| HS Code | 608758 |
| Density | 0.920 g/cc |
| Meltflowrate | 2.0 g/10 min |
| Additivecontent | 20% |
| Carrierresin | LLDPE |
| Form | Pellets |
| Color | White |
| Moisturecontent | <0.10% |
| Pelletsize | 2.00-3.00 mm |
| Bulkdensity | 0.500-0.600 g/cc |
| Processingtemperature | 200-240 °C |
| Shelflife | 12 months |
| Storagetemperature | <30 °C |
| Fdacompliance | Yes |
As an accredited Entec HYBOOST® 242 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Entec HYBOOST® 242 Masterbatch, LLDPE supplied in 25 kg polyethylene-lined bags, 40 bags per pallet (1,000 kg). |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Entec HYBOOST® 242 Masterbatch, LLDPE fully palletized, shrink-wrapped, and secured within container for safe ocean transport. |
| Shipping | Entec HYBOOST® 242 Masterbatch, LLDPE is typically shipped as a non-hazardous solid masterbatch in sealed 25 kg polyethylene-lined bags or octabins. Pallets are stretch-wrapped and labeled. Transport in clean, dry vehicles; keep cool, dry, away from direct sunlight, moisture, and excessive heat. Follow local regulations and supplier instructions. |
| Storage | Store Entec HYBOOST® 242 Masterbatch, LLDPE, in a cool, dry, well-ventilated area at ambient temperature, away from direct sunlight, heat, moisture, and ignition sources. Keep containers tightly closed in original packaging. Avoid contact with strong oxidizers and contaminating materials. Protect from physical damage. Use first-in, first-out stock rotation. Do not stack excessively high. Keep away from food, drink, and feed. |
| Shelf Life | Recommended shelf life: 24 months from manufacture when stored in original, unopened packaging in a cool, dry area away from sunlight. |
Entec HYBOOST® 242 Masterbatch is an LLDPE-carrier chemical foaming masterbatch used in polyolefin downstream conversion where gas nucleation controls density reduction, sink compensation, or dielectric property modification. Before any application-specific dilution, the base LLDPE resin is characterised for melt-mass flow rate under ISO 1133-1:2022 and for moisture content by Karl Fischer coulometry; the masterbatch is brought to ambient temperature from storage before opening to avoid condensation on pellet surfaces. Gravimetric feeding is the preferred addition method because pellet bulk density differences between the masterbatch and base LLDPE create volumetric dosing error. The subsequent scenarios are limited to sectors with documented polyolefin cellular processing experience and do not attempt to transfer the LLDPE carrier outside its compatibility window.
In multilayer blown-film conversion of low-basis-weight e-commerce mailers, the masterbatch is dosed into the core layer at 0.4–1.0 wt% of total layer mass rather than into the skin layers, preserving surface gloss and seal initiation. A three-layer die with 1.2–1.6 mm lip gap and a blow-up ratio of 2.2–2.8 maintains bubble stability; barrel setpoints in the 170–215 °C range are graduated so that LLDPE carrier melting is completed before the mixing section. Feed-zone temperatures below 170 °C produce pellet-shaped gel defects that appear as hard spots in film tested under ISO 527-3:2018. The decomposition gas creates microcellular structure in the core while solid skins are maintained by low shear at the die lip; the frost line is moved downward by 10–20% to stabilise cell walls before machine-direction orientation. Compliance for mailer films rests on REACH Regulation (EC) No 1907/2006 and verification that no substance is present on the Candidate List; where the film is intended for non-food consumer goods, EU Regulation 10/2011 is used as a precautionary migration framework, and for food-contact applications the final film must meet FDA 21 CFR 177.1520 olefin polymer extractives limits. Tensile properties are checked according to ASTM D882-18 at 500 mm/min, and dart impact is evaluated by ASTM D1709-22, Method A. Terminal products include lightweight courier mailers, voided protective wrapping, and tamper-evident polyolefin envelopes. The operational boundary is a minimum total film thickness of 30 µm; below this limit the core layer cannot contain the gas, and pinhole formation becomes measurable. Loadings above 1.2 wt% are outside the stable window for this film gauge.
