Dupont Sclairfilm Lx 3 Lldpe Film Laminating 38 1 µm Thickness

DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 38.1 µm Thickness

    • Product Name: DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 38.1 µm Thickness
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 469221
    Material Linear Low Density Polyethylene (LLDPE)
    Film Type Laminating
    Thickness 38.1 µm
    Density 0.920 g/cm³
    Tensile Strength Ultimate 24.1 MPa
    Tensile Strength Yield 9.65 MPa
    Elongation At Break 600%
    Modulus Of Elasticity 0.207 GPa
    Tear Strength 0.14 N/mm
    Dart Drop Impact 120 g
    Haze 5%
    Gloss 75%
    Coefficient Of Friction 0.2
    Melting Point 120°C
    Vicat Softening Point 100°C
    Water Vapor Transmission Rate 0.5 g/100 in²/day
    Oxygen Transmission Rate 150 cc/100 in²/day

    As an accredited DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 38.1 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged as one roll per carton, moisture-barrier wrapped, containing DuPont™ Sclairfilm® LX-3 LLDPE laminating film, 38.1 µm thick.
    Container Loading (20′ FCL) 20′ FCL loading: DuPont™ Sclairfilm® LX-3 LLDPE laminating film, 38.1 µm thickness, supplied on rolls, palletized, securely braced for ocean transport.
    Shipping DuPont™ Sclairfilm® LX-3 LLDPE laminating film (38.1 µm) ships as non-hazardous rolls on cores, wrapped in protective polyethylene and packed in cartons or crates on pallets. Transport in clean, dry conditions away from sunlight, heat, and sharp objects; normal freight, no special hazmat handling required. Store sealed until use.
    Storage Store DuPont™ Sclairfilm® LX-3 LLDPE Film in a clean, dry, well-ventilated area at ambient temperature, away from direct sunlight, heat, ignition sources, and moisture. Keep in original packaging, supported on its core or flat, to prevent crushing, creasing, or edge damage. Avoid dust, oils, sharp objects, and prolonged UV exposure. Rotate stock and use oldest first.
    Shelf Life Shelf life is 12 months from date of manufacture when stored in original packaging at 23°C and 50% relative humidity.
    Application of DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 38.1 µm Thickness

    The adoption of DuPont™ Sclairfilm® LX-3 LLDPE film at 38.1 µm thickness as the inner sealant web in dry-food pouch structures places the film between a two-component solventless polyurethane adhesive layer and the filled product. Surface preparation is the first processing gate. The corona-treated side of LX-3 must exhibit a wetting tension of at least 38 mN/m by ASTM D2578-17, with readings taken at multiple points across the web because cast LLDPE can exhibit anisotropic wetting decay after 90 days of warehousing. If surface energy falls below 36 mN/m, adhesive de-wetting appears as elongated voids in the lamination after slitting, and the defect is often misidentified as coating roll chatter. On a solventless laminator with servo-driven unwind and load-cell dancer control, the web is run at 0.6–0.8 N/cm of web width to keep elongation below 1%. Higher tension induces transverse neck-in at the nip, reducing overall width by 1.5–3%, which shifts side seal positions downstream and produces intermittent leakers at the pouch former. Lamination is performed at 40–60 °C nip temperature and 3–5 N/mm nip pressure, with coating weights between 1.8 g/m² and 2.5 g/m² depending on the adhesive viscosity at application temperature. Line speeds in the 150–250 m/min range are attainable when the dynamic coefficient of friction of the film remains below 0.35 as measured by ISO 8295:1995; higher slip-agent bloom after heat exposure can reduce the substrate–adhesive interaction and lower the final peel strength.

