Dupont Sclairfilm Sl 3 Lldpe Film Laminating 76 2 µm Thickness

DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness

    • Product Name: DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 290328
    Material Type Linear Low Density Polyethylene (LLDPE)
    Thickness 76.2 µm
    Thickness Mil 3.0
    Density 0.920 g/cm³
    Tensile Strength At Break Md 31.0 MPa
    Tensile Strength At Break Td 27.6 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Elmendorf Tear Strength Md 350 g
    Elmendorf Tear Strength Td 500 g
    Haze 5%
    Gloss 85%
    Coefficient Of Friction 0.20
    Water Vapor Transmission Rate 15.5 g/m²/24h
    Oxygen Transmission Rate 2000 cm³/m²/24h
    Heat Seal Initiation Temperature 110 °C
    Melting Point 122 °C
    Vicat Softening Point 100 °C

    As an accredited DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Each package contains one roll of DuPont™ Sclairfilm® SL-3 LLDPE laminating film, 76.2 µm thick, wrapped for protection.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized rolls of DuPont™ Sclairfilm® SL-3 LLDPE laminating film, 76.2 µm, secured for transport.
    Shipping DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm, ships in original sealed rolls or cartons under clean, dry, ambient conditions. Protect from sunlight, heat, flame, moisture, punctures, and contamination. Handle carefully to prevent creasing. Unless specified, it is not classified as dangerous goods for transport.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep in original, sealed packaging to protect from dust, moisture, and contamination. Protect film from puncture, crushing, and UV exposure. Avoid contact with solvents, oils, and incompatible chemicals. Maintain moderate temperature and humidity; use stock rotation. Keep flat or on core, as recommended.
    Shelf Life Shelf life is 12 months from manufacture when stored in original packaging under cool, dry conditions, away from direct sunlight.
    Application of DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness

    In dry-bond lamination for non-aseptic food pouches, DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness is positioned as the inner sealant layer against reverse-printed BOPP, PET, or aluminium oxide-coated PET. The sealant side is corona-treated to 38-42 mN/m before the coating station. A solventless two-component polyurethane adhesive is metered by a five-roll gravure head at 1.8-2.5 g/m². Line speed is maintained between 150 and 250 m/min to avoid over-wetting the printed web. Nip temperature is held at 55-65 °C. The wound laminate is cured at 30-40 °C for 48-96 h. Heat-seal jaws close at 120-135 °C with dwell 0.3-0.6 s and pressure 300-400 kPa. The seal-strength threshold for 500-1000 g dry product pouches is typically set at or above 8 N/25 mm on production lines using ASTM F88/F88M-21. The film should not be used as the sole barrier for oxygen-sensitive products requiring an oxygen transmission rate below 1 cm³/(m²·day·bar); a metallized PET or aluminium foil ply is required. Indirect food contact is evaluated under FDA 21 CFR 177.1520(c) 3.1a and EU Regulation (EU) No 10/2011 Annex I. Overall migration must be ≤10 mg/dm² for simulated aqueous and fatty food contact. Residual solvent in the printed ply must be held below the packaging specification limit; a common upper control limit is 5 mg/m². If the adhesive is amine-catalyzed, relative humidity above 70% RH in the coating area can generate CO₂ bubbles. Solventless adhesive dew point is monitored at 18-22 °C. For retorting above 121 °C, an alternative high-temperature sealant layer is required. End products include frozen vegetable pouches, stand-up pouches for dry mixes, and dry powder side-gusset pouches.

    What Controls Seal Integrity in ISO 11607-1 Sterile Barrier Trays?

    Rigid thermoformed trays made from APET, HIPS, or PP are sealed with a multilayer lidding stock in which the film functions as the sealant layer bonded to Tyvek 1073B or medical-grade paper. The lamination step is performed on a dry-bond line using a two-component aliphatic polyurethane adhesive at 2.0-3.0 g/m². Complete adhesive conversion is verified by Fourier transform infrared absence of free isocyanate at 2270 cm⁻¹. Seal window on a rotary tray sealer is evaluated between 115 °C and 145 °C in 5 °C increments. Dwell is held at 0.8-1.2 s and pressure at 0.35-0.55 MPa. The lower limit is set by the seal initiation temperature of the LLDPE layer. The upper limit is set by the onset of tray-flange distortion and Tyvek fibre tear. In peelable configurations, seal strength per ASTM F88/F88M-21 is maintained between 1.0 N/15 mm and 3.0 N/15 mm at a 180° peel angle and 300 mm/min crosshead speed. Channel-free seals are confirmed by ASTM F1929-23 dye penetration. Any dye strike-through across the flange constitutes a reject. Sterile barrier validation follows ISO 11607-1:2019 clause 5.2. The packaged device must demonstrate seal integrity after accelerated aging at 55 °C for 60 days. Biocompatibility of the film surface is evaluated under ISO 10993-1:2018. Gamma dose mapping is required; published data for this exact configuration under gamma sterilization is limited. The acceptance matrix below is applied during installation qualification of the tray sealer.

