| HS Code | 696896 |
| Product Name | Entec HYBOOST® 289 Masterbatch, LLDPE |
| Manufacturer | Entec Polymers |
| Carrier Resin | LLDPE |
| Additive Type | Silica |
| Form | Pellets |
| Color | White |
| Density | 0.920 g/cm³ |
| Melt Flow Rate | 2.0 g/10 min |
| Additive Content | 20 % |
| Moisture Content | ≤ 0.10 % |
| Bulk Density | 0.55–0.65 g/cm³ |
| Melting Point | 120–130 °C |
| Recommended Loading | 1–5 % |
| Packaging | 25 kg bags |
As an accredited Entec HYBOOST® 289 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg moisture-resistant bags, palletized for transport, ensuring stability for Entec HYBOOST® 289 Masterbatch, LLDPE. |
| Container Loading (20′ FCL) | 20′ FCL container loading for Entec HYBOOST® 289 Masterbatch, LLDPE: palletized, shrink-wrapped bags, evenly distributed, securely braced for safe transport. |
| Shipping | Entec HYBOOST® 289 Masterbatch, LLDPE is supplied in 25 kg moisture-resistant bags or bulk octabins, palletized and shrink-wrapped. It is non-hazardous for transport, requiring no special UN classification. Ships at ambient temperature by truck, rail, or sea. Keep dry, shaded, and away from ignition sources; follow local handling and labeling rules. |
| Storage | Store Entec HYBOOST® 289 Masterbatch, LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, moisture, and ignition sources. Keep original containers tightly closed when not in use. Avoid contact with strong oxidizing agents. Maintain good housekeeping, rotate stock, follow shelf-life recommendations, and comply with the supplier’s Safety Data Sheet and local regulations. |
| Shelf Life | Shelf life is 12 months from date of manufacture when stored in original, unopened packaging in a cool, dry place. |
In blown film production of printed snack-food packaging, HYBOOST® 289 Masterbatch, LLDPE is introduced at 2.0–4.0 wt% into LLDPE-rich formulations containing 20–30 wt% LDPE to maintain bubble stability on long runs without changing the sealing initiation temperature of the final film. The downstream process uses a single-screw extruder with a screw diameter of 50–75 mm and an L/D ratio of 24:1–30:1, a spiral mandrel die with a die gap of 1.2–2.0 mm, a blow-up ratio of 2.2:1–3.0:1, and melt temperatures maintained at 180–210 °C. Take-off speed typically runs between 60–120 m/min for film thicknesses of 25–60 µm. Extrusion stability is monitored by melt pressure before the screen changer; a pressure variation below 3% over 6 h is used as the acceptance criterion. For food-contact compliance, the olefin polymer carrier and additives are assessed under FDA 21 CFR 177.1520, and the finished film is subject to overall migration testing according to EU No 10/2011 with a limit of 10 mg/dm²; Chinese applications additionally reference GB 9685-2016. Terminal products include printed frozen food bags, breakfast cereal liners, and form-fill-seal pouches. Moisture in the masterbatch should be below 200 ppm; processing above 240 °C for more than 5 min should be avoided to prevent oxidative degradation of the LLDPE carrier.
Three-layer blown film coextrusion lines for heavy-duty sacks running post-industrial LLDPE regrind encounter gel formation and die lip build-up when the recycled fraction carries degraded gel particles from previous heat history. In the core layer of these structures, HYBOOST® 289 Masterbatch, LLDPE is incorporated at 3.0–5.0 wt% to moderate viscosity differences between the recycled and virgin streams and to maintain layer uniformity. The process is typically run on a three-layer die with a diameter of 200–350 mm, a die gap of 1.8–2.4 mm, and core extruder L/D ratios of 30:1. Pressure before the screen changer is recorded continuously; a pressure variation exceeding 5% over 4 h usually indicates screen-pack blinding from gels or filler carry-over. Melt flow rate of the core stream is measured by ISO 1133-1:2022 at 190 °C/2.16 kg, and the skin-to-core MFR ratio is maintained below 1.5 to limit interfacial instability. Compliance for heavy-metal content in the recyclate fraction references EU 94/62/EC with concentration limits established under CONEG TPCH, while the compounded film is checked for dart impact according to ASTM D1709-15 and tensile properties according to ASTM D882-18. Terminal products include 25–50 kg polymer granule sacks, FIBC liner films, and construction aggregate bags with film thicknesses of 80–150 µm. Formulations containing calcium carbonate above 8 wt% should be avoided because inorganic filler can accelerate screen-pack blinding and melt-pressure instability in this regrind-intensive process.