    After lamination to metallized BOPP or PET, the structure is cured for 24–48 h at 25–40 °C. Premature slitting before full adhesive cure produces edge bleed and can contaminate sealing bars with oligomeric components. The cured laminate is then heat-sealed on a vertical form-fill-seal line. The seal initiation temperature for a cast LLDPE sealant of this class is generally observed at 95–110 °C at 0.5–1.0 s dwell and 2–4 bar jaw pressure. Seal strength in the range 15–25 N/15 mm is common for dry-food pouch acceptance, using ASTM F88/F88M-21 with 300 mm/min jaw separation and a 15 mm specimen width. If the seal bar temperature exceeds 120 °C for more than 1.5 s, seal creep initiates and the pouch fails by fibrous tear propagation rather than controlled peel, which is a limitation for high-speed lines with poor temperature uniformity. The single-layer nature of LX-3 means that the film does not provide a high-barrier moisture or oxygen layer. Laminates for dry foods therefore require a metallized or aluminium foil barrier layer, and the sealant film contributes mechanical toughness, seal integrity, and product-side compatibility. In the United States, olefin polymer films of this composition are expected to fall under 21 CFR 177.1520(c), while in the European Union the finished laminate is assessed under EU 10/2011 with overall migration into food simulants tested by EN 1186-1. The film alone cannot support a blanket food-contact claim because adhesive residues, printing inks, and barrier layers have independent migration limits. For lamination to aluminium foil, the absence of long-chain branching in LLDPE yields a sealant with comparatively better hot tack and puncture resistance than LDPE at equivalent thickness. However, the high coefficient of friction of unmodified LLDPE forces converters to select a film variant with controlled slip, and that modification can reduce lamination bond values if the slip agent migrates into the adhesive layer during cure. Published data for this specific grade under high-seal-bar temperature and slip-agent migration are limited, so finished-laminate testing is required before process qualification.

    Why Does a 38.1 µm Cast LLDPE Overlaminate Delaminate on UV-Curable Ink?

    Overlamination of narrow-web pressure-sensitive label facestocks with DuPont™ Sclairfilm® LX-3 at 38.1 µm thickness frequently fails at the print interface rather than at the film-adhesive interface. UV-curable flexographic and inkjet inks can leave residual acrylate monomer and photoinitiator fragments in the upper ink layer; these residues act as a weak boundary layer. If the overlaminate is applied without a primer, peel values measured by FINAT FTM 21 or ASTM D903-98(2017) may fall below 5 N/25 mm, with failure occurring cohesively in the ink. The problem is exacerbated when the film's corona treatment has decayed below 40 mN/m, because the low surface energy of the ink film plus the low film wetting tension prevents adhesive spreading. On a narrow-web laminator with a 300–500 mm web width, variations in unwind tension from 0.5 N/cm to 1.0 N/cm generate hard wrinkles because the film lacks the stiffness of PET overlaminate.

    When solventless overlamination is selected, coating weight is held at 1.0–1.8 g/m² to preserve optical clarity, but the low coating weight requires extremely uniform nip contact. A two-roll laminator with a 70–80 Shore A rubber nip roller at 3–4 N/mm reduces adhesive mottling. Haze of the unlaminated film is generally below 8% by ASTM D1003-21, but the cured adhesive can introduce a visible orange-peel pattern if the coating roll speed ratio is outside 1.0–1.2. Gloss measured at 60° by ISO 2813:2014 is often above 85 GU for a cast LLDPE film, yet the final label gloss depends chiefly on the smoothness of the ink layer and adhesive thickness. Curl control is line-specific; published standards for film-facestock curl are limited, and converters typically use internal flat-sheet gauges rather than a single harmonized ISO method. For UV-curable ink surfaces, adhesion promotion is often required. A water-based primer at 0.3–0.5 g/m² dry coat weight or a corona re-treatment at 1.0–1.5 kW side is used immediately before the nip. Without one of these, delamination can occur after 24 h post-cure when the ink continues releasing monomers. Thermal lamination, if used instead of adhesive, requires a heated nip at 100–130 °C, which is close to the softening point of the film; the film must not be allowed to contact the heated roller for more than 0.5 s to avoid heat-set wrinkles that register as visual defects in the label. The most important operational boundary is that this film is not a high-clarity optical grade in the sense of a coated polypropylene overlaminate; if the final application requires haze below 2%, a different film should be evaluated. Published data for LX-3 under UV ink lamination specifically is limited, so the initial trial must include 48 h aged peel testing and low-temperature 5 °C label application tests to detect adhesive brittle failure.

