| HS Code | 820177 |
| Material Type | Linear Low Density Polyethylene (LLDPE) |
| Film Grade | Laminating |
| Thickness | 38.1 µm |
| Density | 0.920 g/cm³ |
| Tensile Strength Md | 31.0 MPa |
| Tensile Strength Td | 24.1 MPa |
| Elongation At Break | 500% |
| Elmendorf Tear Strength Md | 4.0 g/µm |
| Elmendorf Tear Strength Td | 6.0 g/µm |
| Coefficient Of Friction | 0.20 |
| Haze | 6.0% |
| Gloss | 80% |
| Melting Point | 122°C |
| Vicat Softening Point | 96°C |
| Water Vapor Transmission Rate | 15.5 g/m²/day |
| Oxygen Transmission Rate | 2200 cm³/m²/day |
As an accredited DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 38.1 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged as one roll per carton, DuPont™ Sclairfilm® SL-3 LLDPE laminating film, 38.1 µm thick, in protective moisture-resistant wrap. |
| Container Loading (20′ FCL) | Film rolls palletized, stretch-wrapped, and loaded evenly into a 20′ FCL container, braced to prevent shifting during transport. |
| Shipping | DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 38.1 µm, ships as non-hazardous flexible film in moisture-barrier rolls or cartons on pallets. Transport clean and dry, away from heat, sunlight, and sharp objects. Not regulated for DOT, IMDG, or IATA; no special shipping labels required. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep in original packaging until use. Protect from moisture, dust, dirt, and physical damage. Store flat to prevent creasing, stretching, or puncture. Do not stack heavy items on top. Avoid static discharge, contamination, and follow local regulations. |
| Shelf Life | Shelf life for DuPont™ Sclairfilm® SL-3 LLDPE film is 12 months from date of manufacture when stored in original packaging. |
On a multi-layer stick-pack laminator, the 38.1 µm Sclairfilm® SL-3 LLDPE web is converted as the innermost sealant layer after corona treatment at 38 mN/m to 42 mN/m, measured per ASTM D2578-23. Paper or reverse-printed PET facestock is bonded to the sealant web with solvent-free polyurethane adhesive at coat weights between 1.5 g/m² and 2.5 g/m². Lamination is run on sleeve-type nip stations with surface temperatures of 60 °C to 80 °C and line speeds from 180 m/min to 300 m/min; these ranges are typical for two-component solventless systems and must be confirmed on the specific line because adhesive ratio deviation greater than ±5% can leave unreacted isocyanate that migrates into filled powder. Food-contact status is evaluated under FDA 21 CFR 177.1520 for olefin polymers and under Regulation (EU) No 10/2011, with migration testing according to EN 1186-1 and EN 1186-3 for aqueous and dry-food stimulants. The sealant layer is applied below 60 µm, so overall migration limits are referenced to the surface-area calculation rules in EU No 10/2011 Article 17.
On horizontal form-fill-seal equipment, fin seal jaws are set to 115 °C to 135 °C, with dwell from 0.4 s to 0.8 s and jaw pressure 0.3 MPa to 0.5 MPa. Seal initiation measured by ASTM F1921/F1921M-21 typically falls between 95 °C and 105 °C for clean film surfaces; published data for this specific configuration is limited. Powdered product dust on the seal area shifts the required jaw temperature upward by 10 °C to 15 °C and produces weak-boundary sealing. Vacuum extraction of product dust is therefore used before the sealing station. Finished stick packs are single-serve beverage, sugar, and supplement formats; seal strength tested per ASTM F88/F88-21 is recorded on 15 mm strips after conditioning at 23 °C and 50% RH for 24 h.
