| HS Code | 987491 |
| Manufacturer | DuPont |
| Brand | Sclairfilm |
| Grade | SL-1 |
| Material | Linear Low Density Polyethylene (LLDPE) |
| Film Type | Laminating Film |
| Thickness | 50.8 µm |
| Thickness Mil | 2.0 mil |
| Density | 0.92 g/cm³ (typical) |
| Yield | 15,000 in²/lb (typical) |
| Tensile Strength Md | 5,000 psi (typical) |
| Tensile Strength Td | 4,500 psi (typical) |
| Elongation At Break Md | 600% (typical) |
| Elongation At Break Td | 700% (typical) |
| Elmendorf Tear Md | 300 g (typical) |
| Elmendorf Tear Td | 400 g (typical) |
| Haze | 5% (typical) |
| Gloss | 80% (typical) |
| Coefficient Of Friction | 0.2 (typical) |
| Water Vapor Transmission Rate | 0.25 g/100 in²/24h (typical) |
| Oxygen Transmission Rate | 150 cc/100 in²/24h (typical) |
| Heat Seal Initiation Temperature | 110 °C (typical) |
| Color | Clear |
| Transparency | Transparent |
| Form | Roll |
| Primary Application | Lamination |
As an accredited DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 50.8 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Each carton contains one roll of DuPont™ Sclairfilm® SL-1 LLDPE laminating film, 50.8 µm thick, sealed in moisture-barrier packaging. |
| Container Loading (20′ FCL) | 20′ FCL dry container loaded with palletized rolls of DuPont Sclairfilm SL-1 LLDPE laminating film, 50.8 µm, properly secured. |
| Shipping | DuPont Sclairfilm SL-1 LLDPE laminating film, 50.8 µm, ships as non-hazardous plastic film rolls in sealed moisture-barrier wrap, boxed or palletized. Store/transport at ambient conditions, away from heat, sunlight, sharp objects, and contamination. No special dangerous goods placards required. Handle rolls with care to prevent punctures, crushing, or edge damage. |
| Storage | Store in a cool, dry, well-ventilated area in original unopened packaging. Keep away from direct sunlight, heat, ignition sources, and oxidizing agents. Protect from moisture, dust, sharp objects, and physical damage. Maintain ambient temperature; avoid extreme temperatures. Keep packaging closed when not in use. Store separately from incompatible materials. Ensure good ventilation. Follow the manufacturer’s safety data sheet and local regulations. |
| Shelf Life | Typically, shelf life is 24 months from date of manufacture when stored in original packaging below 30°C, away from direct sunlight. |
Adhesion of a 50.8 µm laminating-grade LLDPE web to reverse-printed polyester, biaxially oriented polypropylene, or paperboard begins with surface energy control on the bonding face. DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 50.8 µm Thickness is characterized as an olefin polymer film that responds to corona discharge treatment; the converter’s in-line treater is set to maintain 38–42 dyn/cm when tested in accordance with ASTM D2578-23. Lower values produce adhesive channeling and visual fish-eye defects, while corona above 48 dyn/cm may lead to blocking during roll compression. In solventless lamination, the film is transported at 150–300 m/min through a coating station where a two-component polyurethane adhesive is applied at 1.6–2.4 g/m² by a chilled steel anilox roll. The laminate enters a nip at 40–60 °C and 4–8 bar line pressure; the 50.8 µm web is held at 40–80 N/m tension. Peel bond is measured after 24 h at 23 °C and 50 % RH using ASTM F88/F88M-15 at 300 mm/min; for food-contact flexible packaging, a peel strength of at least 2.0 N/15 mm is typical, but the exact target is set by the final pack volume and drop resistance. Food-contact compliance rests on 21 CFR 177.1520 for olefin polymers and Regulation (EU) No 10/2011 for plastic materials intended to come into contact with food. Overall migration testing under EN 1186-1:2002 uses 10 % ethanol at 40 °C for 10 days for dry packaged ambient-temperature foods; converters often specify below 10 mg/dm², but published data for this specific laminating grade must be verified from the roll lot certificate because slip additives, antiblock packages, and adhesive residues influence the total extractable fraction. Hot-bar sealing on vertical form-fill-seal lines is conducted at 95–120 °C, 300–500 kPa, and 0.5–1.0 s dwell; hot tack is measured under ASTM F1921-12. At 50.8 µm thickness, seal initiation temperature is governed by the reverse-printed layer’s heat-sink behavior and the adhesive crosslink density rather than polymer film gauge alone. Side-seal machines running 60–80 packs/min require seal strength above 18 N/25 mm after 24 h aging. The laminate is then exposed to a vacuum leak test at −80 kPa for 60 s. A process boundary is fatty acid amide slip additive migration; if overdosed to reduce coefficient of friction, bond strength can fall below 2.0 N/15 mm, so slip agent concentration is specified in the masterbatch rather than by surface bloom only.
