| HS Code | 832729 |
| Productname | Entec HYBOOST® 257 Masterbatch, LLDPE |
| Manufacturer | Entec Polymers |
| Producttype | Masterbatch |
| Carrierresin | LLDPE |
| Additivetype | Slip agent |
| Additivecontent | 5% |
| Form | Pellets |
| Color | Natural |
| Odor | Slight |
| Density | 0.930 g/cm³ |
| Meltflowrate | 20 g/10 min |
| Moisturecontent | ≤0.10% |
| Recommendeddosage | 1–5% |
| Processingtemperature | 160–220°C |
| Shelflife | 24 months |
| Storageconditions | Cool, dry, below 30°C |
| Packaging | 25 kg bags |
As an accredited Entec HYBOOST® 257 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Entec HYBOOST® 257 Masterbatch, LLDPE is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for industrial transport. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Entec HYBOOST® 257 Masterbatch, LLDPE, in 25 kg bags on pallets, securely stowed and weather-protected. |
| Shipping | Entec HYBOOST® 257 Masterbatch, LLDPE is a non-hazardous, solid plastic masterbatch, typically shipped in 25 kg polyethylene bags or cartons, palletized and shrink-wrapped. Normally not regulated for transport under DOT, IMDG, IATA, or ADR. Store dry, away from heat. Refer to SDS for full details. Industrial use only. |
| Storage | Store Entec HYBOOST® 257 Masterbatch, LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and ignition sources. Keep original containers tightly closed, palletized, and off the floor. Protect from moisture, dust, and contaminants. Avoid excessive stacking and prolonged storage above 30°C. Follow manufacturer/SDS guidance for safe handling and shelf life. |
| Shelf Life | Entec HYBOOST® 257 Masterbatch, LLDPE typically has a 12-month shelf life when stored unopened in a cool, dry place away from direct sunlight. |
In blown film extrusion of 100% metallocene LLDPE at die gaps of 1.0–1.5 mm, the primary processing barrier is sharkskin melt fracture. Entec HYBOOST® 257 Masterbatch, LLDPE is introduced as a dry-blend addition at 2–4 wt% in the main resin feed. The LLDPE carrier matches the metallocene base resin and disperses through the melting section of grooved-feed extruders with L/D 24:1 to 30:1 and screw diameters 45–75 mm. Melt temperatures are maintained between 190°C and 230°C, and conditioning is evaluated by the decline in head pressure and screw torque over 30–90 min. Finished film is tested according to ASTM D2457-21 for haze, ASTM D1709-22 for dart impact, and ASTM D882-18 for MD/CD tensile elongation. In food-contact structures, the finished film must meet FDA 21 CFR 177.1520 and EU 10/2011; the masterbatch supplier’s conformity statement does not replace the converter’s overall migration assessment. Global substance restrictions require compliance with Regulation (EC) No 1907/2006 where applicable. Operational boundaries include additions above 5 wt% that can lead to screw slip and throughput surging, and melt temperatures above 240°C that may accelerate additive degradation. End products include heavy-duty sacks, agricultural stretch film, and collation shrink film.
High-speed cast film lines producing 12–25 µm LLDPE stretch wrap encounter edge melt fracture, die lines, and die-lip buildup above 150 m/min. The masterbatch is metered separately at 1.5–3.0 wt% through a gravimetric side feeder to avoid concentration drift. The extrusion line typically uses a 90–150 mm single-screw extruder with 30D L/D and a flat die with 0.6–0.8 mm lip gap. Melt temperature is held between 210°C and 240°C, and the cast roll temperature is set between 15°C and 25°C. Melt mass-flow rate is checked using ASTM D1238-20 at 190°C/2.16 kg and is not expected to shift beyond the normal lot variation at 3 wt%. The active processing aid chemistry reduces the frequency of die-lip accumulation; converter documentation should record the interval between wipe cycles, and any claim of extended cycle time must be tied to that measured baseline. Excessive slip can alter film optics, measurable as an increase in haze under ASTM D2457-21, and can cause draw resonance. For industrial stretch wrap, no direct food-contact standard applies. When the film is sold for food contact, compliance with FDA 21 CFR 177.1520 and EU 10/2011 must be verified on the final product. End products are industrial pallet wrap, thin-gauge stretch film, and protective masking film.