In injection moulding of thick-section LLDPE storage bins and container lids, sink marks at rib-to-wall intersections are generated by volumetric shrinkage after gate freeze. The masterbatch is dosed at 0.3–0.8 wt% to nucleate microcellular voids that compensate for shrinkage during the packing phase; the effect is measurable in ribs thicker than 4 mm. A reciprocating-screw machine with 20:1–24:1 L/D ratio and a reverse-taper nozzle is used, and melt temperature is held between 200 °C and 220 °C. Back pressure is increased by 0.5–1.0 MPa above the solid-moulding baseline to keep decomposition gas in solution until screw recovery; screw decompression after recovery is eliminated to prevent gas breakout at the nozzle. Mould vents of 0.02–0.04 mm are cut at flow-front ends because displaced cavity air and decomposition gas must escape without causing burns. The pack-and-hold profile is shortened by 10–15% and reduced by 15–25% compared with solid moulding, as cell growth replaces melt compensation. Compliance includes RoHS Directive 2011/65/EU for restricted heavy metals, ISO 11469:2016 for resin identification marking, and ASTM D638-14 for tensile yield; when the container may contact food, end-use verification is performed under FDA 21 CFR 177.1520. Terminal parts include LLDPE industrial stack-and-nest boxes, lids for wide-mouth pails, and cold-chain distribution bins. Loading below 0.3 wt% does not generate enough internal pressure to eliminate sink marks in thick sections; loading above 0.8 wt% produces surface silver streaks and a gloss shift measurable under ISO 2813:2014 at 60°.
When closed-cell polyethylene sheet is extruded for vacuum-formed automotive cargo liners and boot floor covers, the masterbatch is introduced into the primary extruder of a tandem sheet line at 0.8–2.0 wt% of total letdown. The primary extruder uses 32:1 L/D and a barrier screw; melt temperature is 195–215 °C. The secondary cooling extruder is run at 150–170 °C, and a screen pack of 60/80/100 mesh traps partially decomposed particles before the die. Melt pressure at die entry is maintained above 6 MPa to keep gas in solution; pressure fluctuations greater than ±0.3 MPa produce density bands across the sheet width. The calender roll stack is set at 40–70 °C to control skin thickness and emboss depth; lower roll temperatures raise skin thickness and reduce gas loss. Apparent density is measured by ISO 845:2006, with stable thermoforming grades in the 0.7–0.85 g/cm³ range, and mean cell diameter is below 150 µm by optical microscopy after cross-section polishing. Automotive compliance is governed by ISO 3795:1989 flammability with a maximum burn rate of 100 mm/min, VDA 277:2019 VOC emission limits, and OEM-specific odour assessment; RoHS applies where electronic tie-downs or sensors are integrated. The sheet is trimmed and vacuum-formed into cargo liners, boot floor trays, and under-seat covers. Regrind above 20 wt% is not recommended in the primary extruder because pre-foamed regrind contains residual active sites and causes bimodal cell populations; when regrind is processed, it is side-fed into the secondary extruder at no more than 15 wt%.
Foam insulation for coaxial and data cable cores consists of a foamed LLDPE dielectric layer applied over a copper conductor, often with an outer solid skin. The masterbatch is dosed at 0.2–0.6 wt% in the insulation compound; loadings above 0.8 wt% create coalesced voids that increase attenuation and reduce crush resistance. A tandem wire-extrusion line with a 30:1 L/D primary extruder and a 24:1 L/D cooling extruder feeds a crosshead die. Primary melt temperature is 190–205 °C; the secondary zone is cooled to 140–160 °C to reduce gas expansion until the die exit. The primary screw includes a barrier section and a Maddock mixing element; vacuum venting at −0.07 MPa removes residual moisture. Conductor preheating is maintained at 80–120 °C to control adhesion; insufficient preheating causes skin-core delamination under ASTM D3032-21, while excessive preheating induces premature gas separation at the die. The foamed dielectric constant is reduced from 2.3 to 1.8–2.0 depending on gas volume fraction, and capacitance stability is verified under IEC 61196-1:2020. Compliance includes UL 1581 for wire and cable mechanical performance and RoHS Directive 2011/65/EU for restricted substances. Terminal products include coaxial cables for CATV, twisted-pair data cable insulation, and low-loss jumper cables for base-station applications. Storage above 60% RH requires pre-drying at 60 °C for 2 h in a dehumidifying hopper dryer before the masterbatch is transferred into the gravimetric feed system.
Extruded closed-cell polyethylene backer rods for concrete expansion joints and sealant control require a skin that resists sealant knife cuts and a core with controlled compressibility. In backer rod profiles, the masterbatch is fed at 0.5–1.5 wt%; loadings below 0.4 wt% do not generate enough cell volume to produce the required 25–35% density reduction, while loadings above 1.5 wt% raise open-cell content beyond 10% measured by ASTM D2856-94. A single-screw extruder with 24:1–30:1 L/D and a low-shear metering screw is run at 175–200 °C. Vacuum calibration at −0.02 to −0.05 MPa freezes the outer skin and controls final round dimensions; water temperature is held at 15–25 °C to limit post-extrusion expansion. Haul-off speed is matched to extruder output to limit drawdown to 5% or less; excessive stretching collapses cells and produces local density bands that alter compression-deflection response. Compliance references ASTM D5249-20 for round backer rod dimensional and physical requirements and ASTM D3575-14 for flexible cellular olefin polymer testing; apparent density is tracked by ISO 845:2006. Terminal products include round backer rods for parking deck joints, bridge expansion joints, and plaza sealant systems. Published data for this specific masterbatch in backer rod applications are limited compared with film and sheet; the loading window is derived from general closed-cell LLDPE profile extrusion practice and should be confirmed on the target line.
