| HS Code | 785275 |
| Productname | DuPont Teijin Films Kaladex® PEN Film Q72 |
| Polymer | Polyethylene naphthalate (PEN) |
| Filmtype | Biaxially oriented PEN film |
| Grade | Q72 |
| Nominalthicknessavailability | Multiple nominal thicknesses available |
| Density | Approximately 1.36 g/cm³ |
| Tensilestrengthmd | Approximately 250–300 MPa |
| Tensilestrengthtd | Approximately 250–300 MPa |
| Tensilemodulusmd | Approximately 6–7 GPa |
| Tensilemodulustd | Approximately 6–7 GPa |
| Elongationatbreakmd | Approximately 70–120% |
| Elongationatbreaktd | Approximately 70–120% |
| Glasstransitiontemperature | Approximately 120 °C |
| Meltingpoint | Approximately 265 °C |
| Thermalshrinkage | Low; typically less than 1% under standard test conditions |
| Dielectricstrength | Approximately 250–300 kV/mm |
| Dielectricconstant | Approximately 3.0 at 1 kHz |
| Dissipationfactor | Approximately 0.005 at 1 kHz |
| Waterabsorption | Approximately 0.3% |
| Coefficientofthermalexpansion | Approximately 20 ppm/°C |
As an accredited DuPont Teijin Films Kaladex® PEN Film Q72 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied as one roll of Kaladex® PEN Film Q72, individually wrapped in moisture-barrier film and labeled with product and lot information. |
| Container Loading (20′ FCL) | DuPont Teijin Films Kaladex® PEN Film Q72 loaded in a 20′ FCL, palletized rolls secured and moisture-protected for ocean shipment. |
| Shipping | DuPont Teijin Films Kaladex® PEN Film Q72 is shipped as non-hazardous polymeric film in sealed rolls, palletized and protected from moisture, heat, sunlight, and mechanical damage. Use clean, dry transport; retain original packaging and labeling; no special hazardous-material classification is required. |
| Storage | Store DuPont Teijin Films Kaladex® PEN Film Q72 in a clean, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, moisture, and incompatible chemicals. Keep in original, undamaged packaging and protect from physical damage. Follow the manufacturer’s SDS/TDS for specific temperature and humidity limits. |
| Shelf Life | Shelf life is generally indefinite when stored in original packaging, dry, at ambient temperature, and away from direct sunlight and moisture. |
Competitive DuPont Teijin Films Kaladex® PEN Film Q72 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont Teijin Films Kaladex® PEN Film Q72 is a biaxially oriented polyethylene naphthalate film grade produced for converting operations in which standard polyethylene terephthalate film exhibits excessive dimensional change under thermal load. The Q72 designation identifies a specific film within the Kaladex range; gauge availability, roll lengths, core inside diameter, and surface treatment condition are defined by the manufacturer’s technical data sheet for the selected thickness. Polyethylene naphthalate differs from polyethylene terephthalate through substitution of the benzene diacid unit with a naphthalene diacid unit in the polymer repeat unit, increasing chain stiffness and raising the glass transition temperature to approximately 120 °C as measured by differential scanning calorimetry according to ASTM D3418. This structural modification also lowers oxygen and carbon dioxide permeability relative to PET at equivalent gauge and orientation. Because Q72 is biaxially oriented, tensile strength and modulus values are balanced between machine and transverse directions; reported tensile properties in the supplier literature are generated from ASTM D882 specimens conditioned at 23 °C and 50 % RH. The film is intended for downstream operations including rotary die-cutting, flatbed die-cutting, adhesive lamination, solventless and solvent-based coating, flexographic printing, and high-temperature release applications. In such operations, the film’s dimensional stability under tension and heat is a primary selection driver.