    TestStandardValidation target
    Peelable lid seal strengthASTM F88/F88M-211.0-3.0 N/15 mm
    Dye penetrationASTM F1929-23No channel across seal area
    Gross leak detectionASTM F2096-11No continuous bubble stream at 200 kPa
    Microbial barrierISO 11607-1:2019No visible penetration

    End products include sterile barrier systems for syringes, catheters, and surgical kits. If the lidding stock is subjected to ethylene oxide sterilization, moisture pre-conditioning at 50-60% RH is required before sealing to avoid seal voids. If gamma sterilization is selected, dose mapping over 25-40 kGy must confirm no post-irradiation embrittlement of the sealant layer. The film is not a substitute for a Tyvek or paper microbial barrier ply; it provides the heat-seal function only.

    For desiccated powder pharmaceutical packaging, aluminium foil sachet lamination uses the film as the heat-seal ply bonded to 20-25 µm soft-annealed foil. The foil is pre-treated with a chromium-free conversion coating. Adhesion is developed with a retortable aliphatic polyurethane adhesive at 2.5-3.2 g/m². The laminate is cured at 40-50 °C for 7-10 days. The final sachet web is slit to widths of 80-140 mm with edge tolerance ±0.5 mm. Side-seal stations on vertical form-fill-seal machines operate at 140-160 °C. The 76.2 µm layer provides the seal-strength reserve needed for fin seals running at 60-100 cycles/min. Use of amine-terminated adhesives is avoided where the drug substance is moisture-sensitive because of potential aromatic amine migration. An EVOH barrier layer may be inserted between the foil and the sealant web. Compliance for pharmaceutical primary packaging includes USP chapter 661.1 plastic materials of construction and Ph. Eur. 3.1.3 polyolefin requirements. Dimensional stability of the printed foil is checked before lamination; the foil gauge must be uniform within ±5% to prevent tunnelling at the heat-seal station. End products include unit-dose desiccant sachets, transdermal patch overwraps, and powder drug side-seal packs. The film is not intended for terminal sterilization above 105 °C in this structure.

    Tube laminate web for high-strength side-seam sealing

    High-strength side-seam tube stock uses the film as the innermost layer over aluminium foil or EVOH barrier. The tube body is formed from a flat laminate consisting of PE/printing/paper/PE/Al/PE, with the film serving as the 76.2 µm inner PE layer. The film is adhesive-laminated to the foil with an anhydride-grafted tie resin applied at 3.0-4.0 g/m². Hot-air side-seam welding is performed at an air temperature of 390-410 °C. The LLDPE layer must have a low gel count and consistent melt flow to prevent pinholes at the welded overlap. Tube flattening and end-sealing use jaws at 160-190 °C. The thicker sealant layer increases heat sink, so dwell time is extended by 0.2-0.4 s compared with 50 µm sealant films. Leak testing per ASTM D3078-02 is performed at 40 kPa vacuum; no bubble stream indicates side-seam integrity. Compliance with EU Regulation (EU) No 10/2011 is documented through migration testing for semi-fatty and aqueous simulants. The film alone does not provide aluminium or EVOH barrier performance. End products include abrasion-resistant toothpaste tubes, barrier tubes for industrial adhesives, and cosmetic cream tubes.