| Seal bar temperature | Dwell | Jaw pressure | Seal strength per ASTM F88/F88-21 | Failure mode |
|---|---|---|---|---|
| 105–115 °C | 0.5 s | 0.35 MPa | 3.5–5.0 N/15 mm | Peel / delamination |
| 115–125 °C | 0.5 s | 0.35 MPa | 5.0–7.0 N/15 mm | Hybrid peel / cohesive |
| 125–135 °C | 0.5 s | 0.35 MPa | 6.5–8.5 N/15 mm | Film break |
Reverse-printed BOPP or PET snack packaging lines use the 38.1 µm LLDPE web as the sealant ply after lamination with aliphatic solventless polyurethane adhesives. The web is corona-treated on the adhesive-facing side at 40 mN/m minimum; ink-bearing facestock is checked for retained solvent below 5 mg/m² before lamination because retained solvents accelerate slip additive migration from the sealant film into the adhesive interlayer. Laminating machine tensions for the 38.1 µm web are held between 40 N/m and 80 N/m to prevent neck-in and gauge-band formation. The finished laminate is slit to width and converted on vertical form-fill-seal machines with serrated twist-tie or lap seal jaws. Seal strength after processing is measured per ASTM F88/F88-21, while coefficient of friction is tested per ISO 8295:1995. Kinetic COF values above 0.45 after 14 days of ageing typically indicate migration of slip additives or excess adhesive ooze at the seal edge. Incompatible amine-catalysed inks or coatings should be avoided because amine species can react with isocyanate adhesives and produce carbon dioxide bubbles in the adhesive layer.
Film break at the seal is preferred over delamination for snack packs with grease or salt contamination. If delamination occurs at 3.0 N/15 mm or lower, the sealing jaw temperature is increased in 5 °C increments until cohesive failure within the LLDPE layer is observed. Production-scale sticky-point testing on a 25.4 mm hot-tack mandrel according to ASTM F1921/F1921M-21 is used to establish the packaging machine speed limit. The maximum sustainable speed for a given laminate depends on product drop distance and seal jaw design; no universal speed can be assigned.
On vertical form-fill-seal lines for frozen vegetable and dry granular products, the sealant response of the 38.1 µm Sclairfilm® SL-3 film is governed by hot-tack strength rather than cool peel strength alone. Hot-tack performance is measured according to ASTM F1921/F1921M-21 using a 25.4 mm sealing bar at 0.3 MPa and a 0.5 s dwell. The seal initiation for clean film surfaces is commonly observed between 90 °C and 105 °C; however, on vertical baggers running frozen product at 80 bags/min to 120 bags/min, jaw temperatures are normally set 20 °C to 30 °C above seal initiation because product dust and water condensation on the seal area suppress interfacial melting. In such lines the seal jaws are typically set at 120 °C to 135 °C with jaw pressure 0.3 MPa to 0.4 MPa and dwell 0.4 s to 0.6 s; these are operational starting points, not universal settings.
Film extrusion gauge uniformity controls seal initiation. A thickness variation of ±5% across the web can create low-temperature seal failure points where the film is thinner than 36 µm, while thicker regions above 40 µm may exhibit delayed heat transfer. Profile control on cast film lines uses air-knife edge-pinning and vacuum box control; blown film lines use internal bubble cooling and gauge scanner feedback. Laminators should reject rolls with average thickness deviation outside ±5% because HFFS and VFFS jaw dwell is not sufficient to compensate for uneven heat transfer.
In laminated tube body stock for cosmetic, pharmaceutical, and oral-care products, the 38.1 µm LLDPE web is used as the sealing layer inside a multi-layer structure of PE-Al foil-PE. The web is adhesive-laminated to 9 µm to 12 µm aluminum foil with polyurethane adhesive at 1.8 g/m² to 2.2 g/m²; the resulting laminate is slit into tube body blanks and side-seam welded by high-frequency or hot-air techniques. Side-seam weld temperature is controlled at 160 °C to 190 °C for the foil/PE composite, with seam cooling under pressure to prevent stress cracking of the LLDPE inner layer. Shoulder injection molding then produces the tube head and cap seat; the sealing surface between the shoulder and body is tested by ASTM D3078-02 bubble emission or ASTM F2096-11 gross leak testing after filling.
Compliance for pharmaceutical tubes requires the inner LLDPE layer to meet Ph. Eur. 3.1.3 or USP Chapter 661.1 as appropriate, and the complete tube is evaluated for extractables under ISO 10993-1:2018 where applicable. The Sclairfilm® SL-3 web in this thickness is not a barrier to oxygen or moisture; barrier properties are supplied by foil. Tubes with high-speed shoulder welding require a sealant layer that maintains cohesive peel above 12 N/25 mm by ASTM D1876-08 after 24 h conditioning at 23 °C and 50% RH; published data for this specific configuration is limited, so validation on the actual tube line is mandatory.