For multi-season greenhouse covers of 150–200 µm thickness, HYBOOST® 289 is added at 4.0–6.0 wt% into LLDPE/LDPE blown film formulations to maintain bubble stability and reduce melt-fracture-related optical haze during long runs. The film is produced on a high-stalk bubble line with internal bubble cooling, a die diameter of 250–400 mm, a die gap of 2.0–2.4 mm, and frost-line height controlled at 600–900 mm above the die. The masterbatch is not a substitute for hindered amine light stabilisers; its function is processing-related, not long-term UV stabilization. Weathering performance of the final structure is evaluated under ISO 4892-3:2016 using UVA-340 fluorescence lamps, while haze is measured by ASTM D1003-21 and dart impact by ASTM D1709-15; the film must also satisfy the classification requirements of EN 13206:2017 for agricultural covering applications. Terminal products include two-season greenhouse films, low-tunnel covers, and silage protection sheets. Avoid barrel temperatures above 230 °C in the presence of high-purity LLDPE without antioxidant compensation, as this can shorten the induction period of the carrier resin.
At line speeds of 300–600 m/min, cast stretch film production imposes a narrow processing window because extensional flow at the slot die and quench roll is highly sensitive to polymer chain orientation. HYBOOST® 289 Masterbatch, LLDPE is introduced at 1.5–3.5 wt% in LLDPE blends containing 5–15% metallocene-catalyzed LLDPE for puncture and cling balance. The extrusion train uses a slot die with a die gap of 0.5–0.8 mm, a chill roll temperature of 18–24 °C, and a vacuum box or air knife to pin the film to the quench drum. Melt temperature at the die lip is maintained at 200–240 °C, and residence time from feed throat to die exit is kept under 6 min to limit gel formation. Cling force, coefficient of friction, and puncture resistance are tested according to ASTM D5458-95(2020), ASTM D1894-14, and ASTM D5748-19; haze is measured by ASTM D1003-21 and tear by ASTM D1922-15. Compliance for food-wrap grades references FDA 21 CFR 177.1520 and EU No 10/2011. Terminal products include machine stretch film, hand pre-stretch film, and agricultural bale wrap. The table below is a compliance checklist for cast stretch film grades, not a substitute for line qualification.
| Parameter | Test method or regulation | Typical requirement |
|---|---|---|
| Kinetic coefficient of friction (film-to-film) | ASTM D1894-14 | Recorded at line speed; target is line-specific |
| Peel cling force | ASTM D5458-95(2020) | Reported as cling force by stretch level |
| Protrusion puncture resistance | ASTM D5748-19 | Reported at specified film gauge |
| Elmendorf tear (machine direction) | ASTM D1922-15 | Reported value; no global minimum |
| Haze | ASTM D1003-21 | Low haze preferred; line-specific acceptance |
| Overall migration for food contact | EU No 10/2011 | <10 mg/dm² |
| US olefin polymer food-contact status | FDA 21 CFR 177.1520 | Meets applicable subchapter |
LLDPE geomembrane sheet extrusion for landfill and water-containment liners uses flat die extrusion with sheet thicknesses from 1.5–3.0 mm and die widths commonly up to 2400 mm. HYBOOST® 289 Masterbatch, LLDPE is evaluated in this application at 4.0–6.0 wt% in LLDPE geomembrane compounds to support processing uniformity during long sheet runs, particularly where pigments and carbon black are separately metered. Sheet is produced on a single-screw extruder with a screw diameter of 90–120 mm and L/D of 30:1, feeding a flat die through a gear pump and screen changer with 80–120 mesh packs. Melt temperature is controlled within 210–240 °C; higher melt temperatures reduce oxidative induction time and narrow the hot-wedge welding window. Oxidative induction time is determined by ASTM D3895-19 at 200 °C with oxygen pressure maintained at 35 kPa, while tensile properties at yield and break follow ASTM D6693-22. Geomembrane specification compliance is assessed against GRI-GM17 for LLDPE smooth and textured sheet, and seam strength is evaluated by ASTM D6392-12(2021) at welded coupons. Terminal products include landfill cell liners, canal liners, and mining pond capping layers. Carbon black concentrates yielding 2.0–3.0% carbon black in the final sheet require separate dispersion monitoring after screen packs; poor dispersion produces microroughness that reduces hot-wedge seam peel reproducibility.
Competitive Entec HYBOOST® 289 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Entec HYBOOST® 289 Masterbatch, LLDPE is supplied as a pelletized additive concentrate in which a proprietary HYBOOST 289 active system is dispersed in a linear low-density polyethylene carrier. The grade designation 289 identifies the additive chemistry and carrier identity; it does not establish a single universal let-down ratio or end-use specification. Melt mass-flow rate is determined by ISO 1133-1:2022 at 190 °C and 2.16 kg, density by ISO 1183-1:2019, and ash content by ISO 3451-1:2019. Published product-specific ranges for HYBOOST 289 are limited, so production qualification should be governed by lot certificates and on-line verification rather than by a fixed nominal data sheet. The LLDPE carrier is intended for compatibility with LLDPE-rich film, extrusion coating, and sheet streams, but the active phase is not assumed to behave like a simple processing aid.
