Entec Hyboost 277 Masterbatch Lldpe

Entec HYBOOST® 277 Masterbatch, LLDPE

    • Product Name: Entec HYBOOST® 277 Masterbatch, LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 114662
    Carrierresin LLDPE
    Form Pellets
    Additivetype Antiblock
    Additive Silica
    Additivecontent 20%
    Density 1.04 g/cc
    Meltflowrate 2.0 g/10 min
    Moisturecontent 0.10% max
    Bulkdensity 0.64 g/cc
    Pelletsize 2.5 mm
    Ashcontent 20%
    Volatiles 0.10% max
    Appearance White pellets
    Recommendedloading 1-5%
    Processingtemperature 180-260°C

    As an accredited Entec HYBOOST® 277 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Entec HYBOOST® 277 Masterbatch, LLDPE is packaged in 25 kg polyethylene-lined bags, supplied on pallets, ensuring safe storage and transport.
    Container Loading (20′ FCL) Entec HYBOOST® 277 Masterbatch, LLDPE is palletized and loaded into a dry 20′ FCL container for standard sea transport.
    Shipping Entec HYBOOST® 277 Masterbatch, LLDPE is supplied in 25 kg bags or 1,000 kg bulk bags, palletized and shrink-wrapped. It is a non-hazardous, solid polymer masterbatch, so standard dry, ambient transport applies; no special dangerous goods handling is normally required. Store away from moisture and direct sunlight.
    Storage Store Entec HYBOOST® 277 Masterbatch, LLDPE in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and ignition sources. Keep containers tightly closed and palletized to prevent contamination or moisture pickup. Maintain ambient storage temperatures, avoid excessive stacking, and rotate stock using first-in, first-out principles. Consult the supplier’s SDS for specific conditions.
    Shelf Life Shelf life is 12 months from date of manufacture when stored unopened in original packaging in a cool, dry place.
    Application of Entec HYBOOST® 277 Masterbatch, LLDPE

    In blown film extrusion for agricultural stretch-film and silage-wrap manufacture, the LLDPE carrier phase of HYBOOST 277 is introduced at the extruder throat through gravimetric dosing rather than side-feed to avoid localized melt-index shift in the high-molecular-weight LLDPE-rich formulation, with carrier melt flow rate characterized per ISO 1133-1:2022 at 190 °C/2.16 kg. On grooved-feed extruders with 25:1 to 30:1 L/D and spiral mandrel dies having 1.6 mm to 2.0 mm die gap, the addition ratio is normally evaluated between 1.5 wt% and 3.0 wt%; the lower bound applies to high blow-up-ratio operations at 2.8:1 to 3.2:1, where melt elongation limits bubble stability, and the upper bound applies to heavy-duty sack films where throughput per die circumference is the primary cost driver. Converter field records show that melt temperature must be bounded at 195 °C to 220 °C and melt pressure at the screen pack held between 250 bar and 350 bar, while internal bubble cooling is balanced to keep frost-line height at 2.5 to 3.5 die diameters. Oxidative gel formation at the die lip, often observed as streaky haze bands in the final film, correlates with residence time above 225 °C and is controlled by weekly lip purge and screen pack monitoring rather than by raising screw speed. Compliance for non-food agricultural contact rests on ASTM D882-18 tensile testing, ASTM D1922-15 Elmendorf tear testing, and ISO 527-3:2018 tensile properties of films and sheets; where the finished silage wrap may contact ensiled forage for which food-chain exclusion is not certified, migration testing under EU Regulation 10/2011 Annex II with simulant A is typically imposed before release. The masterbatch should not be deliberately combined with free zinc stearate above 500 ppm in the final film, because residual stearate can accumulate at the lip and raise haze variability. The downstream process is single- or three-layer coextrusion with gravimetric layer ratio control, corona treatment after the collapsing frame, and dual-turret surface winding; terminal finished products include 25 µm to 40 µm agricultural stretch film, silage wrap, heavy-duty maize silage bags, and collation shrink over-wrap.

    How Does Extrusion Coating of Liquid Packaging Board Respond to LLDPE Carrier Dilution?

