Entec Hyboost 255 Masterbatch Lldpe

Entec HYBOOST® 255 Masterbatch, LLDPE

    • Product Name: Entec HYBOOST® 255 Masterbatch, LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 693108
    Carrier Resin LLDPE
    Form Pellets
    Color White
    Odor Slight
    Specific Gravity 1.25 g/cc
    Melt Flow Rate 2.0 g/10 min
    Moisture Content 0.10%
    Active Content 25%
    Decomposition Temperature 200 °C
    Processing Temperature 200-230 °C
    Recommended Addition Level 1-5%
    Shelf Life 12 months

    As an accredited Entec HYBOOST® 255 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Entec HYBOOST® 255 Masterbatch, LLDPE is supplied in 25 kg polyethylene-lined bags, palletized and shrink-wrapped.
    Container Loading (20′ FCL) Loaded in 20′ FCL: Entec HYBOOST® 255 Masterbatch, LLDPE, 25 kg bags on pallets, shrink-wrapped, secured, approximately 20 MT net.
    Shipping Entec HYBOOST® 255 Masterbatch, LLDPE is a non-hazardous, non-regulated solid. Ship in original sealed 25 kg bags or boxes, unitized on pallets. Not classified as dangerous goods under DOT, IMDG, IATA, or ADR. Protect from moisture, heat, and direct sunlight; follow local regulations.
    Storage Store Entec HYBOOST® 255 Masterbatch, LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and ignition sources. Keep original containers tightly closed, clearly labeled, and off the floor. Protect from moisture, dust, and strong oxidizers. Maintain recommended ambient temperature, avoid prolonged UV exposure, and follow local regulations and supplier SDS.
    Shelf Life Shelf life: 24 months from date of manufacture when stored unopened in original packaging in a cool, dry area, away from direct sunlight.
    Application of Entec HYBOOST® 255 Masterbatch, LLDPE

    Die Pressure Must Exceed Gas Solubility Thresholds in Foamed Sheet Extrusion

    Dosed at 0.5–1.5 wt% of total polymer mass in an LDPE/LLDPE blend, Entec HYBOOST® 255 Masterbatch, LLDPE is introduced into the primary feed throat of a single-screw extruder with an L/D ratio of 30:1–36:1 and a barrier screw equipped with spiral mixing elements. The endothermic decomposition response requires a controlled thermal profile from 175 °C in the feed zone to 210 °C at the die lip; die melt temperature above 225 °C accelerates gas evolution and produces cell wall coalescence. Die pressure is held above 35 bar to keep the CO₂ dissolved in the polymer melt until the die exit, and pressure variation of ±2 bar causes transverse surface defects known as tiger stripes. After foaming, the sheet is calendered and subsequently thermoformed into trays, clamshells, and protective corner profiles. Compliance for food-contact thermoformed products in the EU is governed by EU 10/2011, U.S. olefin polymer requirements are covered by FDA 21 CFR 177.1520, and the masterbatch is documented under REACH.

    Structural-foam injection molding of HDPE and PP reusable logistics containers uses a different thermal history than flat sheet extrusion. Entec HYBOOST® 255 Masterbatch, LLDPE is dosed at 0.8–2.0 wt% into a hydraulic injection molding machine with clamp force of 200–800 t; the screw is a general-purpose design with L/D ratio 20:1–24:1 and a check ring that tolerates low-viscosity melt. Shot size is reduced to 85–95% of the solid-wall part volume, and packing pressure is eliminated or limited to 10–20% of standard holding levels so that cell growth compensates for shrinkage at ribs, bosses, and wall intersections. Injection velocity is set at 150–300 mm/s, and melt temperature is maintained at 200–230 °C for HDPE and 220–240 °C for PP; mold surface temperature is kept below 20 °C for HDPE and below 40 °C for PP. Pre-drying at 70 °C for 2 h is required if relative humidity exceeds 60%; moisture in the feed throat causes uneven nucleation and splay marks. Apparent density is verified under ISO 845 or ASTM D1622, tensile properties are measured per ASTM D638-14, and pallet load performance is evaluated under ISO 8611. Finished products include collapsible pallet boxes, reusable dunnage, and closed-loop logistics trays.

    What Keeps Moisture from Disrupting a Wood-Filled Polyethylene Decking Profile?

