    Specifications
    HS Code 338667
    Product Name EcoInvest Recycled LLDPE Granulate Natural MFI 1.2-1.5
    Material Recycled Linear Low-Density Polyethylene (LLDPE)
    Form Granulate
    Color Natural
    Melt Flow Index Mfi 190 C 2 16 Kg 1.2-1.5 g/10 min
    Density 0.92-0.94 g/cm³
    Melting Point 120-130 °C
    Moisture Content <0.5%
    Filler Content <1%
    Recycled Content 100%
    Bulk Density 0.50-0.60 g/cm³
    Particle Size 2-4 mm
    Tensile Strength At Yield 10-15 MPa
    Elongation At Break >500%
    Flexural Modulus 200-400 MPa
    Vicat Softening Point 90-100 °C
    Hardness Shore D 50-55
    Thermal Stability Good
    Odor Low/Neutral

    As an accredited EcoInvest Recycled LLDPE Granulate Natural MFI 1.2-1.5 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing EcoInvest Recycled LLDPE Granulate Natural MFI 1.2-1.5 is packed in 25 kg PE-lined paper sacks on pallets.
    Container Loading (20′ FCL) 20′ FCL container loaded with EcoInvest Recycled LLDPE Granulate Natural MFI 1.2-1.5, bagged, palletized, and secured for ocean freight.
    Shipping EcoInvest Recycled LLDPE Granulate Natural MFI 1.2–1.5 is shipped as a non-hazardous thermoplastic in 25 kg PE bags or 1000 kg FIBCs, palletized and stretch-wrapped. Store dry, away from direct sunlight and heat. Handle with standard forklift equipment; avoid moisture, contamination, and packaging punctures during transport.
    Storage Store EcoInvest Recycled LLDPE Granulate Natural MFI 1.2–1.5 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep in original sealed bags or containers on pallets, off the floor, to prevent moisture, contamination, and dust. Avoid prolonged UV exposure and static buildup. Follow the supplier’s SDS and local regulations. Do not store near foodstuffs.
    Shelf Life Shelf life is typically 12 months when stored dry in original unopened packaging, away from direct sunlight and heat.
    Application of EcoInvest Recycled LLDPE Granulate Natural MFI 1.2-1.5
    In heavy-duty agricultural and construction film production, recycled LLDPE granulate with MFI 1.2–1.5 g/10 min enters blown-film lines where molecular-weight distribution directly governs bubble stability, gel formation behaviour, and downgauging tolerance. The melt flow rate, determined per ISO 1133-1:2022 at 190 °C under 2.16 kg load, places this material at the high-viscosity end of the general-purpose LLDPE film window, a positioning that allows monolayer and co-extruded structures from 25 μm to 250 μm to sustain stable bubble geometry at blow-up ratios of 2.0:1 to 3.5:1 on die diameters between 200 mm and 350 mm. Single-screw extruders equipped with barrier screws and Maddock mixing sections at L/D ratios of 30:1 or higher are the standard conveying systems for this viscosity class; barrel profile temperatures run from 160 °C at the feed throat to 190–205 °C at the metering zone, with adapter and die zones held at 185–215 °C. Screen-pack filtration at 60/80/100 mesh (250/180/150 μm aperture) is non-negotiable for post-consumer feedstock because recycled LLDPE introduces residual gel particles from prior oxidative degradation, crosslinked fractions from contaminant PET or PP, and occasional metallic fines from shredding equipment. Output rates in this rheological window typically fall between 0.8 kg/h and 1.5 kg/h per millimetre of die circumference, with frost-line heights controlled at 6 to 12 times die diameter to quench crystallinity before winder contact. Die gap settings of 1.8–2.4 mm are selected to minimize melt fracture while retaining sufficient draw-down to 25 μm gauge. Moisture management assumes elevated risk with recycled material: surface-adsorbed water from outdoor storage can exceed 0.05 wt% when ambient RH rises above 60%, and pre-drying at 70–80 °C for 2–4 hours in a desiccant dryer is required to prevent bubble instability manifested as visible film chatter and dart-drop collapse. The recycled fraction directly modulates mechanical performance in agricultural mulch film, construction vapor barrier, and heavy-duty shipping sacks. A systematic blend-gradient assessment under ASTM D1709-22 Method A (dart impact), ASTM D1922-23 (Elmendorf tear), and ASTM D882-18 (tensile) is provided in Table 1. Gel rating per ISO 18553-1 shifts from Category A at 20 wt% recycled content to Category B or C at 60–80 wt%, a transition that eliminates suitability for food-contact film constructions. Compliance for food-contact applications references FDA 21 CFR 177.1520 and EU Regulation No 10/2011; both frameworks require demonstration of contaminant absence and migration limits that recycled feedstock cannot satisfy without documented post-consumer sorting and decontamination validation under EN 15343. Traceability under EN 15343 with an independent certification body is the accepted mechanism for substantiating recycled-content claims in film commerce. Co-extrusion remains the dominant production strategy: recycled LLDPE is confined to the core layer at 30–60 wt% of total structure, while virgin LLDPE or LLDPE/LDPE skins of 15–20 μm thickness provide surface integrity and heat-seal performance. Failure modes on production-scale lines include screen-pack pressure rise exceeding 25 MPa within a continuous 8-hour shift, gel streaks originating from unmelted PET contaminants, and non-uniform film gauge traceable to unstable bubble neck geometry when recycled-fraction melt index drifts outside the 1.2–1.5 specification band.
    Table 1: Property Gradient for 50 μm Monolayer Blown Film as a Function of Virgin LLDPE to Recycled LLDPE Ratio
    Virgin : Recycled RatioDart Drop ASTM D1709-22 Method A (g)Elmendorf Tear MD ASTM D1922-23 (g/mil)Tensile at Break MD ASTM D882-18 (MPa)Gel Rating ISO 18553-1
    100:0180–220250–30032–38A
    80:20140–170220–26030–35A–B
    60:40100–130190–23028–32B
    40:6065–90160–20025–29B–C
    20:8040–60130–17022–26C