In thermal print finishing, the 50.8 µm LLDPE web is applied to single-side or double-side printed paper and board using a heated chrome roll and a silicone rubber backup roll. The steel roll surface temperature is maintained at 95–115 °C; nip pressures range from 4–8 bar, and line speed is typically 12–30 m/min. At the upper temperature boundary, contact time longer than 0.8 s can produce micro-blocking and surface haze because the film’s outer surface begins to soften before the bond line reaches adhesive activation. Haze is measured by ISO 14782:1999 or ASTM D1003-21; clear laminating-grade polyethylene is frequently specified below 4 % haze, but only if the chill-roll temperature is maintained at 18–25 °C and roll profile deviation does not exceed 5 µm. Curl is the dominant defect in one-sided thermal lamination. Dimensional stability is evaluated by a 24 h oven test at 60 °C using ISO 14616:1997; final curl height is then assessed on the laminated sheet with a digital height gauge, and a curl height above 15 mm on an A4 sheet indicates unbalanced machine-direction tension. The unwind station is therefore operated at 60–100 N/m, and the film is introduced in the orientation opposite to the original wind-curl direction. Anti-blocking agents create micro-roughness on the exposed surface; if the arithmetic roughness (Ra) exceeds 0.15 µm, adhesion to water-based primers becomes insufficient for digital toner overprint varnishes. The bonding face is corona treated to a minimum of 40 dyn/cm under ASTM D2578-23, then coated with a water-based primer at 0.5–1.0 g/m² dry weight. Laminated sheets are cased for 24 h at 23 °C and 50 % RH before guillotine cutting; immediate cutting produces edge lift and visible glue lines. For book cover laminating, fold-line cracking is tested by a 180° single fold at 23 °C; film with elongation at break below 400 % under ASTM D882-18 can show stress whitening, so the specification requires machine-direction and transverse-direction elongation above 400 %.
Medical pouch converting places the 50.8 µm laminating web against a 60–90 µm medical-grade paper or a PET/PE secondary web. The primary quality metric is seal-peak reproducibility after terminal sterilization. A hot-bar sealer with a 6 mm wide jaw and a serrated profile operates at 105–125 °C, 400–600 kPa, and 0.7–1.2 s dwell. Seal strength is tested under ASTM F88/F88M-15 at 200 mm/min with a 25 mm wide specimen; non-peelable pouches generally fall in the 8–15 N/25 mm range, while peelable lidding is engineered for 3–8 N/25 mm to permit clean fiber tear on paper-backed stock. After ethylene oxide sterilization in a 100 % EtO cycle at 50–55 °C and 50–80 % RH, residual gas retention and seal-strength decay are quantified under ISO 10993-7; residual ethylene oxide after aeration must be below 4 mg/device for limited-exposure devices. Gamma irradiation at 25 kGy and 40 kGy under ISO 11137-1:2006 introduces free-radical crosslinking in LLDPE; this raises seal initiation temperature by 2–5 °C and can reduce tear resistance, so sterilizer qualification must use the same dose range as routine production. The film must not contribute to particulate migration; ISO 11607-1:2019 requires package integrity after a 60 s pressure decay test at 20 kPa and bubble emission under 30 kPa immersion. One failure mode observed on continuous band sealers is wax-paper dust adhesion to the film surface; this occurs when paper release coatings are friable. The corrective action is not to raise corona above 45 dyn/cm, because higher surface energy attracts dust, but to install an ionizing air bar before the sealing zone. In form-fill-seal operation, dancer roller oscillation of ±2 mm on a 500 mm web path maintains registration within 0.5 mm.