    Medical Device Pouch Lamination and ISO 11607 Seal-Boundary Process Variables

    Lamination of DuPont™ Sclairfilm® LX-3 at 38.1 µm thickness into medical device pouches is allowed only after the converter recognizes that food-contact status does not replace medical-grade evaluation. The film can serve as a lamination layer between a nonwoven or paper substrate and an outer printed layer, or as a sealant web when laminated to an uncoated polyolefin backing. Process validation under ISO 11607-1:2019 requires documented equipment installation qualification and operational qualification of sealing equipment, with seal parameters in the range of 120–145 °C jaw temperature, 0.5–1.0 s dwell, and 3–5 bar pressure for LLDPE-based structures. The seal strength after stabilization is evaluated by ASTM F88/F88M-21; for medical device pouches, a typical acceptance criterion is a minimum seal strength of 1.5 N/15 mm for peel-open pouches, but the value depends on package configuration and sterilization method.

    Sterilization compatibility is a critical threshold. Ethylene oxide sterilization at 50–60 °C and relative humidity 50–70% generally does not severely alter PE film properties, but EtO residual after aeration can be trapped by a solventless laminating adhesive, so the finished pouch must be validated for ethylene oxide residue per ISO 10993-7:2008. Gamma irradiation at 25–40 kGy can increase seal strength by oxidative crosslinking in LLDPE, but it may also raise the seal initiation temperature by 3–6 °C depending on dose rate; if the irradiation is performed after sealing, the seal region may become more brittle. Published data for this specific film under gamma is limited, so dose mapping per ISO 11137-1:2006 and post-irradiation seal testing over the full sterilization dose range are mandatory. The film alone is not a microbial barrier for porous substrates, but in a laminated structure with Tyvek or paper the barrier is determined by the porous material. Peel-open failure between the film and the porous substrate is more common than film tear because the LLDPE layer is tougher than the paper fibres; this shifts failure mode classification from cohesive to substrate failure, which package engineers may choose to control by using a heat-seal coating instead of relying on the LX-3 surface.

    For biocompatibility, the laminated structure is assessed under ISO 10993-5:2009 and ISO 10993-10:2010; solventless adhesive extractables can influence cytotoxicity, so the adhesive choice is often more restrictive than the film. The film should be qualified for absence of phthalates and for heavy metals according to EU MDR 2017/745 or regional device packaging requirements. A common process failure is blocking of the unsealed film roll after EtO pre-conditioning; if wound rolls are stored at temperatures above 40 °C, blocking can occur and the roll hardness should be controlled below established converter-specific limits. The following compliance matrix identifies the principal standards that govern this application.

    StandardTitleRelevant application boundary
    ISO 11607-1:2019Packaging for terminally sterilized medical devicesProcess validation of seal equipment, seal strength, integrity
    ASTM F88/F88M-21Seal strength of flexible barrier materialsPeel force; minimum acceptance depends on pouch configuration
    ISO 10993-5:2009In vitro cytotoxicityEvaluation of finished laminate extractables
    ISO 10993-7:2008Ethylene oxide sterilization residualsAeration validation for adhesive-containing laminates
    ISO 11137-1:2006Sterilization of health care products by radiationDose mapping and post-irradiation seal performance

    When the Film Is Die-Cut as a Carton Window Patch at High Speed

    High-speed window patching lines operating at 20,000–40,000 sheets/h impose die-cutting, handling, adhesive application, and curl constraints on DuPont™ Sclairfilm® LX-3 at 38.1 µm thickness. The film is supplied in slit rolls and is die-cut with rotary dies; a sharp die anvil clearance is required because LLDPE film elongates before fracture and can produce stringy die-cut edges if the die is dull. The objective is to achieve clean shear edges with no angel-hair residues, which can transfer to adhesive rollers and contaminate subsequent sheets. The machine-direction tensile elongation of cast LLDPE is generally above 500% by ASTM D882-18; this high elongation allows the patch to conform to the paperboard window but also makes the web sensitive to draw ratio. A draw ratio above 1.05 between infeed nip and die station produces permanent elongation that shifts the patch registration and alters the film thickness locally. Unwind tension is typically kept below 0.5 N/cm.

