| HS Code | 260610 |
| Thickness | 76.2 µm |
| Density | 0.920 g/cm³ |
| Yield | 14.3 m²/kg |
| Tensile Strength At Break Md | 26 MPa |
| Tensile Strength At Break Td | 24 MPa |
| Elongation At Break Md | 600% |
| Elongation At Break Td | 700% |
| Tear Strength Md | 200 g |
| Tear Strength Td | 300 g |
| Dart Drop Impact | 120 g |
| Haze | 10% |
| Gloss 45 | 60 |
| Coefficient Of Friction | 0.2 |
| Melting Point | 120 °C |
| Vicat Softening Point | 100 °C |
As an accredited DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sold as one roll per carton; DuPont Sclairfilm LX-3, 76.2 µm LLDPE laminating film on core, protected by moisture-barrier wrap. |
| Container Loading (20′ FCL) | Load palletized rolls in dry 20′ FCL; keep upright, secure; ambient conditions. DuPont™ Sclairfilm® LX-3 LLDPE laminating film, 76.2 µm. |
| Shipping | DuPont™ Sclairfilm® LX-3 LLDPE laminating film, 76.2 µm, is shipped as a non-hazardous, non-regulated material. Rolls are wrapped, boxed, and palletized to prevent contamination, moisture, and damage. Transport and store clean, dry, away from heat, sunlight, and sharp objects; avoid compression. Maintain moderate temperatures and follow manufacturer’s handling guidelines. |
| Storage | Store DuPont™ Sclairfilm® LX-3 LLDPE Film in a clean, dry, well-ventilated area at ambient temperature, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep in original sealed packaging, supporting rolls horizontally to prevent deformation. Protect from moisture, dust, oils, sharp objects, and excessive pressure. Keep containers closed when not in use. Use stock rotation; avoid prolonged UV exposure. |
| Shelf Life | Shelf life is typically 24 months from manufacture when stored in original packaging at 23°C and 50% relative humidity. |
When a 76.2 µm LLDPE web is positioned as the sealant ply in a laminated food-contact pouch, the converting sequence begins with incoming roll inspection rather than lamination itself. In a duplex or triplex adhesive-laminated construction, the film is unwound at 80–120 N/m tension and passed through a bare-roll corona treater set to a discharge energy density of 2.0–3.0 W·min/m²; wetting tension is checked with formamide–ethylene glycol monomethyl ether solutions per ASTM D2578, and rolls measuring below 38 mN/m are rejected before solventless polyurethane adhesive is applied. On a production-scale five-roll solventless laminator running at 180–250 m/min, adhesive coat weight is maintained between 1.5 g/m² and 1.8 g/m², with transfer roll temperature at 40–45 °C and nip roll pressure at 3–4 bar; a 76.2 µm web is paired with 12 µm BOPET or 20 µm BOPP through the nip, and primary film tension is reduced to 60–80 N/m because LLDPE elongation at yield can exceed 15% under high draw. The laminated reel is then cured at 35–40 °C for 24–48 h until aromatic primary amine migration falls below the limit specified in EU Regulation 10/2011 Annex II; the food-contact surface of the LLDPE layer is supported by FDA 21 CFR 177.1520(c) when the olefin polymer complies with extractables limits for fatty and aqueous simulants. Heat sealing is performed on rotary jaw or bar sealers at 115–135 °C jaw temperature, 0.5–1.0 s dwell, and 0.28–0.41 MPa jaw pressure; a seal strength below 8 N/25 mm tested per ASTM F88/F88M-21 is rejected for stand-up pouch applications because open-pouch failure at the gusset point is frequently traced to insufficient hot tack at 110–130 °C rather than final seal strength. Hot tack is evaluated on a spring-loaded hot-tack tester at 200–250 mm/s peel speed; values under 3 N/25 mm at 110 °C indicate the sealant layer cannot hold a vertical form-fill-seal back seam without delamination. The 76.2 µm film thickness gives a wider sealing window than 50 µm LLDPE, but it also increases thermal demand at the seal bar; controllers must compensate with higher proportional-integral-derivative output or dwell extension of 0.2–0.4 s when solvent retention in a coex thick sealant is suspected.
