| HS Code | 977242 |
| Material | Linear Low Density Polyethylene (LLDPE) |
| Application | Laminating |
| Thickness | 38.1 µm |
| Density | 0.920 g/cm³ |
| Tensilestrengthmd | 30 MPa |
| Tensilestrengthtd | 26 MPa |
| Elongationatbreakmd | 550% |
| Elongationatbreaktd | 650% |
| Tearstrengthmd | 3.5 N |
| Tearstrengthtd | 4.5 N |
| Dartdropimpact | 110 g |
| Haze | 12% |
| Gloss | 70% |
| Coefficientoffriction | 0.20 |
| Heatsealinitiationtemperature | 115°C |
| Meltingpoint | 122°C |
| Watervaportransmissionrate | 15 g/m²/24h |
| Oxygentransmissionrate | 2000 cm³/m²/24h/atm |
As an accredited DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 38.1 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DuPont™ Sclairfilm® SL-1 LLDPE laminating film, 38.1 µm, supplied as 5 rolls per carton, each roll 300 m, moisture-barrier wrapped. |
| Container Loading (20′ FCL) | 20′ FCL loaded with palletized rolls of DuPont™ Sclairfilm® SL-1 LLDPE laminating film, 38.1 µm thick, secured for transport. |
| Shipping | Non-hazardous and not regulated for transport. Supplied in protective-wrapped rolls, boxed or palletized. Keep dry, clean, and out of direct sunlight; avoid heat, sharp objects, and compression. No UN number, hazard class, or special shipping label required. Handle carefully to prevent punctures and contamination. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep in original, sealed packaging to protect from dust, moisture, and physical damage. Maintain 15–25 °C and moderate humidity. Store rolls horizontally or as recommended, avoiding compression. Keep away from sharp objects and UV radiation. Do not stack heavy items on rolls. |
| Shelf Life | Shelf life is 12 months from date of shipment when stored at 21°C (70°F) and 50% relative humidity in original packaging. |
In dry-food and powdered-beverage flexible packaging, the DuPont™ Sclairfilm® SL-1 38.1 µm laminating web is introduced as the innermost heat-seal layer after a corona treatment step that raises surface energy to 38–42 mN/m as measured under ASTM D2578-17. This activation band is a process window, not a storage condition: below 36 mN/m solventless polyurethane adhesive wets unevenly and bond-strength failures appear under ASTM F904-16; above 46 mN/m the film tends to block in roll form after 48 hours of warehouse storage. Roll-to-roll variation in corona-treated wetting tension should be held within ±2 mN/m, because wider swings create periodic bond-strength valleys on individual slitter lanes. The nominal basis weight of the layer, calculated from the typical LLDPE density interval 0.918–0.922 g/cm³, is 35.1 g/m². In an adhesive lamination with reverse-printed 12 µm polyester or 20 µm biaxially oriented polypropylene, the SL-1 layer contributes 55–65% of the finished laminate mass before ink and adhesive solids are added. This layer-mass fraction, rather than a compounding percentage, is the addition ratio that determines roll yield, adhesive demand per square metre, and sealant availability on the package perimeter.
Lamination is run on a solventless laminator with five-roll metering at 1.4–2.2 g/m² of aliphatic polyurethane adhesive. Nip temperature is held at 60–80 °C, and the wound stock is cured for 24–48 hours at 35–40 °C before slitting. Retained solvent in the printed web must be below 5 mg/m² before lamination to avoid odour and bond decay on high-speed pouch lines. On horizontal form-fill-seal machines, jaw temperatures between 115 °C and 145 °C with dwell 0.25–0.55 s and jaw pressure 0.3–0.5 MPa are used to produce seal strengths above 12 N/25 mm on peel coupons tested under ASTM F88/F88M-21. Hot-tack performance is screened under ASTM F1921-18 Method B at 0.2–0.4 s delay to ensure the pouch does not creep or burst when filled at 120 pouches/min on vertical lines. For direct food contact, the film layer is evaluated under FDA 21 CFR 177.1520(c) 3.1a and 3.2a and under European Commission Regulation (EU) No 10/2011; migration testing is conducted according to Annex III food simulant selection for the intended dry-food contact profile. Finished terminal types include three-side-seal sachets for dried soup, quad-seal stand-up pouches for flavoured rice mixes, stick packs for powdered beverages, and bag-in-box liners for cereal ingredients. The principal operational limitation is storage after corona treatment: if relative humidity exceeds 60% for more than 24 hours before lamination, water uptake on the oxidised surface reduces bond strength and can generate channel leaks at pouch corners.
