Entec Hyboost 230 Masterbatch Lldpe

Entec HYBOOST® 230 Masterbatch, LLDPE

    • Product Name: Entec HYBOOST® 230 Masterbatch, LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 216496
    Additive Type Processing Aid
    Carrier Resin LLDPE
    Form Pellets
    Density 0.920 g/cm³
    Melt Flow Rate 2.0 g/10 min (190°C/2.16 kg)
    Additive Content 20%
    Moisture Content 0.10%
    Pellet Size 2.00 - 3.00 mm
    Bulk Density 0.550 g/cm³
    Thermal Stability 260 °C
    Recommended Dosage 1 - 3%
    Shelf Life 12 months
    Storage Temperature 5 - 30 °C

    As an accredited Entec HYBOOST® 230 Masterbatch, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Entec HYBOOST® 230 Masterbatch, LLDPE is supplied in 25 kg polyethylene-lined paper bags, palletized and shrink-wrapped for industrial handling.
    Container Loading (20′ FCL) Entec HYBOOST® 230 Masterbatch, LLDPE loaded in 20′ FCL on pallets, shrink-wrapped, strapped, moisture-protected, and secured for transport.
    Shipping Entec HYBOOST® 230 Masterbatch, LLDPE is shipped as a non-hazardous, solid polymer masterbatch in moisture-barrier bags or cartons on pallets. Keep dry, avoid direct sunlight, heat, and contamination. Handle with normal industrial hygiene; no special DOT/IATA hazard classification typically required. Store at moderate temperature.
    Storage Store Entec HYBOOST® 230 Masterbatch, LLDPE in a cool, dry, well-ventilated area. Keep original containers tightly closed, away from direct sunlight, heat, ignition sources, moisture, and strong oxidizers. Use first-in, first-out stock rotation. Protect bags from tearing and water. Avoid contamination. Ensure clear labeling. Do not store near food, drink, or animal feed. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life typically 24 months from manufacture when stored in original, unopened packaging, cool, dry, away from sunlight.
    Application of Entec HYBOOST® 230 Masterbatch, LLDPE

    Foamed polyethylene sheet production using Entec HYBOOST® 230 Masterbatch in an LLDPE-rich skin and core structure requires the blowing agent carrier to be matched with the matrix melt index. In single-screw sheet lines of 45 mm to 75 mm screw diameter and L/D 30:1, the masterbatch is dry-blended with LLDPE or LLDPE/LDPE blends at evaluation loadings from 1.0 wt% to 3.0 wt%. Barrel temperatures are typically profiled from 155 °C in the feed zone to 205 °C at the die, with a melt temperature ceiling of 215 °C to prevent premature gas release and surface blemishes. The matrix melt flow rate measured under ISO 1133-1:2022 at 190 °C/2.16 kg is generally selected between 0.5 g/10 min and 2.5 g/10 min for foam bubble stability. Density of the unfoamed matrix measured under ASTM D792-20 is usually 0.925 g/cm³ to 0.935 g/cm³, while foamed sheet density drops into the range of 0.55 g/cm³ to 0.75 g/cm³ depending on die pressure and haul-off tension. Tensile strength and elongation are measured under ASTM D638-14; tensile strength decreases as density falls, while elongation at break may remain above 200% in the machine direction if cell elongation is controlled. Tear strength by ASTM D1922-15 is routinely specified for packaging and cushioning grades. Moisture uptake is an operational boundary: bags opened for more than 30 min at RH > 65% should be pre-dried at 60 °C for 2 h to 4 h to prevent surface pitting. End products include foam pouches, edge protection, industrial cushioning, and underlay membranes. Use in food-contact packaging requires converter verification of the active blowing agent under EU 10/2011 and FDA 21 CFR 177.1520 for the polyethylene carrier because not all chemical blowing agent residues are universally permitted for fatty-food contact.

    What Limits Injection Moulding Pressure Drop Reduction in Chemical Foaming?

    For structural foam components moulded from PP/PE copolymer or HDPE, HYBOOST 230 is metered at 1.0 wt% to 2.5 wt%. The injection moulding machine requires a shut-off nozzle and screw with L/D 20:1 to 22:1; back pressure is held at 0.5 MPa to 1.0 MPa to keep gas in solution upstream of the check valve. Melt temperature is maintained between 190 °C and 220 °C. During injection, the pressure drop across the gate initiates cell nucleation; moulds are filled at high speed with short-shot control because foam expansion completes cavity filling. The observed reduction in hydraulic clamping force is typically 20% to 50% relative to solid moulding at the same wall section, but published data for this specific masterbatch configuration is limited; converters should verify on their existing tooling. Part mass is reduced while wall stiffness is retained only when a compact skin layer is present. Surface silver streaks and gas marks occur when the addition exceeds 2.5 wt% or when the nozzle temperature exceeds 225 °C. Automotive interior parts require emission testing according to VDA 278 or OEM-specific specimen schedules, and flame performance is often evaluated under UL 94 at the final wall thickness. End products include cable management housings, HVAC flaps, trim brackets, and industrial enclosures. Compatibility with toners and carbon black masterbatches must be confirmed because certain pigments shift the decomposition onset and alter cell uniformity.