| Standard or regulation | Test target | Typical condition | Acceptance or action |
|---|---|---|---|
| ASTM D2578 | Wetting tension of lamination face | Formamide/EGME series | Below 38 mN/m rejects roll |
| ASTM F88/F88M-21 | Heat seal strength | 180° peel, 200–300 mm/min | Below 8 N/25 mm rejects pouch |
| EU 10/2011 Annex II | Food-contact migration | Fatty and aqueous simulants | Primary aromatic amine below listed limit |
| FDA 21 CFR 177.1520(c) | Olefin polymer food-contact status | Extractables testing | Must comply with specified end-use extractables |
In terminally sterilized medical device packaging, the Sclairfilm LX-3 web is not normally sealed directly against uncoated Tyvek because the polyolefin lacks sufficient polar adhesion to Tyvek 1073B/2FS; a converter therefore applies a slot-die or gravure coating of an EVA or EMA heat-seal lacquer at 3–6 g/m² dry weight to one surface of the LLDPE. Coating thickness variation exceeding ±0.5 g/m² across the web produces peel strength coefficient of variation above 15% when sealed at 125–140 °C platen temperature, 0.8–1.5 s dwell, and 0.45–0.69 MPa platen pressure on a rotary heat-seal machine. The seal window is bounded on the low-temperature side by incomplete fiber embedment into the EVA/EMA layer, visible as whitening at the seal edge, and on the high-temperature side by film puckering and strike-through when the 76.2 µm LLDPE reaches its crystalline melting region. Peel strength per ASTM F88/F88M-21 is recorded at 180° peel angle and 200–300 mm/min jaw separation; a target of 1.0–2.5 N/15 mm is typical for peelable medical pouches, while higher values can tear the Tyvek. Dye penetration testing per ASTM F1929 uses methylene blue at 0.05% concentration with a 30 s exposure; any dye channel across the seal boundary is a critical defect under ISO 11607-2. The film layer must also survive ethylene oxide sterilization at 50–60 °C and 30–70% relative humidity for 2–4 h, followed by aeration to remove ethylene oxide residues below the limit in ISO 10993-7; published gamma sterilization data for this specific film grade are limited, so dose substantiation per ISO 11137-2 using a 25 kGy reference dose cannot be assumed without testing on the exact adhesive, coating, and Tyvek stack. A production bottleneck occurs when the EVA/EMA coating is not fully cured before lamination; residual solvent above 5 mg/m² can plasticize the seal coat and lower its onset temperature by 4–8 °C, shifting the peel window below validation limits.
Cold pressure-sensitive adhesive lamination over UV-cured digital prints places the 76.2 µm LLDPE film on the exterior surface of signage and point-of-sale graphics where abrasion resistance and curl control are evaluated. The top surface is corona-treated to 40–42 mN/m per ASTM D2578 before a solvent acrylic pressure-sensitive adhesive is transfer-coated at 15–25 g/m² dry weight. On a wide-web cold laminator, nip pressure is held at 4–6 N/mm across a 1.6 m width; film tension below 40 N/m prevents neck-in and gauge-band distortion that causes adhesive strikethrough. Peel adhesion after 24 h dwell on printed vinyl or BOPP is measured per ASTM D3330/D3330M Test Method A at 180° angle and 300 mm/min; values below 5 N/25 mm are rejected because edge lifting begins on curves with radius less than 25 mm. The LLDPE film improves tear initiation resistance relative to a 25 µm BOPP overlaminate, but it will not provide long-term outdoor UV protection unless a hindered amine light stabilizer and a UV absorber are present in an adjacent ink or adhesive layer; without these, surface chalking and gloss loss occur under modified ISO 4892-3 QUV cycling within 500–800 h for unstabilized LLDPE, although published data for LX-3 in this configuration is limited. The dominant process failure is silvering caused by insufficient wet-out over high-density ink deposits; this is resolved by raising the laminator roll temperature to 25–35 °C and reducing line speed below 15 m/min when ink film thickness exceeds 12 µm. Curl after lamination must be kept below 10 mm over a 500 mm flat sheet; a moisture-resistant backside coating is often required if the graphic is installed in a high-humidity environment above 60% RH.