On pressure-sensitive label lines, the 50.8 µm LLDPE web is converted as a clear overlaminate through a cold nip rather than as a heat-seal layer. The film must exhibit low haze and sufficient stiffness to be die-cut in register at 50–150 m/min. It is unwound at 50–90 N/m and laminated to a printed polyethylene or polypropylene label face at 20–30 °C using an acrylic or rubber-based pressure-sensitive adhesive pre-coated on the film. Adhesion to the adhesive layer is ensured by corona treatment to 40–44 dyn/cm under ASTM D2578-23; untreated areas generate laminate voids at the trailing edge of the web. Mechanical properties are measured under ASTM D882-18; for a 50.8 µm gauge, the tensile strength is generally in the range of 20–40 MPa in the machine direction, with elongation at break above 400 %, but published data for this specific Sclairfilm® grade must be checked against the lot certificate because blown-film orientation affects anisotropic tear resistance. Blocking resistance is quantified by ASTM D3354-96; the release criterion is set by storage temperature and roll compression, because slit rolls stored unrefrigerated above 40 °C can form blocking bands. The overlaminate must remain tack-free on its outer surface; silicone-based process aids that migrate from the film can lower the surface energy and degrade printability, so migratory amide slip agents are specified in the supplier formulation rather than applied by surface transfer. During label dispensing, the overlaminate contributes to flexural stiffness; if caliper variation exceeds ±2 µm across the web, die-cut strike-through and label lifting arise.
| Application context | Key regulatory or quality framework | Principal test method | Typical line release criterion |
|---|---|---|---|
| Food-contact flexible packaging | 21 CFR 177.1520; Regulation (EU) No 10/2011 | EN 1186-1:2002; ASTM F1921-12 | Overall migration below 10 mg/dm² for aqueous/10 % ethanol simulant; seal strength above 18 N/25 mm after 24 h |
| Thermal print finishing | REACH; ISO 14616:1997 dimensional stability | ASTM D1003-21; ISO 14782:1999 | Haze below 4 %; curl height below 15 mm on A4 sheet |
| Medical pouch sealing | ISO 11607-1:2019; ISO 11137-1:2006; ISO 10993-7 | ASTM F88/F88M-15; ASTM F1929-12 | Seal 8–15 N/25 mm non-peelable; EO residual below 4 mg/device |
| PSA overlaminate | REACH; supplier extraction limits | ASTM D2578-23; ASTM D882-18 | Surface energy 40–44 dyn/cm; elongation at break above 400 % |
| Industrial protective lamination | EN 13501-1 where fire class applies; ISO 4892-2 for weathering | ASTM D903-98; ISO 1518-1:2019 | Peel strength above 6 N/25 mm; no micro-cracking after 1000 h xenon |
| Aluminium foil lamination | EU food contact if pouch; cGMP for industrial | ASTM F88/F88M-15; ISO 7765-1:1988 | Peel strength above 4 N/25 mm; dart drop threshold per end-user |
Where decorative paper or metallized facings require a clear protective skin, the 50.8 µm LLDPE web is applied over the substrate with a cold-adhesive or heat-assisted laminator. Adhesive is metered at 40–80 g/m² depending on surface porosity, and the film is nipped at 30–60 °C with a line pressure of 4–8 bar. Because the film has low thermal conductivity and high elongation, it accommodates expansion differences in laminated metal panels; however, its combustion behavior is not suitable for unmodified use where EN 13501-1 Euroclass B or lower is required. The film may be highly transparent but degrades under prolonged xenon-arc exposure; ISO 4892-2 testing for 1000 h at 0.35 W/m², 50 °C black panel temperature, and 50 % RH reveals a loss of elongation before mechanical failure becomes visible. For interior decorative surfaces, scratch resistance is evaluated by a linear scratch test under ISO 1518-1:2019; a 50.8 µm polyethylene film is softer than biaxially oriented polyester, so its hardness is the limiting property. Adhesion to galvanized steel and anodized aluminium requires a primer or a post-applied pressure-sensitive adhesive; peel strength is tested under ASTM D903-98 at a separation rate of 300 mm/min. On insulation facing lines, the film is laminated to aluminium foil or metallized polyester with a solventless adhesive at 1.5–2.5 g/m²; the composite passes continuous backlight inspection where pinhole counts are controlled to internal line specifications. A key processing constraint is film memory: if the roll has been stored at a temperature above 40 °C, the elongation set creates transverse chatter at the nip. Stored rolls are conditioned at 23 °C for at least 12 h before lamination.
