Dupont Sclairfilm Sl 1 Lldpe Film Laminating 76 2 µm Thickness

DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness

    • Product Name: DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 891127
    Product Name DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness
    Material Linear Low Density Polyethylene (LLDPE)
    Film Type Laminating Film
    Thickness 76.2 µm
    Thickness Mil 3.0 mil
    Density 0.920 g/cm³
    Tensile Strength At Break Md 24.1 MPa
    Tensile Strength At Break Td 20.7 MPa
    Tensile Strength At Yield Md 9.65 MPa
    Tensile Strength At Yield Td 8.96 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Elmendorf Tear Strength Md 260 g
    Elmendorf Tear Strength Td 520 g
    Coefficient Of Friction 0.200
    Haze 10.0%
    Gloss 70.0%
    Water Vapor Transmission Rate 1.55 g/100 in²/day
    Oxygen Transmission Rate 155 cc/100 in²/day
    Melting Point 122 °C
    Vicat Softening Point 100 °C

    As an accredited DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaging: Each carton contains one roll of 76.2 µm DuPont™ Sclairfilm® SL-1 LLDPE laminating film, securely core-wound and protective-wrapped.
    Container Loading (20′ FCL) Container Loading (20′ FCL): DuPont™ Sclairfilm® SL-1 LLDPE laminating film, 76.2 µm, palletized, dry, ambient, secured for transport.
    Shipping DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness is a non-hazardous, non-regulated plastic film. Ship in original rolls, wrapped and palletized. Protect from puncture, moisture, UV, heat, and crushing. Store cool and dry. No special transport labels required. Handle carefully to prevent roll damage.
    Storage Store in a cool, dry, well-ventilated area in original sealed packaging. Keep away from direct sunlight, heat, sparks, flames, and strong oxidizers. Protect from moisture, dust, and physical damage. Maintain moderate temperature and humidity; store upright, avoiding crushing or creasing. Keep packaging closed when not in use. Follow first-in, first-out rotation and observe manufacturer shelf-life.
    Shelf Life Typically 12 months from date of manufacture when stored unopened in original packaging under recommended cool, dry, dark storage conditions.
    Application of DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness

    DuPont™ Sclairfillm® SL-1 laminating-grade LLDPE supplied at 76.2 µm thickness functions as a heat-sealable web, abrasion-resistant outer ply, or moisture-barrier component after adhesive or thermal lamination to oriented polyester, biaxially oriented polypropylene, aluminum foil, metallized films, paperboard, woven polypropylene, or nonwoven substrates. The film is corona-treatable on the lamination side; bond strength development on a solventless laminator is governed by nip temperature, adhesive coat weight, and initial surface energy of the sealant web as measured under ASTM D2578-17. Because the product is an unplasticized polyolefin with a density in the range typical for LLDPE film grades, calculated basis weight at 76.2 µm is approximately 70 g/m² at a nominal density of 0.920 g/cm³; actual basis weight must be confirmed by ASTM D4321 or equivalent. The following application scenarios are limited to laminating uses of the supplied thickness; they do not cover monolayer shrink film or heavy-duty bag construction without a secondary substrate.

    Solventless Adhesive Lamination to PET, BOPP, and Aluminum Foil in Flexible Food Packaging

    In dry-mix pouch, frozen food, and snack packaging, the 76.2 µm web is positioned as the inner sealant layer against a reverse-printed polyester or BOPP outer web, with optional aluminum foil or metallized PET as a mid-barrier. A two-component solventless polyurethane laminating adhesive is deposited on the primary web at a target coat weight of 1.8–2.5 g/m², mixed at the ratio specified on the adhesive batch ticket—commonly 100:40 to 100:60 parts by weight for polyol-to-isocyanate systems—and the LLDPE web is nipped at 60–70°C with a nip pressure of 0.4–0.6 MPa. The sealant side must retain a wetting tension of at least 38 mN/m prior to lamination, verified by ASTM D2578-17; online corona treatment is normally set between 2.0 W·m²/min and 3.0 W·m²/min depending on line speed. Compliance for food contact rests on FDA 21 CFR 177.1520(c) for olefin polymers used in contact with food types I through IX under conditions of use E through G, and on EU Regulation (EU) 10/2011 with overall migration below 10 mg/dm² when tested by EN 1186-1. Terminal structures include stand-up pouches with a three-side seal geometry, pillow packs for frozen vegetables, and stick-pack laminates; on a vertical form-fill-seal line, the seal initiation temperature of the LLDPE web typically requires a jaw temperature of 110–135°C at 0.5–1.0 s dwell, depending on outer film thickness and jaw profile. The key process conflict is that premature post-cure converting at ambient humidity can leave residual isocyanate near the sealant interface; lamination should not be converted within the adhesive supplier’s minimum maturation window, commonly 24–48 h at 35–40°C, because incomplete cure lowers laminate bond strength and can create tunneling on high-slip LLDPE surfaces.