High-barrier coffee brick packs and valve bags laminate reverse-printed PET or metallized PET to foil and the 38.1 µm LLDPE sealant web. The lamination sequence on a multi-station solventless machine places the sealant web as the final ply under nip temperature 55 °C to 70 °C. During filling, whole bean or ground coffee releases a small fraction of surface oil; oil particles deposited on the sealant web create a weak-boundary layer that lowers seal strength. Seal strengths measured per ASTM F88/F88-21 on oil-contaminated samples are typically 40% to 60% lower than clean samples, depending on oil loading and roast profile. To avoid leaker packages, fillers position product drop tubes so that the seal area remains free of dust and oil mist; some lines apply a rotating brush or vacuum extractor before the sealing jaws.
Seal jaw temperatures for this structure are typically set at 125 °C to 140 °C, with dwell 0.5 s to 0.7 s and jaw pressure 0.35 MPa to 0.5 MPa. Hot-tack value is more critical for corner gussets because the film must hold the brick shape immediately after the jaw opens; hot-tack values below 2.0 N/25 mm at 120 °C can cause gusset pop-open. The LLDPE sealant does not provide aroma or oxygen barrier; the aluminum foil ply controls oxygen ingress and the sealant layer is not a flavour barrier.
For liquid detergent refill pouch laminates and bag-in-box inner liners, the 38.1 µm film is converted as the heat-seal layer after lamination to PET or foil. The sealant layer is selected for resistance to stress cracking under contact with surfactants and for a broad sealing window on high-speed rotary fillers. The laminate is converted on form-fill-seal machines equipped with plough or Doy-style gusset stations; seal bars are set at 130 °C to 150 °C for 0.6 s to 1.0 s because the film must flow into wrinkles and gusset folds without thinning to zero. Environmental stress-crack resistance of the LLDPE layer is evaluated by ASTM D1693-15, but full pouch validation is required with the actual liquid formulation because surfactants reduce the critical strain required to initiate crazing.
Closure and fitment sealing is tested under ASTM F2096-11 for gross leaks and ASTM F88/F88-21 for seal strength; burst strength is measured by ASTM F1140/F1140M-13 at internal pressure above 20 kPa. Filled pouches are dropped per ASTM D5276-19; seal fracture at gussets is not acceptable. Continuous contact with organic solvents above 40 °C should be avoided; published data for this film in solvent-containing liquids is limited.
The 38.1 µm LLDPE web is bonded to aluminum foil as a corrosion-resistant and abuse-resistant inner surface for HVAC duct board and fiberglass insulation facing. Lamination is performed with water-based or solvent-based adhesives; flame spread and smoke development of the finished facing must be tested to ASTM E84-23 or UL 723, with the product required to meet Class A ratings where specified. Water vapor transmission is governed by the foil layer and is tested by ASTM E96/E96M-22; the LLDPE layer contributes tear propagation resistance and serves as a weldable surface for longitudinal seams. The web is heat-sealed to itself or to coated foil at 150 °C to 180 °C on fabricating lines; dwell is 2.0 s to 4.0 s under contact pressure. Foil-to-film bond strength is tested per ASTM D1876-08. Thermal stability of the LLDPE layer at continuous service temperatures below 60 °C is typical; above this range, dimensional change must be evaluated because olefin-based films soften and may delaminate under load. No universal fire-resistance claim can be assigned without assembly-level testing.
Competitive DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 38.1 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont™ Sclairfilm® SL-3 is specified as a linear low-density polyethylene film supplied at a nominal thickness of 38.1 µm (1.5 mil) for laminating operations. The grade is converted as a web component in adhesive and extrusion lamination structures, not as a monolayer finished package. Film construction, surface treatment level, slip package, and roll format are production-specification variables controlled through the manufacturer’s certificate of analysis rather than inferred from the grade designation alone. In final flexible packaging, SL-3 functions as a tough sealant web, a lamination carrier, or an inside ply with moderate moisture resistance; oxygen barrier performance must be supplied by the core or exterior substrates.
Because published data for 38.1 µm SL-3 as a discrete configured product is limited, the following sections distinguish between polymer-class behavior and grade-specific requirements. All property claims are tied to applicable test methods and typical industrial ranges, but the manufacturer’s certificate of analysis remains the authoritative numerical specification.