    A 0.75 mm Geomembrane Liner with 40 Percent Recycled LLDPE: Processing Conflicts

    Flat-die sheet extrusion configured for geomembrane applications presents a process conflict that is frequently underestimated when recycled LLDPE at MFI 1.2–1.5 is introduced. Geomembrane specifications under GRI GM17 and associated project documents typically demand melt flow rates below 1.0 g/10 min for monolayer liner applications; a recycled stream at 1.2–1.5 g/10 min therefore occupies the upper boundary of acceptable rheology, and its use without acceptance testing invites non-conformance findings. Sheet extrusion runs at melt temperatures of 200–240 °C through slot dies with thermally regulated lips, followed by a 3-roll polished chrome stack operating at 50–80 °C. Thickness control between 0.75 mm and 3.0 mm relies on gravimetric feed consistency and melt-pump stability; recycled feedstock with broader pellet geometry and variable bulk density (0.52–0.58 g/cm³ typical for regrind) can disrupt screw feed uniformity and produce gauge variation exceeding ±10% on a 4 m wide sheet. Carbon black is added at 2.0–3.0 wt% per ASTM D1603 to meet UV resistance requirements, with dispersion quality verified under ASTM D5596 at a maximum rating of Category 3. Oxidative stability is measured by standard OIT per ASTM D3895 at 200 °C; specification minimums of >100 minutes are routinely met by virgin LLDPE compounds, but recycled material with pre-existing antioxidant depletion frequently fails at 40–70 minutes, necessitating top-up stabilization with hindered phenolic/phosphite combinations at 0.15–0.35 wt% addition. High-pressure OIT per ASTM D5885 at 150 °C exhibits corresponding sensitivity, with minimums of >400 minutes unattainable when the recycled fraction exceeds 40 wt% without supplemental stabilization. Stress-cracking resistance, the most critical long-term performance attribute, is assessed under ASTM D5397-20 notched constant tensile load (NCTL) at 30% of yield stress; LLDPE demonstrates intrinsic superiority over HDPE in multi-axial strain tolerance, but recycled content introduces micro-contaminants that act as stress concentrators and reduce NCTL failure times from virgin-typical >500 hours to 150–300 hours at 40 wt% recycled fraction. Wedge welding for field seam construction proceeds at 350–420 °C with dual-track welders; weld tensile-shear performance is destructively tested per ASTM D6392-12, and seams containing gels from recycled feedstock show peel separation at 40–60% of parent-sheet strength compared with 80–90% for virgin welds. The operational boundary for this application is explicit: recycled LLDPE at MFI 1.2–1.5 is unsuitable for primary containment liners in hazardous-waste impoundments; it is acceptable for secondary containment, temporary covers, and agricultural pond liners when confined to a co-extruded core layer and when NCTL, OIT, and carbon-black dispersion data are submitted with each production lot.Blow molding operations for intermediate bulk container (IBC) liners and industrial tanks demand a specific combination of melt strength, parison sag resistance, and environmental stress crack resistance (ESCR) that recycled LLDPE at MFI 1.2–1.5 partially satisfies. Accumulator-head blow molding machines with clamp forces from 500 to 1500 tonnes are the predominant equipment platform for vessels between 20 L and 1000 L. Melt temperatures are maintained at 180–210 °C, approximately 60–90 °C above the crystalline melting range of 120–125 °C determined by differential scanning calorimetry per ISO 11357-3:2018. Parison swell in this MFI window typically measures 30–50% in diameter and 15–25% in wall thickness, values that must be compensated in the parison programming profile to achieve uniform container wall distribution. Parison sag for LLDPE at MFI 1.5 becomes problematic when unsupported parison length exceeds 800 mm or shot weight surpasses 15 kg; for 1000 L IBC liners, a blend of 30–50 wt% HDPE with MFI 0.3–0.8 is required to restore adequate melt strength. Mold shrinkage of 1.5–2.5% after cooling must be accommodated in tool dimensions, with post-mold annealing at 60–70 °C reducing warpage in flat-panel sections. ESCR per ASTM D1693-15 Condition A typically exceeds 1000 hours for virgin LLDPE; recycled material with residual catalyst metals and polar contaminants may fail at 200–400 hours, a performance gap that excludes this material from dangerous-goods packaging under UN certification unless ESCR testing is performed on each production lot. Tensile properties measured under ASTM D638-22 Type IV specimens show yield strength of 11–15 MPa and elongation at break of 700–900%, values that satisfy the minimum requirements of ASTM D1998 for polyethylene tanks. Food-contact suitability under FDA 21 CFR 177.1520 paragraph (c) applies only when the recycled feedstock derives from trays or crates used with food and when a functioning migration-control program documents contaminant absence. For industrial, non-food IBC liners, recycled content between 20 wt% and 50 wt% is commercially viable; higher fractions produce unacceptable wall-thickness variation traced to pellet-size non-uniformity in the feed system and should be avoided on machines with screw diameters below 90 mm.

