| HS Code | 293194 |
| Material | Linear Low-Density Polyethylene (LLDPE) |
| Thickness | 25 µm |
| Density | 0.920 g/cm³ |
| Tensilestrengthmd | 35 MPa |
| Tensilestrengthtd | 30 MPa |
| Elongationatbreakmd | 500% |
| Elongationatbreaktd | 600% |
| Tearstrengthmd | 200 g |
| Tearstrengthtd | 250 g |
| Dartdropimpact | 100 g |
| Haze | 10% |
| Gloss45 | 80 |
| Coefficientoffriction | 0.2 |
| Watervaportransmissionrate | 15 g/m²/24h |
| Oxygentransmissionrate | 2500 cm³/m²/24h |
| Heatsealstrength | 10 N/15mm |
| Sealinitiationtemperature | 110°C |
| Meltingpoint | 125°C |
| Vicatsofteningpoint | 95°C |
| Yield | 43.5 m²/kg |
As an accredited DuPont™ Sclairfilm® MPP-3 LLDPE Film, "Super Strength", 25 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DuPont™ Sclairfilm® MPP-3 LLDPE Super Strength film, 25 µm thick, supplied as one roll per carton, ten rolls per case. |
| Container Loading (20′ FCL) | 20′ FCL: load palletized DuPont Sclairfilm MPP-3 LLDPE Film, 25 µm, in dry, ambient conditions; secure cargo within weight limits. |
| Shipping | DuPont™ Sclairfilm® MPP-3 LLDPE Film is non-hazardous and not classified as dangerous goods. Ship in original packaging on pallets; keep dry, away from heat, sunlight, and sharp objects. Maintain stable temperature, avoid crushing and contamination. No special UN number, hazard label, or placard required. Use general freight or parcel service. |
| Storage | Store DuPont™ Sclairfilm® MPP-3 LLDPE Film, 25 µm, in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, open flames, and strong oxidizers. Keep in original, sealed packaging, elevated off the floor, and protect from dust, moisture, sharp objects, and UV light. Avoid excessive stacking, pressure, or prolonged exposure to high temperatures. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is two years from manufacture when stored in original packaging under cool, dry conditions, away from direct sunlight. |
DuPont™ Sclairfilm® MPP-3 LLDPE Film, “Super Strength,” 25 µm thickness enters form-fill-seal (FFS) packaging for 5–25 kg industrial powders as a 100% LLDPE web rather than a coextruded laminate, a substitution that removes delamination risk at the seal zone but imposes a narrow thermal window at the jaw face. On a 65 mm grooved-feed blown-film extruder with 24:1 L/D ratio and a 1.8–2.2 mm die gap, the 25 µm bubble is run at a blow-up ratio of 2.2:1–2.8:1 and a frost-line height of 350–500 mm; air-ring temperature is held at 10–16 °C to stabilize bubble geometry because the MPP-3 molecular weight distribution creates a processing window of approximately ±5 °C before edge curl or ethylene oligomer deposition on the collapsing frame appears. On the FFS line, heated seal jaws are set to 118–132 °C with 0.6–1.2 s dwell and 2.0–3.5 N/mm² jaw pressure, producing corner seals that retain filled-sack integrity after a 0.4 s cooling cycle. Seal acceptance follows ASTM F88/F88M-21; dart-impact acceptance follows ASTM D1709-16a Method A; tensile acceptance follows ISO 527-3:2018. Industrial chemical packaging in non-food service is not governed by EU food-contact migration limits, but converters supplying the construction-chemical and fertilizer sectors typically maintain compliance with REACH Regulation (EC) No 1907/2006 and Regulation (EC) No 1272/2008 for classification and labeling when printed films enter the supply chain.
Addition ratio for monolayer FFS webs is fixed at 100% MPP-3; where converters introduce post-industrial trim from edge slitting or roll ends, the trim is limited to ≤15 wt% in a three-layer core or ≤10 wt% in monolayer re-pelletized form to avoid gel specks that lower dart impact by more than 10%. Print primer or surface-printing ink is deposited at 1.0–1.5 g/m² dry weight; when the 25 µm film is laminated to woven polypropylene or kraft paper, a solvent-free polyurethane adhesive is applied at 2.0–2.5 g/m². Slip and antiblock additives are already incorporated in the film, so downstream converters do not add further masterbatch. Finished product types include valve sacks, gusseted block-bottom sacks, FFS pillow bags, and film-laminated woven sacks for polymer resin, mineral fillers, dry-mix mortar, and granular fertilizer. The critical process conflict is that seal jaw temperature below 112 °C produces low-strength seals while jaw temperature above 135 °C generates molten edge flash that contaminates bottom-forming plates and increases cleaning frequency on 45–70 bag/min lines.