In foil sachets for nutraceutical powders and oleic liquid doses, the 76.2 µm LLDPE film functions as the inner sealant ply over a 9–12 µm aluminium foil that is adhesive-laminated with a retort-grade polyester exterior film. The duplex or triplex structure is run on a vertical form-fill-seal machine with flat or crimped jaws at 135–160 °C jaw temperature, 0.6–1.2 s dwell, and 0.34–0.55 MPa pressure; because the 76.2 µm web retards heat transfer to the foil interface, the outer jaw temperature is set 8–12 °C higher than would be used with 50 µm LLDPE. Seal integrity is tested per ASTM F88/F88M-21 in both tensile peel and burst modes, with burst values below 20 kPa per ASTM F2054 typically rejected for liquid fills. Powder fill lines generate dust that deposits in the seal zone; a waxy magnesium stearate or medium-chain triglyceride residue above 2 g/m² reduces hot tack by occupying polar sites on the LLDPE surface, and the seal-through-contamination performance can only be recovered by raising jaw temperature 5–10 °C or by using a sealant layer with an EVA-rich skin. Pinholing in the aluminium foil is measured by light-table inspection with a limit of 0 pores per 0.01 m² for liquid pharmaceutical sachets; if foil below 9 µm is flex-cracked during form-fill-seal, the LLDPE layer can mask water vapor leaks temporarily while oxygen ingress remains high. Drop testing per ASTM D5276 at 1 m drop height onto a rigid steel surface is used after sealing to detect flex cracks at the bottom gusset; a leak is defined by peel failure at the point of maximum strain. This construction is not retortable beyond 100 °C because the LLDPE sealant begins to flow under back pressure, and the foil/polymer interlayer may delaminate if the structure is heated above 95 °C for more than 30 min.
Greenhouse and tunnel cover conversion uses the film as one ply in a scrim-reinforced laminate; in many lines the 76.2 µm LLDPE web is extrusion-laminated to a high-density polyethylene woven scrim with an LDPE tie layer at 315–330 °C melt temperature and 20–30 g/m² coat weight. The LLDPE ply contributes tear resistance in the machine direction, but the scrim-dominated composite has anisotropic tensile strength per ASTM D882; MD values are typically 1.5–2.0× the transverse direction values, and laminators adjust wind-up tension below 50 N/m to prevent transverse draw-down. The film should contain a hindered-amine light stabilizer package if the laminate is intended for 24-month outdoor service; unstabilized LLDPE develops carbonyl index increases under ISO 4892-2 artificial weathering within 500 h, causing interply delamination. Process conflict arises from the heat-shrinkage of LLDPE as it approaches the extruder die; edge cooling is maintained at 10–15 °C with web stabilizer bars, and shrinkage after lamination per ASTM D1204 at 100 °C is limited to 1–2% MD and 0.5–1% TD. A major failure mode in the field is separation initiated at pinholes from insect abrasion; field repairs with adhesive tapes perform poorly on corona-treated surfaces that have aged beyond 6 months because wetting tension falls below 34 mN/m. This application is classed as industrial film; compliance is normally tested against REACH and RoHS rather than FDA food-contact, and the laminator must not use recycled feedstock in the 76.2 µm web if the final film is specified for nursery soil-contact use because extractable additives may inhibit seedling development.
Building envelope facings for insulation batts and rigid foam boards use a lamination of aluminium foil, glass-reinforced paper, or metallized PET to the 76.2 µm LLDPE film as a water vapor barrier and scuff-resistant interior surface. Water vapor transmission rate is determined per ASTM E96/E96M Procedure B wet cup at 23 °C and 50% RH; for a foil-facing laminate, the LLDPE layer contributes puncture resistance but the foil controls the vapor permeance, and the measured value is typically below 0.1 perm when the foil remains free of pinholes. The film is melt-bonded to the facing with a hot-melt or extrusion lamination process; extrusion lamination uses an LDPE-type extrudate at 300–320 °C and 20–25 g/m² coat weight, while a hot-melt line uses a slot-die coater with a polyolefin-based adhesive at 150–170 °C application temperature. Bond strength is measured per ASTM D1876 T-peel; interfacial failure below 250 N/m is rejected for utility-knife edge wrapping. Field handling exposes the LLDPE exterior to tears from staples and stud friction; Elmendorf tear per ASTM D1922 is specified at ≥8 N in the machine direction for building wrap. The use of unmodified LLDPE without flame retardants means the laminate must be positioned away from open-flame construction activities; if code requires a Class A surface, a separate mineral-filled facing is required because the LLDPE layer alone does not meet ASTM E84 Class A unless compounded with halogen-free intumescent additives. This application has no direct food-contact restriction, but the material must conform to REACH SVHC restrictions for any residual slip additives and to EU Construction Products Regulation for formaldehyde and heavy metal emissions where installed in interior conditioned spaces.
