| HS Code | 674016 |
| Material | Biaxially oriented polyethylene naphthalate (PEN) |
| Nominal Thickness | 2.0 mil (50 µm) |
| Density | 1.36 g/cm³ |
| Tensile Strength Md | 200 MPa |
| Tensile Strength Td | 200 MPa |
| Elongation At Break Md | 110% |
| Elongation At Break Td | 100% |
| Tensile Modulus Md | 4,800 MPa |
| Tensile Modulus Td | 4,800 MPa |
| Coefficient Of Friction | 0.4 |
| Shrinkage At 150 C | 2.0% |
| Melting Point | 265°C |
| Glass Transition Temperature | 121°C |
| Continuous Service Temperature | 180°C |
| Dielectric Strength | 5,000 V/mil |
| Dielectric Constant At 1 Khz | 3.2 |
| Dissipation Factor At 1 Khz | 0.005 |
| Volume Resistivity | >1 × 10^16 Ω·cm |
| Surface Resistivity | >1 × 10^15 Ω/sq |
| Water Absorption | 0.4% |
| Haze | 2.0% |
| Refractive Index | 1.65 |
As an accredited DuPont Teijin Films Kaladex® PEN Film Q02 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DuPont Teijin Films Kaladex® PEN Film Q02 is supplied on a core in roll form, one roll per moisture-barrier-wrapped carton. |
| Container Loading (20′ FCL) | DuPont Teijin Films Kaladex® PEN Film Q02 loaded in a 20-foot FCL, palletized, dry, and secured for ocean freight. |
| Shipping | Kaladex® PEN Film Q02 is typically shipped as non-hazardous polyester film in rolls or cut sheets, protected by moisture-barrier wrap and sturdy cartons/pallets. Transport and store dry at ambient temperature, away from direct sunlight, heat, sharp edges, and static discharge; confirm classifications against the current SDS. |
| Storage | Store DuPont Teijin Films Kaladex® PEN Film Q02 in a clean, dry, well-ventilated area away from direct sunlight, heat sources, flames, and strong oxidizing agents. Keep it in its original, sealed packaging to protect against moisture, dust, and mechanical damage. Avoid sharp objects and excessive pressure. Maintain ambient temperature and inspect packaging periodically for integrity. |
| Shelf Life | Store in original packaging under cool, dry conditions; shelf life is indefinite when unopened and protected from UV, moisture, and mechanical damage. |
Competitive DuPont Teijin Films Kaladex® PEN Film Q02 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont Teijin Films Kaladex® PEN Film Q02 is a biaxially oriented poly(ethylene 2,6-naphthalate) substrate prepared from naphthalene-2,6-dicarboxylic acid and ethylene glycol. The Q02 designation denotes a one-side adhesion-promoted surface treatment intended for lamination with solventborne, waterborne, or reactive adhesives; the exact topcoat composition is proprietary and is not disclosed in standard product literature. The film is produced by sequential extrusion, length-direction stretching, transverse-direction stretching on a tenter frame, and heat-setting. Nominal gauge availability is typically listed from 12 µm to 250 µm, with 25 µm, 50 µm, 75 µm, and 125 µm being common converting grades. For 50 µm film, tensile strength at break is reported in the range of 220–280 MPa in the machine direction and 240–300 MPa in the transverse direction when tested according to ASTM D882-18 at 23 °C and 50 % RH. Elongation at break is 60–90 % in the machine direction and 50–70 % in the transverse direction. Density is 1.36 g/cm³ by ISO 1183-1:2019, and the glass transition temperature obtained by differential scanning calorimetry at 10 K/min is approximately 120 °C.
The base PEN resin before biaxial orientation typically exhibits intrinsic viscosity in the range of 0.55–0.65 dL/g in a 60/40 phenol/1,2-dichlorobenzene solvent at 25 °C. Sequential biaxial stretching is carried out with machine-direction preheat zones near 125–135 °C and transverse-direction preheat zones near 130–145 °C; the heat-set zone is held at approximately 200–220 °C to control shrinkage. The surface-treated side of Q02 is inspected for surface energy using dyne solutions per ASTM D2578-17; typical wetting after treatment is in the range of 42–46 mN/m. The higher cohesive energy density of the naphthalate ring reduces oligomer migration in polymer matrices and improves retention of adhesion after high-temperature aging at 125 °C for 500 h, although end-use peel strength must be measured according to IPC-TM-650 2.4.9 because values vary with adhesive chemistry, coating weight, and lamination pressure.
