Dupont Sclairfilm Lx 1 Lldpe Film Laminating 76 2 µm Thickness

DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness

    • Product Name: DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 210274
    Productname DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness
    Manufacturer DuPont
    Material Linear Low-Density Polyethylene (LLDPE)
    Grade LX-1
    Productline Sclairfilm®
    Application Laminating
    Form Film
    Thickness 76.2 µm
    Thickness Mil 3.0 mil
    Color Clear
    Typicaldensity 0.922 g/cm³
    Typicaltensilestrength Md 22 MPa
    Typicaltensilestrength Td 19 MPa
    Typicalelongationatbreak Md 550%
    Typicalelongationatbreak Td 650%
    Typicaldartdropimpact 150 g
    Typicalhaze 8%
    Typicalgloss 45deg 75%
    Typicalcoefficientoffriction 0.20
    Typicalwatervaportransmissionrate 0.4 g/100 in²/24 h
    Typicaloxygentransmissionrate 100 cc/100 in²/24 h
    Typicalheatsealtemperature 120 °C
    Typicalsealstrength 1.5 lb/in
    Typicalmeltingpoint 122 °C
    Typicalusetemperaturerange -40 °C to 80 °C

    As an accredited DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Each carton contains one roll of DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness, securely wrapped.
    Container Loading (20′ FCL) Standard 20′ FCL container loading: palletized cargo of DuPont™ Sclairfilm® LX-1 LLDPE laminating film, 76.2 µm, dry, ambient, secured, evenly distributed.
    Shipping Shipping: DuPont™ Sclairfilm® LX-1 LLDPE film is non-hazardous and not regulated for transport. Ship in original packaging on pallets, protected from moisture, heat, sunlight, puncture, and contamination. Maintain ambient conditions; handle with care to prevent roll damage. No UN number or hazard class required. Follow local and carrier requirements.
    Storage Store DuPont™ Sclairfilm® LX-1 LLDPE Film in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and incompatible chemicals. Keep in original sealed packaging, protected from dust, moisture, oils, and sharp objects. Lay flat or keep on roll to prevent creasing. Avoid prolonged UV exposure and excessive stacking pressure. Maintain moderate temperature/humidity, follow FIFO, and consult the SDS.
    Shelf Life Shelf life is indefinite when stored in original packaging under cool, dry conditions, away from direct sunlight, heat, and moisture.
    Application of DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness

    DuPont™ Sclairfilm® LX-1 LLDPE film at 76.2 µm thickness is supplied as a one-side corona-treated laminating web for heat-sealable inner plies in multi-layer flexible packaging and protective laminates. The treated surface is intended for adhesive or extrusion bonding. The untreated surface remains available for heat sealing against itself or coated substrates. Converters commonly verify wetting tension after slitting and before lamination using ASTM D2578; a level of 38–42 mN/m is a typical production acceptance window. Surface tension decay below 38 mN/m may produce adhesive dewetting, channeling, or variable bond strength after curing. The web should be stored and conditioned at 20–25 °C and 40–60% relative humidity to minimize blocking and condensation. Direct contact with strong oxidizing agents, halogenated solvents, and aromatic hydrocarbons should be avoided because these substances can swell or degrade linear low-density polyethylene. As an LLDPE sealant layer, the film provides a broad heat-seal plateau and higher hot-tack strength than LDPE homopolymer of equivalent gauge. The following application scenarios reflect established converting practice for LLDPE laminating webs of this thickness. Film-specific published performance data should be confirmed with DuPont technical documentation where cited values are not generated from controlled laminate trials.