    Does MFI 1.2–1.5 Provide Adequate Melt Strength for Corrugated Conduit Vacuum Sizing?

    Historically, corrugated polyethylene drainage pipe specifications restricted recycled content to a maximum of 10–25 wt%; the current ASTM and AASHTO frameworks provide an explicit pathway for higher recycled fractions when material classification metrics are met. Corrugated drainage pipe is manufactured to ASTM F405 for single-wall and ASTM F2306 for dual-wall constructions, with material cell classification required under ASTM D3350-23. A recycled LLDPE with density 0.918–0.925 g/cm³ per ISO 1183-1:2019 and MFI 1.2–1.5 maps to a cell classification of PE 223 or PE 233 depending on stabilizer package, and is acceptable for non-pressure drainage and conduit applications where stiffness is not the dominant design parameter. Vacuum-sizing corrugators operate at forming speeds from 10 m/min to 30 m/min; the corrugation troughs exert continuous vacuum between -0.02 MPa and -0.05 MPa on the parison exterior, and melt strength governs whether the sheet adheres uniformly to the mold blocks without tearing. At MFI 1.5, LLDPE retains sufficient melt elasticity for vacuum conformance at speeds below 20 m/min; above this threshold, corrugation crest thinning exceeding 25% of nominal wall develops, and melt fracture manifests as surface roughness on pipe exteriors. Melt temperature at the die is set between 180 °C and 220 °C, with die-head pressure typically 12–18 MPa for a 150 mm diameter pipe at 1.5 mm minimum wall. Carbon black for UV stabilization is incorporated at 2.0–2.5 wt% per ASTM D3350-23 cell requirement; recycled feedstock already containing carbon black from prior applications may complicate additive consistency unless melt filtration at 150 μm aperture is installed. Pipe stiffness measured under ASTM D2412 for recycled LLDPE corrugated structures at 150 mm nominal diameter typically falls between 240 kPa and 350 kPa, below virgin HDPE equivalents but within gravity-flow drainage envelopes. The critical processing limitation occurs in the corrugator vacuum-transfer zone where recycled material with gel concentrations from Category B or worse per ISO 18553-1 creates localized insulation points that prevent proper quench and produce post-form ovality exceeding 8% of diameter. Published data for continuous production runs exceeding 72 hours at 100% recycled content on corrugated pipe lines with screw diameters above 120 mm is limited; most operators blend at 40–70 wt% recycled fraction with virgin HDPE or LLDPE to maintain line stability.

