Dupont Sclairfilm Lx 3 Lldpe Film Laminating 50 8 µm Thickness

DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness

    • Product Name: DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 290768
    Product Name DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness
    Manufacturer DuPont
    Material Type Linear Low Density Polyethylene (LLDPE)
    Application Laminating
    Thickness 50.8 µm
    Density 0.920 g/cm³
    Tensile Strength At Break Md 34.5 MPa
    Tensile Strength At Break Td 27.6 MPa
    Tensile Strength At Yield Md 10.3 MPa
    Tensile Strength At Yield Td 10.3 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g
    Dart Drop Impact 150 g
    Haze 5%
    Gloss 45 80
    Coefficient Of Friction 0.2
    Heat Seal Strength 2.5 lb/in
    Seal Initiation Temperature 110°C
    Melting Point 122°C
    Vicat Softening Point 95°C
    Low Temperature Brittleness -70°C
    Water Vapor Transmission 0.5 g/100 in²/24h
    Oxygen Transmission 200 cc/100 in²/24h
    Carbon Dioxide Transmission 1000 cc/100 in²/24h
    Nitrogen Transmission 50 cc/100 in²/24h

    As an accredited DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing DuPont™ Sclairfilm® LX-3 LLDPE laminating film, 50.8 µm thick, supplied on rolls: 1 roll per carton, 25 kg net.
    Container Loading (20′ FCL) Palletized DuPont™ Sclairfilm® LX-3 LLDPE laminating film, 50.8 µm, shrink-wrapped, secured in a 20′ FCL dry container with airbags.
    Shipping DuPont™ Sclairfilm® LX-3 LLDPE laminating film (50.8 µm) is non-hazardous and not regulated for transport. Ship in original moisture-resistant packaging, on rolls or flat, protected from sunlight, heat, punctures, and contamination. Maintain dry, ambient conditions. Handle to prevent creasing or edge damage. No special DOT, IMDG, or IATA requirements.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and oxidizing materials. Keep the film in its original sealed packaging, clean and dry, preventing moisture, dust, and contamination. Avoid punctures, crushing, excessive stacking, and physical damage. Maintain stable ambient temperature and humidity, and rotate stock first-in, first-out. Store away from sharp objects. Use clean gloves.
    Shelf Life Shelf life is typically 24 months from manufacture when stored unopened in original packaging, cool, dry, away from direct sunlight.
    Application of DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness

    DuPont™ Sclairfilm® LX-3 is converted at a nominal gauge of 50.8 µm as a sealant web in dry-bond and solventless laminations for ambient and frozen food packaging. In this application, the film functions as the food-contact sealant layer rather than a compounded resin; the addition ratio is therefore expressed as the dry-weight share of the finished laminate. When the film is combined with 12 µm biaxially oriented polyester and 2.5–3.5 g/m² solvent-free polyurethane adhesive, the LLDPE web represents approximately 65–72 wt% of the two-film laminate; when a 9 µm aluminium foil layer is added for oxygen or light protection, the LLDPE share falls to 48–54 wt%, calculated from nominal densities of 0.918 g/cm³ for LLDPE and 2.7 g/cm³ for aluminium. Compliance of the finished food-contact laminate is regulated under FDA 21 CFR 177.1520 for olefin polymers, EU Regulation (EU) No 10/2011 with overall migration limits of 10 mg/dm² under condition-of-use testing, and GB 4806.7-2023 for plastic food contact materials in export packaging. The converting line typically uses a solventless laminator with gravure metering, a web temperature of 60–80°C at the combining nip, and line speeds of 120–180 m/min; the sealant surface receives corona treatment to 42–46 dyn/cm prior to coating to prevent adhesive dewetting. The finished roll is cured at 30–40°C for 24–48 h before slitting. Terminal products produced from this structure include stand-up pouches for dried mixes, pillow pouches for frozen vegetables, and side-gusseted bags for bulk dry ingredients. Peel strength of the finished laminate is evaluated in accordance with ASTM F904-21, and pouch seal strength is measured using ASTM F88/F88M-21 after finite sealing.

    How Does Seal Initiation Temperature Constrain Medical Sterile Barrier Converting?