Pellet geometry and bulk density are controlled to support volumetric or gravimetric feeding. Pellet size is reported by internal sieving or image analysis. Because concentrate density may differ from that of the base resin, feeder calibration should be checked after every lot change. A free-flowing pellet form lowers feed-throat dust relative to powder additives, but does not eliminate the need for preblending when the target addition is below 1%. For such low let-downs, split preblending with cleaned natural LLDPE is used to reduce concentration variance before final metering.
| Parameter | Procedure | Unit | Controlling document |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022, 190 °C/2.16 kg | g/10 min | lot certificate |
| Density | ISO 1183-1:2019 Method A | g/cm³ | lot certificate |
| Ash content | ISO 3451-1:2019 Method A | % | lot certificate |
| Moisture content | ISO 15512:2019 | µg/g | lot certificate |
| Pellet geometry | internal sieving or image analysis | mm | lot certificate |
Across blown-film and cast-film operations, masterbatch addition is controlled by feeder stability, screw mixing capacity, and melt pressure response. Gravimetric feeders are preferred when the HYBOOST 289 let-down is below 2%; volumetric auger feeders may exhibit short-term drift unless equipped with weigh-check feedback. On a single-screw extruder with 24:1 to 30:1 L/D, a barrier screw or a Maddock mixing section can distribute the concentrate if the carrier melt viscosity is not far removed from the base resin. No specific screw configuration is assigned to HYBOOST 289, so a dispersion evaluation is required on the target production line.
Distributive mixing is normally sufficient only if the active phase has been adequately dispersed during masterbatch manufacture. In a simple conveying screw, inadequate mixing can appear as film gel, optical surface defects, or melt-pressure instability. The critical shear rate for dispersing HYBOOST 289 is not published; therefore, a target-line study should vary screw speed from 50 min⁻¹ to 100 min⁻¹ and measure visible gel count on blown-film samples. If gels persist at the highest screw speed, the screw configuration or screen pack should be modified before increasing additive dosage.
Melt pressure before the screen pack should be recorded at constant screw speed after the feed throat reaches steady state. If the masterbatch carrier has higher shear viscosity than the base LLDPE, pressure drop may increase; if lower, it may decrease. The relevant rheological comparison is performed by capillary rheometry according to ISO 11443:2021 across shear rates of 100 s⁻¹ to 1000 s⁻¹. When pressure variation after a lot change exceeds ±1.0 MPa from the previous baseline, screw speed, barrel profile, and screen pack condition should be examined before altering additive dosage.
Barrel temperature settings are determined primarily by the base LLDPE. Typical cast-film profiles range from 120 °C at the feed throat to 200 °C at the metering zone, with melt temperature commonly 210 °C to 240 °C; blown-film profiles vary with die size, output, and base resin rheology. HYBOOST 289 should not be used to compensate for a base resin that requires melt temperature outside its thermal stability envelope. In twin-screw recompounding at 40:1 L/D, the LLDPE carrier may improve distribution of the active phase, but the additional thermal history must be accounted for in gel, color, and volatile evaluations.
Masterbatches with LLDPE carrier are process-sensitive at the feed hopper. LLDPE pellets can soften and bridge if hopper temperature rises above 40 °C due to radiant heat from the barrel. Feed-throat cooling and a well-maintained hopper magnet are recommended. A nitrogen purge is not required under normal melt processing, but extended hopper residence under humid conditions may require moisture verification by ISO 15512.
A comparative selection between HYBOOST 289 and other addition routes is made at the level of inventory, traceability, and process risk. The LLDPE-carrier masterbatch differs from a neat additive powder in that the active phase is already distributed in a polyolefin matrix; this reduces dust exposure and simplifies feeding. It differs from a fully compounded LLDPE in that the concentrate is diluted at the converter, allowing the same base resin to serve multiple product grades. These differences carry measurable implications: the additional carrier modifies the final melt index and may shift seal performance, haze, and gauge uniformity. A neat additive may avoid the carrier but often requires dispersive mixing that is unavailable on a simple single-screw line.
