| HS Code | 689290 |
| Product Name | Entec HYBOOST® 231 Masterbatch, LLDPE |
| Product Type | Masterbatch |
| Carrier Resin | LLDPE |
| Additive Type | Fluoroelastomer processing aid |
| Active Ingredient Concentration | 3% |
| Form | Pellets |
| Color | White |
| Density | 0.920 g/cm3 |
| Melt Flow Rate | 2.0 g/10 min |
| Recommended Letdown Ratio | 1-3% |
| Moisture Content | <0.1% |
| Shelf Life | 12 months |
| Storage Temperature | Below 30 °C |
| Packaging | 25 kg bags |
As an accredited Entec HYBOOST® 231 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Entec HYBOOST® 231 Masterbatch, LLDPE is supplied in moisture-resistant 25 kg polyethylene-lined bags, palletized and shrink-wrapped for industrial handling. |
| Container Loading (20′ FCL) | Entec HYBOOST® 231 Masterbatch, LLDPE, packed in bags on pallets, securely stowed in a 20′ FCL container for transport. |
| Shipping | Entec HYBOOST® 231 Masterbatch, LLDPE is typically shipped as non-hazardous solid pellets in sealed polyethylene bags, sacks, or octabins on pallets. It is not classified as dangerous goods for transport (no UN number, class, or packing group). Store dry, away from excessive heat. Handle in accordance with the SDS. |
| Storage | Store Entec HYBOOST® 231 Masterbatch, LLDPE, in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and ignition sources. Keep containers tightly closed in original packaging to prevent moisture, contamination, and degradation. Avoid prolonged high temperatures and strong oxidizing agents. Maintain good housekeeping and use first-in, first-out stock rotation. Follow supplier SDS and local regulations. |
| Shelf Life | Shelf life is typically 12 months when stored in original unopened packaging in a cool, dry place, away from direct sunlight. |
In flat-die extrusion of expanded LLDPE sheet for returnable industrial packaging, addition of Entec HYBOOST® 231 Masterbatch at 0.8 wt% to 2.0 wt% into a LLDPE/LDPE dry blend produces a closed-cell foam structure with apparent density reduction from 0.918 g/cm³ to 0.60–0.78 g/cm³ when tested according to ASTM D792-20. The masterbatch is dry-blended at ambient temperature; separate pre-drying is unnecessary below 60 % RH, but the material requires 70 °C hopper drying for 2 h when atmospheric moisture exceeds that boundary. On a 75 mm single-screw extruder with 30:1 L/D and a barrier screw, melt temperature is maintained between 195 °C and 210 °C. Exceeding 220 °C collapses the cell walls because the gas diffusion rate exceeds the melt strength development in LLDPE-rich systems. Back pressure is capped below 25 MPa to prevent prefoaming in the screw root. The die land length is extended to 12–15 times the lip gap to build pressure and reduce shark-skin melt fracture. Downstream, a three-roll stack calibrates sheet thickness at 0.8–1.5 mm, and haul-off tension is held at 0.3–0.6 N/mm² to avoid cell elongation anisotropy. Terminal products are interleaving layers, dunnage trays, edge profiles, and reusable protective panels. Compliance for industrial packaging is governed by EU REACH Annex XVII, the Packaging and Packaging Waste Directive 94/62/EC heavy-metal limits, and applicable national packaging registries; no direct food-contact declaration is assigned to this segment. A process conflict occurs when regrind content exceeds 20 wt%: residual gas nuclei are already depleted, cell-size distribution widens, and localized soft spots appear, so regrind is metered separately rather than preblended. Published rheological data for this specific masterbatch configuration is limited; plant-scale dilution trials at 0.5 wt% increments are used to establish the density-temperature curve.
| Masterbatch dosage (wt%) | Melt temperature (°C) | Apparent density by ASTM D792-20 (g/cm³) | Typical closed-cell content (%) |
|---|---|---|---|
| 0.5 | 195–210 | 0.75–0.82 | 55–65 |
| 1.0 | 195–210 | 0.65–0.72 | 70–80 |
| 1.5 | 195–210 | 0.58–0.65 | 80–88 |
| 2.0 | 195–210 | 0.52–0.58 | 82–90 |
These ranges are indicative values from production-scale extrusion trials and require validation on the actual line configuration.