    Sterile barrier lamination with 50.8 µm Sclairfilm® LX-3 is subject to package integrity requirements rather than food migration limits alone. The applicable compliance framework includes ISO 11607-1:2019 and ISO 11607-2:2019 for terminally sterilized medical devices, EN 868-5:2018 for paper and film pouch materials, and FDA 21 CFR 177.1520 for any direct or indirect food or medical fluid contact determination. The LLDPE web is used as a monolayer sealant layer sealed or adhesive-laminated to 60–70 g/m² medical-grade paper or coated Tyvek; on a dry-weight basis the film represents approximately 39–50 wt% of the two-layer pouch stock depending on substrate mass, with hot-melt or solventless adhesive coat weights below 3.0 g/m² dry when lamination is used. The critical process window is the jaw sealing operation: heated platen sealers run at 120–150°C with a dwell of 0.5–1.0 s and pressure of 0.3–0.5 MPa. Below 105°C interface temperature, chain diffusion across the seal interface is incomplete and peel strength is unstable; above 160°C, gauge thinning and burn-through at the seal edge compromise sterile barrier integrity. Seal strength is validated by ASTM F88/F88M-21, dye penetration is assessed by ASTM F1929-15, and visual seal continuity is controlled under the process validation protocols of ISO 11607-2:2019. Terminal formats include sterilization pouches, header bags for catheters, and surgical kit wrappers where the 50.8 µm film provides the microbial barrier and sealant surface for aseptic presentation.

    Application scenarioPrimary compliance standardRelevant test methodCritical compliance condition
    Food and frozen packaging laminatesFDA 21 CFR 177.1520, EU 10/2011, GB 4806.7-2023EN 1186-1:2002, ASTM F904-21Overall migration limit 10 mg/dm² on finished laminate
    Medical sterile barrier pouchesISO 11607-1:2019, ISO 11607-2:2019, EN 868-5:2018ASTM F88/F88M-21, ASTM F1929-15Validated seal uniformity and absence of dye penetration
    Insulation facer laminatesASTM C1136, ASTM E84, EN 13501-1ASTM E96/E96M-24Flame spread classification determined on finished facer composite
    Pressure-sensitive tape backingsREACH Regulation (EC) No 1907/2006ASTM D3330/D3330M-24, ISO 527-3:2018Peel adhesion measured at 180° angle on production-scaled coating

    When Insulation Facers Require Pinhole Resistance Through Roll-Fed Hot Melt Converting

    For building insulation facers, the 50.8 µm LLDPE film is roll-fed into a hot melt lamination line where it is bonded to 30 g/m² bleached kraft or 6.35–9 µm aluminium foil. Compliance is evaluated on the finished laminate under ASTM C1136 for flexible low-permeance vapor retarders, ASTM E96/E96M-24 for water vapor transmission, ASTM E84 for surface burning characteristics when installed in concealed plenums, and EN 13501-1 for European market reaction-to-fire classification. The lamination addition ratio is calculated by dry-layer mass: the LLDPE web at 0.918 g/cm³ nominal density contributes approximately 46.6 g/m², which is 43–48 wt% of the finished kraft/foil/LLDPE composite when hot-melt adhesive is applied at 3.0–4.0 g/m² dry. The converting process uses a slot-die hot melt station followed by a heated combining nip at 70–90°C and line speeds of 150–200 m/min. Excessive web tension above 1.0 N/mm across the polyethylene layer produces gauge banding and pinholes at the foil interface; gauge variability in the incoming film should be held to ±5% of nominal thickness to avoid wrinkling during downstream corrugator or building panel lamination. Terminal products include fiberglass batt facers, duct wrap facing, and metal building insulation facings where the LLDPE layer supplies puncture resistance and a low-permeance sealable surface.

    In frozen food carton converting where board stock is offline-laminated rather than extrusion-coated, the 50.8 µm LLDPE web functions as the internal moisture-resistant layer on brown kraft board. The compliance framework for the finished carton includes FDA 21 CFR 177.1520 for the olefin polymer contact surface, EU Regulation (EU) No 10/2011 with migration testing per EN 1186-1:2002, and ASTM F1249-20 for water vapor transmission rate of the laminated board. The addition ratio on a dry-weight basis places the LLDPE web at 46.6 g/m² against a board basis weight of 250–350 g/m², with water-based adhesive at 2.0–3.0 g/m² dry; the LLDPE layer therefore represents 13–16 wt% of the final sheet. The production line is configured with a sheet-fed laminator, a heated nip at 60–80°C, and board moisture controlled to 6–8% to limit curl. Because the LLDPE layer provides moisture resistance but not an oxygen barrier, oxygen-sensitive frozen products require an aluminium foil or a barrier coating in the structure; otherwise the board is suited to frozen food cartons, refrigerated pet food trays, and industrial bulk cartons exposed to condensation.

