Dupont Sclairfilm Sl 3 Lldpe Film Laminating 50 8 µm Thickness

DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 50.8 µm Thickness

    • Product Name: DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 50.8 µm Thickness
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 631073
    Material Type Linear Low Density Polyethylene (LLDPE)
    Film Type Laminating
    Thickness 50.8 µm
    Density 0.922 g/cm³
    Tensile Strength Md 31 MPa
    Tensile Strength Td 28 MPa
    Tensile Modulus 0.200 GPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Tear Strength Md 200 g
    Tear Strength Td 400 g
    Dart Drop Impact 150 g
    Haze 15%
    Gloss 45 50%
    Coefficient Of Friction 0.20
    Heat Seal Initiation Temperature 110°C
    Water Vapor Transmission Rate 0.5 g/100 in²/day
    Oxygen Transmission Rate 200 cc/100 in²/day

    As an accredited DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 50.8 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged as a single roll in a protective carton; 50.8 µm Sclairfilm SL-3 LLDPE laminating film. Quantity: 1 roll.
    Container Loading (20′ FCL) Container loading (20′ FCL): DuPont™ Sclairfilm® SL-3 LLDPE laminating film, 50.8 µm, palletized rolls, dry ambient conditions, securely stowed.
    Shipping DuPont Sclairfilm SL-3 LLDPE laminating film is shipped as rolls on cores, palletized and stretch-wrapped in moisture-barrier packaging. Transport in clean, dry vehicles at ambient temperature, away from direct sunlight, heat, and sharp objects. Non-hazardous; no special dangerous goods placarding required. Store upright, protect from compression and contamination.
    Storage Store DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 50.8 µm Thickness in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and incompatible chemicals. Keep in original packaging, protected from dust, moisture, and physical damage. Maintain ambient temperature/humidity; avoid crushing rolls. Use proper labeling and stock rotation. Do not expose to UV or excessive heat.
    Shelf Life Shelf life is typically 12 months when stored in original packaging in a cool, dry area, away from direct sunlight.
    Application of DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 50.8 µm Thickness

    Laminating a reverse-printed BOPET web to 50.8 µm Sclairfilm® SL-3 on a solventless line uses a two-component polyurethane adhesive at a dry coat weight of 2.0–3.5 g/m². The SL-3 surface is corona-treated to 38–42 mN/m measured by ASTM D2578 immediately before adhesive application. A polyol-to-isocyanate ratio of 100:50 to 100:75 by volume is typical for high-slip laminating films, but the adhesive supplier’s mixing protocol takes precedence. The laminate is run at 300–450 m/min, wound with controlled tension, and cured at 35–45°C for 24–48 h. Cure completion is checked by ply adhesion per ASTM F904-16. The sealant web is later cut and sealed against the reverse-printed outer ply on horizontal or vertical packaging machines. Seal-jaw settings of 115–145°C, 0.5–1.0 s dwell, and 200–400 N bar force are typical starting points. The end product is a high-barrier pouch for dried foods, snack powders, or powdered beverage mixes. Food-contact status is based on FDA 21 CFR 177.1520 for the polyolefin film and Regulation (EU) No 10/2011 for EU sales. Overall migration must not exceed 10 mg/dm² under the test conditions specified in EN 1186-1. The main process conflict is slip-additive migration from the LLDPE sealant web into the uncured solventless adhesive. This can depress bond strength. Slot-die adhesive application and nitrogen-inerted lamination reduce moisture uptake and amine blush.

    What Limits Hot Tack on High-Speed VFFS Lines When 50.8 µm SL-3 Is the Sealant Web?

    In vertical form-fill-seal converting, the seal bar opens before the LLDPE melt has recrystallized. Hot tack force determined by ASTM F1921-18 at 0.1–0.5 s dwell and 0.5–1.0 N/mm² sealing pressure is the controlling parameter. A typical LLDPE grade enters a useful hot tack plateau between 90°C and 110°C. Published data for this specific Sclairfilm® SL-3 configuration is limited, so the plateau should be mapped on the production line. The forming collar requires a kinetic coefficient of friction below 0.40 measured by ASTM D1894. If the slip additive package lowers the coefficient of friction below 0.20, solventless lamination bonds can fall. This is a known process conflict. The film is sealed at 125–160°C, with dwell times below 0.3 s at line speeds above 60 cycles/min. The laminate structure is often reverse-printed BOPP or BOPET outer web, adhesive, and 50.8 µm SL-3 sealant web. The end product includes frozen vegetable bags, pre-cooked seafood pouches, and ice cream overwrap. Seal strength after freezer conditioning is measured by ASTM F88/F88M-23 at 15 mm jaw width and 300 mm/min crosshead speed. Food-contact compliance mirrors the dry-food laminate segment. The operational boundary is that LLDPE hot tack is lower than ionomer or metallocene sealant resins. Heavier product tare weights require longer cooling or a thicker sealant layer.