    Wood-plastic composite decking and fencing profiles based on 55 wt% to 65 wt% HDPE or LLDPE are processed with HYBOOST 230 introduced into a counter-rotating or conical twin-screw extruder at evaluation loadings of 1.5 wt% to 4.0 wt%. The extrusion melt temperature is kept between 160 °C and 180 °C; die temperature is typically 10 °C to 20 °C lower to contain the gas until the profile exits the die. Wood flour moisture must be below 1.0 wt% measured by ASTM D4442-20; otherwise steam competes with the blowing gas and creates irregular internal voids that cannot be controlled by calibration. The coupling agent, usually a maleic anhydride-grafted polyolefin, affects melt viscosity and cell coalescence. Foamed WPC density reductions of 10% to 30% are commonly targeted; flexural strength and modulus are measured under ASTM D6109-13 or ASTM D7031-11. Maintenance of screw oil temperatures and vacuum venting is critical because residual moisture plus decomposition by-products can exceed the vent capacity on small extruders. End products include decking boards, cladding, fencing profiles, and window trim sections. In high-lubrication WPC formulations, the nucleating effect of the masterbatch can be suppressed; the lubricant package should be rebalanced when the cell structure becomes coarse or the surface roughness increases.

    When Foam Core Wall Collapse Occurs Before Skin Freeze in Non-Pressure Pipe Extrusion

    In three-layer polyolefin pipe coextrusion for drainage, cable duct and agricultural applications, the core layer containing HYBOOST 230 is processed between solid HDPE or PP skins. The middle layer is loaded at 2.0 wt% to 3.5 wt%; the skin layers remain unfoamed. Core extruder diameters of 50 mm to 75 mm with L/D 30:1 are used, with melt temperatures around 190 °C for the core and 200 °C for the skins. The spiral mandrel die must maintain layer flow path temperatures within ±5 °C; deviations cause asymmetric gas expansion and visible wall thickness variation. Ring stiffness is measured under ISO 9969, and long-term pipe performance is evaluated according to EN 13476-1 for non-pressure underground drainage and sewerage systems where applicable. A density reduction in the foam core above 35% can cause the core layer to collapse before the outer skin freezes, especially in large-diameter pipe above 250 mm. The melt strength of the core compound is a limiting parameter; high-molecular-weight HDPE or branched LLDPE grades improve bubble stability. End products include corrugated drainage pipe, cable ducting, land drainage coil, and storage tank insulation profiles. The masterbatch should not be combined with external lubricant packages that reduce die-head pressure below the gas solubility limit.

    Wire Insulation Blowing Agent Dispersion and Capacitance Stability

    Foamed polyethylene insulation for twisted-pair and coaxial communication cables uses HYBOOST 230 at 0.8 wt% to 2.2 wt% in an HDPE or LLDPE insulation compound. The extrusion line is usually a 45 mm/30:1 single-screw extruder with a precision crosshead die. Melt temperature at the die is held between 190 °C and 210 °C; eccentricity and diameter are controlled by laser gauges during the expansion zone. The foamed insulation lowers apparent dielectric constant; capacitance and attenuation are evaluated under IEC 61156-1, with the target capacitance often below 100 pF/m depending on conductor size and pair design. Insulation tensile strength and elongation at break are measured under ASTM D638-14 on extruded tubing or under cable-specific methods such as UL 444. Flame performance is verified on the finished cable under IEC 60332-1-2 or UL 1581 vertical flame methods. Table 1 provides the compliance checklist for a data-cable insulation compound. The critical processing boundary is moisture: moist masterbatch generates pinholes in thin-wall insulation below 0.25 mm wall thickness. Pre-drying at 65 °C to 70 °C for 2 h is required when exposed to high-humidity handling. The masterbatch should not be predispersed in high-shear melt mixers above 220 °C, because early gas evolution reduces capacitance stability and increases return loss variation on high-frequency pairs.