In shuttle and wheel extrusion blow molding machines producing containers from 500 mL to 5 L, parison surface defects appear as longitudinal die lines. The masterbatch is added at 1–2 wt% to the HDPE resin feed on 65–90 mm extruders with 20:1 to 24:1 L/D. The die head temperature is controlled at 170–210°C, and the temperature difference across the head tooling is held within ±5°C to prevent parison curl. The carrier LLDPE at 1 wt% shifts the melt index of a 0.3–0.9 g/10 min HDPE by less than typical lot-to-lot variation when measured by ASTM D1238-20. For food and dairy containers, the final article must meet FDA 21 CFR 177.1520 and EU 10/2011, and organoleptic migration tests under EN 1186-1 or EN 1186-5 are commonly applied. In multilayer containers, the masterbatch is limited to the outer LLDPE-modified layer unless the full wall structure is migration-compliant. Because LLDPE alters the stiffness-to-toughness balance, top-load strength should be re-tested under ASTM D2659-17 or ISO 12048. The use rate should not exceed 3 wt% because higher LLDPE fractions can reduce top-load stiffness and increase bottle weight variation due to altered die swell. End products include HDPE dairy bottles, juice bottles, and multilayer cosmetic containers.
Carbon-black-filled PE100 and PE80 pipe compounds operate at lower melt temperatures but higher filler-related die build-up. Entec HYBOOST® 257 Masterbatch, LLDPE is fed at 1–3 wt% into the main feed throat of a 45–75 mm, 30D single-screw extruder running 180–220°C. The adapter melt pressure is monitored with a 10 MPa pressure transducer, and conditioning is considered stable when the trace varies by less than ±0.1 MPa over 10 min. For potable water pressure pipe, the finished compound must be part of a certified formulation under ISO 4427 and EN 12201; the PE-carrier masterbatch is acceptable only when the certification dossier covers the specific masterbatch and let-down ratio. For corrugated drainage pipe, surface roughness can be assessed by profile parameters under ISO 4287. The LLDPE carrier may slightly reduce flexural modulus; therefore pipe stiffness measurements under ISO 9969 or ASTM D2412 are required when the addition exceeds 2 wt% in solid-wall pressure pipe. Pressure pipe slow crack growth remains controlled by the base PE100 resin, and the masterbatch does not replace the pipe resin’s SCG certification. The melt temperature must not exceed 240°C because stabilizer packages in filled PE compounds can generate volatiles and create surface pitting. End products are non-pressure corrugated culvert pipe, electrical conduit, and pressure pipe when combined with certified PE100 resin.
Cable jackets formulated with magnesium hydroxide or aluminum trihydrate at 55–65 wt% loading are prone to filler agglomeration and melt-fracture-induced surface roughness. The masterbatch is added at 2–4 wt% in the PE-rich let-down phase on 60–90 mm extruders with 25:1 to 30:1 L/D and compression ratios of 2.5:1 to 3.5:1. Melt temperature is limited to 180–210°C to avoid premature dehydration of the hydrated mineral filler; head pressure and screw torque are recorded continuously. Published data for this exact masterbatch in a 60 wt% hydrated-mineral cable jacket is limited, so line trials are required to establish conditioning time. The finished jacket must meet the flame-spread requirements of IEC 60332-1 and, where low halogen content is claimed, the halogen acid gas limit of IEC 60754-1. For the US market, the PE compound can be classified under ASTM D1248-18; global substance restrictions require finished-cable compliance with Directive 2011/65/EU and testing according to IEC 62321 splits. The LLDPE carrier has limited compatibility with EVA-rich polar matrices; in formulations with more than 20 wt% EVA, the masterbatch should be evaluated at ≤1 wt% first and filler dispersion assessed by ISO 18553. End products are low-voltage PE jacketing, fiber-optic duct cable jackets, and halogen-free conduit sheathing.