When clay-coated paper pouch stock is run against the 38.1 µm sealant layer, the first measurable conflict appears at adhesive coat weights above 2.8 g/m², not from the SL-1 film itself but from migration of low-viscosity solventless adhesive components into the mineral clay coating. The film layer, at 35.1 g/m², is bonded to bleached or clay-coated kraft in the range 40–60 g/m², so the PE layer contributes 36–45% of the finished web mass depending on paper substance and adhesive solids. A converter-applied primer at 0.3–0.6 g/m² dry weight restores adhesion on high-clay surfaces and reduces tunneling after roll cure. Paper moisture content is held at 6–8% before lamination; outside this band, dimensional change creates curl and misregister on the pouch line. The paper component is assessed under U.S. 21 CFR 176.170, the polyethylene layer under 21 CFR 177.1520, and European compliance is established through Regulation (EC) No 1935/2004 and (EU) No 10/2011 for the plastic layer; printed surfaces are evaluated under Swiss Ordinance 817.023.21 where export lots require it.
Production lamination is conducted on an in-line flexographic laminator on which the corona-treated SL-1 film is bonded to the printed paper web. Slitting dust from the paper side can transfer to the activated PE surface and create fisheyes, so slitter vacuum and web-cleaning rollers are installed before the coating station. The adhesive is metered at 2.0–3.0 g/m², oven drying is staged at 70 °C / 85 °C / 95 °C, and the combining nip is held at 75–85 °C. After slitting, the material is converted into single-portion pouches on high-speed machinery with serrated seal jaws. The paper side remains below the sealant-seal initiation threshold unless the jaw temperature is raised to 140–165 °C and dwell is extended to 0.4–0.9 s at 0.3–0.6 MPa to compensate for the insulating effect of the paper web. Finished terminal products include sugar stick packs, single-serve salt and pepper pouches, bakery mix bags, and paper-based confectionery sachets. The operational boundary is delamination caused by excessive adhesive coat weight on highly absorptive clay coatings; process validation should include a 48-hour bond-strength check under ASTM F904-16 and a seal-strength test under ASTM F88/F88M-21 after conditioning at 23 ± 2 °C and 50 ± 5% RH.
| Downstream cell | SL-1 mass fraction | Adhesive/coating weight | Sealing or welding window | Verification method |
|---|---|---|---|---|
| Dry-food PET/BOPP laminate | 55–65% | 1.4–2.2 g/m² solventless PU | 115–145 °C, 0.25–0.55 s | ASTM F88/F88M-21; ASTM F1921-18 |
| Clay-coated paper pouch | 36–45% | 2.0–3.0 g/m² laminating adhesive | 140–165 °C, 0.4–0.9 s | ASTM F904-16; ASTM F88/F88M-21 |
| Frozen food VFFS laminate | 62–67% | 1.3–1.8 g/m² solventless PU | 120–150 °C, 0.35–0.60 s | ASTM F88/F88M-21; ASTM F392-93(2019) |
| Aluminium foil insulation facing | 58–63% | 2.2–3.5 g/m² two-component PU | 280–330 °C hot-air welding | ASTM C1136; ASTM E96/E96M |
| Medical sterile barrier top web | 62–65% | 1.8 g/m² solvent-free adhesive | 120–160 °C, 0.4–1.0 s | ISO 11607-1:2019; ASTM F88/F88M-21 |
| Multiwall paper sack inner ply | 20–28% | 4–6 g/m² wet PVAc dispersion | 165–190 °C, 1.0–1.5 s impulse | ASTM F88/F88M-21 |
For vertical form-fill-seal lines running frozen vegetable and prepared potato products, the 38.1 µm SL-1 web is selected less for optical clarity than for low-temperature seal integrity after the package has been shock-frozen to −25 °C. The laminate commonly pairs this film with a 15 µm biaxially oriented polyamide or 12 µm polyester outer web, placing the SL-1 layer at 62–67% of total film mass when adhesive solids are included. At 35.1 g/m², the layer provides adequate drop impact resistance for free-flowing frozen vegetables, but converters using bone-in IQF meat or seafood regularly qualify a 50 µm or 75 µm LLDPE replacement because puncture resistance under ASTM F1306-19 falls below line acceptance for sharp protrusions. Preheating of the film web to 30–35 °C before corona and adhesive coating reduces condensation defects on high-humidity production days and stabilises the wetting tension response.