    Medical pouch converting with uncoated Tyvek 1073B uses Sclairfilm® SL-3 as the sealant ply laminated to a 12 µm polyester outer ply. The laminate is typically constructed as PET 12 µm / adhesive / 50.8 µm SL-3. A rotary tray sealer seals the LLDPE surface to the uncoated Tyvek side. Seal settings of 120–135°C, 60–100 psi platen pressure, and 0.5–1.5 s dwell are common starting points for 50.8 µm LLDPE sealant film. Exact values are set during operational qualification. Seal strength is tested by ASTM F88/F88M-23 with a 15 mm specimen width. Channel defects are detected by dye penetration per ASTM F1929-15. The package system is validated under ISO 11607-1:2019 and ISO 11607-2:2019. Sterilization through ethylene oxide is preferable. Gamma irradiation above 25 kGy can shift additive behavior, increase yellowness, and embrittle the LLDPE surface. Published data for Sclairfilm® SL-3 radiation tolerance is limited. For patient-contact devices, cytotoxicity is evaluated by ISO 10993-5. Pharmaceutical packaging components may require USP <661.1> testing. The end products are terminally sterilized pouches for catheters, syringes, surgical instruments, and single-use device kits. The operational boundary is particulate control. The film is converted in a cleanroom environment to avoid fibre contamination on the sealant side.

    Extrusion Lamination of 9 µm Aluminium Foil to SL-3 as the Secondary Web

    On a tandem extrusion-coating line, the aluminium foil is corona-treated and frequently primed with an ethylene acrylic acid copolymer at 0.1–0.3 g/m². The Sclairfilm® SL-3 web is not extrusion-coated; it is unwound as the secondary substrate. The structure is BOPET 12 µm / print / adhesive / 9 µm foil / LDPE 15–25 µm / 50.8 µm SL-3. The LDPE melt curtain is extruded at 315–325°C die-lip temperature, with an air gap of 15–25 cm to promote oxidative adhesion to the foil and the SL-3 web. Line speed is typically 100–200 m/min for foil laminates. The end product is a high-barrier pouch for powdered beverages, seasonings, or pet food. Ply adhesion is measured by ASTM F904-16. The food-contact obligation for the SL-3 web is FDA 21 CFR 177.1520. The total laminate must also be evaluated for overall migration under Regulation (EU) No 10/2011. The primary process conflict is that low-density polyethylene gives better melt strength than LLDPE in the melt curtain. LLDPE is therefore confined to the secondary web. Foil pinhole formation is controlled by proper tension isolation and 9 µm foil quality. The film’s slip additive can migrate to the outside surface during wind-up. If the laminate is shipped before full cooling, blocking can occur.

    SegmentRegulation or standardClause or methodControlled variable
    Dry food laminateFDA 21 CFR 177.1520Olefin polymer clearanceFood-contact status
    EU food contactRegulation (EU) No 10/2011Annex I, EN 1186-1Overall migration 10 mg/dm²
    Seal strengthASTM F88/F88M-2315 mm width, 300 mm/minHeat-seal integrity
    Hot tackASTM F1921-180.1–0.5 s dwell, 0.5–1.0 N/mm²Hot tack force
    Corona treatASTM D2578Wetting tension38–42 mN/m
    Medical packageISO 11607-1:2019Clause 5Package system validation
    WVTRASTM E96/E96M-2238°C, 90% RHBarrier moisture vapour transmission

    When 50.8 µm SL-3 Is Laminated to Scrim-Reinforced Foil in HVAC Facing Stock

    Glass-fibre scrim reinforced facing stock uses Sclairfilm® SL-3 as the exposed moisture-barrier ply and the aluminium foil as the radiant-barrier ply. A flame-retardant hot-melt adhesive is slot-die coated at 12–20 g/m² between the foil-scrim substrate and the LLDPE web. The laminate is passed through a chilled nip at 10–15°C to stabilize dimensions. Water vapour transmission is measured by ASTM E96/E96M-22 at 38°C and 90% RH. The foil-scrim component controls the barrier. The SL-3 layer contributes puncture resistance and moisture protection at the outer surface. The end product is duct wrap facing, pipe insulation jacket stock, and building-envelope vapor retarder. The laminate must withstand spiral duct forming rolls and repeated flexing without delamination. Ply adhesion after 24 h ageing is checked by ASTM F904-16. Surface burning characteristics are not inherent to the film. If the finished facing stock is installed in a plenum space, the complete laminate must be tested under ASTM E84 by the downstream fabricator. Continuous service above 60°C is outside the expected window for a LLDPE laminating film. The material is not intended for autoclave service or sustained hot-melt exposure above 100°C.