    Building insulation facings require a low-permeance vapour retarder tie

    On a 1,200 mm extrusion coater, a tri-directional fiberglass scrim or aluminium foil facing is bonded to the film. The laminating tie is a LDPE resin extruded at melt temperature 310-325 °C through a die gap of 0.6-0.8 mm. The air gap from die exit to nip is 150-200 mm. Line speed is 100-180 m/min. The foil or scrim side is flame-treated to 42-46 mN/m before coating. T-peel adhesion is measured by ASTM D1876-08; adhesion below 1.5 N/15 mm after 24 h is treated as a lamination defect. The 76.2 µm gauge is selected for puncture and tear resistance during crawl-space installation. Puncture resistance of the finished facing is evaluated by ASTM D751-19. The finished laminate must meet the flame-spread index and smoke-developed index specified by the applicable mechanical code under ASTM E84-23. Compliance with ASTM C1136-21 for flexible, low-permeance vapour retarders applies to the finished facing, not the film alone. Avoid amine-based inks on the foil side because they can reduce interlayer adhesion after thermo-humidity aging at 90% RH and 60 °C. End products include radiant barrier facings, concrete slab vapour retarders, and pipe wrap laminates.

    When closed-cell polyolefin foam cores are joined to decorative nonwoven facings

    For door panel and instrument panel soft-skin laminates, the film is used as an adhesion-promoting interlayer or as a backside sealing film on polyolefin foam cores. The process uses a heated nip laminator. Nip temperature is 110-130 °C, line speed is 8-15 m/min, and nip pressure is 2.5-4.0 bar. If acoustic porosity is required, the film is micro-perforated offline on a hot-needle perforator. Hole density is adjusted between 40 and 60 holes/cm² depending on the target airflow resistance. Adhesion is measured by ASTM D1876-08 T-peel after 72 h at 23 °C and 50% RH. Flammability is tested per ISO 3795:1989; burn rate must fall below the 100 mm/min threshold prescribed by the interior material specification. Fogging is tested per ISO 6452:2021 to the OEM-specified condensate mass limit. The 76.2 µm thickness alters the thermoforming gradient relative to 50 µm interlayers, so line trials are required before full-rate production. Published data for this specific configuration is limited. End products include door panel soft inserts, console armrests, and parcel shelf coverings.

    Free Quote

    Competitive DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness is a monolayer linear low-density polyethylene web supplied in roll form for adhesive lamination, thermal overlamination, and protective surface lamination. The numeric suffix in the product designation corresponds to a nominal thickness of 0.0030 in, which equals 76.2 µm and is frequently described as a 3.0 mil gauge. The product is used as a tough sealant-web or overlaminate layer in flexible packaging and graphic structures. Because public datasheets for this specific DuPont product are limited, processing ranges in this text are drawn from the behavior of 76.2 µm LLDPE laminating webs of similar ethylene/alpha-olefin copolymer composition and should be checked against the roll certificate of analysis. Film thickness is commonly verified by ASTM D5947 or ISO 4593, and the polymer density by ASTM D1505 or ISO 1183-1.

    The laminating grade is normally supplied as slit rolls, and slitting edge quality is controlled to prevent dust generation during high-speed lamination. Roll widths and core dimensions are converter-specific. The web is not an oxygen or moisture barrier; in barrier laminates it is combined with aluminum foil, metallized polyester, or PVDC-coated films, where the LLDPE layer contributes puncture resistance, flex-crack resistance, and heat-seal function rather than gas-barrier performance.

    What Limits Seal Initiation and Hot Tack in 76.2 µm LLDPE Laminating Webs?

    Seal initiation in LLDPE laminating webs is determined by the melting onset and by the time-dependent re-crystallization of the polyethylene chain segments at the sealing interface. Differential scanning calorimetry per ASTM D3418 typically places the main melting peak of a butene-copolymer LLDPE between 118°C and 126°C. The practical seal initiation temperature, however, is lower because only the interfacial zone must reach the molten state. In rotary jaw sealing equipment, 76.2 µm LLDPE films of this class generally show seal initiation between 95°C and 115°C at dwell times of 0.5–1.5 s and jaw pressures of 200–400 kPa. Hot tack becomes the limiting factor on vertical form-fill-seal lines where dwell times fall below 0.3 s; the seal is mechanically loaded before molten polymer has re-crystallized, producing peel failures at the seal edge. Production lines with eccentric jaw temperature profiling may need to offset the trailing jaw by 5–10°C to compensate for heat loss at high cycling rates.

    For dry lamination, the SL-3 web is not sealed directly before bonding; it is adhered to a substrate with a two-component polyurethane or solventless adhesive. The lamination nip temperature must remain below the seal initiation threshold to prevent blocking. Typical tandem laminating lines run the laminating nip at 70–90°C. Above 95°C, local film softening can produce gauge bands and chatter marks on polished rolls, especially when incoming web tension exceeds 80 N per meter. This defines the upper processing boundary; the lower boundary is governed by adhesive wetting and is discussed in the corona treatment section.