    Static dissipation is more critical for LLDPE than for PVC window films. A surface resistivity above 1014 Ω/sq measured by IEC 62631-3-2:2016 can cause double sheets and patch misfeed; ionizing bars or anti-static rollers operating at 50 Hz or high-frequency discharge are used immediately before the die. Optical properties are relevant because the window patch must not exceed a haze value of 8% by ASTM D1003-21 and should maintain a light transmission above 88% by ASTM D1003-21. The film's coefficient of friction should be in the 0.25–0.35 range to allow sheet separation; if slip migration occurs during storage, the static coefficient increases above 0.45 and the patch film may not release from the vacuum feed table. This failure is often observed when rolls are stored at temperatures above 35 °C for more than 4 weeks; published data for this specific film's storage stability under high-temperature warehouse conditions is limited.

    Adhesive selection for window patching typically uses a water-based emulsion or a hot melt. With hot-melt adhesives applied at 150–170 °C, the film must remain stable during 0.1–0.3 s exposure to the hot nozzle; local thermal distortion creates visible waves around the patch perimeter. The film should be evaluated on the intended converting line because the thermal conductivity of the patch and the adhesive open time determine whether the adhesive transfers completely. If the carton is used for food-contact applications, the finished window patch must comply with the relevant food packaging regulation, but the film itself is not certified as a functional barrier against moisture or oxygen unless combined with additional barrier layers. For bakery cartons, the moisture vapour transmission rate of the LX-3 film is high because it is a polyethylene layer of only 38.1 µm; an MVTR above 15 g/m²·day at 38 °C and 90% RH by ASTM F1249-20 is typical for similar cast LLDPE films, which means the window is not a moisture barrier. Published data for this specific grade's MVTR is limited.

    Protective Tape Carrier Webs and the Onset of Anisotropic Necking Under Tension

    Coating of pressure-sensitive adhesives onto the exposed surface of LX-3 at 38.1 µm thickness positions the film as the carrier web for PE protective tapes used on painted metal, glass, and thermoformed parts. The film must be corona-treated to a wetting tension of at least 40 mN/m per ASTM D2578-17 immediately before coating, because polyethylene surface energy decays quickly after treatment and is affected by slip-agent bloom. A solventless or water-based acrylic adhesive is applied at 20–40 g/m² dry coat weight depending on the required peel adhesion. The adhesive anchorage is tested by peeling the adhesive from the film at 180° with 300 mm/min jaw speed per ASTM D3330/D3330M-04(2018); cohesive failure in the adhesive or transfer to the substrate is the primary failure mode to avoid. With proper anchorage, peel adhesion to stainless steel is commonly specified between 1.0 N/25 mm and 4.0 N/25 mm for protective tape, but LX-3 is primarily a carrier rather than an adhesive-coated product in its laminating form, so additional coating trials are required.

    Necking under tension is the main processing hazard. A cast LLDPE film with high MD elongation and comparatively lower TD elongation will neck-in under even small draw ratios. If the drive ratio between coating station and rewinder exceeds 1.02, the web width narrows by more than 1%, and the edge beads of adhesive become uneven. The exact elongation behaviour should be quantified by ASTM D882-18; published data for DuPont™ Sclairfilm® LX-3 specifically is limited, but cast LLDPE films of 38.1 µm thickness typically show MD tensile strength near 20–35 MPa and TD tensile strength near 15–25 MPa. These ranges are not product-specific and should be verified on the actual film. The film's low flexural stiffness also causes it to follow the adhesive coating roll, and at speeds above 150 m/min, air entrainment between the web and the coating roller can create skip-coat defects unless the wrap angle is maintained above 60°. The use of a closed-loop tension control with dancer roll response below 100 ms is recommended for stable coating at high speed.