Competitive Entec HYBOOST® 242 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Entec HYBOOST® 242 Masterbatch, LLDPE is designated as a linear low-density polyethylene carrier-based masterbatch. The numeric suffix 242 is a product line identifier, not a rheological or thermal specification. Because the active additive chemistry is not defined by the trade name, any statement concerning oxidative stability, slip, antiblock, nucleation, or processing-aid behaviour must be verified against the supplier’s lot-specific certificate of analysis and technical data sheet. Published data for this specific configuration is limited; the following sections therefore separate established LLDPE carrier masterbatch behaviour from product-specific values that require direct confirmation.
The masterbatch format consists of a concentrated additive phase dispersed in an LLDPE carrier resin, produced on a co-rotating twin-screw extruder with strand pelletization or underwater pelletization. The LLDPE carrier class typically exhibits a density of 0.915–0.940 g/cm³ when tested according to ISO 1183-1:2019 or ASTM D1505, and a melt mass-flow rate between 1.0 g/10 min and 20 g/10 min under 190°C/2.16 kg when measured by ISO 1133-1:2022 or ASTM D1238-20. These ranges are class-level, not HYBOOST 242-specific, and pellet geometry, bulk density, additive loading, and moisture limit are assigned in the supplier certificate of analysis.
Polyethylene melt flow rate is reported at 190°C with 2.16 kg because this condition is prescribed in ISO 1133-1:2022 and ASTM D1238-20 for polyethylene. For HYBOOST 242, the carrier MFR must be read together with the compounded additive content: high filler or active loading can elevate melt viscosity even when the carrier MFR is unchanged. A masterbatch with a carrier MFR of 5 g/10 min may therefore exhibit a compounded MFR below 2 g/10 min depending on additive type and concentration. Lot-specific MFR values should be compared to the host resin at the proposed let-down ratio to avoid visible dispersion defects such as unmelted particles, die lines, or surface roughness.
| Parameter | Test method | Class-level LLDPE carrier envelope | HYBOOST 242 lot-specific status |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 / ASTM D1238-20 | 1.0 g/10 min to 20 g/10 min at 190°C/2.16 kg | Certificate of analysis required |
| Density | ISO 1183-1:2019 / ASTM D1505 | 0.915–0.940 g/cm³ | Certificate of analysis required |
| Ash content | ISO 3451-1:2019 / ASTM D5630 | Additive-loading-dependent; can range from 0.5 wt% to above 50 wt% for mineral-filled concentrates | Certificate of analysis required |
| Moisture content | ISO 15512:2019 / ASTM D6980-17 | <0.10 wt% typical for non-hygroscopic polyolefin carriers | Certificate of analysis required |
Parameters such as ash content and moisture are determined by the additive chemistry; no universal specification exists for a product line code alone. The ash value cannot be inferred from the LLDPE carrier designation because additive loading varies by grade. A shift in batch-to-batch ash content of ±0.5 wt% absolute should trigger gravimetric feeder recalibration, since the addition rate is based on mass percentage rather than active content.
On production lines, HYBOOST 242 is fed by gravimetric or volumetric dosing into the main feed throat alongside the host LLDPE, LDPE, or HDPE resin at let-down ratios commonly between 1 wt% and 5 wt% for additive concentrates. The exact ratio for this product must be taken from the supplier’s recommendation. Dosing below 1 wt% on a single-screw extruder with a 24:1 L/D screw can produce feed-throat segregation because free-flowing pellets may separate from the host resin in the hopper. Dosing above 5 wt% without static mixing may reduce first-pass additive distribution in short screws. Melt temperature measured at the die exit should generally remain within 180°C to 240°C for LLDPE carrier masterbatches. Sustained temperatures above 250°C, particularly with residence times over 5 min, can initiate chain scission, gel formation, or additive degradation.
Single-screw extrusion of an LLDPE carrier masterbatch relies on distributive mixing in the compression and metering zones. A screw with 24:1 to 30:1 L/D and a Maddock or barrier mixing section is generally adequate for pellet let-down in film. For high active loadings or when the masterbatch is added at rates above 5 wt%, a co-rotating twin-screw extruder with 32:1 to 44:1 L/D and multiple kneading blocks provides the shear required to break up additive agglomerates. Field-scale failures observed on monolayer blown-film lines include unmelted carrier particles embedded in film when the die temperature is below the LLDPE carrier melting range by more than 5°C; these defects appear as gel-like specks in optical inspection but are actually undispersed masterbatch.