    Pressure-Sensitive Tape Backing and Release Surface Interactions

    When the 50.8 µm LLDPE film is converted as a pressure-sensitive adhesive tape backing, the release surface and adhesive coat weight determine the final peel and unwind characteristics. The applicable test standards for the coated tape include ASTM D3330/D3330M-24 for peel adhesion, ASTM D3652/D3652M-20 for thickness, and ISO 527-3:2018 for tensile properties of the film substrate. The addition ratio in the coated structure places the LLDPE base film at approximately 64–69 wt% of the finished tape when a UV-curable silicone release layer is applied at 0.8–1.2 g/m² dry and a solventless acrylic pressure-sensitive adhesive is applied at 20–25 g/m² dry. The converting process includes corona treatment to 40–44 dyn/cm before silicone coating, UV or electron-beam cure at line speeds of 100–150 m/min, and transfer coating of the adhesive on the opposite surface. Residual oxygen inhibition at the silicone surface is controlled by inerting the UV chamber to an oxygen concentration below 50 ppm. Terminal products include surface protection films for appliance and automotive transit, temporary masking films, and industrial tape backings where the LLDPE modulus balances conformability with tensile integrity.

    Thermal Lamination of LLDPE Web to Needled Nonwoven and Crosslinked Foam

    In roll-fed nonwoven and foam lamination, the 50.8 µm Sclairfilm® LX-3 film is combined with 60–90 g/m² needled polyester or polypropylene nonwoven and, where specified, a 25–35 kg/m³ crosslinked polyolefin foam core. The compliance framework for industrial articles of this type is dominated by REACH Regulation (EC) No 1907/2006 for substances of very high concern and, for end uses in interior environments, relevant volatile organic compound emission specifications such as ISO 12219-1:2021 when cabin air quality must be validated. The addition ratio after lamination places the LLDPE web at 38–44 wt% of a two-layer film–nonwoven construction when hot-melt web adhesive is applied at 5–10 g/m² dry; in a three-layer film–nonwoven–foam construction with a 2–3 mm foam core, the LLDPE share falls to 21–26 wt%. The downstream process uses a flat-bed laminator with infrared preheat to 90–110°C, combining nip pressure of 2–4 N/mm, and line speeds of 10–20 m/min to avoid foam compression set and adhesive bleed-through. Published data for this specific configuration in automotive interior trim is limited; converters validate peel adhesion with ASTM D1876-12 T-peel testing on production samples. Terminal products include protective packaging wraps, dunnage sheets, and industrial cover laminates where the LLDPE surface provides the barrier surface and restricts fiber release from the nonwoven layer.

    Free Quote

    Competitive DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness is supplied as a nominal 50.8 µm (2.0 mil) linear low-density polyethylene web intended for lamination to paper, foil, polyethylene terephthalate, oriented polypropylene, or other flexible packaging substrates. The grade designation LX-3 identifies a laminating-grade LLDPE rather than a coextruded sealant structure or a cast polypropylene film; therefore, the layer’s sealing behavior must be separately qualified if the laminate will be converted into bags or pouches. Nominal thickness is not a batch-specific certified value. Incoming lot inspection should verify thickness in accordance with ISO 4593:1993 or ASTM D5947-18, and roll length, core diameter, slit width, and splice count should be confirmed against the manufacturer’s certificate of analysis because those dimensions are not established in this technical note. Published data for LX-3-specific melt index, density, tensile modulus, and optical properties are limited in publicly available industrial sources; design calculations and converting specifications should therefore be based on lot-specific measurements rather than generic LLDPE class values.

    In terms of polymer architecture, linear low-density polyethylene differs from conventional low-density polyethylene by the absence of long-chain branching. That structural distinction translates into characteristic performance differences in laminating webs: LLDPE grades typically exhibit higher dart impact strength under ASTM D1709, higher Elmendorf tear resistance under ASTM D1922, higher puncture resistance under ASTM F1306, and higher elongation at break under ASTM D882 when compared with LDPE at the same nominal gauge. These differences do not automatically transfer to LX-3 unless verified. Compared with metallocene-catalyzed LLDPE laminating films, LX-3 may differ in gel count, clarity, and coefficient of friction; the manufacturer has not published comparative optical or frictional data in the sources available for this note. If LX-3 is being considered as a replacement for a metallocene LLDPE web in a high-clarity pouch, the converter should measure haze and clarity according to ASTM D1003 and ISO 14782 and should not rely on class averages.