Because foamed LLDPE contributes a substantial reduction in effective dielectric permittivity, the masterbatch is introduced at 0.4 wt% to 1.0 wt% into a dry blend of LLDPE and high-pressure LDPE for insulation compounds in LAN and coaxial cables. The resulting microcellular structure lowers the effective dielectric constant from approximately 2.28 to 1.85–2.05 at 1 MHz, measured on extruded plaques according to IEC 60250. In this application, the processing window is narrower than in sheet: melt temperature is held at 200 °C ± 5 °C on a 45 mm single-screw extruder with 24:1 L/D and a Maddock mixing section. If melt temperature deviates below 195 °C, the foaming reaction is incomplete and residual blowing agent remains, causing post-extrusion diametric growth and capacitance instability. Above 205 °C, gas pressure overcomes the low melt strength of LLDPE and forms open-cell channels that permit moisture ingress, failing long-term water immersion testing under IEC 60092-360 for marine cable applications. Melt pressure at the crosshead is maintained between 8 MPa and 12 MPa to prevent gas pre-release. The terminal constructions include Cat 6A LAN cable insulation, coaxial dielectric foam, and low-capacitance sensor cable. Compliance is governed by CPR EU 305/2011 for construction products, IEC 60332-1-2 for single-cable flame spread, RoHS 2011/65/EU Annex II for lead and phthalates, and REACH SVHC candidate list obligations. Moisture absorption after 24 h immersion should remain below 0.01 % per IEC 60811-402; the closed-cell content must therefore exceed 85 % as measured by gas pycnometry. The limitation is that LLDPE carrier viscosity may produce visible gel particles when the masterbatch is stored in direct sunlight or above 30 °C for more than 6 months; production-scale experience requires melt filtration below 80 µm mesh at the extruder head.
| Property | Standard/method | Acceptance criterion applied in cable qualification |
|---|---|---|
| Dielectric constant at 1 MHz | IEC 60250 | 1.85–2.05 |
| Water absorption 24 h | IEC 60811-402 | < 0.01 % |
| Single-cable flame spread | IEC 60332-1-2 | damage height < 425 mm |
| RoHS lead concentration | 2011/65/EU | < 1000 ppm |
| RoHS cadmium concentration | 2011/65/EU | < 100 ppm |
| REACH SVHC concentration | EC 1907/2006 | < 0.1 % w/w |
Injection moulding of polyolefin caps and closures uses the masterbatch at 0.5 wt% to 1.5 wt% to counteract sink marks on ribs and bosses without increasing cycle time. The screw back pressure is set to 5–10 MPa, melt temperature to 210–230 °C, and mould temperature to 10–25 °C to freeze the outer skin rapidly. Short-shot trials are executed first because the foamed core reduces effective part density by 8–15 % and changes the required screw cushion. Holding pressure is reduced by 20–30 % relative to compact LLDPE to avoid gas counterpressure forcing melt back into the nozzle. The mould cavity is vented with 8–12 µm gaps at the parting line; insufficient venting produces gas burn marks and surface blush. Terminal parts are tamper-evident beverage closures, cosmetic caps, and dispensing caps with child-resistant features. Compliance for food-contact closures is evaluated under FDA 21 CFR 177.1520 for olefin polymers, EU Regulation 10/2011 Annex I migration limits using fatty food simulant D2, and CONEG heavy metals total lead, cadmium, mercury, and hexavalent chromium below 100 ppm. Mechanical performance is checked according to ASTM D638-22 for tensile yield and ASTM D256-23 for Izod impact. A critical boundary is that the masterbatch should not be combined with amine-based antifog or certain hindered amine light stabilizers in the same hopper; amine residues reduce effective gas yield and produce inconsistent bubble nucleation, so liquid additives are separately dosed.
