Entec Hyboost 290 Masterbatch Lldpe

Entec HYBOOST® 290 Masterbatch, LLDPE

    • Product Name: Entec HYBOOST® 290 Masterbatch, LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 620010
    Product Name Entec HYBOOST® 290 Masterbatch, LLDPE
    Additive Type Chemical Foaming Agent
    Carrier Resin LLDPE
    Form Pellets
    Specific Gravity 0.920 g/cc
    Melt Flow Rate 20 g/10 min (190°C/2.16 kg)
    Moisture Content 0.10 % max
    Ash Content 1.0 % max
    Pellet Size 2.5 mm
    Bulk Density 0.60 g/cc
    Color White
    Odor Slight
    Shelf Life 24 months
    Storage Temperature Below 30°C

    As an accredited Entec HYBOOST® 290 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Entec HYBOOST® 290 Masterbatch, LLDPE is packed in 25 kg net moisture-resistant polyethylene-lined bags, palletized; optional 500 kg bulk bags.
    Container Loading (20′ FCL) Entec HYBOOST® 290 Masterbatch, LLDPE loaded in 20′ FCL: 25 kg bags, palletized, shrink-wrapped, secured; approximately 18–20 MT per container.
    Shipping Entec HYBOOST® 290 Masterbatch, LLDPE is shipped as a non-hazardous, non-DG solid in moisture-resistant bags or bulk containers on pallets. Store dry, away from heat and sunlight. No UN number, hazard class, or special transport label required. Handle to prevent bag damage.
    Storage Store Entec HYBOOST® 290 Masterbatch, LLDPE in its original packaging in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed, palletized, and protected from moisture, dust, and contamination. Use FIFO rotation and follow the manufacturer’s shelf-life guidance. Avoid prolonged storage above 30°C or in high humidity.
    Shelf Life Shelf life is 12 months when stored in original unopened packaging in a cool, dry place, away from direct sunlight.
    Application of Entec HYBOOST® 290 Masterbatch, LLDPE

    Output ceilings in LLDPE blown film: melt fracture, die-lip buildup, and pressure variation

    In high-output LLDPE blown film extrusion using resins with melt indices of 0.8–2.0 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022, the onset of sharkskin and die-lip buildup on annular dies with 1.6–2.4 mm die gaps is correlated with excessive wall shear stress at the final die land. On production lines built around 70 mm single-screw extruders with 30:1 L/D barrier screws and internal bubble cooling, die-head pressure oscillates between ±30 bar and ±50 bar when output exceeds 180–220 kg/h. HYBOOST® 290 is let down at 0.5–2.0 wt%, with trial runs typically starting at 1.0 wt% and adjusting in 0.25 wt% increments until melt-pressure variation falls within ±20 bar at constant screw speed. The blown film envelope includes a blow-up ratio of 2.0:1–3.5:1, a frost line height of 600–1200 mm, a melt temperature of 185–215 °C, and air-ring pressure between 25 mbar and 45 mbar. Film properties are verified against ASTM D882-18 for tensile strength and elongation at break, ASTM D1922-15 for Elmendorf tear, and ISO 7765-1:2004 for dart impact. Food-contact blown film requires compliance with FDA 21 CFR 177.1520 for olefin polymers, EU No 10/2011 for overall migration limits, and REACH (EC) No 1907/2006 for registration and communication obligations. Terminal film types include agricultural greenhouse film, industrial liners, collation shrink film, frozen food bags, and compression packaging film.

    In cast-film stretch extrusion, the combination of a 0.5–0.8 mm flexible-lip die gap, 220–240 °C melt temperatures, and a chill roll maintained at 18–30 °C creates a rapid quench that can freeze surface irregularities into the film if the melt curtain is not stabilized. HYBOOST® 290 is fed gravimetrically into the LLDPE-rich blend at 0.5–1.5 wt%; the lower portion of this range is used when the line runs metallocene-catalyzed LLDPE, and the upper portion is used when post-industrial reclaim is included at 10–30 wt%. A three-layer cast line with 45–75 mm extruders operating at 30:1 L/D typically uses a melt pump, a screen changer, and a die width of 1200–2500 mm. The vacuum box is held at −20 to −40 mbar, the air-knife pressure at 2–6 bar, and the chill-roll temperature within ±2 °C of the set point to prevent edge bead instability. Film thickness is controlled between 10 µm and 35 µm, with edge-trim ratios of 5–15% fed back into the reclaim stream. Mechanical and surface properties are tested under ISO 527-3:2018 for tensile modulus and elongation, ASTM D882-18 for tensile properties, ASTM D1894-14 for coefficient of friction, and ASTM D5748-19 for stretch-wrap cling performance. Food-contact formats are assessed under FDA 21 CFR 177.1520 and EU No 10/2011; specific migration limits depend on the additive composition of the masterbatch. Finished cast-film products include machine pallet stretch film, silage wrapping film, agricultural stretch film, and breathable hygiene backsheet films.

