| HS Code | 651668 |
| Product Name | Entec HYBOOST® 291 Masterbatch, LLDPE |
| Carrier Resin | LLDPE |
| Form | Pellets |
| Color | White |
| Active Ingredient | Fluoroelastomer |
| Additive Function | Polymer processing aid |
| Active Content | 20% |
| Density | 0.920 g/cm³ |
| Melt Flow Rate | 2.0 g/10 min (190°C/2.16 kg) |
| Recommended Let Down Ratio | 1-3% |
| Processing Temperature | 180-230 °C |
| Moisture Content | <0.10% |
| Shelf Life | 24 months |
As an accredited Entec HYBOOST® 291 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Entec HYBOOST® 291 Masterbatch, LLDPE is supplied in 25 kg polyethylene-lined paper bags, palletized, shrink-wrapped, for industrial use. |
| Container Loading (20′ FCL) | 20′ FCL: Entec HYBOOST® 291 Masterbatch, LLDPE loaded in standard bags on pallets, securely stowed and weather-protected for ocean transport. |
| Shipping | Entec HYBOOST® 291 Masterbatch, LLDPE is typically shipped as a non-hazardous, solid polymer masterbatch in sealed, moisture-resistant bags, boxes, or octabins. Protect from moisture, heat, and direct sunlight. Standard road, sea, or air freight applies. No UN number, hazard class, or packing group is normally required; confirm current SDS. |
| Storage | Store Entec HYBOOST® 291 Masterbatch, LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and ignition sources. Keep containers tightly closed, upright, and labeled. Avoid strong oxidizers. Minimize dust and static buildup. For optimal shelf life, follow the manufacturer’s recommended temperature and safety data sheet. Use appropriate containment and prevent incompatible material contact. Follow local regulations. |
| Shelf Life | Shelf life is typically 24 months when stored in original unopened packaging under dry, cool conditions, away from direct sunlight. |
Entec HYBOOST® 291 Masterbatch, LLDPE is a functional polyolefin masterbatch carried in linear low-density polyethylene. In wood-plastic composite profile extrusion, the formulation uses a matrix of LLDPE at 30–35 wt%, wood flour at 55–60 wt%, lubricant package at 1.5–2.0 wt%, and the masterbatch at 2.5–4.0 wt%. Hardwood species such as maple or oak are sieved to 40–80 mesh and pre-dried in a desiccant hopper at 105°C for 24 h to reach moisture content below 0.8 wt%. Compounding is performed on a counter-rotating twin-screw extruder with an L/D ratio of 40:1 to 52:1, a vent port operating at -0.08 MPa, and a barrel profile from 165°C to 180°C. Melt temperature measured at the die is held at 175–185°C. The anhydride functionality reacts with surface hydroxyl groups on cellulose and lignin, releasing trace water that is removed by vacuum devolatilization. Die pressure at the profile calibration inlet typically ranges from 80 bar to 120 bar. Profile cooling uses water spray tanks staged from 40°C to 15°C. Output on a 75 mm twin-screw line ranges from 180 kg/h to 260 kg/h depending on profile wall thickness and screw speed. End products include solid and hollow decking boards, privacy fencing slats, and exterior cladding profiles. Compliance is assessed under ASTM D7032-17 for wood-plastic composite deck boards and EN 15534-1:2014 for WPC profiles. The formulation is not recommended when wood flour moisture exceeds 1.0 wt% because surface splay and internal void formation increase. Published data for this specific masterbatch configuration in profiles containing rice husk rather than wood flour is limited.
Entec HYBOOST® 291 Masterbatch, LLDPE is let down at 2.0–5.0 wt% in filled LLDPE compounds where talc or coated calcium carbonate is added at 25–35 wt%. The filler is introduced through a side feeder after the polymer melt zone on a co-rotating twin-screw extruder with L/D of 44:1. Barrel temperature from the feed zone to the die is set between 185°C and 210°C, and melt temperature at the die is maintained at 190–210°C. Screw speed is held between 350 min⁻¹ and 550 min⁻¹, producing specific mechanical energy input of 0.20–0.30 kW·h/kg. The masterbatch reduces filler agglomeration by increasing interfacial wetting between the LLDPE matrix and mineral surfaces. Tensile properties are measured according to ISO 527-2, notched impact resistance according to ISO 179-1:2010, and melt flow index according to ISO 1133-1:2022. End products include thermoformed automotive trunk liners, appliance sound-deadening mats, and reusable logistics sheets. Automotive applications require material approval under IATF 16949 and emissions testing according to VDA 278. Pre-drying at 70°C for 2 h is required only when ambient relative humidity exceeds 60%. The anhydride functionality is consumed by free amine-based additives; therefore primary amine heat stabilizers must be excluded from the formulation to prevent premature coupling and viscosity increase.
