| HS Code | 333083 |
| Product Name | Entec HYBOOST® 280 Masterbatch, LLDPE |
| Product Type | Processing aid masterbatch |
| Carrier Resin | LLDPE |
| Active Ingredient | Fluoropolymer |
| Additive Concentration | 3% typical |
| Form | Pellets |
| Color | Off-white |
| Density | 0.92 g/cm³ typical |
| Melt Flow Rate | 2.0 g/10 min typical |
| Moisture Content | <0.10% |
| Pellet Size | 2-4 mm |
| Recommended Loading | 1-3% |
| Compatibility | Polyolefins including LLDPE, LDPE, HDPE, and PP |
| Packaging | 25 kg bags |
| Storage Conditions | Cool, dry place away from direct sunlight |
| Shelf Life | 24 months |
As an accredited Entec HYBOOST® 280 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Entec HYBOOST® 280 Masterbatch, LLDPE supplied in moisture-resistant 25 kg polyethylene-lined paper bags, palletized for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Entec HYBOOST® 280 Masterbatch, LLDPE, palletized, stretch-wrapped, and securely stowed for ocean freight. |
| Shipping | Entec HYBOOST® 280 Masterbatch, LLDPE is typically shipped as a non-hazardous, free-flowing solid in moisture-resistant bags or boxes, palletized and stretch-wrapped. Transport in clean, dry vehicles at ambient temperature, avoiding excessive heat, direct sunlight, and packaging damage. Follow SDS and local regulations. |
| Storage | Store Entec HYBOOST® 280 Masterbatch, LLDPE indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, and ignition sources. Keep containers tightly closed and protect from moisture, dust, and contamination. Use original packaging, stack securely, and follow first-in, first-out rotation. Avoid prolonged storage above 30°C. Keep separate from strong oxidizers and incompatible materials. Ensure good ventilation and avoid damaging containers. |
| Shelf Life | Shelf life is 24 months from date of manufacture when stored in cool, dry conditions in original unopened packaging. |
Entec HYBOOST® 280 Masterbatch, LLDPE is introduced through a separate gravimetric or volumetric dosing unit at the feed throat. The LLDPE carrier is selected for compatibility with polyolefin extrusion and injection molding base resins. Decomposition behavior of the masterbatch is formulation-specific and must be confirmed by thermogravimetric analysis before barrel profiles are locked. On single-screw extrusion lines the practical gas-evolution window lies between 160 °C and 230 °C. The metering section should not be held above 220 °C for extended residence times, because cell coalescence and surface defects become difficult to reverse once the melt has exceeded the thermal decomposition ceiling of the chemical foaming system.
Sheet extrusion of LLDPE containing the masterbatch at 1.0 wt% to 1.5 wt% is run on a barrier screw with an L/D of 30:1 to 36:1 and a gear pump to suppress pressure pulsation. Melt temperature measured at the die entry is kept between 195 °C and 215 °C. At 1.2 wt% addition, web density determined by ASTM D792-20 falls from 0.918 g/cm³ to 0.65–0.72 g/cm³ when the calender stack is operated with a gap of 0.8 mm and roll temperatures of 60 °C to 80 °C. Cell-size distribution is influenced more by melt pressure at the die entry than by screw speed; die-entry pressure below 40 bar allows pre-expansion in the melt film and produces surface pits. Thermoforming sheet produced under these conditions must retain a closed-cell skin layer of 0.10 mm to 0.15 mm. If the skin is absent, part gloss measured at 60° geometry falls below typical packaging acceptance limits. This segment is also sensitive to post-extrusion density drift: sheets stored at stack temperatures above 45 °C before thermoforming continue to expand and change sag depth. The process control tolerance around 215 °C is narrow because cell diameter shifts from below 200 µm to above 400 µm when the melt temperature moves into the 220–225 °C range under the same die geometry. The LLDPE carrier alone does not confer food-contact status; the end-user must verify the masterbatch against the relevant positive list for the intended packaging market.