    In dry lamination, the adhesive coat weight applied to the LLDPE web is typically 2.0–4.5 g/m² for solventless systems and 2.5–5.0 g/m² for solvent-based polyurethane adhesives per laminating machine supplier settings. Heavier coatings increase the risk that the adhesive penetrates gauge bands or oxidized surfaces, but coating weights above 5.0 g/m² can plasticize the interfacial zone and reduce heat-seal strength after cure. This interaction should be tested after 24–48 h at 40–50°C cure because two-component polyurethane adhesion continues to develop after initial winding.

    Adhesion to two-component polyurethane laminating adhesives depends on surface oxidation. A fresh corona-treated 76.2 µm LLDPE web typically exhibits wetting tension between 38 mN/m and 44 mN/m per ASTM D2578. Values below 36 mN/m are not recommended for solventless adhesive systems because incomplete surface spreading leaves microvoids that become delamination initiation sites. The treatment should be measured on both edges and center of the web after slitting; edge loss is common because corona discharge is weaker near the electrode ends.

    When Sclairfilm® SL-3 Replaces LDPE Sealant Webs in Dry Lamination

    Substitution of a 76.2 µm LLDPE web for an equal-thickness LDPE sealant web changes the failure mode of the finished laminate. LLDPE has a higher density of tie molecules, which raises tensile and tear resistance compared with high-pressure LDPE at the same gauge. Under ASTM D882 tensile testing, 76.2 µm LLDPE laminating films of the SL-3 class commonly show machine-direction tensile strength in the range of 25–45 MPa, whereas LDPE laminating films of the same thickness typically fall between 15–25 MPa. Elmendorf tear values per ASTM D1922 are also higher, generally 300–700 g for LLDPE versus 100–300 g for LDPE. In flexible packaging lines, this change reduces pinholing after flex testing per ASTM F392, particularly in corner folds of stand-up pouches. The same substitution may increase heat-seal temperature by 5–15°C, which should be validated on the fill-seal machine before changing suppliers.

    Property Test method SL-3 LLDPE class (76.2 µm) LDPE laminating film (76.2 µm) Cast LLDPE laminating film (76.2 µm)
    Density ASTM D1505 0.918–0.924 g/cm³ 0.916–0.922 g/cm³ 0.917–0.925 g/cm³
    Melt flow index ISO 1133-1 0.8–1.2 g/10 min 0.5–2.0 g/10 min 1.0–2.0 g/10 min
    Tensile strength MD ASTM D882 25–45 MPa 15–25 MPa 20–40 MPa
    Elongation at break MD ASTM D882 500–800% 200–500% 400–700%
    Elmendorf tear MD ASTM D1922 300–700 g 100–300 g 200–600 g
    Haze ASTM D1003 4–10% 5–12% 1–5%
    Seal initiation ASTM F1921 95–115°C 85–105°C 95–115°C

    The above table contains representative industrial ranges for 76.2 µm webs and is not a substitute for the Sclairfilm® SL-3 certificate of analysis. Product-specific data should be requested from the supplier for each intended lamination structure.

    Compared with biaxially oriented polypropylene laminating films of similar gauge, Sclairfilm® SL-3 provides lower tensile modulus and greater elongation. Biaxially oriented polypropylene has a modulus in the range of 2,000–3,500 MPa, while 76.2 µm LLDPE film is typically below 500 MPa. This difference is relevant in pouch corner folds: the LLDPE web absorbs strain by yielding, whereas BOPP may form stress whitening or pinholes after repeated flexing. The trade-off is clarity; BOPP generally shows haze below 3%, while LLDPE blown films show higher haze.

    Surface Treatment Decay and Corona Re-Treatment Limits

    Corona treatment on polyolefin webs decays with time. For a treated 76.2 µm LLDPE laminating film stored at 20–25°C and 40–60% RH, wetting tension may decline by 2–4 mN/m within the first 30 days. Rolls stored beyond this period should be re-qualified by ASTM D2578. On-machine re-treatment is possible but is limited by the generator capacity and electrode condition. Laminating lines equipped with ceramic electrodes and corona discharge generators rated at 2–5 kW per meter of web width are typically able to restore surface wetting tension at line speeds of 50–150 m/min. Above 5 kW per meter, the risk of backside treatment, pinholes, and thermal wrinkling increases because the 76.2 µm gauge has lower thermal inertia than thicker laminating webs. Grounded backup rollers and ozone extraction are mandatory to prevent oxidation variability and workplace exposure.