High-filler PE concentrates containing calcium carbonate at 50–75 wt% loading can suffer from high melt pressure and poor filler wet-out during twin-screw compounding. The masterbatch is fed at 2–4 wt% into the main hopper of a 40–75 mm co-rotating twin-screw extruder with L/D 32:1 to 48:1 and screw speed 300–600 rpm. It is not a filler compatibilizer; its function is to reduce melt-phase friction and stabilize pressure before pelletizing. Melt pressure is measured by a 10 MPa transducer mounted in the die plate adapter, and the filler dispersion of the pelletized concentrate is rated under ISO 18553:2002. Melt mass-flow rate is measured under ISO 1133-1:2022 at 190°C/2.16 kg. In packaging-grade concentrates, the final article must still meet FDA 21 CFR 177.1520 or EU 10/2011 as applicable; the processing aid addition does not independently confer compliance. Feeding at more than 5 wt% can produce screw slip, evidenced by increasing screw speed without a rise in throughput; the test run should be terminated if this occurs. End product is a let-down concentrate for blown film, cast film, or blow molding, not a final consumer article.
Extrusion coating of 15–30 g/m² LLDPE onto paperboard for liquid packaging demands high melt temperature 290–320°C to promote adhesion, which accelerates die-lip oxidation and backflow deposits. The masterbatch is metered at 1.5–3.0 wt% into the coating line extruder, typically 90–150 mm with 30D L/D and a die opening of 0.4–0.6 mm. Because the LLDPE carrier itself participates in the coating layer, the coating weight and adhesion must be re-validated; peel strength is measured under ISO 11339. For food packaging, the coated paperboard must meet FDA 21 CFR 176.170 and EU 10/2011 where applicable. Temperatures above 320°C or residence times above 10 min can degrade the processing aid and generate plate-out. End products are paperboard ice cream cartons, coffee cup stock, and flexible laminate tie layers.
Competitive Entec HYBOOST® 257 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Entec HYBOOST® 257 Masterbatch, LLDPE is a pelletized masterbatch supplied in a linear low-density polyethylene carrier for metered addition to polyolefin extrusion and molding processes. The carrier resin is selected to provide melt-viscosity compatibility with polyethylene-rich formulations while preventing segregation of the active component during silo storage, conveying, and gravimetric feeding. Material characterization is performed using ISO 1133-1:2022 Method A for melt mass-flow rate, ISO 1183-1:2019 for density, and ISO 11358-1:2022 for thermal decomposition screening. Published data for this specific configuration is limited; the numerical ranges below describe the generic LLDPE-carrier masterbatch envelope and must not replace lot-specific certificates of analysis or supplier process recommendations. The masterbatch is normally evaluated at addition ratios between 0.5 wt% and 2.5 wt% of the total melt stream, with the low end associated with thin-gauge film and the high end associated with injection-molded or extruded profiles requiring greater pressure-drop reduction or density control.
LLDPE carrier resins used in foaming masterbatches tend to exhibit a melting peak between 120 °C and 126 °C and melt mass-flow rates commonly in the range of 15 g/10 min to 30 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022. The linear molecular architecture produces shear-thinning behavior that is less steep than branched-LDPE carriers at comparable melt index. On a single-screw extruder with a 30:1 to 40:1 L/D ratio, the feed-throat barrel section should be maintained at a lower temperature than the same zone for a branched-LDPE system to prevent premature pellet blocking and screw channel bridging. Industrial practice for foam extrusion with LLDPE carriers typically sets the first barrel zone between 150 °C and 170 °C, then increases the downstream zones to 190 °C to 230 °C to complete decomposition of the active component. The lower feed-zone temperature prevents the low-melting carrier phase from forming a shear layer too early in the compression zone, which would reduce solids conveying efficiency and create feed-throat pressure instability.