| Attribute | HYBOOST 289 Masterbatch, LLDPE | Fully compounded LLDPE | Neat additive powder |
|---|---|---|---|
| Carrier contribution | adds LLDPE fraction to final blend | base resin is the carrier | no carrier; direct additive |
| Feeding method | pellet loss-in-weight or volumetric feeder | direct extrusion | high-shear pre-mix or liquid injection |
| Dispersion requirement | distributive mixing; carrier aids dilution | not applicable | dispersive mixing required |
| Lot-to-lot document | SDS, lot certificate, supplier food-contact statement | final compound SDS and COA | raw material SDS |
| Main process risk | carrier melt index shift, gel formation if poorly mixed | higher SKU complexity, less formulation flexibility | dust, worker exposure, feeding instability |
Selection of HYBOOST 289 over an LDPE-carrier masterbatch depends on target film toughness and seal response. LLDPE carriers generally exhibit higher low-shear viscosity than LDPE carriers of equivalent melt index; this may increase extruder amperage and melt pressure on non-optimized screws. However, the LLDPE carrier may contribute more impact resistance than an LDPE carrier when final film is exposed to low-temperature distribution conditions. Published data for HYBOOST 289 in this specific carrier comparison is limited, so the effect should be quantified on the intended line using ASTM D1709 and ASTM D1922.
High-proportion LLDPE films exhibit nonlinear shear-thinning behavior and a broad processing window. The incorporation of an LLDPE-carrier masterbatch may alter extensional viscosity and bubble stability in blown-film extrusion. In such applications, the frost line height should be held constant while raising HYBOOST 289 addition to isolate carrier effects. Dart impact resistance is tested by ASTM D1709 Method A, Elmendorf tear by ASTM D1922, tensile by ASTM D882, and haze by ASTM D1003. Heat-seal initiation should be evaluated by ASTM F2029 because an additional LLDPE carrier may shift seal initiation temperature relative to a neat additive route. No universal offset value is assigned to HYBOOST 289; the shift depends on carrier melt index, dosage, and base resin comonomer distribution.
On blown-film dies with die gaps between 0.8 mm and 2.0 mm, a screen pack of 20/40/80 mesh may serve as a dispersive aid; however, backpressure should not exceed the extruder manufacturer's limit. The masterbatch pellets should be uniformly blended with the base LLDPE before the feed hopper to avoid screw surging. If torque fluctuation exceeds 5% at constant screw speed, blending or feeder segregation should be investigated. Surface inspection systems with 50 µm resolution can quantify gel levels and detect a masterbatch lot change earlier than visual inspection.
For cast-film and extrusion-coating lines, the masterbatch may be added through the main hopper when the base resin is LLDPE-rich. Processing trials should record melt temperature, die pressure, screw amperage, and neck-in variation. If neck-in changes disproportionately with HYBOOST 289 addition, the carrier is shifting the low-shear rheology of the melt; a capillary rheometer comparison across the die shear-rate range is required. Published film property data for HYBOOST 289 in this exact configuration is limited, so the test methods above should be used as screening protocols rather than replacements for production validation.
For food-contact and regulated applications, the regulatory status of the LLDPE carrier and the HYBOOST 289 additive system must be assessed separately. Polyethylene homopolymers and copolymers used as food-contact substances are commonly referenced by FDA 21 CFR §177.1520; European plastics are controlled under Commission Regulation (EU) No 10/2011 with overall migration limits specified in Annexes I and II. The HYBOOST 289 active phase must have its own authorisation, migration data, and intended-use restrictions. Supplier documentation should identify whether the grade meets relevant REACH Regulation (EC) No 1907/2006 Article 33 SVHC communication thresholds and RoHS Directive 2011/65/EU maximum concentration values.
Because final article compliance is determined by the converter's complete formulation, a masterbatch supplier declaration alone is insufficient. Test methods relevant to migration include the EN 1186 series for food simulants and, for total migration, EN 1186-1 guidance. If the final film is used in medical packaging, additional standards such as ISO 10993 should be considered; these are outside the basic polyolefin processing scope. Avoid combining HYBOOST 289 with unapproved amine-based or pro-oxidant additives unless the supplier has confirmed compatibility and regulatory status for the final article.
Storage and handling constraints are governed by the thermal and moisture sensitivity of the LLDPE carrier. Store in sealed bags at temperatures below 40 °C and away from strong sunlight. Moisture uptake should be checked by ISO 15512 if the material is held in an unheated warehouse with high relative humidity. If surface condensation is present, drying below 70 °C is generally acceptable for LLDPE-based masterbatch, but the supplier's maximum drying temperature should be confirmed to avoid pellet agglomeration. Avoid melt temperatures above 280 °C and extended residence times because oxidative chain scission can generate gel and color bodies. During purging, a low-MFR LLDPE purge compound is preferable to a general-purpose detergent unless the purge supplier confirms compatibility with additive concentrates.
Thermal stability screening by ISO 11358-1:2022 should be used when a new processing profile exceeds 240 °C melt temperature to document that no rapid mass-loss event occurs. The HYBOOST 289 active phase is proprietary; therefore, off-spec appearance, odor, or pressure drift should not be interpreted as a carrier-only event. Material returned to process after a prolonged stoppage should be purged through the die or vented barrel and checked for discoloration before in-spec product is collected.