. The relevant film tensile properties should be evaluated according to ASTM D882 or ISO 527-3 to determine whether the carrier contribution reaches statistical significance.

    If LDPE-Based Masterbatches Are Replaced with HYBOOST® 329 in High-Speed Cast Film, Which Machine Adjustments Are Required?

    In cast film, the carrier resin influences chill-roll adhesion, neck-in, and die pressure. When an LDPE-based masterbatch is replaced by an LLDPE-based concentrate, the extruder may develop a higher die pressure at equivalent output because of the higher low-shear viscosity of LLDPE. The die should not be arbitrarily opened. Screw speed and barrel temperatures should be trimmed so that melt temperature at the adapter remains within the product window. The chill-roll contact temperature is not influenced by the masterbatch alone, but any change in melt viscosity can shift the air gap required for optimum web stability.

    Operators should anticipate a slightly higher neck-in and possibly a higher film modulus when LLDPE carrier is present at high let-down ratios because the carrier contributes to the final matrix. For a cast line running 150 µm sheet, a masterbatch addition of 3 wt% is unlikely to dominate film properties. At 15 µm thin film, however, the carrier resin may measurably affect tear behaviour, drawdown, and stretch response. A design-of-experiments approach across at least three let-down ratios is recommended before finalising a production specification.

    If the line uses automatic die gap adjustment, the control loop should be retuned after the carrier change. LLDPE-rich melt may generate a different die pressure response slope, and a previously stable controller can oscillate if the gain constants are not updated. Melt pressure transducers upstream and downstream of the breaker plate should be monitored for a minimum of 30 min after stabilisation to detect carrier-induced pressure drift.

    Regulatory documentation for a masterbatch of this type must be separated into carrier and active-substance compliance. The LLDPE carrier can be compared against FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, Annex I, but these references do not automatically clear the complete masterbatch for direct food contact. The active package requires its own positive listing and migration testing under the intended conditions of use. Under REACH Regulation (EC) No 1907/2006, the article or substance tonnage triggers registration and Safety Data Sheet extended exposure scenarios; consult the supplier for current registration status. RoHS Directive 2011/65/EU heavy-metal restrictions apply only if the finished article falls within an electrical and electronic equipment category; nevertheless, cadmium, lead, mercury, and hexavalent chromium content should be tracked through lot certificates.

    Combination with metallic stearate lubricants at high loadings should be avoided without prior thermal stability testing. Metallic stearates can alter the melt viscosity of the carrier and may interfere with active dispersion. Amine-based additives may interact with acid-functional chemistries; if the active package is acid-reactive, such a combination could reduce effectiveness. Published compatibility data for this specific formulation is limited; a small-scale extrusion trial is recommended before plant-wide adoption.

    Comparative Handling and Dilution Characteristics Against HDPE and Neat Additive Systems

    The following matrix compares general carrier-related handling behaviour, not active package performance. The entries are based on publicly reported processing behaviour of LLDPE, LDPE, and HDPE carriers under film extrusion conditions.

    Handling characteristicHYBOOST® 329 LLDPE carrierLDPE carrier masterbatchHDPE carrier masterbatchNeat liquid additive
    Carrier density at 23 °C0.918–0.925 g/cm³0.920–0.930 g/cm³0.940–0.965 g/cm³Not applicable
    Crystalline melting peak120–126 °C105–115 °C130–137 °CNot applicable
    Feed-zone softening tendencyLower than LDPE at same feed temperatureHigher; feed throat must remain below 40 °CLower than LDPENo pellet softening; requires pumping
    Compatibility with LLDPE film matricesHighModerateFairDepends on additive solubility
    Volatile handlingNoneNoneNoneSolvent/volatile emissions may require extraction
    Feeding accuracyGravimetricGravimetricGravimetricLiquid injection with mass-flow meter

    On high-speed lines, a recurrent failure mode is pellet segregation in dry blends when the bulk density difference between masterbatch and matrix exceeds 0.05 g/cm³. This can be eliminated by pellet-to-pellet preblending in a low-shear ribbon blender rather than relying on the screw flight to homogenise. If a side stuffer is available on a twin-screw line with 40:1 L/D and vacuum devolatilisation, the masterbatch should be introduced downstream of the melt seal to minimise exposure to high temperatures. Consistent lot-to-lot additive concentration must be verified by incoming quality control; a single lot with a concentration error above 10% relative can shift the final let-down ratio outside the specification window even when the feeder setpoint remains unchanged.

    Top