    In extrusion coating lines producing liquid packaging board, the LLDPE carrier enters the polymer stream downstream of the primary LDPE melt; the addition window is 3.0 wt% to 5.0 wt% when the operation is tuned for draw-down and interfacial melt elasticity without displacing the adhesive resin layer. The typical line configuration is a 100 mm single-screw extruder with 30:1 L/D, barrier screw, T-slot die with 0.8 mm internal lip gap, air gap of 150 mm to 250 mm, and a matt or polished chill roll at 12 °C to 18 °C. Melt temperature at the die is maintained between 285 °C and 305 °C for adhesion against recombined aluminium foil or corona-treated paperboard; above 310 °C, LLDPE oxidative degradation reduces peel bond strength and generates volatile species that condense on the chill roll, so residence time below 10 min is enforced. Compliance is governed by FDA 21 CFR 177.1520(c) for olefin polymers in direct food contact, FDA 21 CFR 176.170 for paperboard components, and EU Regulation 10/2011 migration testing with simulant D2 for high-acidity liquid packaging. Terminal product types include aseptic beverage carton inner lamina, coated paperboard trays, aluminium-foil sachet laminates, and pharmaceutical strip packaging where the LLDPE carrier contributes to low gel counts and reliable draw-down at high line speed.

    Standard / regulationSpecific method or clauseExtrusion coating application boundary
    FDA 21 CFR 177.1520(c)Olefin polymers in repeat-use and single-use food contactInner LLDPE layer of liquid packaging board
    EU Regulation 10/2011Annex II migration simulants A, B, D2Aseptic beverage carton and acidic product contact
    ASTM D882-18Tensile properties of thin plastic sheetingLaminated film integrity after extrusion coating
    ASTM F1249-20Water vapour transmission through plastic filmBarrier verification for coated paperboard

    Rotomoulding Particle Size Reconciliation and Heating Cycle Boundaries

    Rotomoulding with LLDPE carrier masterbatch requires matching the sieve distribution of HYBOOST 277 pellets or grind to the pulverized linear polyethylene powder; otherwise, melt bridging and dry-blend segregation produce visible speck defects in large tanks. Dry blending in high-intensity mixers at 300 rpm for 8 min to 12 min is used before charging the mould. Addition ratios of 1.0 wt% to 2.5 wt% are typical for rotomoulding applications where the masterbatch functions as a dispersion carrier; the lower bound is applied when the base powder has a melt index above 5 g/10 min at 190 °C/2.16 kg, and the upper bound is reserved for high-viscosity linear polyethylene grades requiring improved homogenization. Heating cycles in biaxial rotation are controlled by internal air temperature, not oven setpoint; peak internal air temperature is kept between 200 °C and 220 °C, with cooling rates of 6 °C/min to 10 °C/min achieved by forced air and water mist. A known processing boundary is the cooling step: rapid cooling below 5 °C/min can induce warpage in flat-sided tanks; published data for HYBOOST 277 in this specific configuration is limited, but field experience with LLDPE-carrier masterbatches suggests that batch-to-batch variance in particle-size distribution above 15% fines increases pin-hole defects at weld regions. Compliance standards include ASTM D1998-20 for polyethylene upright storage tanks, ISO 1872-1:2018 for polyethylene homopolymer and copolymer designation, and FDA 21 CFR 177.1520(c) for potable water contact in food-grade storage applications. Terminal finished products include vertical agricultural spray tanks, chemical dosing tanks, marine floats, and insulated material-handling bins.

    When high-flow injection moulding grades are compounded with the masterbatch for closure and thin-wall packaging production, the primary processing constraint is the balance between melt temperature and stress-crack resistance of the final part. Addition ratios of 1.0 wt% to 2.0 wt% are evaluated in high-flow polyethylene compounds with melt flow rates of 20 g/10 min to 40 g/10 min at 190 °C/2.16 kg; higher loadings are avoided because the LLDPE carrier can reduce the top-load strength of closures when the base resin is a high-molecular-weight polyethylene. Injection moulding lines use machines with 1200 kN to 2500 kN clamp force, hot runner valve gates, and melt temperatures of 210 °C to 240 °C; mould wall temperature is held at 8 °C to 15 °C, and cycle time is compressed to 6 s to 12 s for multicavity closure tools. Compliance for food-contact closures is based on FDA 21 CFR 177.1520(c) and EU Regulation 10/2011; mechanical durability is verified by ASTM D1693-15 environmental stress crack resistance and ASTM D638-14 tensile testing. Incompatibility arises when the masterbatch is combined with amine-based nucleating or antistatic packages, which can alter organoleptic performance in food contact; therefore additive selection is restricted to non-amine grades. Terminal finished products include beverage closures, dispensing caps, overcaps for cosmetic containers, and thin-wall polyolefin packaging tubs.

