Dupont Teijin Films Kaladex Pen Film Pen Hv

DuPont Teijin Films Kaladex® PEN Film PEN HV

    • Product Name: DuPont Teijin Films Kaladex® PEN Film PEN HV
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 189464
    Polymer Type Polyethylene naphthalate (PEN)
    Film Orientation Biaxially oriented
    Density 1.36 g/cm³
    Melting Point 265 °C
    Glass Transition Temperature 120 °C
    Continuous Service Temperature 160 °C
    Tensile Strength 200 MPa (MD); 200 MPa (TD)
    Tensile Modulus 4,000 MPa (MD); 4,000 MPa (TD)
    Elongation At Break 90%
    Coefficient Of Linear Thermal Expansion 20 ppm/°C
    Water Absorption 0.4%
    Dielectric Constant 3.2 at 1 kHz
    Dissipation Factor 0.002 at 1 kHz
    Dielectric Strength 250 kV/mm
    Refractive Index 1.65
    Haze 1.5%

    As an accredited DuPont Teijin Films Kaladex® PEN Film PEN HV factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged as 1 kg rolls, each sealed in protective film and packed in labeled cardboard cases for safe handling and shipment.
    Container Loading (20′ FCL) DuPont Teijin Films Kaladex® PEN Film PEN HV is palletized, secured, and loaded into a dry 20-foot FCL container for shipment.
    Shipping DuPont Teijin Films Kaladex® PEN Film PEN HV is shipped as non-hazardous polyethylene naphthalate film in rolls or cartons. Keep dry and protect from moisture, contamination, impact, and excessive heat. No UN number, hazard class, or special transport label is normally required.
    Storage Store DuPont Teijin Films Kaladex® PEN Film PEN HV in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and oxidizing chemicals. Keep in original packaging, protected from moisture, dust, and mechanical damage. Avoid prolonged UV exposure and extreme temperatures. Store on stable racks or flat; do not stack heavy items. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is typically 12 months from date of manufacture when stored in original packaging under recommended conditions.
    Free Quote

    Competitive DuPont Teijin Films Kaladex® PEN Film PEN HV prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont Teijin Films supplies the biaxially oriented polyethylene naphthalate homopolymer film grade designated Kaladex® PEN Film PEN HV. The PEN HV nomenclature identifies a capacitor-grade film intended for high-voltage dielectric service; the polymer backbone replaces the terephthalate repeat unit of standard PET with a naphthalate repeat unit, introducing a fused aromatic ring that restricts segmental motion. The resulting film exhibits a higher glass transition temperature, lower fractional free volume in the amorphous regions, and greater dimensional stability at elevated temperatures than conventional biaxially oriented PET. Product-specific values for a given gauge and surface treatment are controlled by the manufacturer’s certificate of analysis; the values discussed here are representative of biaxially oriented PEN homopolymer film and should not replace the product datasheet for critical capacitor design or insulation coordination.

    The film is typically characterised according to ISO 527-3 for tensile properties of films and sheets. Representative tensile strength at break falls between 240 MPa and 300 MPa, elongation at break between 45% and 65%, and tensile modulus between 5.0 GPa and 6.5 GPa, depending on gauge, heat-setting history, and test direction. Density measured by ISO 1183-1 is approximately 1.36 g/cm³. Differential scanning calorimetry under ISO 11357-2 places the glass transition temperature near 120 °C, while the crystalline melting point is commonly reported in the range 260 °C to 270 °C. These thermal values explain the product’s use in high-temperature film capacitors, flexible circuit substrates, electrical insulation laminates, and other applications where standard PET grades show excessive shrinkage or loss of stiffness during solder attach or thermal cycling.

    How does PEN HV differ from standard PET capacitor film under thermal and electrical stress?

    Standard biaxially oriented PET capacitor film has a glass transition temperature near 78 °C; PEN HV shifts this transition to approximately 120 °C because the naphthalene unit reduces chain mobility. This shift permits lower dimensional change during high-temperature film processing and improves retention of tensile properties during short-term thermal excursions. The electrical response also changes. PEN HV typically shows a dielectric constant between 3.0 and 3.4 at 1 kHz and 23 °C, with a dissipation factor near 0.004. The lower oxygen and water vapor permeation coefficients of PEN relative to PET at equal thickness are a result of the higher barrier contribution of the naphthalene ring and altered amorphous free-volume distribution. Table 1 provides representative comparative values.

    Representative property comparison: biaxially oriented PEN HV film versus standard biaxially oriented PET film
    PropertyPEN HV representativeStandard PET filmTest basis
    Density1.36 g/cm³1.39 g/cm³ISO 1183-1
    Glass transition temperature120 °C78 °CISO 11357-2
    Tensile modulus5.5 GPa4.0 GPaISO 527-3
    Oxygen permeation0.2 × PET value1.0 × PET valueASTM D3985
    Water vapor permeation0.3 × PET value1.0 × PET valueASTM F1249
    Thermal shrinkage at 150 °C for 30 min≤0.5%1.0% to 2.0%ISO 11501

    The reduction in thermal shrinkage has practical significance in capacitor manufacturing. During winding and heat-setting of metallized capacitor elements, polyethylene terephthalate films may densify and distort, changing the wound element geometry and reducing capacitance retention. PEN HV, with shrinkage below 0.5% at 150 °C, allows a wider heat-setting window before the oriented structure relaxes excessively. This does not mean the film is a substitute for polyimide in continuous service above 200 °C. PEN HV remains a polyester and is subject to ester hydrolysis; for polyimide-level thermal endurance, a different polymer system is required.