Thermal decomposition screening of the active component is run under non-oxidative conditions at a heating rate of 10 K/min in a thermogravimetric analyzer conforming to ISO 11358-1:2022. This method identifies the onset of mass loss, the temperature at maximum mass-loss rate, and the residual char or mineral content. For LLDPE-carrier foaming masterbatches, decomposition onset is typically configured to occur above 180 °C to avoid premature gas release in the feed section, but high-temperature tailing above 230 °C can cause surface defects if melt residence time is excessive. Published data for HYBOOST 257-specific decomposition kinetics is limited, and the thermal behavior of each production lot should be checked because variations in active loading and pellet moisture can shift the decomposition curve by several degrees. Moisture uptake in the carrier can be assessed using ISO 15512:2019 Method A at 160 °C; drying at 70 °C for 2 h to 4 h is typically sufficient only if the supplier’s moisture limit is exceeded, and desiccant drying at higher temperatures should be avoided because it may pre-maturely decompose the active component.
Foaming behavior in extrusion depends on the balance between gas generation rate, melt-phase diffusivity, and the pressure gradient from the metering section to the die exit. In an LLDPE carrier, the gas molecules evolved by the active component must migrate through the surrounding polymer melt and form nuclei at pressure-drop locations such as the breaker plate, screen pack, and die land. The number density of cells is controlled by nucleation density rather than by total gas yield alone; a lower gas yield with a high nucleation rate can produce finer and more uniform cell structure than a high gas yield with poor melt-strength retention. For this reason, comparisons based only on blowing-agent concentration in weight percent are incomplete. The melt-phase viscosity at the die temperature, measured as shear viscosity at 100 s⁻¹ to 1 000 s⁻¹, and the elongational viscosity at the die lip are the controlling rheological parameters. LLDPE-based masterbatches influence the melt-strength balance of the final compound because the carrier is linear and does not introduce the long-chain branching that a branched-LDPE carrier would provide.
Cell coalescence occurs when the local gas pressure in adjacent cells exceeds the melt strength of the cell walls during bubble expansion. The die head pressure is therefore not a cosmetic variable; it determines whether dissolved gas remains in solution until the melt exits the die. In polyethylene foaming lines, die head pressures below 7 MPa frequently result in pre-foaming inside the die land or surface roughness known as shark-skin, while pressures above 12 MPa may reduce gas diffusion and increase motor load without proportional density reduction. The actual threshold depends on gas type, melt temperature, and base resin rheology. Published data for this specific configuration is limited, but the pressure window can be established on a pilot line by varying breaker-plate screen pack density and measuring extruder head pressure with a 0 MPa–30 MPa melt-pressure transducer calibrated to ISO 17025:2017. Nucleation density can be assessed indirectly by optical microscopy of polished cross sections at 50× to 100× magnification and by measuring the mean cell diameter and cell count per unit area using image analysis software.
On production-scale extrusion lines, the masterbatch is added via a gravimetric feeder positioned over the main feedthroat or a side feeder when the base pellet blend contains regrind. Single-screw extruders with grooved feed sections and L/D ratios from 30:1 to 38:1 are used for pipe, profile, and sheet foam extrusion, while twin-screw extruders with 40:1 L/D and co-rotating intermeshing screws are preferred when higher distributive mixing is required. The LLDPE carrier melts rapidly and assists in wetting the active particles before compression. Vent-port operation should be evaluated carefully: excessive vacuum can draw out volatile decomposition products and collapse half-formed cells near the melt surface. The recommended practice is to run the vent at a slight negative pressure; vacuum levels above 0.08 MPa are rarely required and can destabilize foaming. For blown film lines, die gap and blow-up ratio have a larger influence on final density than the masterbatch addition level once gas nucleation is complete.
Variation in let-down ratio changes the concentration of the active component and the carrier-phase morphology. At low let-down levels below 1.0 wt%, the LLDPE carrier has negligible influence on crystalline melt temperature and film optics, but the carrier may still introduce a small gel-like phase if downstream mixing is poor. At higher levels above 2.0 wt%, the linear-low-density carrier can alter bubble stability in blown film because its melt extension behavior differs from that of a branched-LDPE or high-pressure LDPE base resin. Cast film lines operating with chill-roll temperatures below 40 °C can trap gas at the melt-roll interface, leading to micro-void formation and surface haze. For blown film, the frost-line height should be adjusted to allow cell formation before solidification; moving the frost line too close to the die freezes surface cells and creates a dense skin layer. The optimum addition ratio is typically found by running a design of experiments with 0.5 wt%, 1.0 wt%, and 1.5 wt% masterbatch levels while maintaining constant screw speed and die gap, then measuring film density, tensile strength, and dart impact under ISO 527-3:2018 and ISO 7765-1:1988.