Food-contact compliance in frozen applications is verified under FDA 21 CFR 177.1520(c) 3.2a and (EU) No 10/2011. Lamination process control uses a solventless adhesive applied at 1.3–1.8 g/m², combining nip at 70 °C, and 48-hour cure at 40 °C. The pouch maker runs seal jaws at 120–150 °C with dwell 0.35–0.60 s and pressure 0.30–0.45 MPa, and packaging lines set a maximum film-to-metal coefficient of friction of 0.30 measured under ASTM D1894-14 to avoid film tracking failures at 100–140 pouches/min. Batch-to-batch variance in slip additive levels changes COF by ±0.04; incoming rolls should be audited when maximum COF is a critical process parameter. Gelbo flex testing under ASTM F392-93(2019) at −18 °C verifies that the sealant layer does not develop pinholes after repeated flexing in cold-chain distribution. Finished terminal products include frozen vegetable pillow packs, French fry bags with side gussets, IQF fruit pouches, and frozen seafood bags. The operational limit appears when the pouch is expected to survive drops at or below −30 °C; standard practice is to increase seal-layer thickness or move to a compounded metallocene LLDPE with a lower brittle point.
Once the 38.1 µm film is combined with aluminium foil, the insulation facing laminate shifts from a heat-seal-first design to a vapour-barrier-first design. The 7 µm or 9 µm foil supplies the low-permeance core, while the SL-1 layer provides a corrosion-resistant interior surface that also prevents pinhole propagation during embossing. The total nominal thickness is 45–47 µm before adhesive, with the polyethylene layer contributing 58–63% of the laminate mass based on foil density 2.70 g/cm³ and film density 0.920 g/cm³. This mass contribution matters for roll yield calculations on 1,250 mm wide insulation-facing laminators, where a 35.1 g/m² film layer increases roll weight without adding water vapour permeance.
Lamination is performed on a two-tower gravure coating line. The adhesive is a two-component polyurethane applied at 2.2–3.5 g/m² dry weight; the first drying zone is set to 70 °C, the second to 90 °C, the third to 110 °C, and the combining nip is held at 80–85 °C. Curing proceeds for 48 hours at 40 °C before embossing or slitting. In downstream fabrication, the laminate is embossed with roll depth of 0.4–0.6 mm and slit into facings for flexible fiberglass blankets, rigid board, and duct wrap. Welding of facing edges on-site uses hot-air or wedge welders at 280–330 °C air temperature; below this range the LLDPE surface does not form a homogeneous weld, and above this range oxidation at the interface creates brittle weld lines.
Compliance is established against ASTM C1136 for flexible vapor retarders used in thermal insulation, with water vapour permeance tested under ASTM E96/E96M desiccant method. Mechanical properties are measured under ASTM D882-18 for tensile strength and elongation, while bond strength after lamination is screened using ASTM F904-16. European sales require REACH Regulation (EC) No 1907/2006 and, for HVAC ancillary electrical components, Directive 2011/65/EU RoHS with lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE limits at 0.1% by weight in homogeneous materials, except cadmium at 0.01%. For duct wrap installations in U.S. jurisdictions, minimum flame and smoke classifications may be evaluated under ASTM E84, but that test belongs to the facing system as installed, not to the polyethylene layer alone.
Medical device pouch validation subjects the 38.1 µm SL-1 film to a different set of acceptance criteria than food packaging; seal strength to uncoated Tyvek® 1073B and to medical paper under ISO 11607-1:2019 is the primary performance gate. The film is commonly laminated to a 12 µm polyester top web, producing a total thickness near 50 µm and a sealant-layer mass fraction of 62–65% when adhesive at 1.8 g/m² is included. The thickness contribution is held constant because the sterile barrier must survive package validation, handling, and transport without tearing at peeled seals. Retained solvent in the lamination must be below 5 mg/m² before pouch conversion to prevent cytotoxic residue failures after sterilisation.