    Compliance itemTest methodExample converter specification
    Insulation tensile strengthASTM D638-14> 12 MPa
    Elongation at breakASTM D638-14> 200%
    CapacitanceIEC 61156-1< 100 pF/m at 1 kHz
    Vertical flameIEC 60332-1-2Pass per cable design
    RoHS restricted substancesIEC 62321-4, IEC 62321-5, IEC 62321-7-1Below Directive 2011/65/EU Annex II limits

    When a chemical blowing agent is used in rotational moulding of LLDPE for double-walled insulated structures, HYBOOST 230 is dry-blended with the powdered LLDPE at 0.5 wt% to 2.0 wt%. The mould is charged, closed, and rotated biaxially in an oven set to 270 °C to 300 °C; the internal air temperature of the mould reaches 140 °C to 180 °C before the blowing agent decomposes during the densification phase. Lower addition levels are preferred because the process has no screw mixing; dispersion depends entirely on dry-blend uniformity. The absence of pressure during rotational moulding creates larger, irregular cells than extrusion or injection moulding, so density reduction may be limited to 10% to 20% before part stiffness falls below specification. Drop impact and environmental stress crack resistance are measured under ASTM D1998-21 for polyethylene tanks or ASTM D256 for impact strength. End products include insulated coolers, buoyancy floats, docking fenders, and technical containers. The presence of residual blowing agent gas can increase the cooling-time requirement; demoulding too early results in post-mould expansion and warpage. Purging between colour changes is more critical because the foam structure retains pigment and gas residues in the mould surface.

    Free Quote

    Competitive Entec HYBOOST® 230 Masterbatch, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Entec HYBOOST® 230 Masterbatch, LLDPE is introduced as an additive masterbatch in which a linear low-density polyethylene carrier resin is used to deliver a proprietary stabilization package into polyethylene conversion processes. The model designation identifies the grade, the carrier class, and the masterbatch format; the active concentration is not represented by the numerical suffix and must be taken from the batch-specific certificate of analysis. The product is supplied as free-flowing cylindrical pellets, and the LLDPE carrier is selected to provide rheological compatibility with ethylene homo- and copolymers while maintaining a lower melting peak than polypropylene-carrier masterbatches. Incoming inspection for this grade commonly includes melt mass-flow rate determination to ISO 1133-1:2022, apparent density to ISO 60, and moisture content to ISO 15512:2019. A moisture level above 0.10 wt% on receipt indicates exposure to ambient humidity and should trigger drying before use. The material is not a neat additive powder and should not be solvent-dispersed unless a site-specific risk assessment for solvent vapour exposure and masterbatch agglomeration is completed.

    For blown film conversion, the recommended starting let-down ratio for LLDPE-carrier stabilizer masterbatches is 1.0–3.0 wt%, metered through a gravimetric blender at the extruder throat. The exact addition rate for HYBOOST® 230 is derived from the desired oxidative-induction time as measured by ASTM D3895 or ISO 11357-6. At a 2.0 wt% addition level, film-line operators should verify that die pressure remains within the extruder mechanical limit and that the melt temperature measured at the adapter does not exceed 230°C. If the melt temperature exceeds this threshold, the LLDPE carrier can undergo chain scission, producing low-molecular-weight fractions that migrate to the die lip and accumulate as plate-out. In film production, this failure mode appears as edge build-up and bubble instability. When die-lip build-up is observed, the first corrective action is to reduce the temperature in the final barrel zone by 5–10°C and to verify that the masterbatch is not being overfed by a worn gravimetric feeder. The masterbatch pellets are added at the main feed port; side-feeding is unnecessary because the LLDPE carrier melts in the compression zone of a standard barrier screw with L/D 24:1 or higher.

    Thermal stabilization boundary in blown film conversion

    In a monolayer blown film line operating at 45 mm screw diameter and L/D 30:1, the product demonstrates typical LLDPE-carrier processing behaviour. The lower melting peak of LLDPE, in the range 120–130°C by differential scanning calorimetry to ISO 11357-3:2018, allows the masterbatch to soften before the high-molecular-weight host resin reaches full melting. This reduces unmelted-pellet breakthroughs in thin films above 25 kg/h throughput. The melt-pressure response to masterbatch addition is usually linear up to 3 wt%; deviations from linearity suggest incompatible additive dispersion or feed-starved conditions. Gel formation can be monitored by casting a 40µm LLDPE blown film and counting gels on an optical surface scanner; a gel count above 50 gels/m² larger than 100µm is generally considered a dispersion fault, although no universal ISO method applies. In production, excessive gel formation may be reduced by increasing backpressure by 5–10 bar or by raising the pack screen density to 60 mesh. These actions increase shear heating and improve carrier dilution.