When the 25 µm web is converted as the inner sealant layer in frozen poultry and meat packaging, it is bonded to 12 µm polyester or 15 µm biaxially oriented polyamide in a dry-lamination process. Food-contact compliance for the olefin sealant web is anchored to FDA 21 CFR 177.1520(c) for olefin polymers and to Commission Regulation (EU) No 10/2011, Annex I and Annex II, with an overall migration limit of 10 mg/dm²; the converting facility is additionally operated under Regulation (EC) No 2023/2006 good manufacturing practice. The adhesive addition ratio is 1.8–2.5 g/m² dry weight for a solvent-free polyurethane system; the MPP-3 web is corona-treated to 38–42 mN/m measured by ASTM D2578-23 dyne pens before lamination. If extrusion lamination is selected instead of adhesive lamination, a low-density polyethylene tie layer is applied at 10–15 g/m² with a melt temperature of 310–325 °C at the die exit. The lamination nip is held at 60–80 °C and 4–6 bar; cure is 35–45 °C for 24–48 h. Seal initiation is determined by ASTM F1921/F1921M-18 hot-tack testing across 105–145 °C, and production seal strength is verified by ASTM F88/F88M-21 at 115–135 °C.
| Standard | Scope | Typical acceptance window |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymer food-contact status | No migration above regulatory limits |
| EU 10/2011 Annex I/II | Plastics in food contact | OML 10 mg/dm² |
| ASTM F1921/F1921M-18 | Hot-tack seal strength | 105–145 °C plateau |
| ASTM F88/F88M-21 | Seal strength | 2.5–4.0 N/15 mm after 24 h |
Finished product types include vacuum pouches, flow-wrap frozen meat packaging, and recloseable lidding films for modified-atmosphere trays. The critical processing boundary is the seal plateau: below 100 °C, incipient fusion is insufficient to maintain vacuum pouch integrity during -40 °C cold-chain storage; above 150 °C, the 25 µm web thins at tray rims and can produce tear initiation at the seal edge. Roll storage is maintained at ≤30 °C and ≤60% RH because migration of the slip additive to the sealant surface accelerates above 30 °C and reduces seal strength after lamination. Printed outer webs that contact low-viscosity meat purge require an additional primer at 0.2–0.5 g/m² dry weight to maintain ink adhesion during cold-storage condensation cycling.
Anodized aluminum coil service centers employ the 25 µm MPP-3 film as a temporary surface protection web after coating with a UV-cured acrylic pressure-sensitive adhesive. The film is corona-treated to 44–48 mN/m immediately before coating because peel adhesion of the acrylic emulsion falls below 0.5 N/25 mm on untreated film; slot-die or comma coating deposits 18–22 g/m² wet adhesive weight, yielding 5–8 g/m² dry adhesive coverage after a three-zone drying tunnel at 60–90 °C. UV dose is set at 150–250 mJ/cm² for acrylic crosslinking. Addition ratio: primer is applied at 0.2–0.5 g/m² dry weight only where the protected coil will be stored at RH > 70%, because high-humidity storage accelerates interfacial plasticizer migration. Unwind tension is controlled to ≤10 N/m to prevent gauge bands that appear as visible ridges after lamination to mirror-polished sheet. Compliance under REACH Regulation (EC) No 1907/2006 Annex XVII and RoHS Directive 2011/65/EU Annex II restricts lead, mercury, cadmium, and hexavalent chromium to the directive’s maximum concentration values. Finished product types include laser-cutting masks, coil protection film, stainless steel anti-scratch film, and temporary surface protection for pre-painted architectural panels. The operational boundary is outdoor exposure: the adhesive system is not rated beyond 90 days of direct UV exposure; after that point, clean peel from low-energy coated steel becomes inconsistent.