Manufacturing lamination uses a solvent-free adhesive that meets ISO 10993-5:2009 and ISO 10993-10:2021 requirements after full cure. Pouch fabrication on horizontal sterile-barrier machines runs seal bars at 120–160 °C with dwell 0.4–1.0 s and pressure 0.3–0.6 MPa. Seal strength is measured under ASTM F88/F88M-21; typical acceptance windows for Tyvek are 1.5–3.5 N/15 mm, while paper pouches are accepted with peel strengths between 2.5 N/15 mm and 5.0 N/15 mm, because higher values indicate fibre tear of the paper rather than clean peel. Dye penetration testing is carried out under ASTM F1929-15 and whole-pouch leak testing under ASTM F2096-11. Sterilization compatibility is defined for ethylene oxide and low-dose electron beam processes. The operational limitation for this film is repeated gamma irradiation; doses above 25–40 kGy can reduce elongation and seal strength due to free-radical chain scission, so converters must requalify after maximum accumulated dose testing.
Terminal finished goods include pre-sterile flat pouches for syringes, IV line kits, catheter sets, wound care kits, and form-fill-seal pouches for lightweight disposable devices. The ready-to-sterilize pouch must remain within ISO 11607-2:2019 packaging process requirements, with seal parameters recorded on every lot to demonstrate that the 38.1 µm layer remains within qualified limits.
After slitting, the 38.1 µm film is web-laminated to the inner face of a 70–90 g/m² natural kraft ply with a water-based polyvinyl acetate dispersion applied at 4–6 g/m² wet weight and dried in a three-zone tunnel at 60 °C / 75 °C / 90 °C. In the finished sack, the PE film layer contributes 20–28% of the empty sack mass, while the paper plies and adhesive carry the structural load. This proportion is used for dust retention and moisture ingress calculations, not as structural reinforcement. Laminated web moisture is held below 10% before sack forming to prevent curl at the pasted bottomer line.
Compliance for food-grade powders is evaluated under FDA 21 CFR 177.1520 for the polyethylene layer and 21 CFR 176.170 for the paper component. European Union food-contact status is established under (EU) No 10/2011 for the film, while chemical and feed applications require only REACH (EC) No 1907/2006 substance registration and, where export packaging is regulated, UN package performance certification under the applicable modal code. The process limitation is that high-slip surface additives in the film, specified by the converter as coefficient of friction 0.20–0.35 against polished steel under ASTM D1894-14, can reduce heat-seal strength if they exude during the 40–50 °C warehouse ageing period. Published peel strength values for this exact 38.1 µm film on high-slip paper sack grades are limited; therefore, line qualification is performed using ASTM F88/F88M-21 on retention samples rather than relying on generic LLDPE seal-strength curves.
The process slits roll stock into tube stock for stepped-end, pinch-bottom, and pasted-valve sacks. Terminal finished packages include 10–25 kg sacks for milk powder, flour, sugar, fine chemical powders, and hygroscopic feed ingredients. Spout sealing on automatic filling lines uses impulse sealers at 165–190 °C for 1.0–1.5 s; lower temperatures leave leak paths in the PE ply, while higher temperatures burn through the 38.1 µm web at the spout edge. Fines from the filled product can accumulate on the film surface and interfere with impulse sealing, so vacuum pickups are positioned to remove dust immediately before the spout is sealed.
| End use | Component regulated | Standard or regulation | Key limit / test method |
|---|---|---|---|
| Dry-food flexible packaging | LLDPE sealant layer | FDA 21 CFR 177.1520(c) 3.1a/3.2a; (EU) No 10/2011 | Overall migration 10 mg/dm² |
| Paper-based food pouch | Paper and PE layer | FDA 21 CFR 176.170; (EU) No 10/2011; Swiss 817.023.21 | Component-specific migration; ink compliance |
| Frozen food pouch | PE sealant; laminate | FDA 21 CFR 177.1520(c) 3.2a; (EU) No 10/2011 | Low-temperature seal integrity; migration |
| Insulation facing | Complete laminate | ASTM C1136; ASTM E96/E96M; REACH (EC) No 1907/2006; RoHS 2011/65/EU | Low-permeance classification; 0.1% hazardous substances |
| Medical sterile barrier | Adhesive and sealant layer | ISO 11607-1:2019; ISO 10993-5:2009; ISO 10993-10:2021 | Seal strength, dye penetration, cytotoxicity |
| Multiwall paper sack | PE film and paper | FDA 21 CFR 177.1520; 21 CFR 176.170; REACH (EC) No 1907/2006 | Food-contact migration; REACH registration |
Competitive DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 38.1 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont™ Sclairfilm® SL-1 is a linear low density polyethylene (LLDPE) laminating web supplied at a nominal thickness of 38.1 µm, equivalent to 1.5 mil. The product is specified as roll goods for adhesive lamination to oriented polyester, biaxially oriented polypropylene, aluminium foil, and paperboard, where it typically functions as an interior sealant ply rather than as a printed surface or barrier layer. The SL-1 designation identifies the manufacturer’s laminating formulation within the Sclairfilm family; full technical specification, including roll width, core inner diameter, corona treatment level, and slip/antiblock package, is controlled by the product data sheet and certificate of analysis. Incoming material should not be assumed to be two-side treated: treated and untreated surfaces may be present, and wetting tension must be confirmed by ASTM D2578-17. Relative to a high-pressure LDPE laminating web of the same gauge, the LLDPE chemistry provides higher tensile strength, puncture resistance, and elongation under ASTM D882-18 and ASTM D1709-16a, but it also raises melt viscosity and shear heating during extrusion. These differences are material-architecture effects, not additive effects; the linear copolymer backbone alters deformation behavior without changing the polar surface chemistry of polyethylene.