    For applications on unpainted exterior surfaces, the carrier film must withstand outdoor exposure without significant UV degradation. Polyethylene films without adequate UV stabilization lose elongation after 6–12 months of outdoor weathering; accelerated weathering by ISO 4892-2:2013 with xenon-arc exposure is used to estimate relative stability. This laminating film is not designed as a long-term outdoor weatherable film; if the protective tape remains on a surface beyond 6 months, the film may become brittle and leave adhesive residues upon removal. The end user should test removal after the intended service life and at both 23 °C and 5 °C to identify low-temperature stiffening. Published data for this specific grade under xenon-arc weathering is not available; therefore, out-of-scope outdoor use should be validated independently.

    The behaviour of LX-3 at 38.1 µm thickness as the internal sealant in laminated spouted pouches for household liquid detergents is governed by hot tack, seal-through-contamination resistance, and environmental stress cracking resistance. In a representative structure of PET print web / aluminium foil / solventless adhesive / LX-3 sealant, the film is exposed to product contact on the inner surface after the spout is ultrasonically or heat-welded. The sealing process on a horizontal form-fill-seal machine with product drop filling runs at 80–120 pouches/min; the seal bar temperature is normally set 10–20 °C above the film's seal initiation temperature to achieve molten state under dwell times of 0.3–0.8 s. Hot tack force measured by ASTM F1921/F1921M-18 is the critical parameter because the filled pouch opens the seal area immediately after sealing while the polymer is still partially molten. A hot tack value below 2 N/15 mm at the sealing temperature typically results in seal creep and product leakage. Published data for LX-3 hot tack is limited; however, LLDPE sealant films of similar thickness often exhibit hot tack above 2 N/15 mm over a window of 95–115 °C.

    Seal-through-contamination occurs when a droplet of the liquid product is trapped in the seal region. The detergent's surfactants lower the interfacial seal strength by disrupting polymer–polymer interdiffusion. This is evaluated by applying a controlled 0.05 mL droplet of a surfactant solution to the seal area before sealing and testing seal strength per ASTM F88/F88M-21. The film's linear low-density character improves stress crack resistance compared with branched LDPE, particularly in the presence of alcohols or surfactants, but the stress crack resistance should be evaluated on the finished laminate under controlled strain and temperature. Environmental stress cracking resistance of PE is commonly assessed by ASTM D1693-21 under a constant strain in a 10% Igepal CO-630 solution at 50 °C; LLDPE grades typically show much longer failure times than LDPE, but the specific value for this film is not published. The spout weld must also be localized enough to avoid melting through the film; ultrasonic welding with amplitude 15–25 µm and cycle time 0.2–0.6 s is used, with the weld area limited to the spout flange. If the amplitude exceeds 30 µm, the localized heating can melt the film and create pinholing at the spout base, leading to drops of product accumulating outside the pouch.

    The final laminate must pass a drop test according to the customer’s package protocol, commonly based on ISTA 3A or internal standards, with drop heights of 600–900 mm depending on pouch weight. The LX-3 film contributes to puncture resistance and seal area survival, but the aluminium foil layer governs pinhole formation and flex-crack resistance. A package using LX-3 as a sealant is suitable for ambient distribution 5–40 °C; it should not be used in frozen packaging without evaluation of low-temperature seal brittleness. The seal strength at -18 °C may drop by more than 30% relative to ambient, so frozen liquid pouches require additional testing.

    Free Quote

    Competitive DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 38.1 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont™ Sclairfilm® LX-3 is a cast linear low-density polyethylene film supplied in a nominal thickness of 38.1 µm (1.5 mil). The LX-3 designation identifies a laminating grade within the Sclairfilm portfolio; the film is intended for use as a web component in adhesive lamination, extrusion lamination, and thermal lamination of flexible packaging structures. Manufacturer documentation lists the product as a polyethylene film based on ethylene–alpha-olefin copolymer chemistry, with the specific comonomer type and melt flow ratio listed on the certificate of analysis rather than in general literature. The 38.1 µm gauge corresponds to a thickness tolerance commonly controlled by ISO 4593 or ASTM D374; converters using automatic gauge-control systems verify flatness and thickness profile before lamination.

