| HS Code | 468036 |
| Brand | Entec |
| Grade | HYBOOST® 283 |
| Carrier Resin | LLDPE |
| Product Type | Processing Aid Masterbatch |
| Form | Pellets |
| Color | White/Natural |
| Active Ingredient | Fluoroelastomer |
| Active Ingredient Content | 3% |
| Density | 0.92 g/cm³ |
| Melt Flow Rate | 2.0 g/10 min |
| Moisture Content | ≤0.10% |
| Pellet Size | 2–3 mm |
| Bulk Density | 0.65 g/cm³ |
| Recommended Loading | 1–3% |
| Storage Conditions | Cool, dry area |
| Shelf Life | 24 months |
As an accredited Entec HYBOOST® 283 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Entec HYBOOST® 283 Masterbatch, LLDPE is supplied in 25 kg polyethylene-lined bags on shrink-wrapped pallets for secure transport. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Entec HYBOOST® 283 Masterbatch (LLDPE), 25 kg bags on pallets, securely strapped and dunnaged for export. |
| Shipping | Entec HYBOOST® 283 Masterbatch, LLDPE is shipped as a non-hazardous solid in sealed, moisture-resistant bags or bulk sacks, palletized and stretch-wrapped. Transport in clean, dry vehicles at ambient temperature, away from sunlight, moisture, and ignition sources. Store dry; avoid excessive heat. Handle per SDS. No special transport classification normally applies. |
| Storage | Store Entec HYBOOST® 283 Masterbatch, LLDPE in a cool, dry, well-ventilated warehouse. Keep original containers tightly closed, off the floor, and on pallets. Protect from direct sunlight, heat, moisture, and ignition sources. Maintain ambient temperature, ideally below 30°C, avoiding excessive stacking. Segregate from strong oxidizers and incompatible materials. Do not store outdoors. Follow local regulations and the SDS. |
| Shelf Life | Shelf life is 24 months when stored in a cool, dry place in original unopened packaging, away from direct sunlight. |
On a high-humidity subtropical greenhouse site, a 180 µm three-layer LLDPE/LDPE blown cover film is produced with Entec HYBOOST® 283 Masterbatch metered into the inner skin layer at 3.0 wt%. The inner skin layer represents 25% of total film thickness. The coextrusion line uses three single-screw extruders with 30:1 L/D ratios and screw diameters of 50 mm, 70 mm, and 50 mm. Die diameter is 350 mm; die gap is 2.2 mm. Barrel temperatures are set between 170°C and 205°C; measured melt temperature at the die entrance is 198–210°C. Blow-up ratio is held at 2.5:1 and frost-line height at 420 mm. The masterbatch is not pre-dried if bulk moisture remains below 500 ppm; if regrind exceeds 20 wt%, drying at 80°C for 2 h is imposed to prevent micro-bubble formation and surface specks.
Compliance for the greenhouse cover follows EN 13206:2017. Tensile properties are monitored per ASTM D638-14 at 23°C and 50% relative humidity; wetting tension of the inner surface is measured by ASTM D2578-17 and must remain above 38 mN/m after 72 h at 60°C air-oven aging. Anti-drip function is evaluated by placing a filled tray of water beneath the film at 4°C and recording the percentage of surface occupied by discrete droplets after 24 h; the specification is < 20% droplet coverage. The finished product is an anti-drip greenhouse roof cover with a UV-stabilized outer layer, requiring a service life of 24 months in tropical/subtropical light regimes. Published quantitative data for this exact masterbatch grade is limited; therefore the above setpoints are plant-floor boundary conditions established on similar LLDPE-carrier anti-drip masterbatch runs.
Cold-fog persistence in sealed fresh-cut produce packs is controlled by additive bloom rate, internal film crystallinity, and headspace relative humidity. A 20 µm LLDPE cast sealant web is produced with 2.5 wt% Entec HYBOOST® 283 Masterbatch on a 75 mm single-screw cast line with 30:1 L/D. Melt temperature at the flat die is 228°C; die gap is 0.8 mm; chill roll temperature is 18°C; line speed is 180 m/min. The sealant web is laminated to a 12 µm polyester print web. The film is not corona-treated on the sealant side beyond 38 mN/m to avoid excessive surface oxidation that retards surfactant bloom.