    Why Is a 76.2 µm LLDPE Web Used Rather Than 50 µm LDPE in Peelable Medical Sterile Barrier Pouches?

    Medical lidding and pouch stock require a controlled peel separation at the seal without fiber tear of the sterile barrier material. A 76.2 µm LLDPE sealant layer is laminated to Tyvek 1073B, medical-grade paper, or polyester film; the LLDPE thickness provides a wider heat-seal process window than 50 µm low-density polyethylene because the additional mass lowers the risk of burn-through at serrated or knurled sealing jaws. Peelable seal geometry is achieved by pattern-coating a heat-seal adhesive or by using a formulated sealant layer, with coat weight specified at 2.5–4.0 g/m² dry on the lidding web. The seal process on a rotary tray sealer operates at 120–140°C jaw temperature, 0.5–1.5 s dwell, and 0.3–0.7 MPa pressure; the seal is then conditioned and tested according to ASTM F88/F88M for seal strength, with a common acceptance band of 1.0–3.0 N/15 mm for peelable medical pouches, verified against ISO 11607-1:2019 and ISO 11607-2:2019 requirements for sterile barrier system integrity. Compliance also includes EN 868-5 for paper/plastic constructions and ISO 10993-5 for cytotoxicity when the laminate contacts a medical device. Terminal use includes single-use surgical instrument pouches, syringe blister lidding, and IV administration set overwrap. On production equipment with a six-station rotary platen, the critical field issue is seal creep when the LLDPE web is pre-heated above 70°C before sealing; this shifts the peel transfer mechanism from adhesive failure at the sealant interface to cohesive failure in the LLDPE, causing variable peel strength. Operators therefore stage the lidding roll away from the sealing station and maintain unwind tension below 80 N/m to avoid gauge-band stretching.

    Compliance and test framework by converting sector
    SectorMandated referenceTypical condition
    Food contactFDA 21 CFR 177.1520(c); EU 10/2011Overall migration < 10 mg/dm²
    Medical packagingISO 11607-1:2019; ISO 11607-2:2019; ASTM F88/F88MSeal strength 1.0–3.0 N/15 mm
    Building facingASTM E96/E96M; ASTM E84; EN 13501-1WVTR 2.0–4.0 g/(m²·day) for LLDPE layer

    Construction vapor-retarder and insulation-facing laminates use the 76.2 µm LLDPE film as a moisture and puncture-resistant layer over aluminum foil, metallized polyester, or glass scrim. In a typical radiant-barrier facing for fiberglass blanket insulation, the LLDPE web is adhesive-laminated to 12 µm aluminum foil with a solventless two-component polyurethane adhesive applied at 1.5–2.0 g/m², then cured at 30–40°C for 24 h. The film side is subsequently printed with a water-based flexographic ink; film treatment must be maintained above 40 mN/m for ink adhesion and above 36 mN/m for lamination. Vapor transmission is measured by ASTM E96/E96M Procedure A at 23°C and 50% RH; for a 76.2 µm LLDPE layer, published water vapor transmission data for similarly thick polyethylene films generally fall between 2.0 g/(m²·day) and 4.0 g/(m²·day), though the exact value for this specific laminate configuration should be confirmed by a certified laboratory because adhesive chemistry and foil pinhole content shift the result. Fire propagation behavior in building facings is evaluated under ASTM E84 or EN 13501-1, but the LLDPE layer by itself is combustible and must not be used as an exposed interior surface unless the finished laminate meets the local surface-burning classification. End products include faced batt insulation, pipe-wrap outer jackets, and under-slab vapor barriers where the LLDPE side provides abrasion resistance during backfill. The production constraint is web flatness: a 76.2 µm LLDPE film laminated under excessive unwind tension—above 100 N/m—can develop heat-set curl in the finished roll, making it difficult to register subsequent printing and sheeting operations.