    Material Identity and Gauge Specification

    The resin is a linear low-density polyethylene, meaning the polymer backbone contains short-chain branches introduced by alpha-olefin copolymerization. Class-level LLDPE laminating films of this thickness typically show a nominal density of 0.918–0.920 g/cm³ when measured by ISO 1183-1 or ASTM D1505; melt mass-flow rate values for cast film grades are generally in the range of 1.0–2.0 g/10 min under 2.16 kg at 190 °C in accordance with ISO 1133-1. Because Sclairfilm LX-3 supplier literature does not publish a single fixed melt index for every batch, the certificate of analysis and manufacturing batch data control these values. The 38.1 µm thickness is a nominal value; roll-profile uniformity is relevant because gauge variation greater than ±5% across the web can create bagginess, wrinkle, and non-uniform lamination bond. Differential scanning calorimetry of LLDPE films of this class typically records a broad melting endotherm with peak melting temperature near 121–124 °C; the LX-3-specific DSC curve should be obtained from the supplier if heat-sealing or thermal resistance limits are critical.

    What Surface Preparation and Lamination Adhesion Factors Are Critical?

    Adhesion in laminating grades is controlled by surface oxidation and surface energy. LX-3 is supplied with a corona-treated surface for lamination; the treatment level should be verified by wetting tension measurement under ASTM D2578. A minimum treated-surface wetting tension of 38 mN/m is commonly specified for solventless and waterborne polyurethane adhesives; adhesive manufacturers may require 40 mN/m or higher for high-speed lines. Re-treated film is necessary when storage accumulates hydrophobic low-molecular-weight species; migration of slip and antiblock additives to the surface can reduce wetting tension below 36 mN/m and cause bond inconsistency. Lamination bond strength is measured after curing by ASTM F904 or ISO 11339; for a 38.1 µm LLDPE film laminated to biaxially oriented polyethylene terephthalate or aluminum foil, typical peel strengths fall between 200 g/25 mm and 800 g/25 mm, but the acceptable minimum depends on the structure and end-use. The film is also used as a sealing layer or outer ply where the coefficient of friction is controlled; kinetic COF is typically evaluated by ISO 8295.

    In adhesive lamination, the film is unwound at controlled tension, passed through a coating station where adhesive coat weight is maintained at 1.8–2.5 g/m² for solventless polyurethane systems, and laminated at nip temperatures of 50–80 °C. In extrusion lamination, the 38.1 µm LLDPE film is used as a preformed substrate rather than as the extruded melt layer; molten low-density polyethylene or LLDPE is applied between the preformed film and a secondary web such as aluminum foil, paper, or oriented polyester. Neck-in and draw resonance on the extrusion laminator are controlled by melt temperature, die lip gap, and air gap; LLDPE resins typically require lower melt temperatures of 290–310 °C and a die lip gap of 0.7–1.0 mm, but equipment setup must be adjusted for the specific laminator. For thermal lamination, the film is combined with heat-sealable substrates under nip pressures of 2–4 bar and surface temperatures of 90–120 °C; exceeding 80 °C in continuous service after lamination is not recommended because LLDPE softens and creep can reduce bond integrity. The use of on-web corona re-treatment immediately before lamination is standard when stretch film or stored rolls show surface-energy decay.

    Thermal Processing Envelope and Melt Rheology

    The processing window for LLDPE is narrower than for high-pressure LDPE because of the polymer’s linear backbone and lower level of long-chain branching. In extrusion lamination, LLDPE exhibits greater neck-in and lower draw stability than LDPE; these differences require quantification on the specific laminator. Melt viscosity at low shear rates is typically higher for LLDPE than for LDPE of equivalent melt index, which increases back-pressure and screw torque in single-screw extruders. Processors using 45–90 mm single-screw extruders with 24:1 to 30:1 L/D ratios report that LLDPE output may drop by 10–15% relative to LDPE when screw rpm is held constant, but published data for the LX-3 grade are limited. Barrel temperature profiles from feed to die are commonly set at 170–200–220–240–260 °C for cast film processing, while extrusion lamination die temperatures may require 280–320 °C; actual settings are defined by melt temperature measurement with an insertion thermocouple. For the laminating film itself, continuous exposure above 70 °C can cause dimensional distortion; heat seal initiation temperature is a separate property commonly reported in the range of 95–115 °C for LLDPE sealant films, but LX-3 is not marketed as a sealant film and seal-initiation values should be confirmed by the supplier.