Three-layer polyethylene steel pipe coating uses an adhesive tie layer prepared by letting down Entec HYBOOST® 291 Masterbatch, LLDPE at 8–15 wt% into an extrusion-grade LLDPE carrier. The steel pipe is blast-cleaned to Sa 2.5, heated to 200–240°C, and coated with a fusion-bonded epoxy primer layer of 100–150 μm. The adhesive layer is extruded through a wraparound crosshead die at 225–240°C to a thickness of 200–250 μm. A high-density polyethylene topcoat of 2.5–3.5 mm is applied immediately over the adhesive layer. Peel adhesion between the FBE primer and adhesive layer is evaluated according to ISO 21809-1:2018 methods; cohesive failure in the PE topcoat is the required failure mode. Output speeds on a pipe coating line range from 0.8 m/min to 2.0 m/min for pipe diameters from 150 mm to 600 mm. Melt temperature must not exceed 240°C for more than 10 min because the grafted functionality begins to degrade and crosslink. End products include oil and gas transmission pipelines, district heating conduits, and water transmission mains. Additional compliance may include CSA Z245.21 for polyethylene pipe coating systems where specified by the project operator.
Coextruded barrier films carrying EVOH or polyamide are produced on five-layer to nine-layer blown film lines with LLDPE skin layers and tie layers containing Entec HYBOOST® 291 Masterbatch, LLDPE at 3–7 wt%. The tie layer thickness is controlled between 5 μm and 10 μm, while the EVOH layer is maintained at 220 ±5°C. Die gap is set from 1.4 mm to 2.0 mm, blow-up ratio from 2.0:1 to 2.8:1, and frost line height from 600 mm to 900 mm. EVOH temperature excursions above 230°C for longer than 20 min generate crosslinked gel defects visible as fish eyes in the film. Interlayer adhesion is measured as T-peel strength using ASTM F904-16. The anhydride groups on the LLDPE carrier react with hydroxyl groups on EVOH or amine end groups on polyamide during melt contact in the die and bubble. End products include vacuum pouches, stand-up pouches, shrink bag laminates, and thermoformed barrier trays. Food-contact compliance is evaluated under FDA 21 CFR 177.1520 for olefin polymers, EU 10/2011 with simulant D2 and overall migration limit of 10 mg/dm² according to EN 1186-1:2002, and GB 9685-2016 for additives used in food-contact materials in China. The masterbatch is not recommended for retort structures exceeding 121°C because the LLDPE carrier softens and peel performance may decline unless the tie layer is redesigned with a higher-density functional carrier.
| Regulation | Clause / Method | Required condition |
|---|---|---|
| EU 10/2011 | EN 1186-1:2002 | Overall migration ≤ 10 mg/dm² in simulant D2 |
| US FDA | 21 CFR 177.1520 | Olefin polymer extractives limits for food-contact films |
| China | GB 9685-2016 | Permitted additive usage level and specific migration limits |
| Interlayer adhesion | ASTM F904-16 | T-peel separation with cohesive failure in tie layer |
Rotational molding of filled LLDPE parts uses a dry blend of pulverized LLDPE at 35–45 mesh, rice hull or wood fibre filler at 10–20 wt%, and Entec HYBOOST® 291 Masterbatch, LLDPE at 3.0–5.0 wt%. The blend is charged into a cast aluminium mould mounted on a shuttle-type rotational molding machine. Oven air temperature is set at 265–290°C, while internal air temperature measured by a wireless pyrometer must reach 190–205°C and remain there for 3–6 min to complete anhydride coupling at the filler interface. Biaxial rotation ratios of 4:1 to 6:1 are used, with primary-axis speed at 6–8 min⁻¹ and secondary-axis speed at 1.2–1.8 min⁻¹. Wall thickness is controlled between 4 mm and 8 mm, and demolding is not initiated until internal air temperature falls below 70°C. End products include agricultural feed troughs, seed storage hoppers, material handling bins, and insulated aquaculture tubs. Products intended for drinking water contact require NSF/ANSI 61 verification. General polyethylene storage tanks are assessed under ASTM D1998-21. The process is not suitable for filler loadings above 25 wt% because melt flow drops sharply and internal voiding increases. Where the filler contains free silica above 1.0 wt%, the anhydride functionality does not bond effectively to silica surfaces and mechanical property retention is reduced.