    Blocking resistance and coefficient of friction are also affected by surface treatment and film additives. LLDPE laminating films of this gauge often list a static coefficient of friction between 0.30 and 0.60 per ISO 8295 or ASTM D1894, depending on slip additive package. Uncontrolled re-treatment can consume surface slip additives and raise the coefficient of friction above 0.70, causing poor film transport through folding boards and sealing jaws.

    Thickness Uniformity and Roll Winding Tension Are Controlled Separately

    Cross-web thickness variation should be held within ±5% of nominal for stable adhesive coat weight and visual uniformity. Hard band formation in wound rolls occurs when one edge exceeds the other by more than 3–4 µm. On converting lines, roll winding tension for 76.2 µm LLDPE usually falls between 40 N and 80 N per meter of web width; the tension should be reduced as roll diameter increases to avoid blocking and telescoping. Values above 100 N per meter can stretch the web enough to change its registration in overlamination and increase edge tear sensitivity.

    A thickness variation of ±5% around 76.2 µm corresponds to a basis weight variation of roughly ±3.5 g/m². In laminating plants with automatic gravure coaters, this variation can produce alternating adhesive-starved and adhesive-rich bands if the coating head is run in fixed-gap mode. This is more critical for solventless systems, which do not have solvent to level the adhesive film. Maintaining the web flatness and roll hardness profile within the supplier-defined range is therefore necessary before lamination.

    Cast LLDPE alternatives can provide lower haze and higher gloss than blown LLDPE at the same gauge. ASTM D1003 haze values below 5% are common for cast webs, whereas blown LLDPE of the SL-3 class may fall between 4% and 10%. Therefore, if optical clarity through a window is the main requirement, a cast LLDPE may be selected; if tear and puncture resistance dominate, the SL-3 LLDPE class tends to retain advantage over LDPE. Published data for the exact Sclairfilm® SL-3 optical configuration is limited, and roll-specific values should be obtained from the certificate of analysis.

    In thermal overlamination of paper and board, the 76.2 µm LLDPE web is processed through heated nip rolls. Temperature settings of 90–110°C at line speeds of 10–40 m/min are common for polyolefin thermal lamination, but polyethylene alone does not always bond to unprimed paper; an adhesive pre-coating or corona treatment of the board is generally required. The SL-3 film supplies toughness and gloss retention, while the paper or board carries dimensional stability. The lower flexural stiffness of LLDPE compared with biaxially oriented polyester laminates means the structure will remain conformable but will not add dead-fold properties.

    Food-contact and chemical compliance are application-specific. LLDPE films used in direct food contact are evaluated under FDA 21 CFR 177.1520 in the United States and under EU Regulation 10/2011 in the European Union. The overall migration limit under EU Regulation 10/2011 is 10 mg/dm² for general food contact, but the actual test conditions depend on the food simulant and temperature. Compliance for a particular laminate cannot be assigned to the film alone; it includes the adhesive, substrate, and cure state. REACH Regulation EC 1907/2006 SVHC screening and RoHS Directive 2011/65/EU restrictions are evaluated only where the end application falls under the relevant scope. A written supplier declaration should be obtained for each production batch.

    Regulatory instrument Scope Condition for Sclairfilm® SL-3 use
    FDA 21 CFR 177.1520 Olefin polymers in food contact Finished film must meet density and extractables limits; supplier declaration required
    EU Regulation 10/2011 Plastic food-contact materials Migration testing under intended food simulant and time/temperature
    REACH EC 1907/2006 SVHC screening Batch-level SVHC declaration required
    RoHS Directive 2011/65/EU EEE restricted substances Applies only when incorporated into electrical/electronic equipment

    The SL-3 web should not be exposed to strong oxidizing agents, aromatic solvents, or mineral oils at elevated temperatures; polyethylene swells and may stress-crack under these conditions. Avoid adhesive formulations containing free amine additives unless the system is specifically qualified for corona-treated polyolefins, because residual amine species can reduce interfacial adhesion. Pre-drying is not required under normal storage of RH < 60%, but rolls exposed to humidity above 60% RH should be conditioned at 25–30°C for 12–24 h before lamination to remove condensation from the roll edges.

    Top