Filtration through a 200 mesh screen pack is often used to detect agglomerates before the die. A pressure increase greater than 20 bar over 1 h at constant throughput indicates dispersion failure or contaminant accumulation. Because LLDPE carrier masterbatches are non-Newtonian, MFR is only a single-point indicator. A comparison of compounded MFR to host resin MFR on the same pellet lot should be made before line start-up. If the compounded MFR of the masterbatch deviates from the host resin MFR by more than 10 g/10 min, flow instabilities can develop in single-screw extruders with short metering sections.
In blown-film operation, replacing a low-viscosity LDPE masterbatch with an LLDPE carrier masterbatch can increase bubble pressure sensitivity because the higher elongational viscosity of LLDPE raises low-shear viscosity. This effect is measurable as a change in blow-up ratio stability and is best monitored by bubble diameter variation of less than ±5% against a fixed air ring setting. When the masterbatch is used in cast film, edge trim refeed can alter additive concentration if the trim contains higher additive levels due to surface migration.
If film property verification is required, tensile elongation at break can be measured by ASTM D882 and dart impact by ASTM D1709. Comparative tests at 0 wt%, 2 wt%, and 4 wt% masterbatch addition are recommended on the target line. Published data for this specific configuration is limited; such tests should not be replaced by generic LLDPE carrier data.
Substitution of an LDPE-based masterbatch with an LLDPE-based masterbatch in a sealant film changes heat-seal behaviour. LLDPE carriers have a higher melting peak, typically 120–130°C by ISO 11357-3:2018, compared with 105–115°C for LDPE carriers. The seal initiation temperature measured by ASTM F1921 or seal strength measured by ASTM F88 may shift upward by 3–8°C when the carrier concentration in the sealant layer changes from an LDPE to an LLDPE masterbatch at 3 wt%. This shift is not a product limitation but must be accounted for in packaging line dwell times.
| Carrier resin | DSC melting peak, ISO 11357-3:2018 | Typical MFR at 190°C/2.16 kg | Observed film implication |
|---|---|---|---|
| LLDPE | 120–130°C | 1.0–20 g/10 min | Closer viscosity match to LLDPE-rich layers; may require higher extrusion melt temperatures than LDPE. |
| LDPE | 105–115°C | 0.2–20 g/10 min | Broad compatibility; can lower seal initiation temperature but may create viscosity mismatch in LLDPE-rich film. |
| EVA | 70–95°C | 0.3–20 g/10 min depending on vinyl acetate content | Lower processing range; potential acetic acid release above 200°C. |
| PP | 160–170°C | 1.0–25 g/10 min | Higher thermal stability but risk of gel formation and poor interfacial compatibility in polyethylene films. |
An LLDPE carrier provides a closer rheological match to LLDPE-rich host formulations than an LDPE carrier, reducing differences in melt elasticity that can lead to die swell or interfacial distortion in coextruded layers. When EVA carriers are considered, the acetic acid release threshold above 200°C can constrain processing and may create odour or die corrosion; an LLDPE carrier avoids this decomposition mechanism but may have a narrower seal range than an EVA carrier in high-speed packaging, as assessed by ASTM F1921.
Compared with liquid additive dosing systems, a pelletized LLDPE masterbatch eliminates solvent handling and reduces risk of pump diaphragm failure, but requires melt dispersion. Liquid systems can provide faster additive homogeneity and lower melt energy input, yet may cause screw slippage in single-screw extruders if added at high load. Gravimetric pellet feeders typically provide setpoint accuracy of ±0.25%, whereas liquid additive pumps are commonly accurate to ±1% of setpoint. These differences influence lot-to-lot consistency and should be evaluated on the target extrusion line.
Compliance documentation for HYBOOST 242 must be requested as a lot-specific statement. For food-contact applications in the United States, the carrier resin used in an LLDPE masterbatch may be covered by 21 CFR 177.1520, but the additive component must meet its own food-contact clearance. For EU food-contact use, the finished masterbatch falls under Regulation (EU) No 10/2011 only if the additive and carrier have listed migration limits; overall migration testing by EN 1186 and specific migration testing by EN 13130 are required on the final article. REACH and RoHS compliance for the masterbatch cannot be assumed from the LLDPE carrier alone; heavy metal content should be confirmed by IEC 62321-5:2013 for lead and IEC 62321-4:2013 for mercury, cadmium, and chromium.
Store in a dry environment at 10–30°C and 30–70% relative humidity. Prolonged storage above 30°C can accelerate additive migration to pellet surfaces and increase tack. If pellets become tacky due to hygroscopic additives or storage at high relative humidity, drying at 70–80°C for 2–4 h in a desiccant dryer may restore flow, but only when permitted by the supplier. Avoid blending with amine-based additive masterbatches without prior compatibility testing because amine-functional additives can interact with certain active chemistries and shift dispersion or thermal stability.