    In refrigerated liquid pouch converting, the sealant layer is exposed to product residues during sealing. Sclairfilm® SL-3 is used as the inner web in a two-ply laminate with BOPET or BOPP outer ply. The structure is 12 µm BOPET / adhesive / 50.8 µm SL-3. Seal-through-contamination performance is evaluated by filling pouches to 95% with a defined aqueous test fluid and measuring seal strength after cooling. Seal-jaw settings of 130–160°C, 1.0–2.0 s dwell, and 300–500 N bar force are typical for LLDPE. Published data for Sclairfilm® SL-3 in contaminated-seal configurations is limited. The end product includes refrigerated condiment sachets, dairy creamer pouches, and liquid soap refill packs. Seal creep under pasteurization temperatures above 85°C must be checked before hot-fill use. Low-temperature impact resistance after filling is measured by ASTM D1709. Food-contact compliance is based on FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011. The operational boundary is that high levels of erucamide can reduce surface tension and compromise lamination bond. Corona treatment must be completed within 24 h before adhesive coating. The sealant layer must also resist stress cracking when filled with surfactant-based liquid products.

    Free Quote

    Competitive DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 50.8 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont™ Sclairfilm® SL-3 is a monolayer linear low-density polyethylene film supplied at a nominal thickness of 50.8 µm (2.0 mil) for laminating applications. The product designation identifies a laminating-grade web rather than a shrink or high-barrier web. In flexible packaging constructions, the film is typically positioned as the inner sealant layer behind a printed biaxially oriented polypropylene or polyethylene terephthalate outer web, or behind aluminium foil and paper in duplex and triplex laminations. The laminating classification indicates that the film is intended for conversion by dry-bond, solventless, or extrusion lamination rather than direct printing or tape applications. The base polyolefin class is normally evaluated for food-contact suitability under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011; finished-structure compliance depends on the adhesive, ink, and lamination process as well as the film lot. Published data for this specific SL-3 configuration is more limited than generic data for commercial 50.8 µm LLDPE laminating films, so certificate-of-analysis values should govern lot acceptance.

    The film is not a barrier layer. Oxygen and water-vapour transmission are controlled by the selected outer web, foil, or coating; the SL-3 layer contributes heat sealability, flex-crack resistance, and puncture toughness to the finished laminate. Because the film is semicrystalline with a low glass-transition temperature, it remains flexible in refrigerated and frozen storage, but sustained exposure above 80–90 °C can produce dimensional change and blocking.

    What Is Supplied with the 50.8 µm Sclairfilm SL-3 Laminating Web?

    Roll-stock configuration for SL-3 follows conventional laminating-web practice. The film is supplied as parent rolls or converter rolls on 76 mm (3.0 in) or 152 mm (6.0 in) fibre cores, with the treated side identified by core label or edge mark. Width is normally supplied to the converter’s slitting requirement; slit-edge quality and roll hardness should be specified in the purchase order. Thickness capability is measured using ASTM D5947-18, and commercial polyolefin laminating films in this gauge are frequently controlled within ±5% of nominal, although the supplier’s technical datasheet is the governing document. The linear low-density polyethylene base resin typically exhibits a density of 0.918–0.930 g/cm³ when tested by ISO 1183-1:2019 or ASTM D1505-18. From this range and a nominal thickness of 50.8 µm, the calculated basis weight is approximately 46.6–47.2 g/m², giving a theoretical yield of approximately 21.2–21.4 m²/kg. Yield should be confirmed against roll-length measurement rather than assumed from nominal values.

    Tensile strength at break for commercial 50.8 µm LLDPE laminating films measured by ASTM D882-18 commonly falls in the range of 30–50 MPa in the machine direction and 25–45 MPa in the transverse direction. Elongation at break often ranges from 500% to 900%, depending on molecular architecture, orientation, and additive package. Elmendorf tear resistance by ASTM D1922-15 is typically 2.5–6.0 N, and dart impact by ASTM D1709-16a Method A may fall between 150 g and 400 g. These values are representative of commercial linear low-density polyethylene laminating film and are not product-specific release limits.