The building-envelope vapour-retarder route subjects the 25 µm MPP-3 film to lamination against 9–12 µm aluminum foil or 50–70 g/m² kraft paper, where the LLDPE layer functions as the puncture-resistant outer ply of a flexible vapour-control membrane. Compliance for the finished laminate is tested under ASTM E96/E96M-22 Method A desiccant for water vapour transmission and EN 13984:2013 for flexible sheets for vapour control; building-code acceptance often requires a water vapour resistance factor that is verified after lamination, not on the film alone. Adhesive addition ratio is 2.0–3.5 g/m² dry weight for a solvent-free or water-borne laminating adhesive; where extrusion lamination is preferred for high-speed insulation facing lines, low-density polyethylene is deposited at 12–18 g/m² with a melt temperature of 305–325 °C. The lamination nip operates at 70–90 °C and 3–5 bar, followed by post-cure at 30–40 °C for 48 h. Finished product types include glass-wool insulation facing, pipe insulation jacketing, and crawl-space vapour retarder membrane. A process limitation exists in cold-climate applications: at RH > 60% the water vapour transmission of the LLDPE web rises, so the 25 µm MPP-3 film is not specified as the sole vapour retarder in unvented roofs unless combined with aluminum foil or a higher-barrier polymer layer. Published data for this specific configuration is limited, so converter trials should include moisture-cycle testing per EN 13984:2013 before specifying the laminate in hygrothermal models.
After ethylene oxide sterilization, film-to-Tyvek peel adhesion is governed by seal die temperature uniformity across the pouch width and by the surface energy of the uncoated Tyvek 1073B lidding web. The 25 µm MPP-3 film is evaluated as a 100% sealant layer against Tyvek 1073B and against 48–52 g/m² medical-grade paper. Compliance for terminally sterilized medical device packaging is anchored to ISO 11607-1:2019 and ISO 11607-2:2019 for validation and routine control; biocompatibility screening is performed under ISO 10993-5:2009 and ISO 10993-10:2010. Addition ratio: the film is used without adhesive in the seal zone; where a continuous lamination to a polyester support is required for printability, a polyurethane adhesive at 1.0–1.5 g/m² dry weight is applied outside the seal area. Pouch sealing is performed with heated platen sealers at 120–140 °C, dwell 0.5–1.0 s, and pressure 2.0–4.0 N/mm². Peel strength is tested per ASTM F88/F88M-21; a minimum of 1.2 N/15 mm after EtO sterilization is a common acceptance value, but the exact threshold is device-specific. EtO and electron-beam sterilization are compatible with the 25 µm LLDPE web; gamma sterilization at 25–40 kGy may induce oxidative embrittlement, and published data for this specific configuration under gamma is limited, so gamma terminally sterilized applications require dose-mapping and tensile verification per ISO 527-3:2018. Finished product types include low-acuity device pouches, tubing sets, and pre-sterilization containment bags.
Storage of float glass lites under variable warehouse humidity requires an interleaving material that does not transfer additives to the glass surface, and the 25 µm MPP-3 web is slit into rolls 800–1500 mm wide with a width tolerance of ±1 mm for direct insertion on automated glass stacking lines. The film is used uncoated; if anti-slip characteristics are required on steep packaging angles, a water-borne anti-slip varnish is applied at 0.2–0.4 g/m² dry weight only on one side. Slitting is performed on razor or shear knife slitters at 200–300 m/min with taper tension of 8–12 N to avoid ridges that telegraph to soft-coated low-emissivity glass surfaces. Compliance for industrial use is maintained under REACH Regulation (EC) No 1907/2006 Annex XVII and RoHS Directive 2011/65/EU Annex II; because the interleaving web is not a food-contact or medical article, no migration testing is required. Finished product types include glass interleaving rolls, acrylic sheet separator film, and interleaf web for polished metal plate. The critical operating boundary is thermal: the rolls must not be stored above 50 °C or near pelletized PVC, because heat exposure increases blocking and can transfer low-molecular-weight fractions to the glass. Converters should avoid high-slip formulations if the glass surface is destined for subsequent vacuum coating or screen printing.
Competitive DuPont™ Sclairfilm® MPP-3 LLDPE Film, "Super Strength", 25 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The product identified as DuPont™ Sclairfilm® MPP-3 LLDPE Film, “Super Strength”, 25 µm Thickness is a monolayer linear low-density polyethylene rollstock intended for industrial converting applications in which tensile strength, tear resistance, puncture resistance, and seal integrity are controlled by a purchase specification. The MPP-3 grade designation is a manufacturer product identifier, not a polymer classification under ASTM D883 or ISO 472; conformance is therefore evaluated through a set of physical property tests and the supplier’s certificate of analysis.