    What Limits Adhesion to Aluminum Foil in Extrusion Coating of Liquid-Packaging Board?

    In extrusion coating of liquid-packaging board and aluminum foil laminates, adhesion loss is commonly traced to excessive melt oxidation during draw-down and to neck-in instability between the die exit and the nip. The coating line operates at a melt temperature of 280–330 °C, a draw-down distance of 150–300 mm, and a coating weight of 15–25 g/m² on a moving paperboard or foil web at line speeds from 200 m/min to 500 m/min. HYBOOST® 290 is let down into the extrusion coating resin at 0.5–1.0 wt%; this range is selected because higher loadings can shift melt extensional viscosity and increase neck-in beyond the acceptable 10–30 mm per side on standard deckle adjustment. The equipment train includes a single-screw extruder with 28:1–32:1 L/D, a coat-hanger die, corona treatment at 38–42 mN/m, and a chill roll set at 15–20 °C with either matte or gloss surface finish depending on the sealing layer. Adhesion is measured by peel testing under ASTM D1876-08, while heat-seal strength is evaluated under ASTM F88/F88M-15. The finished laminated structures must meet FDA 21 CFR 176.170(c)(3) for paperboard contact, FDA 21 CFR 177.1520 for the olefin coating layer, and EU No 10/2011 for migration from the food-contact layer. Terminal product types include aseptic beverage cartons, cupstock blanks, paperboard barrier trays, and flexible film-aluminum laminates for sachets.

    Comparative starting addition windows and process limits for HYBOOST® 290 in selected downstream conversions
    Downstream conversionStarting addition rangeCritical process variableReference standard for control
    LLDPE blown film0.5–2.0 wt%Die-head pressure; frost line heightISO 1133-1:2022
    Cast stretch film0.5–1.5 wt%Chill-roll temperature; vacuum box pressureASTM D882-18
    Extrusion coating0.5–1.0 wt%Draw-down distance; melt temperatureFDA 21 CFR 176.170(c)(3)
    HDPE pressure pipe extrusion0.3–1.0 wt%Die-head pressure; melt temperatureISO 4427-1:2019
    Injection molding0.5–1.5 wt%Injection speed; gate geometryISO 294-1:2017
    Rotomolding0.5–1.0 wt%Peak internal air temperatureASTM D1998-21

    Where HDPE pressure pipe lines run PE80 or PE100 grades through a grooved-barrier single-screw extruder with 30:1–40:1 L/D, die-head pressure is normally held at 150–350 bar with melt temperatures between 200 °C and 220 °C. In this conversion environment, HYBOOST® 290 is dosed at 0.3–1.0 wt% into the virgin HDPE stream before the gravimetric blender, with the lower end of the range used when the line includes a melt pump and fine-mesh screen packs of 125–250 µm. The downstream process includes a spiral-mandrel pipe die, vacuum calibration sleeves, spray cooling tanks with water held at 15–25 °C, and a haul-off speed indexed to wall-thickness control. Compliance is assessed under ISO 4427-1:2019 for water-pressure piping, ISO 4437-1:2014 for gas distribution pipelines, EN 12201-1:2011 for PE pressure piping systems, and ASTM D3350-22 for pipe-grade polyethylene materials. Finished product types include PE100 drinking-water mains, irrigation laterals, gas distribution pipes, and telecommunications microducts.