    Because wood flour moisture above 1.5% interacts with the gas evolution of Entec HYBOOST® 255 Masterbatch, LLDPE, drying becomes the controlling variable in WPC profile extrusion. The masterbatch is dosed at 0.5–1.2 wt% of total compound mass in an HDPE/wood flour formulation and is metered into a counter-rotating conical twin-screw extruder with venting at the plastication zone and screw cooling in the feed throat. Wood flour is pre-dried to ≤1.0% moisture; residual moisture raises the vapor pressure balance and produces elongated voids and surface roughness. Barrel temperatures are profiled from 160 °C in the feed throat to 175 °C at the die, below the thermal degradation threshold of the wood fraction. Die pressure is maintained between 20 bar and 35 bar, and the resulting microcellular core reduces profile density by 10–20% while a solid skin remains on the exterior. Terminal products are solid or hollow decking boards, cladding, and railing profiles tested under EN 15534-1:2014 and ASTM D7032-21; environmental compliance is documented under REACH and RoHS 2011/65/EU.

    The skin-foam coextrusion line for low-loss coaxial cable insulation places the foamed HDPE core layer under a crosshead pressure range of 80–120 bar to suppress pre-foaming in the adapter. In this configuration, Entec HYBOOST® 255 Masterbatch, LLDPE is added to the HDPE core at 0.5–1.0 wt%, and the solid skin layer is coextruded from HDPE or LLDPE to maintain surface integrity. Melt temperature at the crosshead is held between 200 °C and 230 °C; a drop below 195 °C leaves residual unreacted blowing agent particles, while a rise above 235 °C weakens cell walls and increases high-frequency attenuation. The void fraction of 20–40% lowers the relative dielectric constant from about 2.3 for solid HDPE toward 1.8–1.9, which is the primary electrical design target. Diameter and insulation thickness stability are checked under IEC 60811-501, flame spread is assessed according to UL 1581, and dielectric constant and dissipation factor are measured per ASTM D150. Finished products include RG-6 and RG-11 coaxial cable, Cat 6A/8 data cable, and RF antenna feeder cable.

    When Rotational Molding Cycle Time Must Drop Without Sacrificing Wall Thickness, Foam-Core Morphology Controls

    For foam-core rotomolded polyethylene parts, the powder blend is charged at ambient temperature and heated in an oven held below 290 °C; Entec HYBOOST® 255 Masterbatch, LLDPE is dosed at 0.5–1.0 wt% in an HDPE/LLDPE powder blend. The foam core forms only after the compacted powder layer reaches the decomposition temperature of the masterbatch, and the resulting cell morphology depends on oven time, mold rotation ratio, and demolding temperature. Because the cellular core insulates the inner surface, cycle time does not scale linearly with part thickness; published data for this specific configuration is limited, and processors typically run iterative oven-time trials. Apparent density is measured under ISO 845, and solid-skin tensile properties are evaluated per ASTM D638-14. Environmental compliance is maintained under REACH and RoHS 2011/65/EU for industrial goods. Finished products include double-wall foam-core covers, buoyancy modules, and insulated material-handling bins.

    Extrusion blow molding of medium-density polyethylene packaging containers with 0.5–1.0 wt% Entec HYBOOST® 255 Masterbatch, LLDPE reduces parison melt density and alters swell behavior in the die head. Melt temperature at the die head is controlled between 185 °C and 210 °C; above 215 °C melt strength decreases and cell expansion becomes difficult to control in the flash and pinch-off zones. Blow pressure is set at 6–8 bar, and mold temperature is held at 10–20 °C. The parison programming system is adjusted to redistribute wall thickness and prevent thin spots from over-expanding before the mold closes. Compliance for food-contact containers where applicable relies on FDA 21 CFR 177.1520 and EU 10/2011, with REACH documentation covering industrial packaging. Terminal product types include non-food household chemical containers, cosmetic bottles, and automotive fluid bottles.

    Free Quote

    Competitive Entec HYBOOST® 255 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Entec HYBOOST® 255 Masterbatch, LLDPE is a pelletized additive concentrate supplied in a linear low-density polyethylene carrier. The product model designation consists of the series name HYBOOST® and the numeric grade 255; the carrier type is LLDPE. The lot-specific certificate of analysis is the controlling specification for melt mass-flow rate (ISO 1133-1:2022), density (ISO 1183-1:2019), ash content (ISO 3451-1:2019), and moisture content (ISO 15512:2019). Published data for this specific configuration are limited; therefore, process boundaries described in this document are based on the LLDPE carrier category unless supplier data are cited directly. The active additive package is grade-specific and is disclosed through the safety data sheet and certificate of analysis rather than through a fixed public nominal value.