SL-3 is identified as an LLDPE resin film. LLDPE for laminating webs typically has a density of 0.918–0.926 g/cm³ when measured under ISO 1183-1:2019; the density of the finished film may shift slightly after orientation and corona treatment, so the unprocessed resin specification is the more stable classification. The nominal caliper of 38.1 µm should be confirmed by mechanical scanning to ISO 4593:1993 or by capacitance thickness testing to ASTM D6988-21. A lot average outside the supplier’s published tolerance should be quarantined; nonuniform caliper is transmitted directly into coating-weight variation in adhesive lamination because the gravure or sleeve station controls coat weight by line speed and fluid delivery, not by automatic web-thickness compensation on most production lines.
The grade is normally supplied in roll form on a 76 mm or 152 mm core, but core size, web width, and roll length are converter-specific ordering parameters rather than grade constants. Winding tension and edge alignment are controlled to reduce blocking and telescoping during storage. The film does not require moisture pre-drying; polyolefin equilibrium moisture pickup at 23 °C and 50 % RH is below 0.01 wt%, so moisture-related hydrolysis is not a practical limitation for LLDPE webs.
Compared with LDPE of equal gauge, LLDPE contains a linear backbone with short-chain branches introduced by alpha-olefin comonomer. This molecular architecture produces different flow and solid-state behavior. Under film tensile testing to ASTM D882-18, LLDPE laminating webs typically exhibit higher ultimate tensile strength and elongation at break than branched LDPE of the same thickness, although haze values under ASTM D1003-21 may be higher because surface melt fracture and internal crystallite scattering are more difficult to quench. Dart impact values under ASTM D1709 are commonly 1.5–2 times those of LDPE at the same gauge, but the exact differential is comonomer-dependent and should not be assumed for SL-3 without a comparative lot trial.
Against EVA copolymer films, SL-3 is expected to provide a narrower seal-initiation window but a higher melting plateau. LLDPE laminating grades typically show a peak melting endotherm in the 120–126 °C range by differential scanning calorimetry under ASTM D3418-21, whereas many EVA films melt below 105 °C depending on vinyl acetate content. The higher thermal resistance reduces blocking during storage and allows higher downstream sealing temperatures, but EVA often provides better adhesion to polar substrates and lower minimum seal initiation. A laminator choosing between SL-3 and an EVA sealant web should therefore compare hot-tack and seal-strength curves under ASTM F1921 and ASTM F88/F88M rather than comparing only thickness.
Unoriented cast polypropylene of similar gauge offers higher heat resistance and stiffness than LLDPE, but generally lower low-temperature impact and a less conformable sealant contact. Metallized polyester or biaxially oriented polyester provides gas barrier and dimensional stability but no sealant function. SL-3 is therefore selected when the web must combine sealant toughness, moderate scalability, and lamination compatibility rather than barrier or stiffness.
In adhesive lamination, SL-3 is run as a secondary or tertiary web. Unwind tension for a 38.1 µm LLDPE film should be maintained in the range of 10–25 N/m of web width on common duplex and triplex laminators; higher tension can neck the web and alter coating register. Solventless polyurethane adhesives used at 2.0–4.0 g/m² coat weight are standard for producing final structures such as PET/SL-3, BOPP/SL-3, and paper/SL-3 laminates. The film surface must be placed toward the adhesive with the corona-treated side oriented correctly; incorrect face placement commonly produces peeling at the bond line within the first 24 h of cure. Heated nipping at 40–60 °C followed by 24–72 h of ambient or warm-room cure is typical for solventless polyurethane systems.
In extrusion lamination, LLDPE differs from LDPE in melt strength and neck-in. Typical die melt temperatures for LLDPE laminating are 290–315 °C, with an air gap of 150–250 mm and a chill-roll surface temperature of 15–25 °C. LLDPE generally exhibits lower melt strength than LDPE, so neck-in may be greater and the maximum stable draw-down ratio may be lower. Some lines require a wider die gap of 0.5–0.8 mm to delay melt fracture and reduce extrusion pressure. Draw resonance may appear at high line speed when the draw-down ratio exceeds the resin’s stability limit; for standard LLDPE extrusion-lamination grades, this limit can fall in the 15:1–20:1 range, but the exact value for SL-3 should be established on the production line because published data for this specific configuration is limited.
Chill-roll release and surface replication are controlled by melt temperature, air gap, and roll finish. A matte chill roll reduces blocking and preserves unwind performance; a gloss roll improves contact clarity but may increase blocking tendency if roll hardness is too high. Wound rolls with a film temperature above 30 °C at the rewind should be cooled before storage to avoid blocking and core collapse.