When the 50.8 µm laminating film is bonded to 20–40 µm aluminium foil for barrier laminates, the converter must manage foil wrinkling and film-to-foil stiffness mismatch. The film is applied as the reverse-side sealant or as an outer protective layer over the foil. In a dry-bond lamination line, a two-component solvent-free adhesive is applied at 2.0–3.0 g/m², and the film is combined at 50–70 °C with a nip pressure of 4–8 bar. The coated web is held at 80–120 N/m tension in the unwind section; because the LLDPE layer has a lower modulus than foil, any imbalance in web tension produces transverse waviness that propagates into the wind. The composite is cured for 48 h at 40 °C before slitting; early slitting can transfer uncured adhesive to knife edges. Peel strength between foil and film is tested under ASTM F88/F88M-15 at 300 mm/min; for 25 mm strips, values below 4 N/25 mm indicate adhesive undercure or surface contamination. The film’s elongation at break under ASTM D882-18 provides puncture resistance; when the laminate is used as a barrier pouch for pet food or bulk industrial powders, a dart drop impact test under ISO 7765-1:1988 is applied. A 125 g dart from 500 mm height is one internal qualification threshold, but published data for the specific Sclairfilm® SL-1 configuration is limited because the result depends on adhesive lamination thickness and foil temper. Moisture vapor transmission rate is governed by the foil, not the polyethylene layer; the converter does not attempt to measure the LLDPE film alone. The critical incompatibility is with loose aluminium oxide particles from foil edges; these particles embed in the polymer surface during slitting and form pin-holes when the film is subsequently heated above 70 °C. Slitting dust extraction and edge cleaning are therefore required.
Competitive DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 50.8 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont™ Sclairfilm® SL-1 is supplied as a 50.8 µm nominal-gauge linear low-density polyethylene cast film intended for laminating and heat-seal applications in flexible packaging. The product code SL-1 identifies the grade within the Sclairfilm family; the web is usually positioned as the inner sealant layer in duplex or triplex laminates where oriented polyester, biaxially oriented polypropylene, paper, or aluminium foil delivers primary stiffness, print surface, or barrier. The LLDPE layer contributes seal integrity, puncture resistance, and moisture resistance rather than oxygen barrier. Because surface treatment level, slip/antiblock package, and coefficient of friction are subject to commercial lot variation, converters should not qualify the material for high-speed form-fill-seal use solely on the generic designation; the certificate of analysis must be compared with the print, lamination, and sealing conditions of the specific packaging line.
At the stated 50.8 µm gauge, the theoretical basis weight is approximately 46.7 g/m² when the film density is taken as 0.920 g/cm³. A density change of 0.010 g/cm³ shifts the calculated basis weight by roughly 0.5 g/m², which is significant for roll-length estimation and adhesive coatweight calculation. Thickness verification should follow ASTM D5947 or ISO 4593, and mechanical testing should be conducted after conditioning to ASTM D618 at 23 ± 2 °C and 50 ± 5% RH. Because the film is hydrophobic, moisture absorption is negligible, but surface condensation and static decay vary with storage humidity and can alter unwind performance on laminators.