For extrusion blow moulding of bottles and thin-wall canisters from LLDPE-rich compounds, the masterbatch is used at 1.0 wt% to 2.0 wt% to reduce density and increase wall stiffness without extending cooling time. A die head temperature of 190–205 °C and a parison speed of 0.3–0.7 m/s are maintained; the die gap is widened by 10–15 % compared with compact melt because foam expansion occurs after parison exit. The mould is closed with a counterpressure of 0.2–0.5 MPa for the first 0.5–1.0 s to prevent surface pinholing. The compressibility of the gas phase requires that preblowing pressure be reduced to 0.05–0.10 MPa. Terminal products include lightweight bottle bodies for household chemicals, cosmetic side-squeeze containers, and thin-wall transport canisters. Chemical resistance testing follows ASTM D543-21; top load resistance is measured according to ASTM D2659-21. Food-contact versions require pre-evaluation because lower wall density may increase migration surface area; the declared overall migration under EU 10/2011 with acetic acid 3 % w/v should be verified on the final article, not only on compact plaques. The process boundary is sharp: at 2.5 wt% and above, parison instability results from reduced melt strength and the preform can tear at the part line; production lines therefore operate with closed-loop gravimetric dosing rather than volumetric additive feeders.
Extruded polyolefin thermal break profiles for aluminium fenestration systems are produced with 0.6 wt% to 1.2 wt% of the masterbatch in a LLDPE/EPDM blend to create a microcellular core that reduces thermal conductivity while preserving screw retention. The profile is run on a 65 mm twin-screw extruder with 26:1 L/D and a downstream calibrator vacuum of −0.03 MPa to −0.05 MPa. Melt temperature is controlled between 195 °C and 215 °C, and the die land is extended to 10 times the wall thickness to generate back pressure above 18 MPa. The foaming reaction reaches full decomposition within 15–25 s residence time at these temperatures; shorter residence time leaves unreacted masterbatch visible as high-density inclusions. Terminal profiles are inserted into aluminium frames and must pass ISO 527-2 tensile modulus and ISO 178 flexural modulus after heat aging at 85 °C for 1000 h. Compliance is assessed under EN 14024 for mechanical performance of thermal break profiles and REACH Annex XVII restrictions. The operational boundary is incompatibility with unneutralised acid scavengers in the base compound; high free acidity suppresses gas yield by more than 30 % and requires pH-neutral stearate-based scavengers.
Three-layer blown film lines that incorporate a foamed core layer use the masterbatch only in the middle LLDPE layer at 0.5 wt% to 1.0 wt%, while the outer layers remain compact LDPE. The die temperature is set to 190–200 °C and the blow-up ratio is kept between 2.2:1 and 2.8:1; reducing the blow-up ratio below 2.0:1 increases transverse direction variation because gas cells orient in the machine direction. The frost line height is lowered by 15–20 % to stabilize the foam structure before quench. The resulting film has a dart impact value not less than 200 g at 50 µm total thickness when measured according to ASTM D1709-22 method A. Terminal uses are furniture wrap, glass protective interleaving, and heavy-duty mailer films. Compliance includes EU Packaging and Packaging Waste Directive 94/62/EC for heavy metals and REACH SVHC. The specific limitation is that the masterbatch is not suitable for films thinner than 25 µm because cell diameter approaches film thickness and creates pinholes; a separate blowing agent with finer particle size is required below this gauge.
Competitive Entec HYBOOST® 231 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Entec HYBOOST® 231 Masterbatch, LLDPE is a pelletized additive masterbatch manufactured on a linear low-density polyethylene carrier. The grade identifier 231 is a formulation code; public documentation does not provide a full payload disclosure, and lot-specific composition must be obtained from the supplier’s certificate of analysis before production use. The product is intended for dry-blend let-down into LLDPE-rich extrusion formulations and is supplied in pellet geometry compatible with gravimetric dosing equipment. Because the masterbatch is carrier-based, its melting behaviour, density, and rheological profile are dominated by the LLDPE phase, while the active additive package is delivered as a concentrated solid dispersion. Published data for this specific configuration is limited; therefore, the processing ranges in this document are drawn from established LLDPE extrusion practice and should be verified against lot-specific data.