Comparative thermal analysis shows that PEN maintains mechanical integrity at temperatures where PET begins to lose modulus. The naphthalene ring reduces chain mobility, producing a glass transition temperature near 120 °C versus approximately 78 °C for biaxially oriented PET when tested by ASTM D3418 at 10 °C/min. The melting point of PEN is approximately 265 °C, providing a wider end-use thermal window. In continuous thermal load testing of film restrained in a frame, the higher glass transition temperature reduces creep-related dimensional loss. Published comparative data for Kaladex PEN films report lower shrinkage than PET at 150 °C after 30 min exposure; the exact Q72 shrinkage value is gauge-dependent and must be confirmed against the supplier certificate of analysis. The oxygen permeability of PEN is approximately 5 times lower than PET at equal thickness when measured by ASTM D3985 at 23 °C and 0 % RH. This difference is relevant in flexible electronic encapsulation and barrier-adhesive carrier films. For electrical applications, PEN exhibits dielectric strength typically above 200 kV/mm for thin gauges when measured by ASTM D149, though specific Q72 values are thickness-dependent and should be confirmed. The hydrolytic stability of PEN is superior to PET because the higher aromatic content lowers ester group concentration per unit volume.
| Property | Test method | Kaladex PEN film | Standard BOPET film |
|---|---|---|---|
| Glass transition temperature | ASTM D3418 | 120 °C | 78 °C |
| Melting point | ASTM D3418 | 265 °C | 255 °C |
| Density | ASTM D1505 | 1.36 g/cm³ | 1.39 g/cm³ |
| Tensile strength at break, machine direction | ASTM D882 | 275 MPa | 200 MPa |
| Elongation at break, machine direction | ASTM D882 | 60 % | 120 % |
For incoming quality control of Q72 rolls, film thickness is measured by beta or optical gauges calibrated to ASTM D374; tensile strength and elongation are determined by ASTM D882 using 25 mm wide strips and a jaw separation of 100 mm. Dimensional stability is assessed by unrestrained shrinkage in a circulating air oven according to ASTM D1204 at specified temperature and dwell. Surface treatment level is commonly verified by contact-angle or dyne solution testing to ASTM D2578, where corona-treated PEN film for ink or adhesive adhesion typically requires a surface energy of 40 mN/m to 48 mN/m. Thermal shrinkage in the machine direction and transverse direction should be measured separately because orientation stress can produce anisotropic shrinkage. Q72 film rolled under high tension may exhibit a small amount of residual curl after slitting; converters can measure curl with a 1 m length sample on a flat granite surface. Optical haze and clarity for display-related uses are measured by ASTM D1003, with total luminous transmittance near 88 % to 90 % for clear PEN film of typical gauge. Grade-specific values for Q72, particularly after corona treatment, may fall outside these generic ranges. Roll conformation parameters such as core inside diameter, reel hardness, and splice frequency are specified by the supplier and should be validated on the converting line to prevent web-tracking variation.
PEN films resist hydrolysis because the naphthalene-containing repeat unit reduces the frequency of hydrolysable ester bonds per unit mass relative to PET. In accelerated aging at 121 °C and 100 % RH in a laboratory autoclave, the time to reach 50 % loss of elongation for PEN is generally longer than for standard PET; published data for Q72 specifically are limited, and end-users should request aging curves from the manufacturer if the application requires exposure to pressurized steam. The hydrolysis reaction proceeds through autocatalytic acid generation, and carboxyl end-group accumulation accelerates degradation. Pre-drying at 120 °C for 4 h reduces residual moisture to below 0.01 % by Karl Fischer titration before thermal processing. The chemical resistance profile includes resistance to many aliphatic and aromatic hydrocarbons, mineral acids, and neutral aqueous solutions, but strong bases, hot concentrated acids, and certain amine-based solvents can attack the ester linkage. Q72 is not recommended for continuous immersion in methylene chloride, chloroform, or hot alkaline cleaners above pH 10. In solvent-based coating lines, prompt drying after web wetting reduces the risk of solvent-induced crystallization or surface whitening. Cleaning of rolls during splicing should avoid ketone-based agents if the film is not chemically pre-tested. The lower moisture absorption of PEN compared with PET—typically below 0.4 % by ASTM D570 after 24 h immersion—reduces the severity of hydrolysis during warm rewinding operations. Converters running Q72 in high-humidity plants should precondition rolls at 30 °C to 40 °C and 50 % RH for 24 h to 48 h before adhesive coating to reduce moisture-driven dimensional movement.