    For cast film and sheet extrusion, the masterbatch is metered at the main feed with a loss-in-weight feeder. The narrow pellet geometry reduces bridging in hoppers when bulk density is maintained between 0.50–0.60 g/cm³ to ISO 60. If a cast film line runs above 250 m/min, the compounded additive package must be dispersed before the melt reaches the feedblock, because downstream mixing in a flat-die film line is limited. An initial processing setpoint for the extruder barrel is 180–210°C in the feed section and 210–230°C at the die, with a chrome-plated roll temperature of 20–30°C. The exact temperature window for HYBOOST® 230 should be confirmed against the certificate of analysis, because active content influences heat sensitivity. High-moisture conditions require pre-drying in a desiccant dryer at 60°C for 2–4 h to a dew point of -30°C or lower, especially when the product has been stored in bulk bags at relative humidity above 60%. Without drying, moisture may cause surface splay or hydrolysis of certain acid scavenger components.

    What separates an LLDPE carrier from LDPE and PP carriers?

    The primary difference between this product and an LDPE-carrier masterbatch of identical active concentration is the carrier architecture. LLDPE is a copolymer of ethylene with an α-olefin such as 1-butene or 1-octene; its density typically falls between 0.915–0.930 g/cm³ to ASTM D792-20, and its plastic yield elongation is higher than that of LDPE. A comparison of carrier properties can be made using tensile bars to ASTM D638-14: LLDPE generally retains elongation at break values above 800%, while LDPE carriers may lie in the 600–700% range. For film-grade blends, this higher elongation translates into improved puncture resistance in the host film. Compared with a polypropylene-carrier masterbatch, the LLDPE carrier exhibits a melting peak of 120–130°C rather than 160–170°C, reducing the energy input required to form a homogeneous melt in polyethylene lines. A PP carrier in a polyethylene film may form discrete high-melting domains that appear as gel-like specks; the LLDPE carrier avoids this incompatibility. However, this polymer-class selectivity means that HYBOOST® 230 is not recommended for polypropylene extrusion or injection molding, because the LLDPE carrier would form a dispersed polyethylene phase with reduced mechanical integrity. The active chemistry also differs from a neat additive powder: the masterbatch is dust-suppressed and can be dosed gravimetrically without the segregation and static-attraction problems of powdered stabilizers. The degree of dust suppression can be assessed by measuring the loss on ignition or by an eight-station static charge test, but published data for this specific grade is limited.

    During injection molding of polyethylene closures and thin-wall containers, the masterbatch can be added at 1–2 wt% if the press is equipped with a volumetric disc feeder or gravimetric screw feeder at the feed throat. On a press with clamp force from 100–300 t, the melt temperature should be maintained between 210–240°C. Higher injection velocities may reduce short-shot risk but can increase shear heating. If the mold has hot-runner tips with diameters below 1.0 mm, the masterbatch must be fully dispersed to avoid gate clogging. Operators should monitor screw recovery time. A prolonged recovery time after masterbatch addition may indicate viscosity increase from the carrier or from excessive additive load. In such cases, the let-down ratio is reduced by 0.5 wt% and the screw backpressure is increased by 2–5 bar.

    Gravimetric feeder accuracy and pellet handling boundaries

    Gravimetric dosing accuracy is influenced by pellet geometry, bulk density, and hopper outlet diameter. The product is pelletized to a nominal cylindrical form; typical pellet dimensions for LLDPE masterbatches are 3.0–4.0 mm in diameter and 3.0–5.0 mm in length. These dimensions permit mass flow from a hopper with a minimum outlet diameter of 60 mm without bridge formation. A feeder calibration check to ISO 1183-1:2019 or the feeder manufacturer’s gravimetric procedure should be performed after each lot change. In practice, batch-to-batch variance in bulk density of ±0.03 g/cm³ can produce a dosing deviation of ±2% if the feeder is calibrated to volume rather than mass. The addition rate is therefore specified in weight percent, not volume percent. If the product is conveyed over distances greater than 15 m in dilute-phase pneumatic systems, fines generation may occur. Fines increase dust exposure and can create dust-rich regions in the extruder throat that melt slowly and appear as pinholes in film. A sieve analysis using 500µm mesh can quantify fines; fines content above 0.5 wt% should be investigated.