Thermal laminating pouch conversion uses a 76.2 µm LLDPE layer as a low-melt adhesive component between polyester or polypropylene oversheets and a paper document core. The pouch is activated on a heated-shoe laminator at 100–130 °C surface temperature and 0.4–0.8 m/min feed rate; uniform melting of the LLDPE layer is confirmed by haze testing per ASTM D1003, with delaminated microvoids increasing haze above 10%. The operation relies on the difference between the melting range of LLDPE and the thermally stable polyester oversheet; overshoe temperatures above 140 °C cause adhesive exudation at the sheet edges, producing adhesive contamination on downstream rollers. This pouch application is limited to non-critical graphic finishing; published data for LX-3 specifically in thermal pouch grades is limited, and converters must confirm melt-viscosity compatibility with the heated-shoe dwell time. A short dwell above 2 s does not allow complete wet-out of absorbent paper; wet-out below 85% of the paper surface produces a speckled appearance under transmitted light. Measurement of laminate bond strength is typically not required, but a peel force above 2 N/20 mm is regarded as sufficient for document preservation. The final structure is not suitable for archival preservation if the LLDPE contains octadecamide slip additives above 600 mg/kg because these may migrate to the document surface and alter ink gloss; extraction testing can quantify amide and siloxane species before conversion.
Competitive DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm thickness is a linear low-density polyethylene sealant web specified for adhesive lamination into flexible packaging structures. The 76.2 µm gauge corresponds to 3.0 mil (0.003 in). At a typical solid-state density of 0.920 g/cm³, the nominal area yield is approximately 14.3 m²/kg; at density limits of 0.918 g/cm³ and 0.922 g/cm³, the calculated yield moves to approximately 14.3 m²/kg and 14.2 m²/kg respectively. The film is supplied as roll stock, generally with one surface treated for adhesive or ink anchorage. In a converted laminate it is placed as the innermost sealant ply over substrates such as oriented polyester, biaxially oriented polypropylene, aluminum foil, or barrier-coated paper. Thickness uniformity is controlled because adhesive coating weight and heat-seal reproducibility are sensitive to local gauge deviation; incoming inspection commonly references ISO 4593 or ASTM F2251.
The primary difference is molecular architecture. Homopolymer LDPE is long-chain branched and provides high melt strength but lower solid-state toughness and dart impact. LLDPE produced from ethylene and an alpha-olefin comonomer has a predominantly linear backbone with short-chain branches. Under ASTM D882, LLDPE webs of this gauge class ordinarily show higher elongation at break and more puncture-related energy absorption than LDPE of equal thickness. Compared with EVA sealant film, LX-3 does not contain vinyl acetate comonomer. The absence of vinyl acetate removes a source of acetic acid odor during hot-knife cutting or sealing and lowers the extractable contribution from the base resin. The trade-off is seal initiation temperature. LLDPE seals higher; conventional LLDPE laminating grades often develop measurable seal strength between 105°C and 120°C by ASTM F88, while EVA may seal at 80–95°C. LX-3 is therefore specified where package performance is driven by toughness, organoleptic neutrality, and seal integrity after elevated temperature exposure rather than by the lowest possible seal bar setpoint.
Rheologically, LLDPE melts under seal-bar pressure and loses some of the high shear-thinning character of LDPE. The seal interface develops by chain diffusion and entanglement after wetting. Comonomer content and molecular weight distribution influence both hot-tack force and plateau seal strength. If the comonomer distribution is too broad, seal initiation may decrease but extractable values can increase. Control of melt mass-flow rate and density is therefore critical for both food-contact classification and sealing constancy. Material release under ISO 1133-1 at 190°C/2.16 kg and density under ISO 1183 are part of polymer identity testing. The manufacturer’s certificate of analysis should be used to verify that the specific lot falls within the agreed control plan.