    Surface Preparation, Adhesive Compatibility, and Lamination Line Handling

    In dry-bond and solventless lamination, the SL-3 web functions as the secondary or sealant substrate. For adhesive wet-out, the treated surface should maintain a wetting tension of at least 38 mN/m; many converters specify an upper limit of 42 mN/m to limit surface oxidation and potential heat-seal deterioration. Treatment level is checked by ASTM D2578-17 or ISO 8296:1987 using formamide/ethylene glycol test fluids. Repeated testing on the same area should be avoided because the test fluids can contaminate the surface and create false readings.

    Roll stock should be allowed to equilibrate to pressroom temperature for at least 24 h after transport from cold storage. Failure to acclimatise can produce baggy edges, uneven unwind tension, and tunnelling after lamination. Web tension for a 50.8 µm LLDPE web is usually run below the tension used for PET or foil because the lower modulus of polyethylene can cause permanent elongation and cold flow. Tension settings in the range of 9–15 N/m of web width are often used as a starting point for polyethylene laminating films of this gauge, but the actual value must be adjusted for roll width, unwind diameter, line speed, and the presence of an in-line corona re-treatment station. Electrostatic discharge control and edge trimming are important because thin LLDPE films can attract contamination and develop edge tears at high speed.

    Solvent-based polyurethane adhesives, solventless polyurethane systems, and acrylic laminating adhesives are commonly used with polyolefin laminating webs. The treated surface is designed to provide polar sites for adhesive bonding; however, corona treatment decay is a known operational boundary. If wetting tension falls below 38 mN/m, in-line corona re-treatment is often required immediately before coating or lamination. Interlayer adhesion after lamination is typically measured by T-peel testing according to ASTM D1876-08, and destruct tests should be checked after the adhesive has fully cured. Slip additive bloom influences coefficient of friction over time, so kinetic COF measured by ASTM D1894-14 should be remeasured after 24 h and 7 days because migration kinetics can shift surface friction. Packaging lines that depend on film-to-metal or film-to-film friction should specify a COF window rather than a single point.

    For extrusion lamination, the film is normally used as the secondary substrate. The molten polyethylene or adhesive tie layer is applied against the treated side. The thermoplastic nature of LLDPE requires that the cooling-roll setting and unwind path avoid surface temperatures above 80–90 °C during extended dwell, because blocking and dimensional distortion may occur. Surface resistivity of polyethylene films is generally high, often above 1×1013 Ω/square when measured by ASTM D257-14, so static control should be considered as part of the laminating line setup.

    When This LLDPE Film Replaces High-Pressure LDPE in Lamination Structures

    When a converter replaces a 50.8 µm high-pressure low-density polyethylene laminating web with the same gauge SL-3 LLDPE film, the primary technical difference is the linear polymer backbone and its effect on mechanical properties. LLDPE typically develops higher tensile strength, tear resistance, and puncture resistance at equivalent gauge than high-pressure LDPE. This permits downgauging in some flexible packaging structures, provided that the packaging line’s seal parameters are revalidated. The heat-seal initiation temperature of LLDPE laminating films is generally in the range of 105–120 °C as measured by gradient seal methods based on ASTM F2029-16 or ASTM F1921-12. High-pressure LDPE may seal at slightly lower temperatures, so jaw temperature and dwell-time settings must be re-established when substituting SL-3.

    Compared with metallocene-catalysed LLDPE film grades, Sclairfilm SL-3 is generally positioned as a conventional linear low-density polyethylene laminating web. Metallocene grades can provide a broader hot-tack window and lower seal initiation, but they may also require more precise temperature control and may exhibit different coefficient-of-friction behaviour. SL-3 should not be assumed to match a metallocene film’s hot-tack profile without side-by-side testing on the same form-fill-seal equipment. Similarly, compared with coextruded three-layer laminating films containing a metallocene sealant skin, a monolayer LLDPE web may have a narrower seal range but lower material complexity.

    Flex-crack resistance is another differentiator in pouch applications. Gelbo flex testing according to ASTM F392-20 can be used to compare the pinholing behaviour of laminates made with LLDPE sealant webs against those made with LDPE. LLDPE sealant films generally exhibit lower pinhole formation after repeated flexing, which is the technical basis for selecting SL-3 in pouches that experience high stress during distribution. The laminate’s overall flex-crack performance is also influenced by the outer web and adhesive, so the test should be conducted on the finished structure rather than on the film alone.