On high-speed form-fill-seal equipment, sealant performance is determined by seal initiation temperature, hot-tack strength, and coefficient of friction. Seal initiation for LLDPE is frequently 5–15 °C lower than branched LDPE of the same gauge, which can permit a wider operating window on vertical machines, but the slip package must be specified separately. A film with insufficient slip can exhibit erratic bag tracking; a film with excessive slip can reduce coefficient of friction below 0.15 and cause poor stacking. The converter should specify coefficient of friction limits under ISO 8295 rather than accepting a generic laminating grade when the downstream operation includes high-speed twist or jaw sealing.
Sealing temperature, dwell time, and pressure should be optimized on the actual machine. LLDPE sealant webs usually produce destructive film tear in peel tests once adequate fusion is achieved; lab seal strength should be measured under ASTM F88/F88M after 24–48 h of conditioning. In-line destructive testing should be gated by failure mode: cohesive film break indicates seal integrity, while delamination at the sealant/substrate interface indicates adhesive or surface preparation failure.
Polyolefin film surfaces are nonpolar and require oxidative treatment before lamination. The treated side of SL-3 should have wetting tension of at least 38 mN/m under ASTM D2578, and many solventless adhesive systems give more uniform coating at 40–44 mN/m. Below 36 mN/m, adhesive de-wetting may occur because the liquid adhesive cannot maintain a continuous film. Treatment decays over time; a roll stored at 20–25 °C may lose 2–4 mN/m over six months, but actual decay is influenced by slip additives and storage humidity. Laminators should recheck wetting tension before running aged film and, if necessary, pass the web through a corona treater set to a discharge density that restores the target level without generating excessive surface oxidation.
Adhesive bond strength should be evaluated by T-peel testing under ASTM D1876-15 after full adhesive cure. Failure modes are diagnostic: film tear or deep film elongation indicates that the polyethylene surface treatment is no longer the limiting interface; clean separation between the adhesive and the polyethylene indicates insufficient treatment, contamination, or incorrect treated-side orientation. For extrusion lamination, bond strength depends on oxidation of the molten polyethylene curtain before substrate contact. Excessively short air gaps or low melt temperatures can reduce oxidative adhesion and produce low peel strength.
Compliance for food-contact flexible packaging must be established for the final structure, including adhesives, inks, and substrates. The following methods and designations support typical verification for a polyethylene laminating web.
| Property or requirement | Reference method or designation | Relevance to laminating |
|---|---|---|
| Thickness profile | ISO 4593:1993, ASTM D6988-21 | Confirms nominal 38.1 µm gauge and coating-weight uniformity |
| Tensile properties | ASTM D882-18 | Machine-direction and transverse-direction break stress and elongation |
| Dart impact | ASTM D1709 | Puncture resistance during package distribution |
| Surface wetting tension | ASTM D2578 | Corona treatment target before adhesive coating |
| Density | ISO 1183-1:2019 | Resin class confirmation for LLDPE |
| Melt mass-flow rate | ISO 1133-1:2022 | Extrusion lamination flow classification |
| Water vapour transmission rate | ASTM F1249 | Moisture barrier contribution of the LLDPE web |
| Seal strength | ASTM F88/F88M | Verification of heat-seal performance after lamination |
| Total migration for food contact | EU Regulation (EU) No 10/2011 | Final-structure compliance for intended food simulants |
| US food-contact status for olefin polymers | FDA 21 CFR 177.1520 | Resin and film compliance under conditions of use |
Storage of SL-3 should keep the product in its original packaging until use, avoid direct sunlight, and maintain a warehouse temperature below 35 °C. Corona-treated roll stock should be consumed within 6 months; aged film may require retreatment. Roll edges should not be struck or allowed to contact concrete floors, because edge damage propagates as web breaks during high-speed laminating. The product is not intended for prolonged outdoor exposure or for use above its melting onset; continuous service above 60 °C can cause shrinkage and seal-area distortion. The film should not be combined with incompatible aggressive solvents or high-aromatic printing inks without testing extraction resistance under the applicable EU Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520 conditions of use.
Because the SL-3 grade is specified by caliper and laminating function, converters should maintain a lot-level receiving protocol: compare the certificate of analysis, measure thickness profile, confirm width and core dimensions, record surface wetting tension, and perform a bond trial on a production adhesive before full release to inventory.