    In a thermal overlaminate operation for printed paperboard, book covers, and technical maps, the 76.2 µm LLDPE web is bonded as a protective face ply with a pre-applied EVA or polyurethane-based heat-activated adhesive. The laminating system is run on a thermal laminator with chrome-plated heated rollers at 95–115°C and line speed of 10–25 m/min; nip pressure is maintained at 0.3–0.5 MPa. The adhesive layer is applied in a separate coating pass at 5–8 g/m² dry on the film. This construction is generally compliant with REACH Annex XVII restrictions and EU RoHS Directive 2011/65/EU for heavy metals when the adhesive and printed substrate meet the same requirements; it is not intended for direct food contact unless a full migration assessment is performed under EU 10/2011. Terminal products include laminated point-of-purchase cards, field guides, menu covers, and laboratory identification tags where frequent wiping with isopropanol or quaternary ammonium disinfectants is expected. The main failure mode observed on production laminators is starved bond lines at the trailing edge of the sheet due to retraction of the adhesive coating at high roll temperatures; holding the film roll temperature below 30°C and adjusting the sheet compensator to the film’s thermal expansion coefficient avoids edge lift after cooling.

    When Alkaline Powder Fillers Demand a Low Seal Initiation Temperature in FIBC and Dunnage Bag Liners

    Bulk industrial liners for flexible intermediate bulk containers and dunnage air bags use the 76.2 µm LLDPE film laminated to woven polypropylene or nylon scrim to provide a clean internal surface and controlled air retention. The LLDPE layer is reverse-laminated to a 70–100 g/m² woven substrate with a two-component polyurethane adhesive applied at 2.0–3.0 g/m², then cured fully before slitting. Seal initiation temperature for the LLDPE web is evaluated by hot-tack testing on a J&B type instrument or equivalent; for 76.2 µm LLDPE, hot-tack onset usually appears between 80°C and 95°C, which permits high-speed filling of alkaline powders such as sodium carbonate without the need to raise jaw temperatures above 115°C. Compliance for industrial chemical contact is generally addressed under UN transport packaging performance requirements, with the finished FIBC liner tested by ISO 21898 for UV resistance and cyclic top lift; if the liner is used for food-grade bulk powders, the film must also meet FDA 21 CFR 177.1520(c) and, in the EU, Regulation (EU) 10/2011. End products include one-trip liners for cement, titanium dioxide, calcium carbonate, and dry food ingredients. On a production laminating line, the critical defect is pinholing when the LLDPE web is corona-treated above 2.5 W·m²/min during winding; excessive treatment can create low-molecular-weight oxidation products that reduce laminate shear strength under filled-bag compression.

    For greenhouse and high-tunnel reflective laminates, the 76.2 µm web is adhesive-laminated to a 100–150 µm EVA film with a polyurethane adhesive at 1.5–2.5 g/m²; the laminate is then fabricated into roll-up side curtains, shade screens, or energy screens. The LLDPE layer contributes to tear resistance under tensile loading; ASTM D882-18 tensile strength for similarly thick LLDPE films typically lies between 20 MPa and 40 MPa in the machine direction, with elongation at break between 500% and 800%, but the measured values for this product lot must be taken from the certificate of analysis because film formulation and orientation history shift these ranges. Outdoor weatherability is not inherent; the laminate requires a UV stabilizer package in the EVA or a top-coat, and service life is tested under ASTM G154 or EN 16472 accelerated weathering. End products include multi-layer greenhouse side curtains, mushroom crop blackout films, and mulching film laminates. The operational limit is that the LLDPE layer’s coefficient of linear thermal expansion, approximately 100–200 × 10-6/°C for polyolefins, is higher than polyester; in outdoor installations, the laminate expands and contracts enough to cause edge pull-out if the film is stapled at intervals greater than 300 mm.

    Free Quote

    Competitive DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The designation DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness identifies a cast linear low-density polyethylene web supplied as a laminating-grade sealant or buried ply in flexible packaging structures. The nominal thickness is 76.2 µm (3.0 mil), and the resin class falls within unfilled LLDPE with published density ranges for commercial cast webs generally between 0.915 g/cm³ and 0.925 g/cm³ when tested by ISO 1183-1:2019 or ASTM D1505. Because the web is produced by cast film extrusion rather than blown film extrusion, thickness uniformity, low gel count, and surface smoothness are qualification criteria for lamination to paper, aluminium foil, metallized oriented polyester, and biaxially oriented polypropylene. The 76.2 µm gauge is selected when a structure must resist puncture and provide a sealing ply without the bending stiffness of a 100 µm or 125 µm web. Lot-specific values for tensile properties, tear resistance, slip, haze, and corona treatment are stated on the certificate of analysis; published data for this exact SL-1 configuration are limited outside that documentation.

    What Converting Variables Are Altered by a Fixed 76.2 µm LLDPE Web?