At 4°C storage, condensation on the inner surface forms a continuous transparent water layer instead of scattering droplets. Contact angle per ASTM D5946-17 on the sealant surface is below 35° after 24 h. The regulatory framework covers Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm², and 21 CFR 177.1520(c) for the LLDPE carrier under conditions of use C through G. A Declaration of Compliance from the masterbatch producer is mandatory before use in food-contact packaging. The terminal output is a flat-barrier flow-wrap for washed baby leaf and ready-to-eat salad mixes.
| Film structure | Thickness | Masterbatch letdown | Processing method | Test condition | Endpoint |
|---|---|---|---|---|---|
| Three-layer blown greenhouse cover | 180 µm | 3.0 wt% | Coextrusion blown film | 4°C closed cabinet | < 20% droplet coverage after 24 h |
| Cast sealant web for MAP | 20 µm | 2.5 wt% | Cast film | 4°C | Contact angle < 35° after 24 h |
| Chilled poultry overwrap | 12 µm | 4.0 wt% | Cast film | 4°C display cabinet | No visible fog on 90% surface after 2 h |
| Dairy lidding sealant | 8 µm skin in 30 µm web | 2.0 wt% | Cast coextrusion | 20°C | Haze increase < 5% after 72 h |
A 12 µm cast LLDPE overwrap film formulated with 4.0 wt% Entec HYBOOST® 283 Masterbatch is applied over rigid polypropylene trays containing chilled poultry portions on a high-speed wrapper running 60 m/min. The film is extruded through a 1.0 mm slot die; melt temperature is 235–245°C; die-to-chill-roll distance is 15 mm; chill roll temperature is 15°C. Additive plate-out on the chill roll is controlled by maintaining the chill roll surface roughness below 0.05 µm Ra and by purging the die gap with a polyolefin purging compound after every 48 h of continuous operation.
Compliance is controlled under Regulation (EC) No 1935/2004 and 21 CFR 177.1520(c). Seal strength of the overwrap is evaluated per ASTM F88/F88M-23; a seal initiation temperature of 105°C at 0.275 MPa jaw pressure is confirmed once per shift. The anti-fog function is inspected in a vertical display cabinet at 4°C and 80% relative humidity; after 2 h, 90% of the package surface must be free of discrete visible fog. The finished packaged product is a chilled poultry tray with an optically clear overwrap that prevents optical masking of the meat surface.
Bakery and dairy display webs are produced as 30 µm PP/PE cast coextrusions in which the sealant layer is an 8 µm LLDPE skin containing 2.0 wt% Entec HYBOOST® 283 Masterbatch. The polypropylene layer is extruded at 240°C; the LLDPE sealant layer is extruded at 220°C. Chill roll temperature is 18°C; line speed is 150 m/min. The sealant layer receives no corona treatment on the food-contact surface. Seal initiation temperature is measured per ASTM F88/F88M-23 and held at 105–115°C for broad heat-seal window performance on high-output thermoform-fill-seal lines.
The anti-fog requirement is driven by warm bakery goods and chilled dairy products that release headspace moisture after packing. Film haze is measured per ASTM D1003-21; the specification is a haze increase of less than 5% after 72 h at 4°C and 85% relative humidity inside a closed display cabinet. Coefficient of friction is measured per ISO 8295:1995 and must remain below 0.55 to avoid film tracking defects on vertical form-fill-seal machines. Migration compliance is controlled under Regulation (EU) No 10/2011 and 21 CFR 177.1520(c). A documented incompatibility exists with erucamide-containing slip masterbatches above 1,000 ppm total erucamide, because competitive surface bloom displaces the wetting agent and produces intermittent fog patches.