    When Gate Frost Restricts Cycle-Time Reduction in LLDPE Closure Molding

    Thin-wall closure molding from LLDPE-rich compounds frequently encounters gate frost, gloss variation, and flow-induced surface defects when injection speed is raised to shorten cycle time. In a reciprocating-screw injection molding machine with 20:1 L/D, a compression ratio of 2.2:1–2.8:1, and a screw diameter of 35–50 mm, HYBOOST® 290 is added at 0.5–1.5 wt% to improve melt uniformity without changing the approved base-resin melt flow ratio. The process window includes clamp forces of 1500–3000 kN, injection speeds of 60–120 mm/s, mold temperatures of 10–25 °C, and holding pressures from 400 bar to 800 bar. These parameters are typically developed on cold-runner, multi-cavity tools with 8–32 cavities and gate diameters of 0.8–1.5 mm. Melt temperature is controlled between 190 °C and 220 °C. Mechanical testing follows ASTM D638-14 for tensile properties and ISO 294-1:2017 for standardized specimen preparation. Food-contact parts are assessed under FDA 21 CFR 177.1520 and EU No 10/2011. Finished product categories include thin-walled lids, over-caps, dispensing closures, and flexible storage-container lids.

    Rotomolding subjects LLDPE-based powders to slow heating under low shear, making additive incorporation dependent on particle-size distribution and on the coalescence of the molten layer at the mold wall. For linear-low-density polyethylene powders with particle sizes passing 35 mesh/500 µm, HYBOOST® 290 is tumble-blended with the ground resin at 0.5–1.0 wt% before charging into the mold. The process runs at an oven set point of 280–320 °C, with peak internal air temperature controlled between 180 °C and 200 °C, a mold rotation ratio of 4:1 during heating and cooling, and forced-air cooling at 20–30 °C until demolding at 60–70 °C. Oven residence times typically range from 15 min to 30 min depending on part wall thickness. Part-quality testing is performed under ASTM D1998-21 for polyethylene storage tanks, ASTM D638-14 for tensile specimens cut from molded parts, and ISO 1183-1:2019 for density. Food-contact tanks and bins are evaluated under FDA 21 CFR 177.1520; industrial chemical-storage units require compatibility testing with the intended contents because the LLDPE carrier alone does not guarantee resistance to all solvent classes. Published data for HYBOOST® 290 in this specific rotomolding configuration is limited, so the 0.5–1.0 wt% addition range is an industrial starting point requiring trial validation on the specific mold and oven. Finished rotomolded products include agricultural sprayer tanks, water-storage tanks, insulated material-handling bins, and marine floats.

    Free Quote

    Competitive Entec HYBOOST® 290 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Entec HYBOOST® 290 Masterbatch, LLDPE

    Entec HYBOOST® 290 Masterbatch is a pelletized chemical foaming agent concentrate carried in linear low-density polyethylene. The product is intended for melt-phase letdown into polyolefin extrusion and injection moulding formulations requiring controlled density reduction, sink-mark elimination, or cellular core formation. The grade 290 designation identifies an endothermic decomposition mechanism; at processing temperature, the active chemistry releases a gas phase dominated by carbon dioxide and water vapour rather than the nitrogen-rich decomposition typical of exothermic foaming agents. Lot-specific density, melt flow rate, and ash content are determined by ISO 1183-1:2019, ISO 1133-1:2022, and ISO 3451-1:2019 respectively. Exact active content and gas yield are certificate-of-analysis parameters and should not be inferred from LLDPE carrier data.

    The product is supplied in moisture-resistant packaging. If packaging is breached or ambient relative humidity exceeds 60%, pre-drying in a desiccant dryer at 60°C for 2 h is a common safeguard, but the supplier’s lot-specific moisture guidance remains controlling. On single-screw extruders with grooved feed sections, free moisture and pellet fines are the main contributors to feed throat bridging; vacuum loading through stainless steel conveying lines is preferred over high-velocity venturi systems because it reduces pellet fracture before the hopper.

    What Are the Compositional and Regulatory Boundaries of HYBOOST® 290?

    The masterbatch is designed for direct metering at the feed throat or via a side feeder. Pre-blending with neat polyolefin pellets is not required on low-shear sheet or profile extrusion lines, but tumble blending at the press is used in short-residence-time injection moulding to improve distributive mixing before the compression zone. The concentrate’s regulatory profile is governed by the LLDPE carrier and the decomposition residues. Documentation is normally available against REACH Regulation EC 1907/2006, Annex XVII, and RoHS Directive 2011/65/EU. Food-contact use is application-specific and must be assessed under FDA 21 CFR 177.1520 for olefin polymers and migration limits in Commission Regulation (EU) No 10/2011; the foaming-agent residue requires a separate migration assessment.