    On a center-driven unwind feeding a laminator or coating line, a 76.2 µm cast LLDPE web presents lower bending stiffness than a 100 µm sealant web and higher bending stiffness than a 50 µm blown LDPE web. Caliper uniformity measured by ISO 4593 or ASTM D6988 should be checked at the roll edges, the core transition, and the outer lap; commercial cast-film thickness tolerance is commonly held within ±8% to ±10%, but a hard band of thickness variation greater than 2 µm across 500 mm of width can generate telescoping during acceleration. Web tension at the unwind and rewind is typically maintained between 30 N/m and 80 N/m. Tension below 30 N/m permits low-frequency flutter and crepe wrinkles, while tension above 80 N/m can neck the film and alter its gauge distribution before the lamination nip. Because LLDPE is hydrophobic, dimensional change from humidity is negligible; the film does not require a dryer and does not change caliper at 60% RH. Static charge becomes a handling issue below 30% RH. Surface resistivity above 1014 Ω/sq measured by ASTM D257 allows charge accumulation at line speeds above 200 m/min, and static dissipators are commonly required to prevent cling to idler rollers. The coefficient of friction, measured by ASTM D1894, is controlled by the slip additive package; kinetic COF values outside 0.15 to 0.30 can create forming-collar drag or roll instability depending on the packaging machine.

    When SL-1 Replaces EVA or LDPE in a Thermal Lamination Line

    Replacement of an EVA sealant web with SL-1 alters the heat-seal response because LLDPE has a higher seal initiation temperature than EVA and a broader plateau before melt-through. Under a typical jaw condition of 0.3 MPa pressure and 0.5 s dwell, seal initiation for a 76.2 µm LLDPE laminating web is normally observed between 105°C and 120°C when measured by ASTM F88. EVA films of the same gauge can initiate around 85°C to 100°C. The higher initiation temperature is not a deficit in all structures; it extends the seal window before the peel force drops into the char or delamination region at jaw setpoints typically between 135°C and 150°C. Hot tack, measured by ASTM F1921, becomes the limiting parameter on vertical form-fill-seal machines above 60 packs/min, where the seal must resist opening forces before crystallisation is complete. Production data from polyolefin sealant webs indicate that hot tack in LLDPE is more sensitive to resin comonomer distribution than to film gauge; a narrow hot-tack peak may occur between 115°C and 130°C, after which hot tack decays as the melt loses cohesive strength.

    When SL-1 is used in adhesive lamination rather than direct heat sealing, the process conflict shifts from jaw dwell to coating wetting. Solventless polyurethane adhesives deposited at 1.8 g/m² to 2.5 g/m² require a film surface energy of at least 38 mN/m on the coating side, measured by ASTM D2578. If surface energy is below 36 mN/m, the adhesive can reticulate and form an uneven bond line; peel adhesion measured by ASTM F904 then shows high standard deviation and tunnel failure modes. In extrusion lamination where a molten polyethylene curtain is applied to the web, the SL-1 film may act as a substrate or pre-laminated ply. Melt temperature of the extrudate is normally 300°C to 330°C, but published data for this specific configuration are limited and the converter should verify that air-gap and cooling-roll temperatures do not distort the film or bloom slip additives to the surface.

    On a flexographic or gravure lamination line, the 76.2 µm web is usually unwound with a driven flying splice at speeds from 150 m/min to 300 m/min. Splice integrity can be checked by ASTM D882 after a full roll change; a splice failure at these speeds causes wrap-up on the coating roll. Because cast LLDPE has higher tear resistance than LDPE of equal thickness, measured by ISO 6383-2 or ASTM D1922, it tolerates notching at the slitter edge and reduces web breaks from micro-tears at the roll core. Slitting cleanliness remains critical: a dull shear blade increases edge roughness and can generate particulate contamination that transfers to the coating roll and creates streak defects at the laminate bond line.

    Comparative Optical, Mechanical, and Seal-Initiation Profiles

    The table below situates SL-1 within the publicly reported envelope for cast LLDPE laminating webs at 76.2 µm. It is not a replacement for lot-specific documentation, because additive packages for slip, antiblock, and processing stabilisers shift measured values.

    PropertyTest MethodRepresentative Range at 76.2 µmComparison Against LDPE/EVA Webs
    Nominal thicknessISO 459376.2 µm (3.0 mil)Equal caliper; less gauge variation than blown LDPE
    Tensile strength at break, machine directionISO 527-3:201825–35 MPaHigher than LDPE; lower than oriented polyester
    Tensile strength at break, transverse directionISO 527-3:201818–28 MPaHigher extension than LDPE
    Elongation at break, machine directionISO 527-3:2018500–700%Comparable to EVA; ductile failure mode
    Elongation at break, transverse directionISO 527-3:2018600–800%Comparable to EVA
    Dart impact, Type AASTM D1709-16a100–250 gHigher than unmodified LDPE at equal gauge
    HazeASTM D10033–8%Lower than blown LDPE; additive dependent
    Gloss, 45°ASTM D245760–80Higher than blown LDPE
    Kinetic coefficient of friction, film-to-filmASTM D18940.15–0.30Lower than EVA; controlled by slip additive
    Seal initiationASTM F88105–120°CHigher than EVA at 85–100°C; lower than MDPE