| Application | Market regulation | Material standard | Test method | Controlled parameter |
|---|---|---|---|---|
| Greenhouse cover | EN 13206:2017 | ASTM D638-14 | ASTM D2578-17 | Wetting tension > 38 mN/m |
| Fresh produce MAP | Regulation (EU) No 10/2011 | 21 CFR 177.1520(c) | ASTM D5946-17 | Contact angle < 35° |
| Poultry overwrap | Regulation (EC) No 1935/2004 | 21 CFR 177.1520(c) | ASTM F88/F88M-23 | Seal initiation 105°C |
| Dairy lidding | Regulation (EU) No 10/2011 | 21 CFR 177.1520(c) | ASTM D1003-21 | Haze increase < 5% |
When masterbatch letdown exceeds 5.0 wt% in a three-layer coextruded frozen food film, the processing window narrows because the additive package reduces the LLDPE melt viscosity. On a 45 mm high-shear extruder with 25:1 L/D, the die melt pressure can fluctuate from 1.2 MPa to 2.6 MPa across a 2 h campaign if the masterbatch is not pre-dispersed. Pre-dispersion through a side feeder or tumble blending for 20 min at 30 rpm is required. The melt temperature must not exceed 245°C; above this threshold, the anti-fog additive undergoes thermal decomposition and generates low-molecular-weight oxidation by-products that appear as die-lip plate-out. Film substrate thickness is 45 µm; the additive-bearing sealant layer represents 20% of the total structure.
Frozen food packages are not visually evaluated at freezer temperature; the anti-fog function is assessed after thawing for 30 min at 23°C and 60% relative humidity. A uniform water film is required across the inner sealant surface without visible droplet formation. Seal strength is measured per ASTM F88/F88M-23 and must remain above 2.5 N/15 mm after thawing. The relevant food-contact regulation is 21 CFR 177.1520(c) in the United States and Regulation (EU) No 10/2011 in the European Union; a dual-use export pack must hold both supplier declarations. The terminal product is a gusseted frozen seafood bag with a LLDPE sealant layer that resists fog when the consumer opens and partially thaws the pack at ambient temperature.
Competitive Entec HYBOOST® 283 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Entec HYBOOST® 283 Masterbatch, LLDPE is a pelletized chemical blowing agent concentrate carried in a linear low-density polyethylene matrix. The carrier is not a neutral diluent; it controls the initial softening point, shear heating under screw rotation, and the point at which the active particles are released into the main polyolefin melt. In practice the product is handled as a minor phase, usually metered at 0.5–3.0 wt% into injection moulding or single- and twin-screw extrusion. The masterbatch is intended for polyolefin processes where a closed-cell or partially closed-cell foam is generated during forming, not for open-cell low-density foam manufacture. Its designation as an LLDPE carrier grade indicates that the base polymer is a linear low-density ethylene copolymer with a calculated melting onset lower than that of a conventional HDPE carrier; this permits dispersion in low-temperature zones before the blowing reaction begins. The active ingredient is an endothermic or partially endothermic system of the type used to release carbon dioxide and water vapour upon heating. This differentiates it from exothermic azodicarbonamide concentrates, which release high-purity nitrogen but also create a strong exotherm and may generate yellowing or plateout under prolonged residence time. Suppliers’ published data for the exact decomposition enthalpy and gas yield of this specific grade are limited; qualification therefore should map the response on the target line rather than rely only on a single thermogravimetric result.
The first measurable effect of the carrier is rheological. The masterbatch’s melt flow rate is normally determined by ISO 1133-1:2022 at 190°C under 2.16 kg. A higher carrier melt flow lowers the viscosity of the minor phase, but it does not guarantee dispersion because the viscosity ratio between the carrier and the base resin under processing shear can be orders of magnitude different from that measured in the melt flow index test. A capillary rheometer should be run under ISO 11443:2021 between 100 s⁻¹ and 1,000 s⁻¹ at the actual melt temperature to compare the shear viscosity of the carrier with the target polyolefin. If the viscosity ratio lies outside 0.2:1 to 5:1, the masterbatch can remain as streaks or accumulate behind restrictive mixing sections. On a 25 mm co-rotating twin-screw extruder with L/D 44:1, dispersion is typically achieved with two or three kneading block groups placed after the first atmospheric vent and before the side feeder. The LLDPE carrier softens at lower barrel temperature than HDPE, so it can be conveyed into the main melt without excessive torque increase. However, this early softening also means that if the side feeder is placed too near the feed throat, the carrier may melt before the main polymer is fully molten, creating a two-phase melt pool that reduces drag flow.