    Heavy-Gauge Sheet Extrusion and Vacuum Thermoforming Windows

    The substitution of recycled LLDPE into heavy-gauge industrial thermoforming applications—truck bed liners, chemical containment trays, dunnage platforms, and material-handling components—requires recognition that the MFI 1.2–1.5 window drives sheet line energy inputs and forming cycle behaviour differently than amorphous resins such as HIPS or ABS. Sheet extrusion proceeds on single-screw machines with L/D ratios of 32:1 to 38:1, slot-die widths from 1.2 m to 2.5 m, and melt temperatures of 200–240 °C. The elevated viscosity at MFI 1.2 necessitates screw speeds 15–25% lower than equivalent MFI 4.0 LDPE to maintain melt-pressure ceilings below 25 MPa at the breaker plate. Three-roll stack cooling controls sheet gloss and thickness tolerance; roll temperatures of 50–80 °C prevent premature crystallization and maintain sheet flatness for downstream forming. Heavy-gauge sheets from 3 mm to 12 mm are formed on single-station vacuum or plug-assist machines. The thermoforming window is defined by the crystalline melting onset at 120–125 °C and the sag threshold above 145 °C; sheet surface temperatures of 125–145 °C must be achieved uniformly using IR ceramic or quartz heating panels with zone-control tolerance of ±5 °C to prevent localized thinning or burn. Vacuum levels of -0.08 MPa are standard for heavy-gauge LLDPE; plug assistance with syntactic foam or PTFE-coated aluminum plugs reduces wall thinning at draw ratios exceeding 2:1. Mold shrinkage between 1.5% and 2.5% is observed when cooling to 25 °C, and tool design must incorporate this amount to achieve final part dimensional stability. Yield strength per ASTM D638-22 measures 11–15 MPa and flexural modulus per ASTM D790-17 ranges from 250 MPa to 400 MPa, values that support load-bearing dunnage at service temperatures below 60 °C but exclude continuous exposure near engine compartments. ESCR values exceeding 1000 hours per ASTM D1693-15 Condition A position LLDPE above HDPE for chemical containment trays subject to surfactant or solvent stress. The recycled fraction in this segment is typically 30–60 wt%; higher fractions degrade surface finish due to micro-gels and reduce sag resistance during the heating cycle, forcing the operator to lower forming temperature to 120–130 °C and accept increased plug-assist force and longer cycle times.For fiber optic cable jacket applications and low-voltage power cable sheathing, recycled LLDPE at MFI 1.2–1.5 occupies a narrow position between traditional LDPE jacket compounds (MFI 0.2–2.0) and the higher-MFI LLDPE used in thin-wall high-speed lines. Jacket extrusion is performed on single-screw machines with L/D ratios of 24:1 to 30:1, using pressure dies that maintain melt compression against the cable core and eliminate air entrapment. Melt temperatures at the die land are maintained at 200–220 °C, with screw barrel profiles from 160 °C in the feed section to 205 °C in the metering zone. Jacket thickness specifications range from 0.8 mm to 2.5 mm for fiber optic and low-voltage constructions under IEC 60502-1; line speeds up to 200 m/min are achievable for thin-wall jackets on 50 mm to 90 mm extruders. Carbon black masterbatch is incorporated to a final content of 2.5 ± 0.5 wt% per ASTM D1603 for UV stabilization, a requirement codified in ASTM D1248 for outdoor-grade polyethylene. Tensile strength and elongation at break are tested per IEC 60811-501; minimum requirements of 10 MPa tensile and 300% elongation are satisfied by recycled LLDPE at 150% to 200% of specification. Surface quality is the principal production constraint: gels from recycled feedstock cause jacket surface roughness visible at 0.5 mm thickness, and print adhesion on recycled LLDPE is measurably inferior to virgin due to oxidized surface groups, requiring corona treatment at 40–45 mN/m before cable marking. Batch-to-batch color variation from mixed recycled streams is an additional limitation for applications where jacket color is a specification parameter; operators compensate with pre-compounded color masterbatch at 2–4 wt% addition. The operational boundary is explicit for UL-listed or armoured cable products: recycled content above 20 wt% is not recommended without full re-qualification, while non-critical fiber optic duct jackets and temporary power cable sheathing can tolerate up to 100% recycled LLDPE when surface quality, tensile, and elongation are verified per lot.