    Where SL-1 is compared directly with an EVA sealant web of equivalent gauge, the principal difference is not only seal initiation but also the shape of the seal-strength curve. EVA reaches a peak and then declines rapidly at melt-through temperatures, while LLDPE tends to maintain a broad plateau over 20–30°C above initiation. This plateau allows a static jaw machine to accommodate temperature drift without immediate seal failure. The trade-off is that LLDPE generally produces lower ultimate seal strength than an ionomer or a high-VA EVA at temperatures below 110°C; low-temperature sealing applications should therefore validate the structure across the full jaw temperature range rather than relying on a single setpoint. Relative to a metallocene-catalysed LLDPE laminating web of similar gauge, SL-1 may exhibit a broader seal initiation curve and slightly higher haze depending on the catalyst and additive system. Metallocene LLDPE generally provides lower extractables and a lower seal initiation temperature due to more uniform comonomer incorporation, but may have lower melt strength in extrusion lamination. Selection between SL-1 and mLLDPE should be driven by the lamination method and the required seal-through-contaminant performance rather than by thickness alone. Published comparative data for the exact SL-1 resin differentiation from mLLDPE are limited, and the converter should request seal curves from the film supplier.

    Quantifying Corona Decay Before the Coating Deck

    Incoming SL-1 rolls are normally corona-treated on the laminating side, with wetting tension reported on the roll ticket. A surface energy of 38–42 mN/m by ASTM D2578 is standard for lamination, but the value should be re-checked immediately before coating. Corona treatment decay follows a logarithmic-like loss, with the fastest decay occurring in the first 72 h after film production. Storage temperature above 35°C accelerates additive migration; erucamide and other slip additives can bloom to the surface and partially mask corona-generated polar sites, producing a wetting tension drop of 2–5 mN/m over 4 weeks in published studies of polyolefin webs. When the value falls below 36 mN/m, water-based laminating adhesives exhibit retraction and pinhole voids, while solventless adhesives may still wet if the contact angle is below 10°.

    To re-establish surface energy, in-line corona treatment is applied at a discharge density of 2–4 W·min/m². This is not a surface-cleaning step; it introduces polar oxidation products but can also raise film temperature above 50°C, increasing the risk of blocking if tension is high. The treatment must be uniform across the web because untreated lanes will bond weakly and can be identified by dyne pen testing across the width.

    Processing Setpoints and Acceptance Indicators

    Process VariableMeasurement or StandardAcceptance Range for 76.2 µm LLDPE Laminating Web
    Unwind tensionLoad cell on fly-splice unwind30–80 N/m
    Wetting tension, coating sideASTM D2578≥38 mN/m; solventless tolerance ≥36 mN/m
    Solventless adhesive coat weightInline mass balance1.8–2.5 g/m²
    Lamination nip temperatureContact thermocouple at nip50–70°C
    Heat-seal jaw temperatureVFFS controller setpoint110–135°C
    Seal dwellMachine timer0.3–0.8 s depending on jaw type
    Storage relative humidityFacility RH sensor30–60% RH

    Where the film is used in food-contact structures, compliance is assessed under FDA 21 CFR 177.1520 for olefin polymers, with end-use migration limits under FDA 21 CFR 176.170 or EU 10/2011 as applicable. The main compositional constraints for an unfilled LLDPE web involve total extractables and specific migration of additives rather than residual monomer. The converter should obtain the manufacturer’s statement of compliance for the exact SL-1 roll lot and verify that the adhesive, printing ink, and outer substrate do not introduce migrants that exceed the regulatory limit for the finished package.

    Blocking and Static Charge Control the Storage Envelope

    Rolls of SL-1 should be stored at 10–30°C and protected from direct sunlight. The film begins to soften near 100°C, but local frictional heating at slitter knives or a stalled nip can exceed the blocking threshold. Blocking is evaluated by ASTM D3354; blocking force above 1 N/cm of film width often causes nonuniform unwind and registration drift on the laminator. Static charge in low-humidity conditions can retain dust and increase slip variability. Since LLDPE does not require moisture conditioning, the only storage humidity concern is electrostatic, not dimensional. Rolls should be suspended from end cheeks and never stored on flat surfaces to avoid flat spots at the core transition.

    Top