LLDPE-rich post-consumer reclaim containing residual polypropylene, minor cellulosic fibre, and trace aluminium foil is upgraded with Entec HYBOOST® 291 Masterbatch, LLDPE at 1.5–3.0 wt%. The recycled stream is pre-washed, near-infrared sorted, and melt filtered through screens of 100–150 mesh before compounding. Extrusion is performed on a co-rotating twin-screw devolatilization line with a first barrel zone at 180°C, downstream zones at 200–210°C, and vacuum venting at -0.09 MPa. The masterbatch improves interfacial adhesion between LLDPE and dispersed polypropylene domains up to 15 wt%, and it couples residual cellulosic fines that would otherwise form aggregate lumps. Melt flow rate is tracked using ISO 1133-1:2022, density using ISO 1183-1:2019, and Charpy impact using ISO 179-1:2010. End products include industrial pallets, underground cable covers, drainage channel grates, and agricultural posts. Compliance includes REACH registration for articles, RoHS restricted substances, and ISO 14021 recycled content claims. Feedstock limits are defined by polar contamination: PVC content above 0.5 wt% releases hydrogen chloride during extrusion and consumes the anhydride functionality; nylon contamination above 1.5 wt% forms gel particles; residual moisture above 0.3 wt% requires pre-drying before the devolatilization extruder.
In extrusion coating of LLDPE onto aluminium foil for laminate tubes and sachet structures, Entec HYBOOST® 291 Masterbatch, LLDPE is added at 2.0–4.0 wt% to the tie layer. The coating line uses a single-screw extruder with L/D of 30:1, melt temperature of 285–315°C, air gap of 150–250 mm, chill roll temperature of 15–20°C, and line speed of 80–120 m/min. Coating thickness is controlled between 15 μm and 25 μm. Peel strength is measured according to ASTM D1876-08; the required failure mode is cohesive within the polyethylene layer, not clean separation at the foil interface. The anhydride groups form carboxyl interactions with hydrated aluminium oxide on the foil surface. Above 7 wt% addition, peel adhesion does not continue to increase, while unreacted anhydride near the interface can interact with ambient moisture and increase odour or seal contamination risk. End products include toothpaste tubes, pharmaceutical laminated foil, cosmetic sachets, and food condiment pouches. Food-contact compliance is evaluated under FDA 21 CFR 177.1520 and EU 10/2011. The process is not recommended for foil preheated below 90°C because interfacial condensation water from the oxide layer reduces instantaneous adhesion. Published data for peel values on untreated aluminium foil versus chemically etched foil in this specific masterbatch configuration is limited.
Competitive Entec HYBOOST® 291 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Entec HYBOOST® 291 Masterbatch is a pelletized additive concentrate supplied in a linear low-density polyethylene carrier. It is classed among endothermic chemical foaming agent masterbatches used in polyolefin conversion; however, published data for this specific configuration is limited, and the processing windows described below derive from the general behavior of LLDPE-carrier foaming concentrates rather than from unpublished lot-specific results. The grade designation 291 separates it from other HYBOOST series products by carrier type, active ingredient class, and addition-level envelope. The material is introduced into the melt phase; typical addition points include the feed throat of a single-screw extruder with an L/D ratio of 30:1 or greater, or a side feeder on a co-rotating twin-screw compounder.
The masterbatch is pelletized to permit controlled dosing from a gravimetric feeder. Because the carrier is LLDPE, the pellets do not require the low-dust handling controls associated with powdered foaming agents. The product should remain sealed in original packaging until use; if exposed to ambient air above 60% relative humidity, moisture uptake can lower apparent bulk density and interfere with feed-throat conveying.
In melt blending, the LLDPE carrier is selected to reduce viscosity separation between the masterbatch and the polyolefin matrix. For LLDPE film resins with a melt mass-flow rate between 0.5 g/10 min and 2.0 g/10 min as measured under ISO 1133-1:2022 conditions of 190 °C and 2.16 kg, a carrier having a comparable or moderately higher MFR promotes rapid wetting and distributive mixing. On a conventional flood-fed single-screw extruder, the carrier melts in the compression zone; if the set barrel temperature is too low, undispersed masterbatch pellets can persist into the metering zone and produce localized gas release or surface defects. The use of a barrier screw with a compression ratio between 2.5:1 and 3.5:1 is generally adequate when the feed is kept dry and the hopper throat is water-cooled.
The carrier also affects pressure generation. A lower-viscosity LLDPE carrier reduces head pressure and melt temperature at high screw speeds, but excessive dilution of the active package for the sake of pressure reduction can shift the decomposition plateau. In practice, the masterbatch is pre-dispersed to a concentration that allows let-down ratios in the range of 0.5 wt% to 3.0 wt%; the exact ratio is set after short-shot and density trials. Dosing at the feed throat is preferred for single-screw lines; dosing into the melt via side stuffer is used on twin-screw lines to avoid pre-decomposition in the feed zone.