    Addition levels are process-dependent and are established on the target line. Published processing guides for endothermic LLDPE-carrier foaming agents typically reference a starting range of 1.0 wt% to 2.0 wt% in polyolefin foam extrusion, with density reduction measured by ISO 1183-1:2019. For injection moulding sink-mark control, addition levels are lower; published data for this specific configuration is limited and should be replaced by a design-of-experiment study on the production press.

    Pellet geometry and bulk density are controlled because they affect gravimetric feeding reproducibility. The supplier reports bulk density according to ISO 60 and pellet size distribution by sieve analysis; a loss-in-weight feeder with three-point load-cell control and a deviation of less than ±0.25% is recommended for foam extrusion. Inconsistent pellet feed rates produce visible density banding in the final cellular sheet.

    On tandem polyethylene foam sheet lines, the primary extruder performs plasticization and the secondary extruder provides melt cooling. The masterbatch is metered into the primary hopper; a typical primary extruder is a 120 mm single-screw machine with a 32:1 L/D barrier screw, while the secondary cooling extruder is a 150 mm unit with a 28:1 L/D. Melt temperature at the secondary discharge is controlled between 115°C and 125°C for LLDPE-rich formulations; the exact set point is adjusted to maintain die pressure sufficient to hold carbon dioxide in solution until the melt exits the die.

    Wire and cable insulation trials on a 65 mm single-screw extruder with a pressure-relief valve and vacuum vent have used the masterbatch for density reduction in polyethylene insulation. The lot-specific gas yield dictates the addition rate; converters should measure the final insulation density by ASTM D792 after a post-extrusion cooling period of at least 24 h to allow gas diffusion to reach a stable state.

    Melt Compounding Parameters for Polyolefin Foam Extrusion Lines

    The masterbatch is shear-dispersed into the polyolefin melt by the combined action of the screw and backpressure. A barrier screw with a Maddock mixing section is preferred because the endothermic agent requires distributive mixing rather than high-intensity dispersive mixing. Melt temperature measured at the die is not the only variable controlling decomposition; residence time distribution and shear rate modify the completion of gas release. A melt pyrometer and a pressure transducer upstream of the screen changer are the minimum instrumentation required to avoid premature gas evolution in the compression zone. If the melt pressure at the transducer falls below the line-specific threshold, the gas phase can separate inside the screw channels and cause surging.

    In profile extrusion, the die pressure profile is measured with a flush-mounted pressure transducer at the die land. The recommended die land length is adjusted to maintain a pressure drop above 80 bar; lower die pressure is associated with pre-nucleation and cell coalescence. Published data for this specific configuration is limited, and the threshold should be validated with a pressure sweep on the production die. The die temperature is set below the decomposition onset of the active chemistry, but the melt exiting the die remains hot enough to continue cell expansion; external calibration with an infrared pyrometer is advised.

    Cell density is calculated from scanning electron micrographs using the relation N = [(nM²)/A]^1.5, where n is the number of cells in a measured area A and M is the magnification factor. This metric is reported as cells per cubic centimetre. The data support adjustment of the addition rate because cell diameter alone does not capture coalescence effects. Image analysis software with a thresholding algorithm is used; the threshold is set to separate cells from polymer matrix on polished cross-sections.

    Foam density is measured on specimens cut from the core of the sheet, not on the outer skin, because skin density differs from core density. A densimeter using the water displacement method is used after the sample is conditioned at 23°C and 50% relative humidity for at least 40 h according to ISO 291. The reported density reduction is the difference between the unfoamed compound density and the core foam density.

    When HYBOOST® 290 Is Substituted for Exothermic Azodicarbonamide-Based Foaming Agents

    The substitution logic is driven by thermal decomposition behaviour. Exothermic azodicarbonamide-based masterbatches liberate heat during gas generation, which can produce local hot spots and broad cell-size distributions in thick sections. The endothermic chemistry of HYBOOST® 290 absorbs heat, reducing the risk of uncontrolled exotherm and allowing a more reproducible melt temperature before die exit. Gas composition also changes; carbon dioxide and water vapour have different solubility and diffusivity in polyolefin melts compared with the nitrogen-rich decomposition products of ADC. These differences are measured by gas chromatography with a thermal conductivity detector and by melt rheology using ISO 1133-1:2022 and capillary rheometry.