In monolayer LLDPE blown film, dispersion of a pelletized masterbatch is governed by screw design, melt temperature, and die pressure. The masterbatch is introduced at the main feed port with the base LLDPE; a gravimetric feeder with a stated accuracy of ±0.5% to ±1.0% of set rate is typical. Extruders with 24:1 to 30:1 L/D and a barrier or Maddock-style mixing section provide the distributive mixing needed to eliminate additive-rich domains. Melt temperature measured at the adapter is commonly maintained between 190 °C and 230 °C, with die-body temperatures up to 240 °C. Die pressure should be monitored; a sudden drop at constant screw speed indicates abnormal melting or feed instability. Because the active chemistry is not publicly specified, a small-scale let-down trial is required to identify shear-induced degradation thresholds. Film tensile and dart impact after let-down should be evaluated according to ISO 527-3 and ASTM D1709 to confirm that the carrier addition does not shift the property balance beyond the target specification.
Cast film extrusion introduces the same LLDPE-based masterbatch at the feed throat, but the shorter die-land length and rapid quench on the chill roll reduce residence time compared with blown film. A typical cast line running LLDPE at 200 °C to 230 °C melt temperature and 50 µm to 150 µm film thickness should not use melt temperatures above 250 °C unless the lot-specific thermal stability data support it. The use of a screen pack with 40/80/120 mesh layers is common to trap undispersed particles and protect the flat die. Chill-roll temperature is usually held between 15 °C and 30 °C to control crystallinity and film haze; the effect of the masterbatch carrier on optical properties should be quantified using ASTM D1003.
The effective let-down ratio depends on the declared additive payload in the masterbatch. For LLDPE additive masterbatches with a payload between 5% and 20% by mass, a 2% to 5% let-down in the final product delivers an active concentration of 0.1% to 1.0% by mass. Without a supplier payload declaration, no single let-down ratio can be specified for HYBOOST® 231. Feed accuracy is critical at these low inclusion levels. Loss-in-weight gravimetric feeders operating in throughput ranges of 10 kg/h to 100 kg/h normally maintain ±0.5% to ±1.0% of set rate, while volumetric auger feeders may deviate by ±3% or more when pellet bulk density shifts due to regrind or fines. Pellet segregation between base resin and masterbatch should be minimized by maintaining similar pellet dimensions; if segregation occurs, the feeder hopper should be fitted with a low-level mass-flow insert or an internal agitator. The final film or sheet must be tested for consistency of the intended additive function, with sampling intervals of 15 min to 30 min during start-up until steady-state is verified by analytical results.
Production-scale behaviour of LLDPE carrier masterbatches is influenced by extruder size. On lines above 75 mm screw diameter, higher throughput reduces residence time and increases the risk of undispersed particles unless screw mixing sections are retained. On smaller 45 mm lines, residence time increases and thermal degradation of the additive becomes the limiting variable. Melt pressure measured before the screen pack should be recorded and compared with the neat base resin baseline; an increase greater than 1.0 MPa to 2.0 MPa at constant output may indicate screen blocking or incomplete melting. Batch-to-batch variation in pellet bulk density can also shift volumetric feeder output independently of screw speed; therefore, gravimetric control is preferred for let-down ratios below 3%.
The choice of an LLDPE carrier rather than LDPE, HDPE, or an EVA/wax carrier influences the melt rheology, crystallization kinetics, and compatibility of the masterbatch in LLDPE-rich systems. LLDPE has a narrower short-chain branching distribution and generally higher molecular weight than LDPE at a comparable melt index; its zero-shear viscosity and shear-thinning behaviour can prolong dispersion time but reduce the risk of additive phase separation. In contrast, an LDPE carrier may melt earlier and deliver additives quickly but can introduce a branched-polyethylene fraction that modifies the melt strength of blown film. An HDPE carrier has a higher crystalline melting range; at LLDPE processing temperatures, unmelted HDPE domains may persist and produce gel-like defects. EVA or wax carriers can plasticize the melt and alter heat-seal initiation temperature; the resulting seal-strength shift is measurable by ASTM F88. For applications requiring low haze and stable coefficient of friction, the carrier should be considered as a formulation variable rather than an inert diluent. Differences between carriers are assessed by ISO 1133-1 for melt mass-flow rate, ISO 11357-3 for melting/crystallization, and ISO 1183-1 for density. Where the end-use specification includes dart impact, tensile elongation at break, or tear resistance, the corresponding methods ASTM D1709, ISO 527-3, and ASTM D1922 provide the minimum dataset for carrier-selection comparisons.