    When Recycled LLDPE Replaces Virgin LDPE as the Carrier Phase in Filled Masterbatch

    Co-rotating twin-screw compounding lines processing filled masterbatch formulations evaluate carrier resin by three parameters: melt viscosity under shear, filler wetting capacity, and devolatilization behaviour. Recycled LLDPE at MFI 1.2–1.5 presents a measurable trade-off against conventional LDPE carriers with MFI 4.0–20.0. The processing platform is a co-rotating twin-screw extruder with L/D ratio of 36:1 to 48:1 and screw diameter from 50 mm to 92 mm; barrel zones are profiled from 180 °C in the feed section to 220–230 °C at the die. Specific energy input for filler dispersion at 60–80 wt% CaCO3 loading ranges from 0.18 kWh/kg to 0.30 kWh/kg, with torque at 60–85% of motor maximum at screw speeds of 400–600 rpm. Filler loading capacity decreases by 10–15% relative to MFI 8.0 LDPE carrier because the higher-viscosity LLDPE matrix reaches maximum torque earlier; at 80 wt% CaCO3, the twin-screw may stall unless screw speed is reduced to 350 rpm and barrel temperature is raised 10–15 °C. Carbon black masterbatch production at 40–50 wt% pigment loading presents similar boundaries: the higher melt viscosity improves pigment wetting and dispersion quality (measured per ISO 18553-1 as fewer undispersed aggregate counts), but increases die-plate pressure by 15–25% and demands underwater pelletizing die-plate temperatures of 180–220 °C to prevent freeze-off. Vacuum devolatilization at -0.08 MPa is essential for recycled material to strip residual moisture and low-molecular-weight volatile contaminants before filler incorporation. Compatibilizer addition of maleic-anhydride-grafted LLDPE at 2–5 wt% is required for mineral-filled systems to achieve tensile properties equivalent to virgin-carrier formulations; without compatibilizer, tensile strength at 70 wt% CaCO3 loading drops by 20–30% per ISO 527-2:2012. Letdown ratios for carbon black masterbatch in downstream film or sheet applications range from 2% to 5%; for conductive compounds, resistivity per IEC 60093 can be tuned below 10³ Ω·cm at appropriate loading. The operational boundary for this application is defined by screw torque: at MFI 1.2, recycled LLDPE carrier imposes 20–30% higher torque than virgin LDPE of equivalent density, a penalty that limits throughput on machines with motor capacity below 15 kW per 100 kg/h output when filler loading exceeds 70 wt%.
    Table 2: Compliance and Processing Boundary Matrix Across Principal Downstream Segments
    Application SegmentPrimary SpecificationCore Test MethodsRecycled Content Limit (Documented)Processing Boundary Condition
    Heavy-duty blown filmISO 1183-1:2019 density profileISO 1133-1:2022, ASTM D1709-22, ASTM D882-1860 wt% (non-food)Dart drop falls below 100 g at 60% recycled
    Geomembrane linerGRI GM17ASTM D5397-20, ASTM D3895, ASTM D559640 wt% (secondary containment)OIT <100 min at >40% recycled without stabilization top-up
    Extrusion blow moldingASTM D1998ASTM D638-22, ASTM D1693-1550 wt% (industrial IBC liners)Parison sag beyond 800 mm length at >15 kg shot weight
    Corrugated pipe/conduitASTM F405, ASTM F2306, ASTM D3350-23ASTM D2412100 wt% (non-pressure drainage)Corrugator speed must remain below 20 m/min at MFI 1.5
    Thermoformed sheetInternal industrial specificationASTM D638-22, ASTM D790-1760 wt%Forming window narrows to 120–130 °C at >50% recycled
    Cable jacketIEC 60502-1IEC 60811-501, ASTM D1603100 wt% (non-critical jacket)Surface roughness at 0.5 mm wall for gel Categories B–C
    Masterbatch carrierISO 1133-1:2022 consistencyISO 527-2:2012, ISO 18553-1N/A (carrier phase)Torque ceiling at 70–80 wt% CaCO3 loading on 75 mm twin-screw
    Free Quote