    Initial blown film processing window for HYBOOST® 230 Masterbatch, LLDPE
    ParameterSuggested starting rangeEquipment or method
    Let-down ratio1.0–3.0 wt%Gravimetric blender
    Melt temperature at die190–230°CInfrared melt probe
    Die gap1.6–2.4 mmFixed-lip blown film die
    Blow-up ratio2.2:1–2.8:1Bubble geometry
    Frost line height4–6 die diametersAir ring and internal bubble cooling
    Drying condition60°C for 2–4 h if RH >60%Desiccant dryer
    Feed throat temperature40–60°CWater-cooled feed section
    Screen pack60 mesh recommendedBreaker plate filtration

    For regrind-rich polyethylene streams containing post-industrial scrap, the masterbatch is usually added to the recycled fraction at the let-down ratio calculated on total output. Because oxidation level in regrind varies with thermal history, the required addition level is best determined by OIT at 200°C according to ASTM D3895. A target OIT of 20–30 min is commonly used for long-lived rigid packaging; film applications may require 15–20 min. If the regrind contains oxidized gel particles, melt filtration is recommended at 80–100 mesh before the masterbatch is introduced. This reduces gel-related pinholes and improves apparent dispersion. When the product is used in a recycled LLDPE/LDPE blend containing residual printing inks and adhesives, it does not remove gels but can slow additional oxidative gel formation. No cleaning or compatibilizing function should be assumed unless specifically stated in the batch certificate.

    When coextruded film layers are thinned below 10µm

    When the masterbatch is introduced into a coextrusion tie-layer or a thin outer layer below 10µm, the dispersion requirement becomes stricter. A monolayer film can tolerate occasional soft agglomerates, but a thin coextruded layer concentrates stress at agglomerate boundaries and may fail during film stretching. In such cases, the masterbatch should be melt-filtered through a 100 mesh screen pack, and the carrier should be matched to the layer resin melt flow rate within 0.5 g/10 min to ISO 1133-1:2022. If the carrier MFR and the layer resin MFR differ by more than 1.0 g/10 min, localized viscosity inhomogeneity can cause visible streak formation. Haze of the resulting film can be measured by ASTM D1003-13; a haze increase of more than 2% at 40µm thickness suggests unstable masterbatch dispersion. In coextruded structures, the additive package may migrate from the LLDPE carrier into adjacent polyethylene layers over time. Migration follows Fickian diffusion; the migration rate increases with storage temperature and comonomer content. For food-contact applications, the final article must be tested under EN 1186-1 for overall migration and, where applicable, under Regulation (EU) No 10/2011 for specific migration of the active substances. The masterbatch supplier’s certificate should identify the carrier resin and any additives with specific migration limits. Published data for this specific grade in thin coextruded architectures is limited, so pilot-scale film validation at the intended thickness and line speed is required before production commit.

    For regulatory documentation, the following review matrix should be used as an incoming audit. The supplier must provide statements where a normative status is claimed. Absence of a supplier statement should be treated as non-demonstration, not non-compliance.

    Regulatory and standards review matrix
    RequirementNormative referenceCondition
    REACH substance communicationRegulation (EC) No 1907/2006, Articles 7 and 33SVHC declaration required at ≥0.1 wt% in article
    RoHS restricted substancesDirective 2011/65/EU, Annex IIPb, Hg, Cr(VI), PBB, PBDE each ≤1000 ppm; Cd ≤100 ppm
    EU plastic food-contactRegulation (EU) No 10/2011Overall migration <10 mg/dm²; specific migration where applicable
    US olefin polymer food-contact21 CFR 177.1520Carrier polymer compliance subject to extractive limits and end-use restrictions
    Packaging heavy metalsDirective 94/62/ECSum of Pb, Cd, Hg, Cr(VI) <100 ppm in packaging
    Recycled content claimISO 14021:2016Mass-balance documentation required for voluntary claims

    Storage in ambient conditions below 40°C and in sealed packaging prevents moisture uptake and dust contamination. If the product is stored in silos under external heat or direct sunlight, partial sintering of pellets may occur, especially at the surface. Blocked pellets can overload the rotary valve and cause feed interruptions. A maximum storage time of 24 months from manufacture is commonly applied to LLDPE-carrier stabilizer masterbatches; after this period, the acid scavenger and phosphite stabilizer may be partially hydrolyzed. Before use after prolonged storage, melt flow rate and moisture tests should be repeated.

    In extrusion blow molding of polyethylene bottles, the masterbatch is added at 1–2 wt%; the parison melt temperature is maintained at 190–210°C. The LLDPE carrier imparts slightly lower die swell than LDPE carriers, which can alter parison hang strength. Operators should verify part weight and wall-thickness distribution after lot changes, because die swell changes of 2–5% are possible when switching from LDPE-carrier masterbatches.