Nominal thickness is 25 µm, determined in accordance with ASTM D6988 or ISO 4593. Gauge measurements should be recorded across the mill roll at intervals not exceeding 150 mm, with the roll conditioned for at least 40 h at 23 ± 2 °C and 50 ± 10 % RH per ASTM D618. Cross-web thickness variation influences seal initiation temperature, coefficient of friction, and roll conformity on high-speed bag-making lines; if the measured profile exceeds the supplier’s stated tolerance, equipment adjustments should address film transport before the material is released to production.
The base resin class is linear low-density polyethylene, typically in the density range 0.918–0.935 g/cm³ under ASTM D1505. The actual density of MPP-3 should be taken from the supplier’s technical datasheet because additive content and comonomer type shift the value within this range. Melt index, when reported by the supplier under ASTM D1238 at 190 °C and 2.16 kg, is a resin-processability indicator and not a substitute for end-use mechanical properties of the converted film.
For incoming inspection, the following test matrix is applied as a compliance checklist. No single test value replaces the supplier’s current product specification.
| Property | Test Method | Unit | Condition / Note |
|---|---|---|---|
| Nominal thickness | ASTM D6988 / ISO 4593 | µm | 23 ± 2 °C |
| Tensile properties | ASTM D882 | MPa, % | 500 mm/min, 23 °C |
| Dart drop impact | ASTM D1709 | g/µm | Method A or B per supplier |
| Elmendorf tear | ASTM D1922 | N or gf | 25 µm nominal gauge |
| Puncture / penetration resistance | ASTM D5748 or ASTM F1306 | N | 23 °C |
| Seal strength | ASTM F88 | N/25 mm | Seal conditions specified by converter |
| Hot tack | ASTM F1921 | N/25 mm | Production-relevant seal dwell and pressure |
| Haze | ASTM D1003 | % | 25 µm film |
| Gloss | ASTM D2457 | GU | 60° geometry |
| Coefficient of friction | ASTM D1894 | dimensionless | 23 ± 2 °C |
| Water vapor transmission rate | ASTM F1249 | g/m²·day | 37.8 °C, 90 % RH |
| Oxygen transmission rate | ASTM D3985 | cc/m²·day | 23 °C, 0 % RH |
Because polyethylene film properties are direction-dependent and may be affected by slip and antiblock additives, storage time, and corona treatment level, a tensile value without a stated pull speed, sample width, and conditioning history is not suitable for supplier qualification under ASTM D882. Batch-to-batch variation in coefficient of friction and seal initiation can be caused by additive concentrate lot changes or by storage time after extrusion. Incoming inspection should therefore track the production date, the film side, and the corona treatment level because these variables affect downstream processing more than the nominal thickness alone.
The “Super Strength” descriptor indicates the product’s position in the supplier’s LLDPE line; the designation is not defined by a standardized test method. Differentiation from general-purpose LLDPE of the same nominal gauge is assessed through ASTM D1709 dart drop impact, ASTM D1922 Elmendorf tear, ASTM D5748 puncture resistance, and ASTM F88 seal strength. In converter evaluations, the relevant measure is not a single tensile value but the film’s ability to resist initiating and propagating failure when filled contents contain abrasives, sharp edges, or high-stiffness protrusions. However, published product-specific comparative data for this configuration is limited; the supplier’s current technical datasheet and a statistically valid incoming inspection plan should be the controlling documents.
Because LLDPE films are viscoelastic, low-strain-rate tensile data do not fully predict high-speed packaging failures. Puncture and drop dart tests are required to rank grades for heavy-duty bags. The choice between Method A and Method B in ASTM D1709 depends on the expected impact energy; Method A uses a 38 mm diameter dart and a 0.66 m drop height for thinner films, while Method B uses a larger dart for higher impact levels. Without this methodological detail, a reported dart value cannot be compared across film sources.
Slitting and converting lines expose the film to both machine-direction and transverse-direction stresses. The MD/TD tear balance of the supplied rollstock should be characterized on the incoming material because film orientation affects zippering behavior. A single tear value, often quoted as the lower of MD and TD, can mask severe anisotropy; converters running high-speed form-fill-seal equipment should record both directions and specify a minimum value for the controlling axis.