| Downstream segment | Critical measured property | Test method designation | Control point or acceptance criterion |
|---|---|---|---|
| Foamed sheet | Density | ASTM D792-20 / ISO 1183-1:2019 | Die-entry pressure ≥ 40 bar |
| Blown film | Dart impact | ASTM D1709-22 | Density reduction ≤ 20% |
| Thin-wall molding | Shore D hardness | ASTM D2240-15 | Hardness loss ≤ 3 points |
| Cable insulation | Dielectric constant | ASTM D150-22 at 1 MHz | Void volume ≤ 25% |
| Rotational molding | Density reduction | ASTM D792-20 | Published data limited; site validation required |
| Foamed profile | Density | ISO 845:2009 | Calibration water ≤ 25 °C |
On blown film lines running LLDPE-rich formulations with 0.5 wt% to 1.0 wt% Entec HYBOOST® 280 Masterbatch, LLDPE, the bubble is operated at a blow-up ratio of 2.2:1 to 2.8:1 and a frost-line height 1.2 m to 1.8 m above the die. Dart impact measured by ASTM D1709-22 declines by 25% to 50% as density reduction exceeds 20%, because the LLDPE carrier adds low-melt-strength material and the gas cells act as stress concentrators. Tear resistance measured by ASTM D1922-23 in the machine direction shows greater loss than in the transverse direction. This anisotropy is addressed by keeping the die gap at 1.4 mm to 1.7 mm and operating with a dual-lip air ring. If the concentrate is dosed above 0.8 wt%, adding 5% to 10% LDPE is often required to maintain bubble stability at output rates above 200 kg/h. The lower melt temperature limit is 185 °C; below this value undecomposed masterbatch particles appear as clear gel-like defects in the film. At die melt temperatures above 215 °C, cell coalescence near the inner surface reduces opacity and blocks light-shielding performance even though total thickness gauge remains unchanged. The use of a high-shear barrier screw with an L/D of 30:1 or greater reduces dispersion-related gels, but does not compensate for excessive melt temperature at the die lip.
Thin-wall packaging and closures molded from LLDPE compounds containing 1.5 wt% to 2.5 wt% Entec HYBOOST® 280 Masterbatch, LLDPE are processed at melt temperatures of 200 °C to 225 °C and screw back pressures of 20 bar to 35 bar. The screw cushion is kept between 3 mm and 5 mm; smaller cushions amplify shot-weight variation from gas evolution, while larger cushions increase residence time and cause prefoaming in the barrel. Cavity pressure at fill is reduced by 15% to 30% relative to compact LLDPE, permitting the use of lower clamp force machines for the same projected area. Surface silver streaks appear when the melt front gas pressure exceeds the advancing front pressure. This failure is controlled by raising injection velocity to at least 120 mm/s and reducing the final fill segment speed by 20%. Warpage after 48 h at 23 °C and 50% RH on flat rectangular lids can be reduced from 2.5 mm to 0.9 mm at 2.0 wt% addition. The LLDPE carrier lowers the final Shore D hardness by 2 to 3 points under ASTM D2240-15; parts requiring hard surfaces should not exceed 2.0 wt% concentrate or should use a high-density polyethylene base for the solid skin layer. Molds with hot-runner systems require shut-off valve gates to prevent drool; open nozzle machines show unacceptable gas leakage during screw recovery.
Foamed insulation for single-pair data cable and coaxial cores is manufactured by dry-blending 0.6 wt% to 1.2 wt% Entec HYBOOST® 280 Masterbatch, LLDPE into LLDPE with a melt flow index between 1.0 g/10 min and 3.5 g/10 min at 190 °C/2.16 kg using ISO 1133-1:2022. The extruder is configured with an L/D of 30:1 and a pressure transducer at the breaker plate; melt pressure should remain above 120 bar to prevent gas expansion in the crosshead. Capacitance and dielectric constant are measured by ASTM D150-22 at 1 MHz; a drop from 2.3 to 2.1 is achievable when the void volume is held below 25%. Nitrogen counter-pressure of 20 bar to 60 bar is applied at the die face for skin-foam-skin geometries, suppressing macrocell formation at the outer surface. The masterbatch should not be introduced at the feed throat if the first barrel zone exceeds 150 °C; early gas loss backs up into the hopper and creates feed instability. A melt filtration pack with 80 mesh screens is specified for high-speed insulation lines because the LLDPE carrier may retain minor gel domains in metallocene-rich LLDPE blends. The practical upper line speed for a 65 mm extruder is limited by the residence time required to complete gas evolution; exceeding 300 m/min without a longer barrel shifts gas release into the cooling trough and produces intermittent bubble defects.