Mechanical property testing is performed after conditioning for not less than 40 h at 23°C ± 2°C and 50% ± 5% RH under ASTM D618. Tensile specimens are cut in both machine and transverse directions. Machine-direction yield and tensile behavior govern web handling, while transverse-direction elongation is relevant to bag expansion and fold resistance. Elmendorf tear and dart drop are used as release surrogates for package damage resistance. Coefficient of friction is dynamic; slip additives bloom to the surface over time and reduce COF measured by ASTM D1894. A freshly corona-treated roll may show kinetic COF near 0.25, which can drift below 0.10 after additive migration. In high-speed bag making, excessively low COF produces roll telescoping and unstable film advance. Sampling plans for incoming film commonly follow ANSI/ASQ Z1.4 or ISO 2859-1 to limit inspection risk.
| Property | Reference method | Process relevance |
|---|---|---|
| Thickness | ISO 4593, ASTM F2251 | Adhesive coating weight and seal geometry |
| Density | ISO 1183, ASTM D1505 | Polymer class confirmation and area yield |
| Melt mass-flow rate | ISO 1133-1, 190°C/2.16 kg | Seal melt flow and heat-bar penetration |
| Tensile strength and elongation | ASTM D882, ISO 527-3 | Web handling and package integrity |
| Elmendorf tear | ASTM D1922, ISO 6383-2 | Tear initiation at nicks and splices |
| Dart drop impact | ASTM D1709, ISO 7765-1 | Puncture resistance in filled packages |
| Haze and gloss | ASTM D1003, ASTM D2457 | Optical clarity in display laminates |
| Kinetic coefficient of friction | ASTM D1894, ISO 8295 | Machinability on form-fill-seal and bagging lines |
| Wetting tension | ASTM D5946, ISO 8296 | Adhesive and ink anchorage on treated side |
| Seal strength | ASTM F88, ASTM F2029 | Seal integrity and hot-tack limits |
Polyethylene is nonpolar, so the laminating surface must be oxidized by corona discharge or another treatment. Untreated LLDPE commonly exhibits a wetting tension below 34 mN/m. Laminating-grade LX-3 is supplied with a treated side, usually in the range of 38–42 mN/m when tested with ASTM D5946 or ISO 8296. If a roll has been stored for extended periods or exposed to additive bloom, the treated side can fall below 36 mN/m, producing retraction or fish-eye defects in solventless adhesive coating. In-line corona re-treatment is then used before the coating station. Over-treatment above 50 mN/m is not advised because it can oxidize the surface to a brittle low-molecular-weight layer and may interfere with the heat-seal wetting of the untreated side if treatment wraps around the web edge. The treated side must not be heat-sealed as the sealant surface; conversion should preserve the untreated side as the package inner face.
Adhesive lamination to aluminum foil or oriented polyester requires compatibility with reactive polyurethane systems. The film does not absorb moisture, so the curing rate of solventless polyurethane adhesives is governed by coating station temperature, nip temperature, and ambient humidity rather than by film moisture. On lamination equipment with a gravure or sleeve adhesive station running 1.0–1.2 g/m² coat weight, nip temperatures of 60–70°C are typical. LLDPE softening begins above 90°C, so higher nip temperatures risk surface deformation and blocking. Solvent-based laminating dryers are commonly staged between 60°C and 80°C; the film should not be exposed to temperatures above 70°C for extended dwell because roll geometry and gauge profile can change under tension. Use of dissimilar webs, such as thicker PE against 25 µm PET, requires differential tension control to avoid curl and tunneling.
On vertical form-fill-seal machines operating at 120–160 cycles/min, jaw contact time can be 0.05–0.3 s. Under these conditions, hot-tack force is a better predictor of package integrity than equilibrium seal strength. A 76.2 µm LLDPE sealant provides more melt volume than a 50.8 µm sealant, which is useful in folding gussets and sealing through powdered product contamination. Hot-tack force is typically measured with laboratory hot-tack equipment using ASTM F1921 or ASTM F2029. At short dwell the measured force is lower than the 0.5 s or 1.0 s equilibrium value. The required jaw pressure for LLDPE is often higher than for EVA because the LLDPE melt stiffens more rapidly on cooling. A production change from EVA to LX-3 may require a 5–15°C increase in jaw setpoint and a narrower temperature band across the sealing bar. Temperature variation of ±5°C across the bar can generate cold-seal defects at high speed. For products carrying talc, starch, or lipid residues, the sealant must wet the residues and incorporate them into the seal; fluoropolymer-coated sealing jaws or sonic sealing may be used to maintain release and reduce contamination. On rotary pouch lines, seal quality is verified by burst test methods such as ASTM F2054 or by peel testing at ASTM F88.