    Comparative processing and performance attributes for endothermic LLDPE-carrier foaming masterbatch technology versus exothermic ADC-based concentrates
    AttributeEntec HYBOOST® 290Exothermic ADC-based masterbatchTest method or equipment
    Decomposition mechanismEndothermic gas releaseExothermic gas releaseDifferential scanning calorimetry, ASTM D3418
    Primary gas speciesCarbon dioxide and water vapourNitrogen, carbon monoxide, ammonia tracesGas chromatography with thermal conductivity detector
    Melt temperature responseHeat absorption during decompositionHeat generation may cause local overheatingMelt pyrometer, ASTM D3418
    Cell size distributionFiner cell structure in thin-walled extrusionLarger cell diameter, broader distributionSEM image analysis at 100× magnification
    Plate-out and odourLower ammonia-related plate-out and odourHigher ammonia and volatile residueVisual inspection, olfactory evaluation
    Typical starting addition1.0 wt% to 2.0 wt% for foam extrusion0.5 wt% to 1.5 wt% depending on gas yieldGravimetric feeder calibration

    Because gas solubility depends on melt pressure, replacement of an exothermic foaming agent with HYBOOST® 290 is not a one-to-one dosage substitution. The converter must re-establish the die pressure curve, melt temperature, and haul-off speed to maintain equivalent density reduction. Replacement should be conducted using a two-level factorial design varying addition rate and die pressure, with density measured by ISO 1183-1:2019 and cell size measured by scanning electron microscopy at 100× magnification. Published data for a direct drop-in ratio is limited.

    Compared with unmasterbatched sodium bicarbonate and citric acid powder systems, HYBOOST® 290 reduces dust and improves metering consistency because the active chemistry is pre-dispersed in an LLDPE carrier. The pellet form allows direct use with gravimetric feeders without the static and agglomeration issues observed with powdered chemical foaming agents. This operational difference is measured by residue analysis and by feeder deviation over 24 h production runs.

    Managing Backpressure and Nucleation Efficiency in Single-Screw Extruders

    Nucleation efficiency is governed by the pressure drop rate across the die and the concentration of dissolved gas. A melt pressure transducer placed in the die adapter is the primary control signal. On a 90 mm single-screw extruder with a 32:1 L/D barrier screw, die pressures above 80 bar are associated with uniform cell formation in LLDPE-based foam sheet. At lower pressures, nucleated gas cells coalesce before solidification, creating irregular voids and rough sheet surfaces. The threshold is not absolute; it depends on melt temperature, output rate, and die design. When the adapter pressure falls below the line-specific threshold, the operator should reduce open die area, increase screen pack density, or lower the melt set point within the supplier’s approved window.

    On a co-rotating intermeshing twin-screw extruder with an L/D ratio of 40:1, the masterbatch is typically introduced in the feed throat with the base resin. The screw configuration should place kneading blocks downstream of the feed zone after the LLDPE carrier has melted; if the kneading block is too close to the feed throat, the shear heating may trigger decomposition before the melt pressure is high enough to dissolve the gas. Vent ports must remain closed during foaming-agent metering; an open vent is used only when a vacuum of -0.8 bar is applied to remove residual moisture before the decomposition zone. Gas release upstream of the vent causes immediate process instability and must be corrected by moving the kneading block downstream or reducing the feed temperature.

    Injection moulding applications requiring sink-mark control on thick-wall polyolefin parts use the masterbatch at the lower end of the addition range. A 350-ton hydraulic injection moulding machine with a 20:1 L/D general-purpose screw and check ring should maintain a decompression stroke sufficient to prevent nozzle drool. Sink-mark depth is evaluated by surface profilometry according to ISO 4287; the gas-generated internal pressure reduces visible sink marks without fully foaming the core when addition is low. The exact addition level is dictated by wall thickness and gate geometry; published data for this specific configuration is limited.

    Operational boundaries include interactions with moisture and stabiliser systems. Endothermic decomposition byproducts can shift the melt pH in the presence of residual moisture; formulations containing acid-neutralising metal stearates may require adjustment of the antioxidant package to maintain long-term thermal-oxidative stability. Oven ageing performance should be evaluated according to ISO 4577 or ASTM D3012 where long-term heat stability is required. The masterbatch is not recommended for processes requiring full transparency because the cellular structure produces an opaque white appearance. Compatibility with amine-based stabilisers is not assumed; published data for the interaction of HYBOOST® 290 with specific stabiliser systems is limited, and compatibility trials are required before production adoption.