Conversion of SL-1 class LLDPE laminating film involves cast or blown film extrusion followed by primary and secondary web handling that is sensitive to temperature, line speed, and winding tension. On a cast-film line, the melt temperature should be held within 210–250 °C; at lower temperatures, the copolymer may exhibit flow lines or poor draw, while above 260 °C oxidative degradation may shift extractables and color. The die lip gap is commonly set between 0.5 mm and 0.8 mm, with the air gap kept short—10–30 mm—to minimize neck-in and edge bead. Chill roll temperatures in the range of 20–30 °C are typical for clarity and blocking resistance. Production-scale experience on cast-film lines with 30:1 L/D extruders indicates that screw speed and back-pressure are higher than for high-pressure LDPE at equivalent output; barrel zones should therefore be profiled to avoid excessive shear heating above 250 °C at the melt flange.
Primary web treatment for lamination should target a wetting tension of 38–42 mN/m on the adhesive-receiving surface. Treatment decay is nonlinear; rolls stored at ambient warehouse temperatures may retain acceptable levels for several months, but hot or humid storage accelerates decay. QC should measure treatment on the intended laminating side at 24 h after treatment and again before lamination. Winding tension must be controlled to avoid axial wrinkles because thin LLDPE has low bending stiffness and will form gauge bands if the winding profile exceeds ±5% of set tension.
Published SL-1-specific data are vendor-controlled; however, class-typical values for a 38.1 µm cast LLDPE laminating web provide a useful incoming QC envelope. The table below is not a substitute for the commercial certificate of analysis and should be used only for preliminary incoming inspection limits. Testing is conducted after 40 h conditioning at 23 ± 2 °C and 50 ± 5% relative humidity unless otherwise specified.
| Property | Typical window | Test protocol |
|---|---|---|
| Nominal thickness | 38.1 µm (1.5 mil) | ASTM D6988-21 / ISO 4593:2013 |
| Tensile stress at break, MD | 25–45 MPa | ASTM D882-18 / ISO 527-3:2018 |
| Tensile stress at break, TD | 20–35 MPa | ASTM D882-18 / ISO 527-3:2018 |
| Elongation at break, MD | 400–700% | ASTM D882-18 |
| Elongation at break, TD | 500–800% | ASTM D882-18 |
| Elmendorf tear, MD | 300–800 gf | ASTM D1922-15 |
| Elmendorf tear, TD | 500–1,200 gf | ASTM D1922-15 |
| Dart impact | 150–400 g | ASTM D1709-16a, Method A |
| Haze | 1.0–3.0% | ASTM D1003-21 |
| Gloss at 45° | 75–95 GU | ASTM D2457-21 |
| Kinetic coefficient of friction, film-to-film | 0.15–0.35 | ASTM D1894-14 |
These values reflect the LLDPE cast-film class rather than a guaranteed specification for every SL-1 lot. If a particular laminate requires tensile strength above 40 MPa or haze below 1.5%, the converter should request a lot-specific certificate of analysis and compare against the product data sheet. The greatest variability is usually in tear and dart impact because those tests are sensitive to gauge distribution and orientation; a coefficient of variation above 10% within a roll often signals draw resonance or chill roll temperature drift.