Slip migration and heat-seal performance are linked. Slip additives such as erucamide or oleamide bloom to the film surface over time, lowering COF but potentially reducing heat-seal strength if excessive additive transfers to the seal interface. Seal tests should therefore be performed on aged laminate samples, not only on fresh film. Storage at elevated temperatures increases the diffusion rate of the slip additive. A warehouse temperature above 40°C accelerates bloom and can produce uneven sealability across the web. In a lamination operation, the material should be allowed to equilibrate in the pressroom for 24 h before slitting to reduce static charging and telescoping. Slitting blades must be kept sharp because polyethylene can stretch and produce fibrils at the slit edge; a dull blade generates edge defects that later propagate as web breaks.
The choice is not universal; it depends on the failure mode of the package. A 50.8 µm metallocene LLDPE sealant provides higher area yield and often lower seal initiation temperature than conventional LLDPE. However, the thinner web may fail earlier in Elmendorf tear measured by ASTM D1922 and dart impact measured by ASTM D1709. The LX-3 gauge of 76.2 µm is selected when gusseted stand-up pouches or frozen food packs show failures at fold creases, puncture from sharp product, or stress cracking at the seal edge. Compared with a 76.2 µm EVA sealant, LX-3 eliminates vinyl acetate and thereby reduces the potential for odor, acid transfer, and seal-bar build-up. EVA remains preferred where low-temperature sealing at 80°C is required or where the packaging machine has limited heat capacity. The final selection should be supported by measured seal initiation, hot-tack window, and burst strength on the actual laminate structure, not on film data alone.
Ionomer sealant webs can seal through heavy contamination and provide low-temperature performance, but they are more moisture-sensitive and typically higher in cost. LX-3 is a hydrocarbon polyolefin and is not equivalent to an ionomer caulking sealant. Its use is appropriate when the sealing requirement does not demand the extreme contaminant tolerance of ionomer and when a lower-cost LLDPE sealant can meet the required seal strength and hot-tack values.
LLDPE sealant films are generally covered under olefin polymer food-contact provisions. In the United States, compliance is evaluated under FDA 21 CFR 177.1520(c), which defines allowed substrates and imposes extractable and use-temperature restrictions depending on food type. Converters should obtain a supplier letter confirming that the specific lot and grade meet the relevant paragraphs, because lamination adhesives and printing systems have separate regulatory status. In the European Union, plastic food-contact materials are regulated by EU Regulation 10/2011; the overall migration limit is 10 mg/dm², and specific migration limits apply to monomers and additives. The film also falls within the general information and documentation requirements of REACH 1907/2006, including SVHC disclosure if relevant. Electrical and electronic packaging applications may be evaluated against RoHS 2011/65/EU restricted substances. The table below summarizes the common regulatory matrix.
| Regulation or standard | Scope | Boundary condition |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymer films for food contact | Use temperature and extractable limits apply; lot-specific certification required |
| EU Regulation 10/2011 | Plastic food-contact materials and articles | Overall migration 10 mg/dm²; specific migration for authorized substances |
| REACH 1907/2006 | Chemical safety and SVHC information | No SVHC above threshold; documentation through supply chain |
| RoHS 2011/65/EU | Electrical and electronic equipment packaging | Restricted heavy metals and flame retardants if applicable |
Operational boundaries should not be inferred from food-contact status alone. The film should be protected from direct sunlight and rain, stored at temperatures below 40°C, and used within the supplier’s recommended shelf life, often 12 months from the certificate date. The product is not a barrier film; oxygen and moisture barrier are provided by the foil, metallized, or coated substrate in the laminate. If the film is used in retort or hot-fill applications, the converter must validate the sealed seam under the actual thermal process because LLDPE seal strength can decline near its softening range. Adhesion levels in the finished laminate are structure-dependent and must be tested by peel methods after conditioning at 23°C and 50% RH for at least 24 h. The suitability of LX-3 for pharmaceutical or medical packaging is not established by the film grade alone; additional biocompatibility and sterilization validation may be required.