The naphthalate ring stiffens the polymer backbone and raises the glass transition to approximately 120 °C, compared with 78–80 °C for conventional poly(ethylene terephthalate). This does not provide polyimide-level thermal endurance, but it creates a measurable processing window advantage. For 50 µm film, tensile modulus in the machine direction is commonly reported between 4.8 GPa and 6.9 GPa; PET film of the same gauge is typically 3.5–4.5 GPa. The same orientation process on a tenter frame applies sequential draw ratios of approximately 3.0–3.5 : 1 in the machine direction and 3.5–4.0 : 1 in the transverse direction. These draw ratios are not unique to Q02, but they establish the crystallinity and orientation that control dimensional shrinkage. The naphthalate repeat unit also influences gas transport; at 50 µm gauge, oxygen transmission rate is generally 3.5–5.5 cm³/(m²·day·atm) at 23 °C and 50 % RH under ASTM D3985-17, whereas PET film of comparable thickness is typically 8.0–12.0 cm³/(m²·day·atm). Water vapor transmission rate is lower as well; Q02 values near 1.5–2.5 g/(m²·day) at 38 °C and 90 % RH by ASTM F1249-13 compare with 6.0–9.0 g/(m²·day) for standard PET.
| Property | Test method | Kaladex® PEN Film Q02, 50 µm typical | Biaxially oriented PET film, 50 µm typical |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 1.36 g/cm³ | 1.39 g/cm³ |
| Tensile strength, machine direction | ASTM D882-18 | 220–280 MPa | 180–220 MPa |
| Tensile strength, transverse direction | ASTM D882-18 | 240–300 MPa | 200–250 MPa |
| Elongation at break, machine direction | ASTM D882-18 | 60–90 % | 80–120 % |
| Elongation at break, transverse direction | ASTM D882-18 | 50–70 % | 70–110 % |
| Tensile modulus, machine direction | ASTM D882-18 | 4.8–6.9 GPa | 3.5–4.5 GPa |
| Tensile modulus, transverse direction | ASTM D882-18 | 5.2–7.5 GPa | 4.0–5.0 GPa |
| Thermal shrinkage, 150 °C, 30 min | ASTM D1204-14 | 1.0–1.5 % MD / 0.3–0.8 % TD | 1.5–2.5 % MD / 0.5–1.5 % TD |
| Oxygen transmission rate, 23 °C, 50 % RH | ASTM D3985-17 | 3.5–5.5 cm³/(m²·day·atm) | 8.0–12.0 cm³/(m²·day·atm) |
| Water vapor transmission rate, 38 °C, 90 % RH | ASTM F1249-13 | 1.5–2.5 g/(m²·day) | 6.0–9.0 g/(m²·day) |
| Dielectric strength, short-time | ASTM D149-20 | 220–280 kV/mm | 250–300 kV/mm |
| Volume resistivity, 23 °C | ASTM D257-14 | 1016–1017 Ω·cm | 1016–1017 Ω·cm |
| Dielectric constant, 1 kHz | ASTM D150-18 | 2.9–3.1 | 3.0–3.2 |
| Glass transition temperature | DSC, 10 K/min | 120 °C | 78–80 °C |
During roll-to-roll adhesive lamination of Q02, web tension is typically maintained between 80 N and 150 N per meter width, depending on gauge, to prevent large-scale blocking and minimize curl. Pre-drying is required when the film has been exposed to relative humidity above 60 % RH; desiccant drying for 4–6 h at 150–160 °C with a dew point below -40 °C is a standard polyester converting practice. If moisture exceeds 0.02 % before extrusion lamination, hydrolytic degradation can reduce intrinsic viscosity and create gels in the molten polymer stream. On a twin-screw extruder with L/D ratio of 30:1, melt temperatures for PEN-based compounds are commonly kept in the range of 290–315 °C. Q02 itself is not typically re-extruded; these values are relevant when Q02 is laminated to coextruded tie layers or fillers. The film can be thermoformed at mold temperatures of 150–170 °C, although deep-draw ratios are reduced compared with amorphous PET because the higher glass transition resists flow at lower draw temperatures. Cross-web thickness variation above 2–3 % tends to produce baggy edges on rewinders, which is a practical converting limitation observed on slitting lines running rolls above 1,000 m in length.