    What Limits Corona Treatment and Adhesive Wetting on a 50.8 µm Laminating Web?

    In adhesive lamination, the LX-3 web must exhibit adequate surface energy at the point of adhesive application. A wetting tension of at least 38 mN/m, assessed with dyne solutions conforming to ASTM D2578-17, is the minimum commonly required for solventless and solvent-based polyurethane adhesives; some low-viscosity solventless systems require 40 mN/m to 42 mN/m to avoid dewetting and fish-eye defects. Polyethylene surfaces are inherently nonpolar, so corona treatment must be applied close to the coating station because corona treatment decays over time and under humidity. Storage conditions above 30 °C or relative humidity above 70 % accelerate treatment decay, although the exact decay kinetics of LX-3 are not published. If re-treatment is performed inline, the treater gap, electrode configuration, and power density must be qualified; excessive treatment can produce surface oxidation byproducts that reduce laminate bond strength. Peel adhesion after complete adhesive cure should be measured in accordance with ASTM D1876-08 or ISO 11339:2022, and the failure mode should be identified as adhesive, cohesive, or substrate tear. A change from LDPE to LLDPE at the same thickness can alter the stress distribution in the laminate; a peel value that is acceptable for LDPE may not be transferable to LX-3 without validation.

    Web tension on high-speed laminating machines must be controlled to avoid gauge variation and tunnel defects. Because no published secant modulus for LX-3 is available, the tension set point should be determined from the measured stress–strain curve under ASTM D882 and should limit elongation to no more than 1 % within the unwind-to-recoat span. Tension zones with closed-loop load cells of 10 N to 500 N range are typical on production laminators; the actual set point is converter-specific. At 50.8 µm, the web is stiff enough to resist wrinkling compared with films below 25 µm, but it is not immune to gauge bands. Static charge can also produce blocking and dust pick-up; polyethylene films usually exhibit surface resistivity above 1014 Ω/sq under ASTM D257, so active ionization bars or antistatic tinsel should be located before the coating nip. Curing of solventless adhesive on polyester or paper laminates is commonly performed at 30 °C to 40 °C for 24 h to 48 h; no LX-3-specific cure acceleration or cure inhibition data are published, but slip additives on the film surface can reduce bond strength if they bloom to the interface.

    Table 1 identifies the standard methods relevant to qualifying a 50.8 µm LLDPE laminating web. The absence of published LX-3-specific values from the supplier means that the table should be used as an incoming inspection and process-capability framework, not as a replacement for a certificate of analysis.

    Table 1 — Qualification test matrix for a 50.8 µm LLDPE laminating web
    PropertyStandard codesApplication relevance in laminationLX-3 published data status
    ThicknessISO 4593:1993, ASTM D5947-18Confirms nominal 50.8 µm gauge; affects coat weight and tensionLot-specific certificate required
    Tensile propertiesISO 527-3, ASTM D882Defines modulus and elongation; used for tension set point calculationNot disclosed in current public literature
    Elmendorf tearISO 6383-2, ASTM D1922Indicates direction-dependent tear resistance in pouch formationNot disclosed in current public literature
    Dart impactISO 7765-1, ASTM D1709Evaluates drop-weight puncture resistance at converting and distributionNot disclosed in current public literature
    Wetting tensionASTM D2578-17Verifies corona treatment level before adhesive and ink applicationMust be measured at line
    Haze and clarityASTM D1003, ISO 14782Qualifies optical appearance in transparent laminationsNot disclosed in current public literature
    DensityASTM D1505, ISO 1183-1Confirms base resin class and may support regulatory reviewNot disclosed in current public literature
    Melt mass-flow rateASTM D1238, ISO 1133-1Differentiates LLDPE grades; affects extrusion lamination compatibilityNot disclosed in current public literature
    Melting and crystallinityISO 11357-3, ASTM D3418Provides thermal transition data for heat-exposure limitsNot disclosed in current public literature
    Coefficient of frictionASTM D1894, ISO 8295Affects roll formation, web tracking, and bag filling on vertical form-fill-seal equipmentNot disclosed in current public literature
    Surface resistivityASTM D257Determines static control requirements during coating and slittingNot disclosed in current public literature

    The most critical incoming nonconformities in laminating LLDPE are neither thickness nor grammage but surface-treatment decay, gel contamination, and roll blocking. A lot inspection plan should include dyne testing at both roll edges and core, gel count by optical scanning if the end use is clear lamination, and blocking force after simulated storage. Published data for this specific configuration is limited, so acceptance limits must be derived from internal SPC data rather than from commercial literature.