In a replacement trial where a 40 µm LDPE sleeve is substituted with 25 µm MPP-3, a plant-specific validation is necessary because drop-shock loading is not replicated by low-rate tensile elongation. The trial protocol should include ASTM D1709 dart impact, puncture or penetration resistance, and a filled-bag drop test using the actual product mass and closure design. Sealing-jaw temperature, dwell time, and pressure should be recorded because edge tearing at the seal is a common failure mode when the sealing conditions exceed the film’s hot-tack window.
Heat-seal characterization is performed by ASTM F88 on a laboratory sealer with flat 25 mm wide jaws, but that test measures cold-seal strength. Hot tack measured by ASTM F1921 is often the controlling parameter on vertical form-fill-seal equipment because the seal must support the filled mass before the melt crystallizes. A continuous bagger operating above 60 bags/min should evaluate hot tack across the entire jaw width, not only at the center, because jaw pressure distribution and film thickness variation can produce edge failures that are absent in hand-sealed specimens.
When the product is used as a lamination sealant web, its surface energy must be matched to the adhesive system. Corona-treated LLDPE is typically characterized by ASTM D2578 wetting-tension fluids; common targets for solventless lamination range from 38 mN/m to 42 mN/m, but the required level is adhesive-specific. The treatment level decays with storage time and humidity, so the converter should verify wettability at the point of adhesive application rather than at the incoming inspection station.
For multi-material laminations, the MPP-3 layer may be combined with biaxially oriented polypropylene or polyethylene terephthalate. The adhesive selection should account for the low surface energy of untreated polyethylene and for the presence of migratable additives. If the film is corona treated at 40 mN/m and laminated within 24 h, adhesion is typically more consistent; longer storage may require retreatment.
Printability of LLDPE films depends on surface treatment uniformity and the ink system. Solvent-based flexographic inks may require a wetting tension above 36 mN/m, while UV-curable inks may require a higher level. Surface treatment levels should be confirmed with dyne solutions at the press; a single-point measurement from the center of the web is insufficient because corona treatment can vary across the web width.
Unconverted rollstock should be kept in original moisture-barrier wrapping at 10–30 °C and 50 ± 10 % RH. Storage outside these limits can change the coefficient of friction measured by ASTM D1894 because slip additives migrate to the film surface at different rates depending on temperature. Slip and antiblock additives are used in LLDPE films to control blocking and web transport; their concentration and migration behavior are part of the grade formulation and should not be inferred from base resin density alone.
Blocking, telescoping, and web wander are common roll-condition failures observed on converting lines. If slitting induces telescoping, roll hardness, taper tension, and cross-web gauge should be examined before the film is faulted. In an unwind system using tape-driven shaft tension control, surface scuffing can occur when web tension is too high for the gauge; values above 35 N/m have been associated with visible surface markings on thin LLDPE rollstock in some converting operations, though the specific onset threshold for MPP-3 should be determined in production trials.
Compared to general-purpose LDPE film of equal thickness, LLDPE grades typically show higher tensile elongation and improved tear resistance. The MPP-3 “Super Strength” position is intended to shift that balance further toward dart impact and puncture resistance; however, LLDPE may exhibit lower stiffness and a different sealing response than LDPE. Formulations containing high slip or an antiblock package may reduce film-to-film friction but can also lower heat-seal strength if additive bloom covers the seal area; this trade-off should be quantified by ASTM F88 and ASTM D1894 on the same roll.
For food-contact applications, the base polyolefin must satisfy FDA 21 CFR 177.1520, and extraction limits depend on food type and use condition under paragraph 177.1520(c). European Union food-contact compliance is assessed under Regulation 10/2011 as amended, with the film supplier providing a declaration of compliance for the specific grade. REACH and RoHS obligations should be verified through the safety data sheet and the supplier’s product stewardship documentation because the final converted article may contain printing inks, adhesives, or coatings that lie outside the base film certification.
Operational boundaries for the film include avoiding contact with strong oxidizing acids, aromatic and halogenated hydrocarbons, and some amine-containing curing agents at elevated temperature because these substances can promote environmental stress cracking or interlayer adhesion loss. The film should not be used as a direct barrier for high-acid foods or aggressive chemical intermediates unless specific permeability and compatibility data for the packaged article are generated under end-use conditions. Published data for this specific MPP-3 configuration is limited; the supplier’s technical datasheet, certificate of analysis, and production-scale trial results are the controlling documents.