The grade is classified as a single-layer linear low-density polyethylene film. Unlike low-density polyethylene produced by high-pressure free-radical polymerization, LLDPE contains short-chain branches introduced by an alpha-olefin comonomer. This molecular structure raises the concentration of tie molecules between crystalline lamellae and shifts the mechanical response toward higher elongation at break and greater puncture resistance when compared at equal thickness. The cast-film conversion route used for this laminating grade typically yields a surface with lower haze and better thickness uniformity than blown-film equivalents, but the absence of biaxial orientation reduces the tensile modulus in the transverse direction relative to oriented polyester or biaxially oriented polypropylene.
The nominal density of an LLDPE laminating web of this class falls between 0.918 g/cm³ and 0.930 g/cm³. Density below 0.918 g/cm³ would move the material toward plastomer behavior with lower stiffness and higher tack, while density above 0.930 g/cm³ would increase crystallinity and raise the seal initiation temperature. Melt-flow-rate data for LLDPE cast-film resins often lie between 1 g/10 min and 4 g/10 min at 190 °C under 2.16 kg, measured by ASTM D1238 or ISO 1133-1:2022. Converters comparing SL-1 with alternative sealant webs should request density, melt-flow-rate, and comonomer-type data from the lot certificate rather than relying on category-level values.
| Parameter | Reference band | Test standard |
|---|---|---|
| Thickness | 50.8 µm nominal; ±5% typical commercial tolerance | ASTM D5947 |
| Basis weight | 46.7 g/m² calculated at 0.920 g/cm³ | calculated |
| Density | 0.918–0.930 g/cm³ | ASTM D1505 |
| Wetting tension | 38–42 mN/m | ASTM D2578 |
| Tensile strength | MD 20–45 MPa; TD 15–35 MPa | ASTM D882 |
| Elongation at break | 400–800% | ASTM D882 |
| Dart impact | 60–150 g at 50.8 µm | ASTM D1709 |
| Elmendorf tear | MD 100–300 g; TD 300–700 g | ASTM D1922 |
| Haze | 2–10% | ASTM D1003 |
| Kinematic coefficient of friction | 0.2–0.6 | ASTM D1894 |
These values are typical of 50.8 µm LLDPE cast laminating films; actual SL-1 batch values may fall outside the band and must not be used as vendor acceptance limits without written confirmation.
Laminating a 50.8 µm LLDPE web on a high-speed converting line imposes different demands from blown-film sealing or pouch stock. On a solventless laminator with steel and rubber nip rolls, the PE web should be unwound with a controlled tension typically below 100 N/m width to avoid necking and tunneling in the final laminate. If the film is used as the secondary web in an adhesive laminating process, the adhesive coatweight for a solventless polyurethane system is commonly set between 1.2 g/m² and 1.8 g/m², but the exact level must be determined by the adhesive supplier for the substrate roughness and surface energy of the primary web. Lower coatweight can create skip-lamination on high-frequency heat-seal areas; higher coatweight may increase solvent retention or cure time.
The heat-seal response of LLDPE sealant layers is usually characterized by a hot-tack curve rather than a single seal initiation value. In flexible packaging operations, the sealant web is expected to maintain hot-tack strength during vertical form-fill-seal filling when the package jaw opens while product still exerts a drop load. Test methods for this property include ASTM F1921 for hot-tack strength and ASTM F2029 for heat-seal curves. A typical LLDPE cast sealant web of this gauge may display seal initiation between 90 °C and 115 °C, but the actual SL-1 response must be generated from the lot-specific curve because the comonomer type and additive package shift the plateau.
For extrusion lamination, the thermal load from the molten polyethylene curtain can soften the 50.8 µm film if it is used as a preformed web rather than as the melt layer. The melt temperature for LLDPE extrusion lamination often ranges from 290 °C to 330 °C, and chill-roll temperature is usually held between 15 °C and 30 °C. If the SL-1 web is instead the outer sealant layer and not the melt carrier, the main risk is thermal shrinkage at the nip; converters should verify shrinkage performance using ASTM D2732 or equivalent and adjust line speed so that the web residence time under the melt curtain remains below the distortion threshold.