    Seal strength of the finished laminate is measured by ASTM F88/F88M-15. Acceptable seal-strength values vary by package type, but many flexible packaging operations require minimum seal strengths of 10–25 N/25 mm for dry food pouches. Because the SL-3 web is a heat-sealable layer, jaw temperature, pressure, and dwell are the controlling variables. For LLDPE, the upper end of the sealing range is often limited by melt distortion rather than by film degradation; temperatures above approximately 130–135 °C can produce edge stringing and jaw contamination. Heat-seal testing should be conducted after 24 h conditioning at 23 ± 2 °C and 50 ± 5% RH in accordance with ASTM D618-21.

    Representative Property Ranges and Incoming Inspection Matrix

    Because lot-to-lot variation and additive package influence final values, the following table consolidates representative ranges for commercial 50.8 µm LLDPE laminating films. These values are not to be read as certificate-of-analysis limits for SL-3; they provide an engineering reference for initial feasibility studies and should be replaced with supplier data before production.

    Property Test method Representative range Engineering note
    Thickness ASTM D5947-18 50.8 µm nominal; common commercial tolerance ±5% Verify profile across web; not a single-centre reading.
    Density ISO 1183-1:2019 / ASTM D1505-18 0.918–0.930 g/cm³ Used for yield and basis-weight calculation.
    Calculated yield From density and thickness 21.2–21.4 m²/kg Confirm against roll-length measurement.
    Tensile strength at break, MD ASTM D882-18 30–50 MPa Higher than LDPE at equal gauge; supports downgauging.
    Elongation at break, MD ASTM D882-18 500–900% Provides conformability and puncture resistance.
    Elmendorf tear ASTM D1922-15 2.5–6.0 N MD/TD imbalance influences zippered-pouch tear propagation.
    Dart impact ASTM D1709-16a Method A 150–400 g Method selection must match expected impact level.
    Kinetic COF ASTM D1894-14 0.20–0.55 Slip bloom kinetics require remeasurement at 24 h and 7 days.
    Wetting tension, treated side ASTM D2578-17 38–42 mN/m Below 38 mN/m may require in-line re-treatment.

    Incoming inspection for the laminating web should be based on the following control points. The supplier’s certificate of analysis is the authoritative document for release testing.

    Control point Method or instrumentation Typical control window Failure response
    Treated-side wetting tension ASTM D2578-17 / ISO 8296:1987 dyne pens ≥38 mN/m Quarantine for possible re-treatment or supplier disposition.
    Gauge profile Capacitance gauge or micrometer per ASTM D5947-18 ±5% of nominal 50.8 µm Reject rolls with hard bands or thinning.
    Roll hardness and edge alignment Shore durometer, visual edge inspection Uniform hardness; no telescoped edges Flag for converting department; may cause lamination tunnels.
    Roll width and core ID Calibrated steel tape, core gauge As purchase order; common cores 76 mm or 152 mm Return non-conforming rolls to slitting.
    COF ASTM D1894-14 As specified; often 0.20–0.55 Hold for packaging-line trial if out of window.
    Surface defects Online camera or strobe inspection No gels, scratches, or adhesive contamination Sort or downgrade.

    Adhesive selection for SL-3 structures should begin with a lamination audit on the actual line rather than a table value. Because the film is a polyolefin, solvent-based primers are not normally required if the corona-treated surface is within specification; however, reverse-printed substrates may require a primer on the film when laminating to certain solventless systems. Retained solvent and outgassing should be monitored because the film’s low glass-transition temperature does not prevent migration of low-molecular-weight fractions from adhesive or ink.

    Field data from polyolefin laminating lines indicate that the most common process failures are treatment decay, static-induced contamination, baggy edges after poor ambient acclimatisation, and heat-seal jaw contamination when seal temperatures exceed the film’s practical range. LLDPE sealant webs are not suitable for retort or ovenable packaging above approximately 120–125 °C sustained; for such structures, cast polypropylene, retort-grade coextruded films, or aluminium-foil-containing laminates are used. Regulatory status should be confirmed with the supplier’s material declaration, because LLDPE base polymers may fall under the polymer exemption provisions of REACH, while additives and processing aids require individual verification. Packaging films supplied for electrical and electronic equipment must be reviewed separately against packaging directive and RoHS Directive 2011/65/EU requirements where applicable. Rolls that fail incoming inspection criteria should be quarantined and subjected to supplier disposition.