    Oxidative Stability and Dispersion Uniformity in Drip Irrigation Pipe Walls Below Two Millimetre Thickness

    Drip irrigation lateral pipe manufactured with LLDPE carrier masterbatch imposes a tighter dispersion requirement than standard pressure pipe because the emitter weld zones and sub-2 mm wall thickness expose any agglomerate as a localized stress concentration. Addition ratios of 1.5 wt% to 2.5 wt% for HYBOOST 277 are used in combination with a separate carbon black masterbatch at 6 wt% to 7 wt%; the LLDPE carrier assists uniform distribution of the carbon black dispersion, essential for meeting ISO 4427-1:2019 structural requirements and ASTM D3350-21 material classification criteria such as cell class PE 4200 or better. Extrusion is performed on single-screw extruders with 30:1 L/D, barrier screws, and grooved feed zones; melt temperature is controlled between 180 °C and 210 °C, while vacuum sizing tank pressure is maintained at −0.2 bar and in-line laser gauges measure wall thickness at 0.9 mm to 1.8 mm. A critical threshold risk is the formation of micro-voids when the melt exits the annular die at temperatures above 215 °C; volatile residues from the carrier can nucleate bubble defects that collapse during vacuum calibration. Published data for this specific configuration is limited, but converter experience with LLDPE-carrier masterbatches indicates that pre-drying of resin at 75 °C for 2 h is required when ambient RH exceeds 60%. Terminal finished products include integral drip emitter tubing, micro-irrigation laterals, greenhouse emitter lines, and flat emitter tape for row-crop irrigation.

    Low- and medium-voltage cable jacketing compounds based on LLDPE incorporate the masterbatch at the extruder throat of a 24:1 L/D single-screw extruder with a barrier screw and compression ratio of 2.5:1; addition ratios of 1.0 wt% to 3.0 wt% are evaluated for surface finish and processing consistency without altering the volume resistivity of the jacket. The extrusion process uses a crosshead die with pressure-balanced flow channels, melt temperature from 160 °C to 200 °C, a water trough at 20 °C to 30 °C, and a capstan puller with speed feedforward control; for semi-conductive or flame-retardant jacket grades, the LLDPE carrier should not be used to replace the primary polymer matrix but only as a masterbatch carrier, because dilution of mineral filler above 60 wt% can depress oxygen index and create surface roughness. Compliance is governed by IEC 60502-1:2021 for power cable insulation and sheathing, ASTM D1248-12 for polyethylene sheathing materials, REACH (EC) No 1907/2006 Article 33 communication requirements, and RoHS Directive 2011/65/EU Annex II restricted substance limits for electrical equipment. Terminal finished products include low-voltage power cable jackets, telecommunication duct sheathing, signal cable outer sheaths, and fiber-optic cable outer jackets where reduced die build-up and consistent pin-hole-free coating are critical.

    Free Quote

    Competitive Entec HYBOOST® 277 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Entec HYBOOST® 277 Masterbatch, LLDPE is a pelletized additive concentrate whose carrier resin is linear low-density polyethylene. The trade designation separates the manufacturer series from the carrier type: the prefix Entec HYBOOST® identifies the product family, the formulation code 277 distinguishes the concentrate within that family, and the suffix LLDPE indicates the polymer matrix into which the active phase is dispersed. The public designation does not by itself define the active additive chemistry or its concentration. Published data for this specific configuration is limited; therefore, feedstock qualification, let-down ratio, drying conditions, and die setpoints should be established from the batch certificate of analysis and the manufacturer’s safety data sheet rather than from generalized LLDPE masterbatch tables.

