| HS Code | 336145 |
| Product Name | Ecopond AFR-97 High Flow/Impact Heat Stable Polylactic Acid/PC Alloy |
| Material Type | Polylactic Acid/PC Alloy |
| Key Properties | High Flow, Impact Resistant, Heat Stable |
| Density | 1.20 g/cm³ |
| Melt Flow Rate | 20 g/10 min at 230°C/2.16 kg |
| Tensile Strength | 55 MPa |
| Tensile Elongation At Break | 100% |
| Flexural Modulus | 2,200 MPa |
| Flexural Strength | 80 MPa |
| Notched Izod Impact | 60 J/m |
| Unnotched Izod Impact | 10 J/m |
| Heat Deflection Temperature | 95°C at 1.82 MPa |
| Vicat Softening Temperature | 110°C |
| Rockwell Hardness | R110 |
| Mold Shrinkage | 0.5–0.7% |
| Bio Based Content | 30% |
| Processing Method | Injection Molding |
| Processing Temperature | 200–230°C |
| Drying Conditions | 80°C for 4 hours |
| Color | Natural |
| Form | Pellets |
As an accredited Ecopond AFR-97 High Flow/Impact Heat Stable Polylactic Acid/PC Alloy factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Ecopond AFR-97 is packaged in 25 kg moisture-resistant bags, palletized for transport, with optional 500 kg bulk containers. |
| Container Loading (20′ FCL) | Ecopond AFR-97 High Flow/Impact Heat Stable PLA/PC Alloy loaded in 20′ FCL: palletized, moisture-protected, evenly distributed, secured, and sealed for export. |
| Shipping | Ecopond AFR-97 is shipped as non-hazardous, non-regulated polymer pellets in sealed, moisture-barrier bags, drums, or supersacks on pallets. It has no UN number, hazard class, or marine pollutant designation. Store and transport dry, in a cool, ventilated area away from excessive heat, sunlight, and oxidizers. Follow local regulations. |
| Storage | Store Ecopond AFR-97 High Flow/Impact Heat Stable Polylactic Acid/PC Alloy in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers tightly sealed, labeled, and off the floor to prevent moisture pickup and contamination. Avoid excessive stacking and protect from UV. Use within recommended shelf life; dry before processing if specified. |
| Shelf Life | Shelf life is generally 24 months when stored in original sealed packaging, cool, dry, well-ventilated, away from direct sunlight. |
Competitive Ecopond AFR-97 High Flow/Impact Heat Stable Polylactic Acid/PC Alloy prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618136850665 or mail to admin@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618136850665
Email: admin@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!