Decomposition timing is controlled primarily by the barrel temperature profile and the residence time distribution. The active component in an endothermic blowing system responds to both conductive heat from the barrel and shear-induced melt temperature rise. The decomposition onset can be approximated by dynamic scanning calorimetry using ISO 11357-1:2023 at a heating rate of 10°C/min, but the production heating rate is often five to twenty times higher, so the apparent onset in the machine may shift upward. Gas yield is best assessed by thermogravimetric analysis using ISO 11358-1:2022 under nitrogen; a comparison of the masterbatch’s mass loss between 150°C and 250°C provides a practical decomposition window for quality assurance. The processor should not treat these values as direct proof of foaming performance because cell nucleation depends on gas saturation, pressure drop, and die geometry more than on total gas volume alone.
Before metering HYBOOST® 283, the hopper, feed throat, and gravimetric feeder should be dry. If ambient relative humidity exceeds 60%, moisture uptake at the pellet surface can produce feeding irregularities and premature vent foaming. A tray dryer at 50°C for 4 h is a common starting point for LLDPE-carrier masterbatches, but sealed-container material should not be dried beyond the supplier’s stated maximum to avoid pellet tack. The masterbatch should be added through a calibrated gravimetric feeder with a feed screw sized for pelleted material; volumetric dosing is not recommended because changes in bulk density and pellet geometry can shift the actual let-down by more than the target ±0.2 wt% band. At let-down ratios below 0.5 wt%, the gas concentration may be below the critical nucleation threshold in thick cross-sections, and shrinkage compensation is weak. At ratios above 3.0 wt%, cell coalescence may dominate, producing an irregular skin and a sharp loss in tensile strength. The optimal set point is therefore process-specific, and the common first-pass range is 1.0–2.0 wt% for injection moulding and 0.5–1.5 wt% for profile extrusion.
In twin-screw foam extrusion, the first visible failure of a poorly set chemical foaming system is usually not a poor surface but a fluctuating melt-pressure signal at the die. The pressure transducer before the vacuum vent and the transducer at the die adapter should be recorded simultaneously. On a 40:1 L/D co-rotating twin-screw line with barrel zones from 160°C to 210°C, premature gas generation in the compression zone can push unincorporated gas backward into the feed opening or forward into the vent. This produces surging of the melt cushion, variation in pellet intake, and repeated vent blockage. The corrective action is to maintain the feed and plastication zones below the decomposition onset and position the melting seal before the side feeder. The active foaming reaction should begin after the melt seal, with the first visible pressure drop occurring after the mixing elements in the second half of the screw. A typical diagnostic set-up uses three melt-pressure transducers: one after the side feeder, one before the vacuum port, and one at the die. The pressure at the vent should remain positive but low; a vacuum of 0.8 bar is often applied to remove moisture and low-molecular-weight diluents, but if the melt has already foamed, the vacuum line will extract the blowing gas and the die will show no density reduction. This is a specific process conflict: the same vacuum needed to remove residual moisture can strip the foaming gas if decomposition occurs too early.
Die pressure is another diagnostic variable. The pressure drop at the die should be high enough to maintain gas in solution until the melt exits. If the die length is too short or the open area too large, gas separates early and creates surface streaks. A capillary rheometer with an orifice die can be used to estimate the pressure coefficient, but the best production check is a die-pressure sweep: increase screw speed until the die pressure reaches a value in the range 80–120 bar, then maintain that value while adjusting barrel profile. Published data for this specific configuration is limited; therefore these values are guidance for polyolefin foam extrusion and should be validated on the specific screw and die.
In injection moulding, the measurable response to HYBOOST® 283 is not part weight alone; it is the interaction between shot size, packing pressure, cavity pressure, and gate-seal time. A typical screw-back-pressure setting of 0.8–1.5 MPa hydraulic is used to hold the gas in solution during plastication. The melt is then injected at a reduced shot size, commonly 3–8% lower than the solid moulding, so that the foam expansion completes the filling. The gate is frozen as quickly as practical to prevent gas from escaping backward; consequently, the material should be evaluated on a gate size and runner system that already performs well with the solid resin. If the gate freeze time is too long, the part will show flow lines at the gate and lower internal pressure. Cavity pressure sensors in the region opposite the gate can quantify the internal pressure boost caused by gas expansion. A well-adjusted process usually shows a flatter pressure decay profile after the screw reaches transfer position, but the exact curve depends on wall thickness, stiffening ribs, and mould temperature. Mould temperature also controls skin thickness: a colder mould creates a thicker solid skin and a more uniform appearance, but it can also freeze the surface before the foam has fully expanded, leaving visible splay at the end of fill. For a wall thickness of 2.0–3.0 mm, tool temperature is often set between 25°C and 40°C; above 3.0 mm, lower coolant temperatures or longer hold may be required to prevent post-blow.