Injection-molding applications require the masterbatch to be thoroughly premixed before plastication. The LLDPE carrier may contribute to screw slippage if the barrel feed zone is overheated, particularly in high-speed injection units with check-ring valves. To avoid inconsistent shot weight, the feed temperature should be kept at the low end of the polyolefin processing range, and decompression should be minimized after screw recovery. The mold should be vented at the perimeter and along the flow front to allow displaced gas to escape; vent depths below 0.02 mm are generally too shallow for foam escape in polyolefin melts, while depths above 0.05 mm can cause flash with low-viscosity grades. Published case-specific data for HYBOOST 257 in all mold geometries is limited; therefore, tooling trials should be based on a structured qualification plan.
Azodicarbonamide-based exothermic masterbatches produce a high gas yield per unit mass and decompose over a narrow exothermic interval, but their byproducts can include ammonia and cyanuric acid residues that plate out on the die lip and cause surface defects. Sodium bicarbonate-based endothermic masterbatches release carbon dioxide and water, generate finer cell structure at lower gas yield, and are generally less likely to form plate-out, but they can increase moisture-related surface roughness if not dried. The choice between these systems is dictated by the target density reduction, food-contact constraints, odor requirements, and die-pressure stability. HYBOOST 257 with an LLDPE carrier is supplied for processes where controlled nucleated foaming and polyolefin compatibility are required; however, the active chemistry and gas yield should be confirmed from the supplier safety data sheet and thermal analysis before replacing an existing frothing or foaming system. Differential scanning calorimetry using ISO 11357-1:2016 and ISO 11357-3:2018 can identify whether the active component is endothermic or exothermic and at what temperature interval the major energy change occurs.
Density reduction is measured by water displacement using ISO 1183-1:2019 or ASTM D792-20. Mechanical properties are evaluated in tension according to ISO 527-1:2019 and ISO 527-2:2012 for films or ASTM D638-14 for rigid specimens. Charpy impact of notched specimens is determined by ISO 179-1:2020, while dart impact for film is determined by ISO 7765-1:1988. Water absorption is measured by ISO 62:2008, and heat deflection temperature by ISO 75-2:2013 Method A at 1.8 MPa. The table below summarizes the standard designations and the outputs that should be recorded during trials.
| Standard | Test | Application | Recorded output |
|---|---|---|---|
| ISO 1133-1:2022 | Melt mass-flow rate | Masterbatch carrier | g/10 min |
| ISO 1183-1:2019 | Density | Foamed and unfoamed specimens | g/cm³ |
| ISO 11358-1:2022 | Thermogravimetric decomposition | Active component thermal stability | °C onset, % residue |
| ISO 527-3:2018 | Tensile properties of film | Foamed film | MPa tensile strength, % elongation |
| ISO 179-1:2020 | Charpy impact | Notched rigid specimen | kJ/m² |
| ISO 7765-1:1988 | Dart impact | Film | g |
| ISO 62:2008 | Water absorption | Foam plaque | % mass change |
| ISO 75-2:2013 | Heat deflection temperature | Foamed specimen | °C |
Process variables that require lot-to-lot documentation include screw speed, die head pressure, melt temperature at the adapter, feeder setpoint, and the pressure differential across the screen pack. The following table defines the measurement points and sensor types for production-scale qualification.
| Variable | Sensor | Location | Typical acceptance criterion |
|---|---|---|---|
| Let-down rate | Gravimetric feeder | Feed throat | ±0.1 wt% of setpoint |
| Melt pressure | Melt-pressure transducer | Extruder head | ±0.5 MPa stability |
| Melt temperature | Immersion thermocouple | Adapter | ±2 °C stability |
| Screw speed | Tachometer | Drive shaft | ±1 rpm stability |
| Die pressure | Strain-gauge transducer | Die land | 7 MPa–12 MPa for nucleation |
| Screen pack differential | Dual pressure transducers | Upstream/downstream of screen changer | < 3 MPa increase before change |