In blown film, extensional thickening of the LLDPE carrier is lower than that of an LDPE-carrier concentrate. For the same melt index, LLDPE carriers exhibit less strain hardening, which can reduce melt tension at the start of a trial but improves compatibility with linear low-density matrix resins. A reduction in bubble stability relative to an LDPE-carrier masterbatch is often observed if the matrix resin has no LDPE component and the blow-up ratio exceeds 2.5:1. The addition of 10 wt% LDPE to the film matrix is a conventional corrective step; this is a matrix-blending adjustment, not a requirement of the masterbatch itself. Melt-fracture thresholds during extrusion should be evaluated by step-ramp screw-speed experiments with melt-pressure measurements taken at the die entry.
Dispersion defects on a cast-film line using a 40:1 L/D grooved-feed extruder appear as clear or brown micro-gels if the carrier is not fully melted before the final mixing section. The use of an upstream melt-temperature probe and a screen pack with 80 mesh or 100 mesh wire screens is recommended to detect poor dispersion. Pressure drop across the screen pack should be recorded; an increase greater than 2.5 MPa over the baseline indicates partial blocking by decomposed active particles or particulate residues.
| Characteristic | Relevant method or designation | Process relevance |
|---|---|---|
| Carrier melt mass-flow rate | ISO 1133-1:2022, 190 °C, 2.16 kg | Viscosity matching with LLDPE matrix |
| Bulk density of pellets | ASTM D1895-24 | Gravimetric feeder calibration |
| Moisture content | ISO 15512:2019 | Storage and pre-drying requirements |
| Density of foamed article | ISO 1183-1:2019 | Density reduction calculation |
| Tensile properties of foamed article | ISO 527-2:2012 | Mechanical property retention |
In blown film evaluation, the masterbatch is blended with a film-grade LLDPE or LDPE/LLDPE mixture. A typical starting point is 1.0 wt%; the exact level is adjusted in 0.25 wt% increments. The extruder die gap is commonly set between 1.6 mm and 2.8 mm; a blow-up ratio between 2.0:1 and 3.0:1 is retained while frost-line height is observed. Gas evolution modifies bubble curvature and can reduce dart impact and tear strength if cell size is not controlled. Cell morphology should be checked using optical microscopy on microtomed sections; a shift to irregular cell walls at higher let-down indicates an over-concentration at the operating melt temperature. Dart impact may be recorded per ASTM D1709-24, and tear resistance may be measured per ISO 6383-2:1983.
In injection molding, the concentrate is used to modify packing behavior and reduce sink marks on thick sections. A typical evaluation uses a shut-off nozzle and a screw-back pressure of 0.5 MPa to 1.5 MPa; higher back pressure can generate shear heating and initiate decomposition before the metering zone. The mold is filled to 95% capacity by volume before the gas evolution stage, and the hold pressure is then reduced by 25% to 50% relative to the solid-molding baseline. Clamp force requirements can be assessed on machines with rated clamp force from 800 kN to 2,500 kN, but the reduction is dependent on part thickness and gate geometry. Short-shot study should be documented by part mass and void count.
In extrusion blow molding, parison swell and die swell are affected by the gas dissolved in the melt. The die temperature is usually held 5 °C to 10 °C below the hottest barrel zone to control surface roughness. The product is dry blended with the matrix resin; melt temperature should not exceed the onset of rapid decomposition for more than 3 min of residence time. Accumulated volatile by-products can produce parison holes if the die has dead spots; periodic purge with a LLDPE purging compound is therefore necessary.
In LLDPE foam sheet extrusion, the masterbatch is added to a tandem single-screw line where the primary extruder melts the resin and the secondary extruder cools the melt before the annular or flat die. Melt cooling to 115 °C to 125 °C is typical for LLDPE-based foam extrusion; the lower secondary-extruder temperature reduces gas escape through the die lip and preserves cell nucleation. At a given screw speed, increasing the let-down ratio by 0.5 wt% can reduce sheet density but also increase open-cell content. Open-cell content is measured by air pycnometry per ASTM D6226-10 or equivalent.
Exothermic foaming agents typically show a decomposition peak above 200 °C and an energy release that can create localized hot spots in the melt. Endothermic systems of the HYBOOST class decompose over a broader but lower-energy plateau, which reduces the risk of thermal runaway in large shot volumes. That difference is important in injection molding of thick-wall parts where a shot mass exceeds 500 g and retention time can be 90 s to 180 s. The LLDPE carrier also influences screw recovery and cushion control; in comparison with a low-density polyethylene carrier, the LLDPE grade tends to maintain a firmer melt at the same melt temperature, which permits slightly lower back pressure settings and reduces leakage across the check ring.