Lead-free reflow processes using SAC305 solder paste reach peak zone temperatures of 245 °C to 260 °C, which exceed the practical continuous-use ceiling of PET and approach the upper deflection limits of lower-cost polyester films. Kaladex Q72 is positioned for flexible printed circuit and membrane circuit carrier applications in which the film must survive brief thermal excursion without catastrophic distortion or outgassing. Dimensional stability for PEN film under solder float conditions is superior to PET, but the absolute shrinkage of Q72 depends on prior thermal history, gauge, and restraint during the thermal profile. Published data for this specific Q72 configuration under SAC305 reflow are limited; users should verify shrinkage and flatness using a 150 mm × 150 mm coupon exposed to a standard profile in a reflow oven fitted with thermocouple logging. The film should be pre-baked at 120 °C for 4 h to remove absorbed moisture before soldering if the reel has been stored in an uncontrolled environment, particularly above 60 % RH. For flexible printed circuit boards, dimensional change is also influenced by adhesive lamination and copper foil constraint; therefore, measurements of composite laminate movement, rather than bare film shrinkage, are required for actual design tolerance. Kaladex Q72 offers lower moisture uptake and higher glass transition temperature than PET, but it does not match the continuous-use temperature of polyimide film. For applications requiring sustained operation above 180 °C or exposure to 300 °C assembly peaks, polyimide should be evaluated. Selection of Q72 is appropriate when a converter requires a balance of solder excursion tolerance, lower cost than polyimide, and better dimensional stability than PET.
In high-tension adhesive coating and lamination, web tension must be set below the stress threshold defined by the film’s tensile modulus. The modulus of PEN film is approximately 6.2 GPa in both machine and transverse directions when measured by ASTM D882; therefore, a 100 mm wide web at 25 µm gauge cannot be assumed to respond to the same dancer loading as PET. On narrow-web slitting machines with rewind diameters above 600 mm, alternating high- and low-tension regions can produce telescoped rolls if the core does not maintain uniform grip. Pneumatic differential shafts should be specified to match the core inside diameter, and web load cells should be calibrated at the operating tension range. For rotary die-cutting lines, the sharper glass transition of PEN can cause brittle cutting behavior at low temperatures; warming the web to 25 °C to 30 °C before die stations reduces edge cracking. In solventless lamination, the film’s surface energy after corona treatment decays with storage time; converter trials on reels stored for 90 days should include dyne re-test because adhesion to polyurethane adhesives can shift after post-treatment aging. Lamination adhesive selection should avoid catalysts containing strong amines that can attack polyester linkages during long-term aging. Published data for Q72-specific shelf life and corona decay are limited; incoming adhesion tests on a pilot laminator using 2 kg/ream to 4 kg/ream coat weight are recommended before full production.
Because of its gas-barrier characteristics and thermal stability, Q72 is also evaluated in barrier-adhesive constructions and protective carrier webs. Oxygen transmission rate testing according to ASTM D3985 and water vapor transmission testing according to ASTM F1249 should be performed at the actual gauge and adhesive construction rather than inferred from film-only data. For food-contact uses, compliance must be confirmed against 21 CFR sections applicable to polyethylene naphthalate, and for electronics applications, conformance to RoHS and REACH must be documented through the supplier’s compliance declaration. These regulatory references are use-specific and do not by themselves establish fitness for a particular end use.
For electrical insulation, Q72 is evaluated by dielectric breakdown voltage per ASTM D149, volume resistivity per ASTM D257, and dimensional stability after thermal aging per IEC 60216. Values for Q72 are gauge-dependent and must be taken from the manufacturer’s UL file or certificate of compliance. Because polyethylene naphthalate has a higher glass transition temperature than PET, its retention of dielectric strength after aging at 130 °C is generally superior. However, Q72 should not be represented as a direct substitute for aramid paper or polyimide film in Class H systems without full system testing. Motor manufacturers typically require thermal aging data at 155 °C, 180 °C, and 200 °C for insulation system approval. Published data for this specific Q72 configuration is limited; requests for UL Recognized Component data should reference the specific thickness and orientation.