    Competitive EcoInvest Recycled LLDPE Granulate Natural MFI 1.2-1.5 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    EcoInvest Recycled LLDPE Granulate Natural MFI 1.2–1.5 is a reprocessed linear low-density polyethylene pelletised as natural translucent granules with a target melt flow rate of 1.2–1.5 g/10 min when measured at 190 °C under 2.16 kg load in accordance with ISO 1133-1:2022. The product designation is EcoInvest Recycled LLDPE Natural MFI 1.2–1.5; its specification boundary includes a nominal density of 0.920–0.925 g/cm³ tested to ISO 1183-1, a packaging moisture content not exceeding 0.05 wt%, and a natural unpigmented appearance that permits downstream masterbatch loading without interference from pre-coloured regrind. The granulate is obtained from controlled post-industrial and post-commercial flexible packaging scrap, washed, melt-filtered through a screen pack of 100–120 mesh, and pelletised under melt temperatures not exceeding 230 °C to limit oxidative chain scission. In downstream converting, the grade functions as a low-flow LLDPE for blown film, extrusion blow moulding, sheet, geomembrane, and heavy-duty sack applications where higher melt strength and puncture resistance are weighted more heavily than fast cavity filling.

    Unlike high-flow recycled LLDPE grades with melt flow rates above 3.0 g/10 min, this material retains a longer stress relaxation spectrum and greater bubble stability in high-stalk film lines. It also differs from recycled LDPE of similar melt flow by a narrower molecular weight distribution and a lower degree of long-chain branching, which affects die swell and melt tension in opposite directions. When compared with virgin C6-LLDPE, the principal operational differences are an increased gel-particle background, slightly wider lot-to-lot density fluctuation, and a higher dependence on melt filtration and pre-drying.

    When the Melt Flow Index Drops to 1.2–1.5, Film Bubble Stability Changes

    At 1.2–1.5 g/10 min, the melt phase exhibits higher apparent viscosity than reprocessed LLDPE grades in the 2.0–4.0 g/10 min band. In blown film lines, this translates into a more stable bubble under high-stalk processing, particularly at blow-up ratios between 2.0:1 and 3.0:1. Production-scale lines running barrel temperatures of 180–210 °C in the feed section and 210–230 °C in the metering section have observed that the low-MFI grade permits frost line heights of 5–8 die diameters without the bubble flutter associated with lower-viscosity recycled streams.

    Screw selection becomes more critical when the melt flow index is held at 1.2–1.5. Single-screw extruders with L/D 30:1, barrier flights, and compression ratios between 2.5:1 and 3.0:1 are used to complete melting before the mixing section. Screen pack configuration is normally 60/100 mesh in continuous film production, with pressure-buildup limits above 80 bar relative to clean-screen baseline triggering filter replacement. A screen pack with 100/120 mesh is specified only when gel-particle control in film thickness below 50 µm is required, but it increases head pressure and melt temperature by friction and shortens the interval between screen changes.

    Melt temperature should not exceed 230 °C to avoid oxidative degradation of the recycled polyethylene backbone; barrel profile set points of 180–210 °C for the feed zone, 210–225 °C for compression, and 215–230 °C for metering are employed. Die lip temperatures below 190 °C can initiate sharkskin melt fracture at die shear rates above 500 s⁻¹; fluoropolymer processing aids at 300–1,200 ppm are added on some lines to extend the shear-rate window before surface matteness occurs. The grade’s low MFI also requires a die gap of 1.8–2.4 mm rather than the 1.0–1.4 mm gap common with higher-MFI LLDPE, preventing excessive die pressure and maintaining gauge uniformity across the web.

    Pre-drying is required when moisture content exceeds 0.05 wt% or when sacks have been stored uncovered at relative humidity above 60%. A desiccant hopper dryer operated at 70–80 °C for 2–4 h lowers surface moisture sufficiently to eliminate steam-induced voids in film. The material does not undergo hydrolytic chain cleavage in the same manner as condensation polymers; moisture-related defects are physical, not chemical.

    In lean-phase pneumatic conveying, pellet bulk density is typically between 0.50 g/cm³ and 0.56 g/cm³; silo discharge reliability decreases below 0.48 g/cm³ due to hopper bridging in conical outlets. Round tubular granules of 3.0–4.0 mm diameter and 2.5–3.5 mm length are common. Natural granules are not dust-free; fines content above 0.2 wt% measured by ISO 14681 can reduce extruder feeding stability and should be sieved before use in thin-gauge film.

    What separates this granulate from virgin LLDPE and high-flow recycled film scrap?