    How Is the LLDPE Carrier Stabilized for Consistent Metering at Low Letdown Ratios?

    On production lines using loss-in-weight feeders, pelletized LLDPE carrier is metered in the range 1–5 wt%. The feeder hopper is typically configured with a 50 L stainless-steel bin and an antistatic liner; screw speed is adjusted to maintain a short-term dosing accuracy of ±0.5 wt% over a 30 s cycle. Feed-throat jacket temperature is held below 50°C to prevent pellet stickiness and subsequent bridging. At hopper residence times greater than 4 h, the transition chute is inspected for compaction; a 0.5 Hz pneumatic knocker can be used on single-screw extruders with L/D 24:1 or shorter because these machines have shorter melting zones and can allow partially softened pellets to agglomerate before the compression section.

    Because the carrier is an LLDPE, its flow curve under shear is more shear-thinning than that of a high-pressure LDPE of identical melt index. Capillary rheometry per ISO 11443 on LLDPE carrier grades of this category commonly yields apparent shear viscosity in the interval 250–800 Pa·s at 100 s⁻¹ and 190°C. The power-law index is between 0.45 and 0.65. At shear rates above 500 s⁻¹, the viscosity drops further, but viscous dissipation raises local melt temperature by 8–15°C. Twin-screw compounding lines with L/D 32:1 are preferred for letdown ratios above 3 wt% because distributive mixing improves when the barrel temperature profile is set to 170–190°C in the feed zones and 200–220°C before the die.

    Thermal Degradation Pathways and Melt-Filtration Demands

    Thermal stability is assessed by oxidative induction time under ISO 11357-6 and by dynamic thermogravimetric analysis under ISO 11358-1:2022. LLDPE carriers without supplemental stabilizers may show onset of rapid volatilization above 200°C in air; oxidation becomes autocatalytic above 220°C. The processing time at melt temperature should not exceed 8 min if the die exit temperature exceeds 220°C, unless the lot certificate confirms a higher stabilizer level. Melt filtration with a 20/40/60/80 mesh screen pack removes agglomerates and low-level crosslinked material; a head-pressure increase greater than 5% from baseline during 30 min of continuous operation indicates screen blockage and requires a change. Pressure monitoring is performed with a transducer having ±0.5% full-scale accuracy.

    In a thin-gauge blown film operation, the melt temperature window at the die is often narrower than ±5°C. The use of a static mixer between extruder and die reduces thermal stratification; mixer length is typically 3–5 × screw diameter. Thermocouples are placed at the adapter and die lip because barrel-zone readings lag the true melt temperature by 5–15°C. If the die setpoint is 215°C, localized hot spots may approach 230°C under high shear, causing unpigmented film to yellow. The operator should reduce screw speed when the die pressure fluctuation exceeds ±3 bar over 10 min.

    When Letdown Ratios Shift in Multi-Layer Coextrusion

    During five-layer coextrusion with die lip diameters of 50–75 mm and individual layer thickness below 30 µm, the addition of HYBOOST® 255 in a skin layer at 2–3 wt% can alter the melt elasticity of that layer relative to a neat core. If adjacent-layer viscosity mismatch at the die shear rate exceeds 10–15%, interfacial waviness is observed in the cross-machine direction. The defect is detected by optical microscopy of freeze-fractured films or by in-line optical gauging; the coefficient of variation for layer thickness is maintained below 5%. Letdown changes are made in 0.5 wt% increments, and the line is allowed 15–20 min of stabilization before sampling. Higher letdown ratios are permissible only after a designed experiment on the target line because published predictive data for this specific masterbatch configuration are limited.

    Compared with an LDPE carrier, an LLDPE carrier contributes higher dart impact resistance to the final film. Film dart impact is measured by ISO 7765-1:2015; published polyolefin carrier class data show LLDPE tensile elongation at break of 600–800% versus LDPE at 400–600% under ISO 527-2:2012. Environmental stress-crack resistance, measured according to ASTM D1693, is also higher for LLDPE carriers than for LDPE carriers, with bend-strip failure times depending on comonomer and additive formulation. This difference is relevant in agricultural films and pallet-wrap structures that require puncture and tear resistance.