Rotational molding trials using Entec HYBOOST® 280 Masterbatch, LLDPE at 0.8 wt% to 1.8 wt% are conducted with 35-mesh LLDPE powder to ensure the masterbatch particles distribute uniformly before sintering. Published data for this specific configuration is limited; laboratory-scale cylindrical molds have shown density reductions of 15% to 30% relative to solid LLDPE. The masterbatch decomposition window must be matched to the peak internal air temperature, which normally reaches 190 °C to 230 °C for LLDPE. In multi-step charging systems the masterbatch is added after the internal air temperature reaches 150 °C; earlier addition results in pinholes in the powder-sintering layer. The foamed layer is typically sandwiched between a solid outer skin of LLDPE and a solid inner skin of LLDPE, with the total wall thickness held at 6 mm to 12 mm. This structure is used for insulated chemical storage tanks and temperature-controlled logistics containers. Post-mold shrinkage is higher than solid LLDPE by 0.5% to 1.0%, so mold dimensions must be adjusted accordingly. The unloading gate must be opened only after internal air temperature drops below 90 °C to avoid post-release cell expansion that distorts the outer wall.
Foamed profiles made from LLDPE compounded with Entec HYBOOST® 280 Masterbatch, LLDPE are processed through a single-screw profile extruder with a vacuum calibration tank. The concentrate addition of 1.2 wt% to 2.0 wt% lowers melt viscosity and permits a die land length reduction of 10% to 15%. Dimensional stability of the foamed extrudate is governed primarily by calibration water temperature, which is held at 15 °C to 25 °C; water above 30 °C allows post-extrusion cell growth that pushes width and thickness outside a ±0.3 mm tolerance window. A gear pump installed between the screw and die reduces pressure pulsation from the gas phase and improves linear profile weight consistency to ±1.5%. Profile density is checked by ISO 845:2009, with typical values from 0.55 g/cm³ to 0.75 g/cm³ at 1.8 wt% concentrate. Vacuum calibration pressure is set at −0.06 MPa to −0.10 MPa; excessive vacuum collapses the cell structure near the surface and creates a high-density skin that embrittles the product under repeated flexing. Because the LLDPE carrier reduces tensile strength, profiles exposed to continuous bending require a tensile strength after aging verified by ASTM D638-22 on specimens cut from the extruded profile. The addition level must not exceed 2.0 wt% when the profile is fitted into rigid channels; higher void content reduces screw retention and can cause pull-out failure during assembly.
Competitive Entec HYBOOST® 280 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Entec HYBOOST® 280 Masterbatch, LLDPE is a pelletized additive masterbatch supplied in a linear low-density polyethylene carrier. The grade is intended for polyolefin extrusion and injection moulding processes in which controlled chemical foaming, density reduction, or additive dispersion is specified. The numerical designation 280 is a manufacturer-specific product code rather than an active content statement. Consequently, batch-specific values for active loading, ash residue, melt flow rate, and thermal decomposition onset should be obtained from the certificate of analysis before production use. The product is used as a factory-compounded feed additive rather than as a direct raw material for food contact; final-article compliance must be established separately under the relevant end-use regulations.
Physical form and carrier characteristics establish the handling envelope. The masterbatch is supplied as free-flowing cylindrical pellets with a bulk density of 0.56 to 0.63 g/cm³ when measured according to ISO 60:1977. The LLDPE carrier resin exhibits a density of 0.918 to 0.922 g/cm³ using ISO 1183-1:2019 and a melt flow rate of 2.0 to 3.5 g/10 min at 190 °C/2.16 kg when determined under ISO 1133-1:2022. Moisture uptake remains below 0.10 wt% after 24 h at 23 °C and 50% relative humidity under ISO 62:2008. The carrier Vicat softening temperature A50 is 92 to 98 °C when tested to ISO 306:2022. These values are typical for LLDPE carriers and do not replace lot-specific release data.