    The clearest separation from virgin hexene or butene LLDPE is the recycled input-stream composition and the resulting lot-to-lot variance in comonomer distribution. Virgin LLDPE is produced with a controlled comonomer type—1-hexene or 1-butene—and predictable molecular weight distribution, while post-industrial LLDPE scrap typically contains a mixture of C4, C6, and C8 copolymers with differing branch distributions. The EcoInvest grade is therefore specified with a melt flow rate window of 1.2–1.5 g/10 min rather than a single nominal point, and density control accepts a spread of 0.005 g/cm³ to accommodate feedstock heterogeneity.

    Against high-flow recycled film scrap with MFI values between 2.0 g/10 min and 4.0 g/10 min, the lower MFI value of 1.2–1.5 g/10 min indicates higher average molecular weight and higher melt strength. This difference is measurable as a longer parison hang time in extrusion blow moulding and reduced neck-in during extrusion coating; it is a disadvantage in thin-wall injection moulding where spiral flow length decreases with decreasing MFI. The tensile yield stress of LLDPE in the 0.920–0.925 g/cm³ density band is typically between 10 MPa and 12 MPa when tested to ISO 527-2, with elongation at break normally above 500%. High-flow recycled grades in the same density band may show reduced elongation and puncture resistance because of greater chain scission during extra reprocessing cycles.

    Compared with recycled LDPE of equivalent melt flow, the linear polyethylene structure has limited long-chain branching; die swell is therefore lower, melt tension is lower at equal MI, and the shear-thinning response is less pronounced. The consequence is that the LLDPE grade processes with lower bubble stability than LDPE in very high-stalk film, but it imparts higher puncture and tear strength to the finished film when blended or used as the main layer. Table 1 summarises typical comparative screening values, not certified lot specifications.

    PropertyMethodEcoInvest Recycled LLDPE MFI 1.2–1.5High-flow recycled LLDPERecycled LDPE equivalent MI
    Melt flow rateISO 1133-1:20221.2–1.5 g/10 min2.0–4.0 g/10 min1.2–1.5 g/10 min
    DensityISO 1183-10.920–0.925 g/cm³0.918–0.923 g/cm³0.917–0.925 g/cm³
    Tensile yield stressISO 527-210–12 MPa9–11 MPa8–10 MPa
    Elongation at breakISO 527-2>500%>450%>400%
    Vicat softening temperatureISO 306/A5092–96 °C90–95 °C88–94 °C

    Blending this granulate with high-pressure LDPE at 10–30 wt% is used on film lines to obtain a compromise between linear-grade toughness and LDPE melt elasticity. At LDPE additions above 30 wt%, the tensile yield stress and puncture energy of the blend can decline faster than expected from a linear mixing rule because the stress-bearing load shifts to the lower-yield LDPE phase. Below 10 wt%, bubble stability improvements are often too small to justify the additional silo. These thresholds are alignment guidelines rather than thermodynamic phase boundaries; published data for this specific recycled lot configuration is limited, and film properties should be confirmed on a mono-layer pilot line before commercial conversion.

    Thermal analysis of the granulate to ISO 11357-3 typically identifies a peak melting endotherm between 122 °C and 126 °C for linear low-density polyethylene with a density of 0.920–0.925 g/cm³. The crystallisation temperature under a cooling rate of 10 K/min is normally 102–108 °C. Differences in comonomer sequencing across recycled feedstock can broaden the melting curve by 2–4 K relative to virgin C8-LLDPE. A broadened melting endotherm is not a processing defect, but it alters the location of the sealing initiation temperature in film converting; heat-seal settings must be verified by differential scanning calorimetry and hot-tack tests according to ASTM F1921.

    Capillary rheometry at 190 °C and 100 s⁻¹ for LLDPE in the MFI band of 1.2–1.5 g/10 min commonly lies in the apparent viscosity range of 600–900 Pa·s, while at 1,000 s⁻¹ the value may fall to 150–250 Pa·s. These values are not fixed lot specifications; they depend on comonomer type, molecular weight distribution breadth, and feedstock recycling history. The practical consequence is that film dies designed for virgin LLDPE at MFI 2.0–3.0 will generate higher melt pressure and require either a wider die gap or a higher melt temperature when this low-MFI recycled grade is substituted.