Q02 grades are used where dimensional stability under thermal stress is a pass/fail criterion. The coefficient of linear thermal expansion between 25 °C and 100 °C is approximately 15–25 ppm/°C in the machine direction and 20–30 ppm/°C in the transverse direction, measured by thermomechanical analysis; this is lower than typical PET and is one reason the film is selected for membrane touch switch spacers and flexible printed circuit stiffeners. The electrical insulation parameters are thickness-dependent. For 50 µm film, dielectric strength is typically 220–280 kV/mm when tested according to ASTM D149-20 using short-time breakdown. Volume resistivity at 23 °C is in the range of 1016–1017 Ω·cm by ASTM D257-14. Dielectric constant at 1 kHz is approximately 2.9–3.1 by ASTM D150-18. These values do not constitute insulation system approval; a finished motor, transformer, or heater assembly must be evaluated according to the relevant electrical insulation standard. The one-side treatment of Q02 produces polar groups that raise surface energy to 42–46 mN/m, but post-exposure to humid air can reduce this within days if the film is not stored in sealed polyethylene packaging. Batch-to-batch variation in surface-treated Q02 is commonly monitored by dyne solution per ASTM D2578-17 and by peel adhesion to a reference acrylic adhesive; variation greater than 2 mN/m on a treated surface typically indicates storage-induced bloom or contamination.
Q02 is specified in flexible printed circuits, membrane touch switches, and high-temperature labels where polyimide is over-specified or where PET lacks thermal margin. In these applications, the film must be tested in the final multilayer construction, because adhesive, coverlay, and stiffener layers alter the effective service temperature. For a flexible circuit base substrate, Q02 has a modulus near 5–6 GPa, which is higher than that of a typical polyimide film at 2.5 GPa, but the continuous use temperature of Q02 is lower, generally limited to 150–155 °C in air unless oxidative stabilizers or coatings are employed. This comparison means Q02 can provide a stiffer flexural platform, but not a drop-in replacement for polyimide in 260 °C solder-float requirements. When replacing PET, Q02 pushes the upper processing temperature from roughly 120 °C to 150 °C, reducing edge curl in infrared reflow at 230–250 °C. Solder-float testing at 288 °C for 10 s is not recommended for unmodified Q02 because thermal oxidative degradation and blistering can occur. Adhesive anchorage is assessed by IPC-TM-650 2.4.9 peel strength after lamination; published data for this exact Q02 laminate configuration is limited, so incoming lot qualification on a cooled laminator is required.
| Compliance dimension | Reference | Typical evaluation basis for Q02 |
|---|---|---|
| Restriction of hazardous substances | Directive 2011/65/EU, Annex II | Pb, Cd, Hg, Cr(VI), PBB, and PBDE at or below 0.1 wt%, except Cd at 0.01 wt%, subject to batch certificate. |
| Registration, evaluation, authorisation and restriction of chemicals | Regulation (EC) No 1907/2006 | Candidate List substances not intentionally added; each lot must be checked against the current SVHC list at ≥ 0.1 wt% per article. |
| Flame rating | UL 94 | Thickness-dependent; final laminated or coated Q02 construction must be tested, as thin films may yield VTM-0 or HB depending on end-use construction. |
| Thermal endurance data | UL 746B / IEC 60216 | Relative thermal index must be established on the final insulation system, not on standalone film. |
| Food-contact status | FDA 21 CFR §177.1630 | Applicable to polyethylene phthalate polymer classes; Q02 end-use compliance must be confirmed for the specific additive package and surface treatment. |
| Surface wetting | ASTM D2578-17 | Treated side typically 42–46 mN/m; lower values indicate storage humidity exposure or contamination. |
The naphthalate structure improves hydrolytic stability relative to PET, but Q02 is not immune to hydrolysis. At temperatures above 100 °C in saturated steam or in alkaline solutions with pH above 10, ester bond cleavage progresses rapidly and reduces tensile elongation. Chemical resistance testing by ASTM D543-21 should be performed for any prolonged contact with amines, strong acids, or chlorinated solvents; polyesters are susceptible to aminolysis and can undergo environmental stress cracking under restrained bending in chlorinated solvents. The film is not recommended for direct lamination to copper foils without an adhesive unless the oxide surface is treated and coated on a clean-room coater; bare metal adhesion is sensitive to copper surface chemistry and to the thickness of the treated side. For outdoor exposure, UV stabilization is required because the naphthalate chromophore absorbs strongly below 370 nm and can generate colored quinoid species upon prolonged weathering.