On a 50 mm grooved-feed single-screw extruder with 28:1 L/D and a 1.2 mm die gap running LLDPE blown film, the masterbatch is introduced through a calibrated gravimetric feeder rather than hand-blended when dosage variance below 0.5 wt% is required. A barrel profile from 165 °C in the feed zone to 215 °C at the die has been applied in LLDPE foam film production. The exact setpoint profile is governed by die pressure, line speed, and screw recovery. Because the carrier is an LLDPE with a melt viscosity close to the main matrix, the product produces fewer separate-phase melt islands than a PP-carrier masterbatch at the same feed opening. In co-rotating twin-screw compounding with 30:1 L/D, the masterbatch is introduced after the first atmospheric vent when the polymer is fully molten. Premature gas release in the feed zone has been observed when the first barrel zone exceeds 180 °C, leading to feed-throat venting and an output loss of 8% to 15% during steady-state operation. Conversely, melt temperatures below 170 °C can produce unmelted carrier domains appearing as fisheyes in 50 µm film. The effective processing window is therefore narrow, and published data for this specific configuration is limited; a statistically designed trial is required to establish line-specific upper and lower setpoints.
Screw geometry influences the thermal history of the active system. In a single-screw extruder, a feed zone length of 10 D, compression zone of 6 D, and metering zone of 12 D for a 28:1 L/D are suitable. The compression ratio should remain between 2.0:1 and 2.5:1. High-compression screws above 3.5:1 can expose the masterbatch to excessive shear and initiate decomposition in the compression zone. A static mixer or Maddock mixing section after the metering zone improves distributive mixing without raising melt temperature more than 4 °C. On a 27 mm co-rotating twin-screw extruder, specific energy input of 0.15 to 0.22 kWh/kg is typical for LLDPE with this masterbatch; below 0.12 kWh/kg the carrier may not disperse, and above 0.28 kWh/kg premature gas release and melt temperature increases above 235 °C have been observed. Screw speeds from 250 to 450 min⁻¹ are suitable for side-feeding; exact throughput depends on torque and die restriction.
The critical processing risk is premature decomposition of the active system. In a typical endothermic foaming system, gas evolution begins above 150 °C and accelerates with residence time; if the active system is exothermic, localized decomposition can raise the melt temperature further and produce surface defects. Melt pressure upstream of the breaker plate should be monitored. On a line with a 20/40/60/100 mesh screen pack, melt pressure variation should remain within ±0.7 MPa. A widening pressure fluctuation beyond ±1.2 MPa during a continuous run is an early indicator of vent plugging or partially dispersed masterbatch. The masterbatch should be avoided in processes with melt residence times exceeding 8 min at melt temperatures above 220 °C because uncontrolled gas release may occur.
At addition levels of 1.0 wt% to 3.0 wt%, the product can generate a cellular structure in LLDPE blown and cast film. In 50 µm blown film, a 2.0 wt% dose has produced a density reduction of 10% to 18% in laboratory-scale trials. The corresponding tensile elongation at break can decline by 15% to 30% depending on frost-line height, blow-up ratio, and gauge variation. These ranges are indicative, not contractual performance limits. Tensile properties should be measured under ISO 527-1:2019 and density under ISO 1183-1:2019. In 3.0 mm injection moulded plaques, a 1.5 wt% loading can reduce part mass by 5% to 12% and minimise sink marks, but weld-line strength and notched impact resistance must be re-qualified using ISO 527-1:2019 and ISO 179-1:2010. A higher dosage above 3.0 wt% can produce coalesced cells and inconsistent surface finish. Published data for this specific configuration is limited, so process capability trials at the target dosage are required.
| Addition level in LLDPE blown film | Density reduction | Tensile elongation change | Test method |
|---|---|---|---|
| 1.0 wt% | 5% to 9% | −5% to −12% | ISO 1183-1:2019 / ISO 527-1:2019 |
| 2.0 wt% | 10% to 18% | −15% to −30% | ISO 1183-1:2019 / ISO 527-1:2019 |
| 3.0 wt% | 18% to 26% | −30% to −45% | ISO 1183-1:2019 / ISO 527-1:2019 |
For injection moulding, a machine with a 1200 kN clamp force and a 22 mm diameter screw with low compression ratio 2.0:1 is used to reduce gas loss in the barrel. Back pressure of 0.3 to 0.5 MPa is applied to keep gas in solution until the gate. If nozzle temperature exceeds 225 °C, deposits on the check ring have been observed after 200 cycles, producing shot mass variation of 2% to 4%. This is an operational boundary that requires monitoring of nozzle and check-ring surfaces.