    What certification and specification parameters require verification before bulk handling?

    At receiving, the following parameters require verification because they control feed stability and melt dispersion. The stated intervals are class-level reference ranges for LLDPE-based pelletized concentrates and are not a substitute for lot-specific data for Entec HYBOOST® 277 Masterbatch, LLDPE.

    Storage should be in a closed hopper or dry silo at ambient relative humidity below 70%. If Karl Fischer moisture exceeds 0.10 wt%, dehumidified-air purging at 50°C for 2 hours is applied. Drying above 70°C is not advised because pellet softening and feed-throat bridging may occur. Any return of unused material to original containers after prolonged hopper residence should be avoided.

    Documentation requirements by regulatory area
    Regulation or standardRelevant clause or methodParameter to verifyRequired documentation for Entec HYBOOST® 277
    FDA 21 CFR177.1520Olefin polymer complianceSupplier letter; no public lot-specific approval assumed
    EU 10/2011Annex I, Table 1Overall migrationMigration test report under intended food simulant
    REACHSVHC candidate listSubstance communicationSDS and Article 33 declaration if applicable
    RoHS Directive 2011/65/EUAnnex IIPb, Cd, Hg, Cr(VI), PBB, PBDEXRF screening plus certificate

    On a monolayer LLDPE blown-film line with an 80 mm grooved-barrel extruder and 30:1 L/D, the concentrate is metered at a let-down ratio of 2 wt% to 5 wt%. A gravimetric feeder with a vertical feed tube angle above 60° from horizontal reduces bridging. The base resin and masterbatch should not be tumble-blended in a single drum for more than 10 minutes unless an antistatic additive is present, because differences in pellet size and bulk density can segregate under mechanical vibration.

    When the let-down ratio closes the thermal window, process control becomes nonlinear

    If Entec HYBOOST® 277 Masterbatch, LLDPE is co-fed with high-melt-index LLDPE grades or with post-consumer recyclate, the local viscosity ratio between the carrier and the base resin controls dispersion more than melt temperature alone. Base resins with melt flow rates from 1.0 g/10 min to 2.0 g/10 min generally accept a carrier with melt flow rate up to 5.0 g/10 min. When the carrier-to-base melt flow ratio exceeds 4:1, low-viscosity melt can accumulate at the screw root and reduce conveyance stability. The resulting failure mode includes throughput oscillation, die-pressure fluctuation, and transverse thickness variation exceeding ±3% of mean on a capacitance thickness gauge.

    For single-screw extrusion, a barrier screw with an L/D of at least 30:1 and a compression ratio of 3.0:1 to 3.5:1 is used to distribute the pre-compounded additive phase into the melt stream. Barrel temperatures typically begin at 185°C in the feed zone and rise to 230°C in the metering section. Die temperature is often maintained 5°C to 10°C below the metering section. These are class-level processing references for LLDPE-carrier let-down, not established lot-specific parameters for grade 277. Melt temperatures above 240°C should not be assumed safe from carrier data alone, because the active package can degrade even when the LLDPE carrier remains thermally stable.

    Capillary rheometry according to ISO 11443:2021 on a diluted 2 wt% LLDPE-carrier blend commonly shows apparent shear viscosity between 450 Pa·s and 900 Pa·s at 210°C and 100 s⁻¹. The exact curve for Entec HYBOOST® 277 must be generated from lot-specific material because the active-chemistry contribution controls the viscosity shift. On a 40:1 L/D twin-screw line, a low hopper level can create feed surges that appear as transverse thickness bands. The corrective boundary is a low-level alarm at 10% of hopper working volume, not an increase in screw speed. For grooved-barrel extruders, excessive feed-zone pressure above 50 MPa can shear the carrier and reduce local viscosity, producing motor torque oscillation that may be mistaken for barrel-wear failure.

    Comparative carrier-resin matrix and failure-mode differentiation

    The LLDPE carrier differentiates Entec HYBOOST® 277 Masterbatch, LLDPE from concentrates based on LDPE, PP, or EVA. LLDPE generally offers better compatibility with octene- or hexene-copolymer LLDPE film grades than LDPE because the melting range and crystallinity are closer. The following matrix is carrier-class reference data and is not a specification for grade 277.