    On converting lines, Kaladex® PEN HV is supplied as a roll and processed by slitting, metallizing, laminating, and winding. The higher tensile modulus of the film requires lower elongation setpoints during slitting and winding than PET at the same thickness. Roll storage should be conducted in sealed packaging until the film reaches the temperature of the surrounding converting room. If rolls are removed from cold storage or exposed to ambient humidity above 60% RH, condensation can create surface defects that later reduce corona adhesion or metal adhesion in vacuum metallizers. Surface energy for conversion should be verified by wetting tension testing under ASTM D2578, and the film should be processed in a controlled environment of approximately 23 °C ± 2 °C and 50% ± 5% RH unless the converter has qualified other conditions.

    Thermal and dielectric qualification of high-voltage wound capacitors

    High-voltage capacitor qualification for PEN HV normally combines thermal endurance, electrical strength, partial discharge behaviour, and defect-density control. Because the product is intended for dielectric service, incoming quality control places particular weight on pinhole count per square metre and on gauge uniformity. In production-scale metallizing, thickness variation greater than ±2% across the web can produce visible banding and non-uniform capacitance distribution in wound elements. Published product-specific data for PEN HV under long-term capacitor test profiles is limited; therefore, capacitor manufacturers validate lot performance under the relevant product standard, commonly IEC 61071 for power electronic capacitors or IEC 60384-1 for fixed capacitors.

    Dielectric strength is measured by IEC 60243-1 or ASTM D149. Dissipation factor and permittivity are determined by IEC 60250. A dissipation factor below 0.005 at 1 kHz is desirable to limit self-heating under AC ripple. During high-voltage operation, the film must avoid thermal runaway caused by dielectric loss accumulation. Surface roughness is intentionally controlled for metallized high-voltage grades because the metal adhesion and self-healing behaviour depend on the dielectric surface profile. Roughness should be measured by profilometry and correlated with metal adhesion after vacuum deposition. A film with excessively smooth dielectric surfaces may show lower metal adhesion; excessively rough surfaces may increase electrical field concentration.

    Typical qualification matrix for PEN HV as capacitor dielectric and electrical insulation substrate
    Property or requirementReference standard or regulationTypical acceptance criterion
    DC electric strengthIEC 60243-1Reported in kV/mm; lot minimum per product specification
    Dissipation factor at 1 kHzIEC 60250≤0.005
    Dielectric constant at 1 kHzIEC 602503.0 to 3.4
    Tensile strength and elongationISO 527-3Machine and transverse directions per datasheet
    Thermal shrinkageISO 11501≤0.5% at 150 °C for 30 min
    FlammabilityUL 94 VTM-0Pass at specified thin gauge
    RoHSDirective 2011/65/EU as amended by (EU) 2015/863Homogeneous material compliant by supplier declaration
    REACH SVHCRegulation (EC) No 1907/2006No SVHC above 0.1% w/w where declared

    PEN HV is not recommended where prolonged contact with water or steam above 100 °C occurs, because ester hydrolysis can degrade mechanical and dielectric properties. Strong alkalis, primary amines, and phenyl-containing solvents may attack the film surface or cause stress cracking. In particular, uncured amine-based adhesives should be avoided in direct contact with the film during elevated-temperature cure cycles; aminolysis can reduce elongation and create surface defects that lower breakdown strength. Solvent cleaning with ketones, chlorinated solvents, or terpene-based agents should be validated before production use because residual solvent can plasticise or crystallise the stressed surface. These limitations are relevant when PEN HV is laminated into flexible circuits, capacitive sensors, or motor insulation assemblies.

    When PEN HV is selected for flexible circuit substrates and electrical insulation laminates

    Flexible printed circuit manufacturing exposes substrate films to thermal lamination, adhesive bonding, and soldering. Standard PET film may be marginal for lead-free solder temperatures near 260 °C; polyimide film may be thermally excessive but costly. PEN HV occupies an intermediate thermal position. The in-plane coefficient of thermal expansion for biaxially oriented PEN is reported in the literature in the range 12 ppm/K to 20 ppm/K, depending on orientation balance and test method. This is lower than many high-shrinkage PET films and improves registration stability in multilayer flexible circuits. The film is above its glass transition temperature during solder attach, so creep under mechanical load is possible; lamination fixtures must control both temperature and tension to avoid permanent distortion.

    Electrical insulation applications use the film as slot liner material, phase insulation, or coverlay substrate. The relevant electrical standards include IEC 60664-1 for insulation coordination and IEC 60674 for plastic films used for electrical purposes. Flexible laminates may be evaluated under UL 746 for polymeric materials in electrical equipment if long-term thermal endurance is required. Product-specific RTI values for PEN HV are not reproduced here; the manufacturer’s Yellow Card or technical datasheet should be consulted for the specific thickness and laminate construction. The film should not be selected for continuous operating temperatures above 150 °C without validated aging data from the end-use insulation system.

    Compared with polyimide film, PEN HV has substantially lower water vapor permeation and lower hygroscopic expansion. This can be beneficial in high-humidity sensor packaging and thin-film photovoltaic backsheet laminates where moisture ingress must be limited. Compared with PET, PEN HV provides a higher modulus, lower oxygen permeation, and better thermal shrinkage behaviour. The trade-off is that PEN HV is typically processed at higher temperatures than PET and may require adjustment of corona discharge, lamination, and thermoforming settings. No single film grade covers every application; the selection of PEN HV is technically justified when the thermal exposure exceeds the practical working range of PET but does not require the extreme thermal endurance of polyimide.

    Specifications for the exact thickness and surface treatment selected for a production lot should be taken from the supplier’s certificate of analysis and the latest product datasheet, because the values in this webpage are representative of biaxially oriented PEN homopolymer film rather than product-specific lot data.