Compared with a conventional low-density polyethylene laminating film of the same gauge, an LLDPE web such as Sclairfilm® SL-1 generally provides higher dart impact strength when measured under ASTM D1709, higher Elmendorf tear strength under ASTM D1922, and a lower seal initiation temperature under ASTM F2029. These differences arise from the linear backbone and controlled short-chain branching of LLDPE. In pouch and pillow-pack structures, this permits either a downgauging exercise from 60 µm to 50 µm or an improvement in drop resistance at constant gauge. However, LLDPE does not match the clarity of a metallocene-catalysed LLDPE film in all cases, and it may exhibit a broader melting endotherm, which can widen the heat-seal range but also reduce the sharpness of seal initiation when compared with certain plastomer sealants.
When the comparison is made against metallocene-catalysed LLDPE, the conventional SL-1 class may show lower hot-tack peak values in the 100 °C–120 °C jaw-temperature interval and may require a higher seal bar temperature to reach equivalent seal strength. On the other hand, conventional LLDPE laminating webs often have adequate process stability in adhesive lamination because the broader molecular weight distribution reduces melt resonance and edge weave on cast extrusion lines. The converter should not infer that all cast LLDPE films are interchangeable; the additive package affects coefficient of friction and surface wetting tension, and these factors control feed-ability on form-fill-seal machines using ASTM D1894 friction measurements and ASTM D2578 wetting tension checks.
Against a high-vinyl-acetate EVA sealant film, the LLDPE web offers better moisture resistance and lower surface tack, but EVA generally provides a lower heat-seal initiation temperature and higher hot tack at very low sealing temperatures. Thus Sclairfilm® SL-1 is better suited to dry-product packaging, frozen-food laminates, and general moisture-resistant pouches than to high-speed cold-seal replacements. The selection between SL-1 and EVA or ionomer sealants should be made through a structured design-of-experiments measuring seal strength on the production jaw at ASTM F88/F88M and drop performance using the actual package geometry rather than through material type alone.
Surface treatment on the 50.8 µm web is critical for lamination. LLDPE is non-polar, and untreated film typically shows a wetting tension below 31 mN/m, which is inadequate for most laminating adhesives and printing. Corona treatment used on the cast-film line raises the wetting tension to a target of 38–42 mN/m measured under ASTM D2578. Treatment above 48 mN/m is generally unnecessary for lamination and may create brittle oxidized species that reduce heat-seal strength or promote blocking during roll storage. The treated side must be identified on the roll ticket; lamination to the untreated side causes adhesive delamination at the polyethylene interface even when the adhesive itself has cured.
Storage conditions and reel handling introduce batch-to-batch operational boundaries. The film should be stored at 10–30 °C and below 60% RH, with reels allowed to equilibrate to the converting room before unwinding. If a cold reel is brought into a humid laminating hall, condensation on the treated side can hydrolyse moisture-sensitive polyurethane adhesives or reduce surface energy locally. Do not store reels in direct sunlight or above 40 °C because slip additive migration to the surface can reduce wetting tension and alter coefficient of friction. On a slitter or laminator, damaged core plugs and soft winding can induce camber and web wander; these defects are not corrected by the film itself and become visible as wrinkle-lamination defects on gravure or adhesive coating stations.
| Requirement | Reference | Verification |
|---|---|---|
| U.S. food contact | 21 CFR 177.1520 | supplier certificate of compliance |
| EU plastic food contact | EU 10/2011 | overall migration under EN 1186 if applicable |
| REACH | EC 1907/2006 | SVHC declaration |
| RoHS | Directive 2011/65/EU | not applicable unless converted into electrical/electronic article |
Regulatory verification for direct food-contact use must confirm that the formulated film meets 21 CFR 177.1520 for olefin polymers in the United States and EU 10/2011 for plastic materials and articles intended to come into contact with food in the European Union. The final laminate must also account for the adhesive and primary substrate: the adhesive layer should be covered by 21 CFR 175.105 where applicable, and the total migration of the complete structure should be evaluated under EN 1186 conditions if the package is sold into EU food-contact applications. REACH compliance under EC 1907/2006 and RoHS compliance under Directive 2011/65/EU are usually declared by the supplier on request. Because published data for this specific product configuration can be limited, the certificate of conformance is the controlling document for lot-specific regulatory status.