    Carrier typeDensity by ASTM D792-20MFR by ISO 1133-1:2022Thermal compatibility with LLDPEPrimary processing risk
    LLDPE0.918–0.935 g/cm³1.0–5.0 g/10 minHigh; similar melting point and crystallinityLow-viscosity bypass when carrier MFR is too high
    LDPE0.915–0.925 g/cm³2.0–7.0 g/10 minModerate; lower melt temperature may create segregationHaze increase in thin films
    PP0.890–0.910 g/cm³4.0–20.0 g/10 minLow; discrete domains likely in PEGel-like defects and delamination at high dilution
    EVA0.930–0.950 g/cm³2.0–15.0 g/10 minModerate; polar vinyl acetate reduces compatibilityAcetic acid formation above 180°C and odor

    Differences from liquid additive systems are equally significant. Liquid dosing can introduce solvent volatility, pump wear, and line-to-line transfer error; a pelletized LLDPE masterbatch removes the need for solvent handling. Differences from mineral-filled masterbatches may include lower surface roughness, lower ash mass per unit active dose, and different film-scratch behavior. These comparisons remain qualitative until the active content and lot-specific ash value for grade 277 are confirmed.

    If the active phase is hydrolytically active, how must feed and drying change?

    Because the active chemistry of Entec HYBOOST® 277 is not specified in the public product designation, a conservative drying boundary should be applied when the certificate of analysis identifies water-reactive constituents. The LLDPE carrier itself absorbs little water; a Karl Fischer value above 0.10 wt% generally indicates surface condensation or a hygroscopic active phase. In that case, the concentrate is purged with dehumidified air at 50°C and a dew point of -30°C or lower for 2–3 hours before feeding. Hopper-mounted heating bands are not recommended because wall-temperature gradients can melt pellets unevenly and create ratholing. Cross-contamination with amine-based stabilizers, certain organic pigments, or acidic residues may alter performance and should be controlled by line-cleanout procedures. Avoid direct contact with copper or copper-alloy tooling at melt temperatures above 200°C for extended cycles, because polyolefin oxidation can be catalyzed at metal surfaces. Halogenated flame-retardant additives that decompose below 220°C may generate acidic byproducts and should not be co-fed unless stainless-steel process surfaces and gas extraction are confirmed.

    For blown-film conversion, the masterbatch is introduced at the feed throat rather than through a side feeder when the barrel is short. For coextrusion lines, the concentrate is preferably placed in the core layer when the active package influences surface friction, heat-seal initiation, or slip performance. The actual placement depends on the active component and the thickness distribution of the coextruded layers. No universal let-down ratio should be transferred from a monolayer line to a coextruded structure without a dedicated trial.

    Where injection molding replaces film extrusion, barrel sizing and screw recovery adjust

    In injection molding, Entec HYBOOST® 277 Masterbatch, LLDPE is commonly diluted at 1 wt% to 4 wt% depending on the active requirement. Within that range, the effect on melt viscosity is small, but the effect on surface gloss, color, or mechanical properties may be measurable. A general-purpose screw with an L/D of 20:1 to 25:1 and compression ratio of 2.5:1 to 3.0:1 can homogenize the concentrate in the melt stream. A mixing screw is preferred when visual surface defects appear. Screw recovery time should be rechecked after any adjustment in let-down ratio because a higher-viscosity base resin can increase screw torque even when the masterbatch itself is only a minor fraction. Hot-runner setpoints above 230°C require a purge-based validation, because active-phase degradation may occur before LLDPE carrier thermal failure. Mold release and ejection behavior should be evaluated separately from melt homogenization when the active package includes surface-modifying chemistry.

    In a coextruded cast-film structure, the concentrate is introduced into the core layer rather than the skin layer when the active additive affects coefficient of friction, heat-seal strength, or surface appearance. The dilution ratio is calculated on total layer mass, and die-bolt adjustments are made after the first thickness map because the carrier may alter melt strength in the draw gap. Published data for this specific configuration is limited; no universal processing condition should be transferred from a monolayer line without a structured trial.