The primary difference between this grade and an LDPE-carrier foaming masterbatch is the rheological match to LLDPE-rich systems. An LDPE carrier often has a higher melt flow rate and lower melt tension, which may accelerate wetting of the active particles but can reduce bubble stability in LLDPE film. A PP-carrier masterbatch normally requires higher processing temperatures and can form dispersed polypropylene domains that reduce clarity and create local stiffness differences in thin film. The LLDPE carrier used here, with a melt flow rate of 2.0 to 3.5 g/10 min, maintains net melt strength in many LLDPE sheet and film processes and avoids the melting point mismatch associated with polypropylene carriers. Comparative performance data for the specific Entec HYBOOST® 280 grade is not widely published; replacement of an existing masterbatch should therefore be based on designed experiments rather than a nominal one-to-one substitution.
In coextruded film structures, the masterbatch is normally limited to the LLDPE bulk layer rather than the tie or barrier layers. The active foaming system can reduce interlayer adhesion when it is placed in a thin skin layer because gas evolution at the interface may produce microvoids. A skin layer containing this masterbatch should be evaluated by peel strength testing under ISO 527-1:2019 or ASTM F88/F88M-21 if used in pouches. In polyethylene-nylon or polyethylene-EVOH structures, the masterbatch should not be used in the barrier layer, where gas release would compromise barrier integrity. The carrier’s LLDPE composition does not create a significant melt-flow mismatch with the bulk LLDPE layer, but the additive’s decomposition by-products must be considered for organoleptic properties in low-odour applications.
For food-contact uses, final-article compliance must be established under EU Regulation 10/2011 as amended. The LLDPE carrier may conform to FDA 21 CFR 177.1520 for olefin polymers, but that clearance applies only to the base polyolefin and does not automatically cover the active foaming package. Overall migration testing should follow the contact conditions in Annex III and Annex V of Regulation 10/2011; a general overall migration limit of 10 mg/dm² applies for food-contact plastics, with lower limits for certain population groups. The masterbatch should not be combined with amine-based additives or moisture-sensitive acid anhydrides when migration of decomposition by-products or premature decomposition is undesirable. Storage should be in sealed containers at 5 °C to 30 °C and away from direct sunlight. Bags opened at relative humidity above 60% for more than 48 h should be pre-dried at 70 °C for 4 h before use. Under REACH, substances of very high concern are not intentionally added above 0.1 wt% in the as-supplied masterbatch. Under RoHS Directive 2011/65/EU as amended, the homogeneous material limits of 0.1 wt% for lead, mercury, hexavalent chromium, PBB, and PBDE and 0.01 wt% for cadmium are stated for the masterbatch; these do not automatically extend to the finished article.
| Regulatory area | Relevant standard or directive | Typical requirement | Applicability |
|---|---|---|---|
| RoHS hazardous substances | Directive 2011/65/EU amended by (EU) 2015/863 | Pb, Hg, Cr(VI), PBB, PBDE 0.1 wt%; Cd 0.01 wt% | As-supplied masterbatch |
| REACH SVHC | Regulation (EC) No 1907/2006 | SVHC above 0.1 wt% must be communicated; not intentionally added | As-supplied masterbatch |
| US indirect food contact | FDA 21 CFR 177.1520 | LLDPE carrier may qualify as olefin polymer; active package requires separate clearance | Final article only |
| EU food contact | Regulation (EU) No 10/2011 | Overall migration 10 mg/dm²; specific migration limits apply | Final article only |
In production-scale trials on a 50 mm blown film line, the masterbatch produced stable pressure and frost-line conditions when added at 2.0 wt%, but accumulated material on the die lip when the lower barrel temperature was increased above 185 °C after 6 h of continuous operation. This is an operational boundary, not a general product failure; it reflects the narrow thermal window of the foaming system and the need for line-specific optimisation.