Regrind use modifies the effective let-down ratio because the regrind already contains a fraction of the masterbatch carrier and its active additive. When film edge trim or start-up scrap is reintroduced into the feed blend, the amount of fresh masterbatch must be reduced to avoid additive over-addition. A material balance based on 10% regrind with 100% recycled masterbatch-containing film requires a fresh let-down decrease equal to the regrind fraction multiplied by the original let-down level. For example, a 3% fresh let-down at 10% regrind would be adjusted to 2.7% if the regrind carries the same 3% loading. Failure to correct for regrind can cause additive concentration drift and batch-to-batch property variation; melt pressure and output should be logged continuously to detect drift.
Compared with fully compounded LLDPE resin containing the same additive at final concentration, a masterbatch offers inventory flexibility but introduces an additional melt-blending step. The final dispersion quality depends on screw mixing; if the downstream extruder has only a simple conveying screw without a mixing element, the additive may not be distributed sufficiently. In such cases, a lower-viscosity carrier or a pre-compounded resin should be considered. Melt rheology of the let-down blend can be checked by small-amplitude oscillatory shear using ISO 6721-10 or capillary rheometry; a masterbatch-induced viscosity shift should be within the normal base-resin lot variation before line speed is increased.
Before production use, the lot-specific certificate of analysis and safety data sheet should be reviewed. Where the final article is intended for food contact, the supplier must state whether the masterbatch complies with FDA 21 CFR 177.1520 for olefin polymers or with Commission Regulation (EU) No 10/2011. In the absence of an explicit written statement, the product must be treated as non-food-contact. Electrical and electronic end-use compliance with Directive 2011/65/EU (RoHS) is relevant only for final equipment categories; polymer films used in food packaging or industrial film generally fall outside the RoHS scope unless incorporated into EEA equipment. For REACH, the supplier should provide an Article 33 declaration if any candidate-list substance is present above 0.1% by mass. Storage recommendations for LLDPE-based masterbatches include sealed containers, ambient temperature below 40 °C, and protection from ultraviolet light and moisture condensation. If bulk moisture exceeds 0.05% by mass due to condensation, drying at 60 °C to 70 °C for 2 h to 4 h in a desiccant or hot-air hopper dryer is typical. LLDPE does not hydrolyze; the drying step is for pellet surface moisture and conveying reliability, not polymer degradation avoidance.
Compatibility limitations apply when the active additive package is unknown. The masterbatch should not be melt-blended with strongly acidic or strongly oxidizing additives unless a prior mixing trial establishes inertness. If the downstream formulation contains amine-based processing aids or acid-scavenging zinc stearate packages, the supplier must confirm that the acid-base chemistry of HYBOOST® 231 does not cause additive consumption or discoloration. Contamination by insoluble particulates can be detected by pressure-rise monitoring across a 100-mesh screen pack during extrusion.
| Standard / Test Method | Property | Required Status |
|---|---|---|
| ISO 1133-1:2022 / ASTM D1238-23 | Melt mass-flow rate of carrier | Supplier certificate required |
| ISO 1183-1:2019 / ASTM D792-20 | Density | Supplier certificate required |
| ISO 11357-3:2018 / ASTM D3418-21 | Melting and crystallization peak | Supplier certificate required |
| ISO 3451-1:2019 | Ash content after combustion | Supplier certificate required |
| ISO 306:2022 / ASTM D1525-17e1 | Vicat softening temperature | Report only |
| ASTM D638-14 / ISO 527-3:2018 | Tensile properties after let-down | End-use specification dependent |
| ASTM D1709-22 | Dart impact of LLDPE film | End-use specification dependent |
| ASTM D1003-21 | Film haze | End-use specification dependent |