    Dry food pouch converters laminate the 76.2 µm web to reverse-printed biaxially oriented polypropylene or polyethylene terephthalate using a two-component solventless polyurethane adhesive. The lamination nip temperature is typically controlled between 60 °C and 80 °C. Adhesive coat weights are maintained in the range of 1.8–2.5 g/m² on smooth-roll or gravure coating stations. The untreated LLDPE surface becomes the inner sealant layer on vertical form-fill-seal machines operating above 80 packs/min. Seal jaw temperatures are set between 115 °C and 145 °C with dwell times from 0.3 s to 0.8 s. Hot-tack onset below 100 °C measured by ASTM F1921 permits product drop immediately after seal release. A seal strength of 18–25 N/25 mm tested per ASTM F88 is commonly specified for dry snack laminates. Food-contact status is evaluated under FDA 21 CFR 177.1520 and EU 10/2011. Overall migration for the finished plastic layer must not exceed 10 mg/dm² under the intended food simulant. The 76.2 µm gauge adds web stiffness relative to 50 µm sealant films, which reduces neck-in during lamination and improves layflat on high-speed packing lines. However, published peel strength data for this specific Sclairfilm® LX-1 configuration in high-fat dry food structures is limited. Converters should perform migration tests on the actual laminate with the intended food simulant and sealing temperature profile.

    In medical device packaging, the LLDPE laminating web is bonded to coated paper, Tyvek®, or polyester lidding substrates to create peelable or destruct-seal pouches. The heat-seal coating on the rigid or semi-rigid counterpart governs the seal transfer parameters. Platen sealers and rotary sealers require different dwell, pressure, and temperature mapping because Tyvek® and coated paper have different thermal conductivity than polyethylene. ISO 11607-1 establishes requirements for sterile barrier system design and seal integrity. ISO 11607-2 covers process validation for production and equipment. Seal strength is measured by ASTM F88; package integrity is evaluated by ASTM D3078 vacuum leak testing. The LLDPE layer contributes puncture resistance and tear resistance during transit and storage. Sterilization compatibility must be verified for ethylene oxide, gamma irradiation, or electron beam processes. Gamma irradiation at 25–40 kGy can induce chain scission or crosslinking in polyethylene depending on the stabilizer package and dose rate. Published data for Sclairfilm® LX-1 at 76.2 µm in gamma-sterilized medical pouch structures is limited. Therefore qualification must include post-sterilization seal strength retention and visual inspection for delamination. The film should be sealed at temperatures that prevent burn-through of the polyethylene layer. Adhesive-laminated medical structures should be aged for at least 24 h at 20–25 °C before final seal testing to allow adhesive cure.

    Standard or regulationApplication areaCritical requirement
    FDA 21 CFR 177.1520Food contact olefin polymersFinished laminate must meet extractives limits for the intended food type and use condition.
    EU 10/2011Plastics in food contactOverall migration ≤ 10 mg/dm²; specific migration limits apply to monomers and additives.
    EC 1935/2004Framework RegulationFinished article must not transfer constituents to foods in quantities that endanger health or alter food composition.
    ISO 11607-1Sterile barrier system designSeal integrity, strength, and design requirements verified before release.
    ISO 11607-2Sterile barrier system validationInstallation qualification, operational qualification, and performance qualification required.
    REACHSubstance compliance in EUSVHC concentration ≤ 0.1% w/w per article if applicable.

    Can 76.2 µm LLDPE Maintain Seal Integrity Under Frozen Distribution Conditions?

    Frozen food laminates incorporating Sclairfilm® LX-1 as the sealant web are typically constructed as PET/ink/adhesive/LLDPE or BOPP/adhesive/LLDPE. The sealant layer must resist flex cracking and puncture after exposure to temperatures as low as -40 °C. LLDPE retains low-temperature toughness better than LDPE homopolymer because the molecular structure has less long-chain branching density. Seal strength after frozen storage is tested after conditioning at -18 °C for 24 h. Packaging converters commonly specify a minimum heat-seal strength of 15 N/25 mm per ASTM F88 after thawing. The 76.2 µm gauge adds puncture resistance against sharp frozen food edges such as cut vegetables or frozen seafood shells. The outer printed web controls moisture barrier and stiffness. The LLDPE layer does not provide high oxygen barrier; aroma and oxygen barrier are supplied by PET or metallized layers. Corona treatment retention on the adhesive side after storage should be re-verified before lamination. If wetting tension falls below 38 mN/m, an inline corona treater may be used at 2–4 kW depending on line speed and electrode coverage. The seal initiation window for LLDPE is broad compared with ionomer or EVA sealant resins. Seal-through frost performance is a known production bottleneck on high-speed vertical fillers for frozen products. Residual moisture on the seal area can produce channel leakers. A hot-bar sealer with knurled jaws is often used to displace moisture during sealing. Film-to-film sealant layers may require differential temperature settings because the LLDPE web is thicker than the outer web. Parameters should be validated on production-scale sealers because laboratory sealers may not replicate jaw pressure distribution across the seal area.