    Differences From Wax-Based and Neat Additive Systems

    Wax-based masterbatches disperse rapidly but can produce screw slippage at high throughput and contribute a low-molecular-weight fraction that may migrate in the final article. LLDPE-carrier concentrates maintain higher melt viscosity and melt strength; this reduces phase segregation during extrusion and is preferred in blown film. Neat additive powders maximize active content and avoid carrier dilution but require side-stuffing units and local exhaust ventilation to control dust. A pelletized LLDPE masterbatch can be added through the main hopper with a gravimetric feeder delivering 0.5–15 kg/h on a small line or up to 300 kg/h on a large compounding line. The trade-off is that the LLDPE carrier adds to the total polymer mass; the effective active fraction must be calculated from the lot certificate. In clean-room environments, pelletized concentrate reduces airborne particulate counts relative to powder charging; ISO class 8 zones are attainable with standard local exhaust.

    Property LLDPE carrier LDPE carrier PP carrier
    Density range 0.915–0.940 g/cm³ 0.915–0.935 g/cm³ 0.890–0.910 g/cm³
    Typical melt mass-flow rate for carrier use 2–20 g/10 min 2–20 g/10 min 2–25 g/10 min
    Heat deflection temperature 45–60°C 40–55°C 90–105°C
    Moisture uptake at 23°C/50% RH <0.1 wt% <0.1 wt% <0.1 wt%
    Typical melting peak 120–126°C 105–115°C 160–165°C

    The selection of LLDPE carrier over a PP carrier is appropriate when the base stream is predominantly polyethylene. LLDPE melts at 120–126°C; PP carrier melts at 160–165°C and is suitable for PP base resins processed at 210–240°C. Using an LLDPE-carrier concentrate in a PP base resin can create low-temperature unmelt early in the screw and may require feed-zone adjustment. The inverse is also true: PP carrier in a PE stream can remain undispersed if the PE processing temperature is below the PP melting peak.

    Compliance for food-contact articles requires that the final article meet the end-use migration limits as well as the raw material conformity. The LLDPE carrier falls within olefin polymers recognized in FDA 21 CFR 177.1520; for EU applications, the product must meet specific migration limits in EU Regulation 10/2011 Annex II, including overall migration of 10 mg/dm² or 60 mg/kg depending on packaging type. REACH registration under EC No 1907/2006 applies, and the safety data sheet is the source for substances of very high concern. Under RoHS 2011/65/EU as amended by (EU) 2015/863, lead, mercury, hexavalent chromium, PBB, PBDE, and four phthalates are restricted to 0.1 wt% in homogeneous materials; cadmium is restricted to 0.01 wt%. Electrical and electronic applications are not assumed unless the masterbatch is evaluated in the final homogeneous material.

    Property Standard designation Scope in masterbatch qualification
    Melt mass-flow rate ISO 1133-1:2022 Carrier flow characterization under 190°C or 230°C with 2.16 kg
    Density ISO 1183-1:2019 Carrier identification and blend ratio verification
    Ash content ISO 3451-1:2019 Inorganic additive or filler content
    Moisture content ISO 15512:2019 Pre-drying requirement; target <0.08 wt% for thin film
    Vicat softening temperature ISO 306:2022 Heat resistance of final article
    Tensile properties ISO 527-2:2012 Mechanical property verification
    Elmendorf tear resistance ISO 6383-2:2015 Tear propagation in film

    Moisture uptake exceeding 0.1 wt% in storage requires drying in a desiccant drier at 60–70°C for 2–4 h before processing. Avoid pre-blending with amine-based additive masterbatches unless compatibility is confirmed by oven-ageing at 200°C for 30 min; acid-base reactions between carrier stabilizers and amines can cause color shift and screen-pack fouling. Purge with a polyolefin purge compound after shutdown; a residual melt pool held above 240°C for 30 min can carbonize in the adapter and generate black specks. Equipment surfaces can be cleaned with a standard polyolefin purging sequence; no solvent cleaning is required. Published data for this specific configuration are limited; final process windows should be generated on the target line.

    Top