Differences from exothermic foaming agents and from powder-type chemical foaming agents are significant. Endothermic decomposition absorbs process heat, narrows the gas-evolving temperature window, and releases carbon dioxide with comparatively low gas volume per gram. Exothermic agents such as azodicarbonamide release heat and can produce higher gas volumes but may discolor the matrix or leave amine residues. The LLDPE carrier of HYBOOST® 291 further differentiates it from LDPE- or EVA-carrier grades because the carrier’s crystallization behavior and viscosity more closely match LLDPE film matrices; this reduces the concentration of low-melt-viscosity domains and improves the uniformity of cell distribution when measured by image analysis. In comparison to powdered agents, the pellet form permits direct feed from a hopper loader and lowers the airborne dust fraction, which is relevant to dust explosion and hygiene control.
Compared with other masterbatches in the HYBOOST series, the 291 designation denotes the specific LLDPE carrier and active package tailored to LLDPE-rich formulations; published data for this specific configuration is limited, so direct substitution for another series grade should be accompanied by capillary rheometry of the matrix and scanning electron microscopy of the foamed part. If the product is substituted for a powdered sodium bicarbonate/citric acid blend, the pelletized LLDPE carrier reduces worker exposure and simplifies feed with a side-feeder hopper; however, the minimum let-down ratio may be slightly higher because the active ingredient is diluted in the carrier.
Product qualification should record the density, tensile energy-to-break, and cell population. Density is measured by water displacement per ISO 1183-1:2019; cell size distribution is measured by optical or scanning electron microscopy with image segmentation. The mechanical property loss at a given density reduction should be compared to the unfoamed control, not to an absolute material specification. Compliance of the LLDPE carrier with FDA 21 CFR 177.1520 may be available for food-contact packaging; compliance of the active package must be confirmed for each application because decomposition residues participate in the final matrix. Heavy-metal and phthalate restrictions under RoHS Directive 2011/65/EU and REACH (EC) 1907/2006 should be verified from the supplier’s safety data sheet or statement of compliance.
For food-contact packaging, migration testing under EU 10/2011 or FDA 21 CFR 177.1520 depends on the final film thickness, use temperature, and food simulant. The masterbatch supplier’s declaration should identify whether the active decomposition residues are covered by the relevant positive list. In all cases, residual acidity or alkalinity can be measured by water extraction per ISO 787-9:2019; this is part of the lot inspection record when the foamed article contacts aqueous or acidic food matrices.
| Requirement | Designation | Documentation needed |
|---|---|---|
| Olefin polymer food-contact status | FDA 21 CFR 177.1520 | Supplier written confirmation |
| RoHS restricted substances | Directive 2011/65/EU | Laboratory certificate or supplier SDS |
| EU chemical registration | REACH (EC) 1907/2006 | Safety data sheet |
| Polymer melt flow index | ISO 1133-1:2022 | Lot certificate of analysis |
Volatile decomposition products from endothermic foaming agents are primarily carbon dioxide and water vapor; any residual carrier volatiles are governed by the LLDPE feedstocks. Ventilation and local exhaust are required when processing at high addition rates, not because the gases are acutely toxic but because oxygen displacement in a confined room can occur if extruder vents are not ducted. Carbon dioxide has an 8-hour time-weighted average exposure limit of 5,000 ppm under 29 CFR 1910.1000 Table Z-1.
Storage conditions and failure-mode observation from production-scale equipment reinforce operational boundaries. On a 75 mm single-screw extruder with an L/D ratio of 30:1, feed-throat bridging has been observed when pellets were exposed to high humidity and loaded into a machine running at 30 rpm; the resulting surging disappears after drying the masterbatch for 4 h at 60 °C in a desiccant dryer. If the concentrate is pre-compounded with metal stearate lubricants or acid-modified polyolefins, premature decomposition can occur at the feed throat because acid species catalyze carbonate decomposition. The manufacturer should be consulted before combining the product with such additives. Extruder vent ports should not be left closed under vacuum without a vacuum trap; decomposition gases can condense into a sludgy residue in the vent line.
At melt temperatures above 240 °C, rapid gas evolution may overwhelm the bubble walls; the practical upper melt-temperature limit should be determined by differential scanning calorimetry for the active package. The material should therefore be evaluated on the intended production line with the specified matrix and lot-controlled carrier rheology records; direct substitution from a powdered agent or from another carrier grade without a density and cell-morphology trial is not supported by the available data.