The relationship between gas loading and mechanical properties is nonlinear. Density reduction by gas expansion initially lowers mass while retaining much of the bending stiffness because stiffness is partly determined by the outer skin. As density reduction continues, the cell walls become thinner and the distance between load-bearing bulk regions increases. Tensile strength and notched impact strength then drop more rapidly than density alone. The transition point is often called the property cliff edge; for polyolefin foam compounds it commonly appears between 10% and 15% density reduction, depending on cell size distribution and skin thickness. At let-down ratios above 3.0 wt%, cell coalescence may create large voids that reduce tensile strength in the transverse direction and produce an excessive drop in notched impact strength. The appropriate tests are ISO 527-2:2012 for tensile properties and ISO 179-1:2010 for Charpy notched impact. Density should be measured by ISO 1183-1:2019. Shrinkage measurements after 24 h and 48 h by ISO 294-4:2018 should be performed because chemical foaming can reduce sink marks but can also produce delayed post-mould dimensional change if the gas pressure is released through semi-solidified regions.
The following matrix is a starting evaluation grid, not a supplier’s guaranteed performance window.
| Let-down (wt%) | Target density reduction (%) | Mechanical or dimensional test method | Observed failure mode if exceeded |
|---|---|---|---|
| 0.5 | 3–5 | ISO 1183-1:2019, ISO 527-2:2012 | Insufficient sink mark compensation |
| 1.0–2.0 | 6–10 | ISO 179-1:2010, ISO 294-4:2018 | Surface splay if gate speed too high |
| 2.5–3.0 | 11–15 | ISO 527-2:2012, ISO 179-1:2010 | Cell coalescence, loss of notched impact |
| >3.0 | >15 | ISO 1183-1:2019, visual cross-section | Gas streaks, screw slip, uneven skin |
Combination with additives that generate acidic degradation products should be screened. Endothermic chemical blowing agents often operate by an acid-carbonate reaction; residual acid from external lubricants, flame retardants, or certain maleated coupling agents can shift the reaction pH and alter the onset temperature. Similarly, if the compound contains low levels of residual moisture from natural-fibre fillers or aluminium trihydrate, the masterbatch may produce early gas release in the vent. For filled systems, the filler particle size, surface area, and moisture content should be specified before introduction. A moisture level above 500 mg/kg by ISO 15512:2019 in the base resin or filler is often sufficient to change the foaming reproducibility. If that occurs, the first correction is not a change in HYBOOST® 283 let-down; it is the addition or repair of drying capacity.
Scale-up from a 25 mm twin-screw line to a 58 mm production line is not a simple ratio adjustment. The larger machine has a lower surface-to-volume ratio, which means the conductive heating per unit of polymer mass is lower. As a result, the real melt temperature in the larger screw may be lower at the same barrel set-point, and the decomposition reaction may start later. A direct transfer of the small-line barrel profile can therefore produce a soft or unfoamed melt in the production line. Conversely, if the production line uses a longer mixing section, the additional shear heating may push the melt temperature above the intended window and cause premature foaming. For this reason the production-scale validation should map the melt temperature with an immersion thermocouple at the die, not the barrel temperature alone. The same logic applies to injection screw diameter: a 60 mm recovery section can transfer more shear heat than a 25 mm screw at the same screw speed, so back pressure and recovery speed should be adjusted downward during scale-up.
For regulatory submissions, the LLDPE carrier should be evaluated under 21 CFR 177.1520 for olefin polymers used in contact with food, but the finished part must be tested for end-use compliance because the active foaming agent and its decomposition residues are not automatically covered by the carrier resin clearance. A REACH and RoHS conformity declaration should be obtained from the masterbatch supplier for the specific batch. The same applies to EN 71-3 migration limits when the foam is used in toy or childcare applications; the migration limits are based on the end part, not on the masterbatch alone.