    When LX-3 Replaces LDPE or EVA in Laminating Structures

    LDPE laminating films offer easier melt processing and higher draw stability but lower tensile strength, puncture resistance, and dart impact strength than LLDPE. A 38.1 µm LX-3 LLDPE film can often replace a 50 µm LDPE film in a flexible package without reducing abuse resistance, as measured by dart impact ASTM D1709 and slow-rate puncture ASTM F1306; downgauging assessments must include seal-through and tear tests because LLDPE can exhibit lower Elmendorf tear values in some orientations, measured by ASTM D1922. Compared with EVA copolymer films, the LX-3 class provides a higher melting peak and better thermal resistance, but lower polar adhesion to aluminum foil and less low-temperature seal performance. EVA laminating films typically contain 5–18 wt% vinyl acetate, which reduces melt temperature and increases adhesion to polar surfaces; however, EVA can contribute higher odor, higher surface tack, and higher moisture permeability. For aseptic or retort-like structures, LX-3 is not a substitute for retort-grade polypropylene or polyester films because its continuous service temperature limit is below typical retort conditions of 121 °C. The choice between LX-3 and other Sclairfilm grades depends on whether the converter requires a laminating corona-treated surface or a slip-modified film; LX-3 is specifically designated for laminating applications, whereas other Sclairfilm grades may be formulated for shrink, overwrap, or lamination with different additive packages.

    Representative comparative values for laminating film classes
    PropertyTest methodLX-3 class LLDPELDPE laminating filmEVA laminating film
    Nominal thicknessISO 459338.1 µm50 µm50 µm
    DensityASTM D15050.918–0.920 g/cm³0.916–0.925 g/cm³0.925–0.945 g/cm³
    Dart impact strengthASTM D1709Higher than LDPE at equal gaugeLowerIntermediate
    Low-temperature sealASTM F1921FairPoorGood
    Adhesion to aluminum foilASTM F904Requires coronaRequires coronaHigher polar adhesion
    Continuous service temperature limitSupplier data70–80 °C60–70 °C60–70 °C

    Compliance, Migration Testing, and Food-Contact Status

    Polyethylene food-contact status is addressed through 21 CFR 177.1520 in the United States and Regulation (EU) No 10/2011 in the European Union. 21 CFR 177.1520(c) describes olefin polymers, including LLDPE copolymers, provided the finished film meets extractive limitations and is used in accordance with good manufacturing practices. The EU regulation establishes an overall migration limit of 10 mg/dm² for food-contact plastics; testing is carried out under the time and temperature conditions specified in EN 1186-1 and EN 1186-14 for aqueous, acidic, alcoholic, and fatty food simulants. Specific migration of monomers and additives must be below the SMLs listed in Annex I of Regulation (EU) No 10/2011. The raw resin supplier’s compliance statement is required to confirm that the LX-3 resin does not contain SVHCs above 0.1% w/w under REACH Article 33; RoHS Directive 2011/65/EU may be requested for packaging used with electronic equipment, but RoHS substance restrictions apply to homogeneous materials and may not be automatically satisfied by base polyethylene. Heavy metal conformity is tested by inductively coupled plasma optical emission spectrometry; the absence of cadmium, lead, mercury, and hexavalent chromium below the RoHS threshold is confirmed by supplier declaration rather than by inference from the polymer class.

    Compliance matrix for flexible packaging laminating films
    Regulation / standardScopeTest method / limit
    FDA 21 CFR 177.1520Olefin polymers in contact with foodExtraction limits by 21 CFR 177.1520(c)
    EU Regulation (EU) No 10/2011Plastic materials and articles intended to come into contact with foodOverall migration 10 mg/dm²; EN 1186 series
    REACH (EC) No 1907/2006SVHC communication0.1% w/w threshold, Article 33