    Extrusion Lamination to Aluminum Foil Demands Tight Melt Curtain Control

    Extrusion lamination of Sclairfilm® LX-1 to aluminum foil or metallized substrates uses a molten polymer tie layer between the pre-formed film and the foil. The 76.2 µm LLDPE web is fed from a dancer-loaded unwind. Low and consistent tension is essential to prevent tunneling and wrinkle formation. The molten tie-layer curtain is extruded from a flat die and drawn into a nip formed by a chill roll and pressure roll. The air gap is typically set between 90 mm and 250 mm to limit neck-in and oxidative degradation. Melt temperature for LDPE tie resin is controlled between 315 °C and 330 °C. Chill roll water temperature is commonly held at 15–25 °C to solidify the tie layer without condensation. The foil layer at 9 µm thickness provides near-zero moisture and oxygen transmission when intact. Foil is susceptible to flex cracking and pinhole formation during transport and filling. The LLDPE layer adds bulk, puncture resistance, and low-temperature abuse resistance to the foil structure. In adhesive lamination of foil to LLDPE, solventless adhesive coat weights of 2.0–3.0 g/m² are common. Adhesion is tested per ASTM F88 or ASTM D1876. A properly bonded foil laminate should fail by film tear or foil elongation rather than adhesive peeling. The LLDPE film must not contain high levels of migratory slip agents that can reduce adhesive bond strength over time. Erucamide slip migration from the polyethylene layer can contaminate the adhesive interface during aging. A low-slip or medium-slip formulation may be specified for lamination grades; the exact additive package should be confirmed with the film supplier. A typical seal strength target for foil sachets is 20–30 N/25 mm per ASTM F88. For retortable foil structures, standard LLDPE is not rated for retort exposure above 121 °C under pressurized steam unless a higher-density or specially stabilized grade is used. Trials should include post-retort bond and seal retention testing. Published data for this specific Sclairfilm® LX-1 film under retort conditions is limited.

    Converting variableTypical control rangeMeasurement method
    Surface wetting tension38–42 mN/mASTM D2578
    Adhesive coat weight1.8–3.0 g/m²Gravimetric coat weight check
    Lamination nip temperature60–80 °CInfrared thermometer
    Seal jaw temperature115–145 °CThermocouple in seal jaw
    Hot tack onset≥ 95 °CASTM F1921
    Seal strength target15–30 N/25 mmASTM F88
    Gamma irradiation dose25–40 kGyDosimeter mapping

    When thermal lamination is used to bond the film to nonwoven polypropylene for automotive trunk liners and load floors, the process relies on heat and pressure rather than adhesive. The nonwoven web is preheated and pressed against the LLDPE web by a heated calender or flatbed laminator. The nip temperature is selected between 105 °C and 125 °C to soften the polyethylene surface without melting the nonwoven structure. Typical nip pressures range from 3 bar to 6 bar depending on roller width and embossing pattern. The resulting laminate provides a moisture barrier and improves abrasion resistance in interior load areas. LLDPE contributes flexibility at cold temperatures. The laminate must pass fogging tests according to DIN 75201 or OEM-specific variants. Low volatile organic compound emissions are required for automotive interiors. The film's additive package should be checked for compatibility with these requirements because migratory slip agents or antiblock additives may contribute to volatile condensate. The 76.2 µm gauge allows the laminate to be die-cut without excessive edge fraying. Sharp die blades and hard anvils are recommended to avoid film elongation. The film's elongation at break tested by ASTM D882 is typically above 400% for LLDPE, which allows limited deep drawing. However, for automotive interior use, the finished laminate must meet flammability standard FMVSS 302. Published data for Sclairfilm® LX-1 in this specific nonwoven configuration is limited. Processors should conduct full flammability and emission testing on the final laminate.