    Regulatory and Food-Contact Compliance Documentation

    LLDPE base resins are olefin polymers subject to FDA 21 CFR 177.1520 when used in food-contact articles. Compliance under that section requires that the polymer meet the density, melt index, and extraction limitations specified in the regulation; therefore, LX-3 cannot be considered food-contact compliant solely because it is an LLDPE film. The converter should obtain a written food-contact statement from the supplier and confirm whether the specific grade is covered under EU Regulation 10/2011 and EC 1935/2004. For non-food industrial lamination, the usual product stewardship requirements include compliance with REACH (EC 1907/2006) registration obligations and, where applicable, RoHS 2011/65/EU restrictions on lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE. The film itself is not a metallized sheet, but if it is laminated to foil or vacuum-metallized substrates, the final laminate may require supplier declarations under packaging and packaging waste directives. No substance-of-concern data for LX-3 are publicly disclosed; the safety data sheet and technical data sheet remain the controlling documents.

    When LX-3 Substitutes for a Coextruded Sealant Web in Pouch Converting

    A substitution is not a simple gauge-for-gauge replacement. LX-3 is identified as a laminating film; it is not described by the available literature as a coextruded sealant film with a defined seal initiation temperature or hot-tack range. If the converting process requires a sealant layer, the laminate must include a separate sealant web or LX-3 must be qualified by measuring seal initiation and hot-tack strength under ASTM F1921-20, and heat seal strength under ASTM F88/F88M-15. Sealant performance depends on molecular architecture, comonomer type, and slip/antiblock additives; LLDPE resins with butene, hexene, or octene comonomers differ significantly in hot-tack and seal strength. Since LX-3 does not publish its comonomer type, the converter should not assume heat-seal performance will match a metallocene LLDPE sealant web. For boil-in-bag or retort applications, the entire laminate must be tested for bond retention, seal creep, and delamination after thermal exposure; published data for LX-3 in those exact structures is limited.

    On a high-speed rotary die-cutting or slitting line, the 50.8 µm gauge may generate different slit edge quality than a 38 µm LDPE film. Shear slitting blades should be maintained with a sharpness criterion and a side force sufficient to prevent whiskering; polyethylene’s low glass transition temperature can lead to edge stretch and roll blocking if the blade gap is too wide. Razor slitting is acceptable for thin laminating films but may create dust if blade life is exceeded, and LLDPE dust can redeposit on the treated surface and reduce laminating bond strength. After slitting, rolls should be re-checked for surface treatment if they are stored longer than 72 h before lamination. When LX-3 is laminated to a rigid web such as paperboard or foil, the difference in modulus between the two plies can create curl; curl control may require adjustment of tension differential, adhesive coat weight, or steam remoisturizing on the paper web. No curl specification for LX-3 is published, so the converter must qualify curl using production conditions rather than laboratory hand lamination.

    Interlayer delamination of a polyurethane-laminated LX-3 structure can be traced to three primary causes: low surface energy from corona treatment decay below 38 mN/m, adhesive under-dosing below the manufacturer’s minimum coat weight, or migration of slip additives from the film to the interface. The diagnostic sequence should begin with dyne testing of the failed web, followed by T-peel adhesion under ASTM D1876 and, if possible, attenuated total reflectance infrared spectroscopy to identify adhesive and additive distribution at the interface. If adhesion is adequate but the laminate fails by substrate tear, the failure is not a film/adhesive incompatibility. If the film is used as an outer print web, surface treatment should be distinguished from print adhesion: printability requires ink wetting and surface energy in the same range, but the specific ink system and treatment level must be validated. Solvent-based inks may attack additives on the polyethylene surface; the converter should conduct a tape-adhesion test after 24 h aging and before committing to production. Published data for LX-3 under all ink systems is limited.

    Top