    Extrusion Blow Moulding, Sheet, and Geomembrane Usage Limits

    In extrusion blow moulding, the low melt flow index provides parison hang-time control at die temperatures of 200–220 °C and clamp tonnage requirements governed by product surface area rather than melt flow. The natural translucence permits light inspection of weld seams; however, the absence of carbon black means that ultraviolet stabilisation is mandatory for outdoor containers. Without UV stabiliser, polyethylene exposed above 1,000 h of accelerated weathering to ISO 4892-2 may lose more than half of its tensile elongation at break. This is not a defect of the recycled base resin but an inherent boundary of unpigmented LLDPE.

    Heavy-duty sacks and industrial film made from this grade are typically produced with a blend of 80–100 wt% EcoInvest Recycled LLDPE and 0–20 wt% LDPE. Mono-extruded films below 30 µm with 100% recycle content require the higher filtration level of 120 mesh and are limited by gel count. At gauges below 20 µm, the melt temperature should be raised to 225–230 °C to reduce melt viscosity and improve gauge control.

    Geomembrane applications require testing against ISO 527-3 for film and sheet tensile properties, ISO 6383-2 for tear resistance, and ISO 11358-1 for thermogravimetric purity; published data for this specific recycled granulate in geomembrane certification is limited, so converter-level qualification is required. Extrusion coating and lamination are possible at melt temperatures of 230–240 °C, but the low MFI narrows the line-speed window compared with coating grades of 7–10 g/10 min.

    Dry-batch colouring with a linear-low-density-compatible masterbatch is typical; the natural base allows loading levels of 2–6 wt% for standard monochromatic film. The base granulate is not pre-dried beyond packaging moisture control, but carrier resins in masterbatches may introduce moisture, bringing the total feed moisture above 0.05 wt%. Therefore converters should measure moisture of both granulate and masterbatch together, not independently.

    Injection moulding is possible but not the primary design target. The low melt flow rate of 1.2–1.5 g/10 min reduces spiral flow length compared with recycled LLDPE grades above 5 g/10 min; moulding of thick-section parts requires melt temperatures of 220–240 °C, injection pressures of 80–120 MPa, and mould temperatures of 20–40 °C. Thin-wall parts below 1.0 mm wall thickness are outside the practical operating window because short-shot frequency increases sharply. The material should not be used as a direct replacement for high-flow injection moulding grades of 30–50 g/10 min.

    Regulatory Traceability and Recycled-Content Certification Boundaries

    The grade is supplied with a recycled-content claim that should be verified through chain-of-custody documentation under EN 15343:2007. Recycled content percentages are lot-dependent; converters should request batch-specific attribution. The material is subject to REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU for restricted substances in electrical and electronic equipment. For packaging applications, the sum of lead, cadmium, mercury, and hexavalent chromium should be verified against the 100 mg/kg limit in EU 94/62/EC.

    For food-contact packaging, the as-received recycled granulate does not carry a standing functional barrier approval. Compliance with 21 CFR 177.1520 in the United States may be possible only when the olefin polymer satisfies the relevant paragraph (a) conditions and the converter completes end-use testing; European food-contact use under EU 10/2011 requires migration testing and a declaration of compliance from the finished package manufacturer. The natural grade should not be used for direct food contact without explicit lot-level certification.

    The absence of heavy metal contamination can be checked by EN 16785-1:2015 for recycled polymers; odour and volatile substance limits follow converter-specific methods such as VDA 277 for automotive interior emission. The product has no intrinsic flame-retardant formulation; compliance with EN 13501-1 fire classification is achieved only by downstream additive addition and is not claimed by the base granulate.

    Standard / RegulationScopeRelevant check
    ISO 1133-1:2022GlobalMelt flow rate at 190 °C/2.16 kg
    ISO 1183-1GlobalDensity
    ISO 527-2GlobalTensile yield, elongation
    REACH EC 1907/2006EUSVHC monitoring
    RoHS 2011/65/EUEURestricted substances in EEE
    EU 94/62/ECEUPackaging heavy metal sum 100 mg/kg
    EN 15343:2007EURecycled content traceability
    FDA 21 CFR 177.1520USOlefin polymers for food contact if lot certified

    Warehousing under ambient conditions is acceptable when sacks remain unopened and relative humidity is below 60%; opened sacks should be re-sealed and consumed within 48 h where thin film is being produced. Bags stored in direct sunlight can develop surface oxidation and yellowing of the natural pellet over extended periods; storage below 35 °C and away from UV light preserves melt stability. These constraints are typical for unpigmented recycled polyethylene and not unique to this model.