Differentiation from other lamination films is best made on the basis of seal initiation, hot-tack, tensile strength, optics, and cost. High-pressure LDPE laminating films process at lower melt temperatures and provide a broad seal-peel plateau, but their tensile strength and dart impact are lower at equal thickness. Ethylene vinyl acetate films provide lower seal initiation and higher flex resistance, but introduce vinyl acetate monomer migration potential and higher odor. Single-site metallocene LLDPE webs may offer better optics and lower seal initiation than conventional LLDPE such as SL-1, but their low seal strength in contaminated environments and higher resin cost can be drawbacks. SL-1 therefore competes most directly against conventional LDPE and general-purpose LLDPE laminating films for dry-food pouches, multi-wall bag liners, and industrial adhesive lamination where barrier is supplied by a different ply. Seal initiation temperatures for conventional LLDPE typically fall between 90 °C and 110 °C; published SL-1-specific hot-tack curves are limited.
Compared with blown LLDPE laminating film, cast SL-1 class webs generally yield lower haze, higher gloss, and more uniform thickness, but the transverse-direction tear strength is lower because cast film orientation is unbalanced. This distinction matters for laminates that will be punctured in the transverse direction or subjected to high-speed packaging machine stress. For blown-film iterations, the frost line height and blow-up ratio can be adjusted to balance tear; published data for this specific configuration is limited if the product is not supplied as blown film.
Solventless polyurethane lamination imposes stricter controls than water-based or solvent-based adhesives because the adhesive is applied at 1.0–2.5 g/m² and relies on surface wetting and controlled migration. For SL-1, the adhesive-receiving surface should be treated to 38 mN/m or higher; if wetting tension falls below 36 mN/m, surface coverage may be incomplete and bond strength after cure may drop. Extractable or migratory slip additives can interfere with isocyanate crosslinking, particularly when the film is stored at elevated temperature. Lamination bond strengths measured by ASTM F904-16 should be checked after 24 h and 48 h to distinguish delayed cure from permanent adhesive failure. If the structure is intended for retort or hot-fill, the film’s antioxidant package and adhesive crosslinker must be confirmed for the specific thermal cycle.
Incoming rolls should be stored at 5–35 °C and 30–70% relative humidity, away from direct sunlight and ozone-generating equipment. Roll blocking may occur if wound with excessive tension at temperatures above 35 °C. If the film is to be used as a heat-seal layer, seal conditions should be established by ASTM F1921-12 for hot-tack and ASTM F88/F88M-21 for seal strength; typical seal initiation for LLDPE laminating films is in the 90–110 °C jaw-temperature range, but jaw pressure and dwell must be optimized for the entire laminate, not for the film alone.
Food-contact status for SL-1 is governed by olefin polymer regulations in the intended market. For the United States, the film must meet FDA 21 CFR 177.1520, which covers olefin polymers, with end-use conditions of use selected by the converter. For the European Union, compliance is evaluated under Regulation (EU) No 10/2011, with an overall migration limit of 10 mg/dm² and specific migration limits for additives supplied in the formulation. A complete declaration should include the certificate of compliance and lot-specific analytical data for antioxidants, slip agents, and antiblock materials. The product is not inherently an oxygen or moisture barrier; regulatory compliance does not imply barrier performance.
| Obligation | Standard or regulation | Typical documentation |
|---|---|---|
| US food contact | FDA 21 CFR 177.1520 | Certificate of compliance |
| EU plastic food-contact | Regulation (EU) No 10/2011 | Declaration of compliance |
| Overall migration limit | 10 mg/dm² | Commission Regulation methods |
| General safety | EC 1935/2004 | GMP evidence |
| REACH | EC 1907/2006 | SVHC status |
| RoHS heavy metals | Directive 2011/65/EU | Pb 0.1% wt, Cd 0.01% wt |
Operational boundaries include the absence of high barrier properties, limited high-temperature retort resistance unless explicitly specified, and incompatibility with strong oxidizing acids or prolonged outdoor UV exposure. The film should not be combined with amine-based adhesion promoters unless the supplier confirms that no surface reaction accelerates slip-agent exudation or compromises seal performance. If the lamination will be used for medical device packaging, additional ISO 11607-1:2019 validation is required; the material supplier’s food-contact certificate does not by itself establish the package as a sterile barrier system.