    When High-Barrier Metallized PET Is Adhesive-Laminated to the Sealant Web

    High-barrier laminates for coffee, powdered beverages, and oxygen-sensitive dry foods may use metallized PET as the outer web and Sclairfilm® LX-1 as the inner sealant layer. The structure is bonded with a two-component solventless or solvent-based adhesive. Metal adhesion to the LLDPE requires a continuous adhesive layer because metallized PET surfaces are sensitive to moisture and acid penetration. The LLDPE layer contributes puncture resistance and seal-through-product-dust tolerance. Product dust on the seal area is a critical failure source in powder filling operations. A thicker sealant layer of 76.2 µm can improve seal contamination tolerance compared with 50 µm films by providing more polymer volume for flow into seal gap defects. Seal integrity is checked by peel testing per ASTM F88 and vacuum leak testing per ASTM D3078. The metallized barrier layer may undergo crazing during flexing. The LLDPE layer cannot prevent all flex crack propagation, but its thicker gauge may reduce stress concentration at the foil interface. Oxygen transmission of the finished laminate is governed by the metallized PET layer. The water vapor transmission rate is also governed by the outer web and adhesive. The LLDPE layer does not significantly improve barrier but provides mechanical durability. Adhesive selection must consider slip additive migration from the LLDPE. Erucamide migration can reduce adhesive bond strength over a 30–60 day aging period. Converters should specify a film grade with no migrating slip additives if long laydown times are expected. The laminate is typically cured at 35–40 °C for 24–48 h in an oven. After curing, the roll must be cooled to room temperature before slitting. Hot slitting can create edge welding of the LLDPE layer. The finished pouches are filled and sealed on multi-head weighers with forming collars. Seal jaw temperatures of 120–135 °C are typical for high-barrier coffee pouches. The film must maintain consistent surface tension and low blocking tendency during high-speed unwinding. The coefficient of friction of the untreated sealant side may be controlled by an antiblock package. A coefficient of friction below 0.3 is often specified to prevent film sticking to metal surfaces, but the value depends on the film formulation and test method. Published data for this specific film under high-humidity coffee packaging conditions is limited.

    Free Quote

    Competitive DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm thickness, is supplied as a linear low-density polyethylene web intended for the sealant and laminating position in multilayer flexible packaging, protective thermal lamination, and industrial sheet assembly. The laminating designation separates the grade from general-purpose overwrap and shrink films through a tighter roll-profile specification, a controlled surface-oxidation step for adhesive wetting, and a nominal gauge of 76.2 µm (3.0 mil) that shifts failure modes from pinhole formation to substrate delamination on board and nonwoven laminates. Because the product is not a coated or metallized film, downstream converters must match the adhesive, ink, or extrusion coating to the treated polyethylene surface. Published data for this specific configuration is limited; the values discussed in this document are representative of linear low-density polyethylene laminating film class and must be verified against the supplier’s certificate of analysis.

    Material Identity, Gauge Designation, and Roll-Stock Configuration

    The product identification “DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness” encodes the resin family, intended converting operation, and nominal thickness. The 76.2 µm gauge is equivalent to 3.0 mil and is typically controlled to a thickness tolerance of ± 5%. The film is supplied as roll stock, slit to converter-specified widths, and is commonly wound on 76 mm (3 in) or 152 mm (6 in) fiber cores. Roll diameter, reel hardness, and winding tension are specified to reduce telescoping and blocking during storage. The outer surface receiving lamination adhesive or extrusion polymer is oxidized by corona or atmospheric plasma treatment; the treated surface is evaluated using ASTM D2578 wetting tension and is generally maintained between 38 and 42 mN/m. Untreated film surfaces usually measure 31 to 34 mN/m and are inadequate for solvent-borne and water-borne laminating adhesives.

    The LLDPE class is polymerised with an alpha-olefin comonomer, which introduces short-chain branches along the polyethylene backbone. This structure yields a density in the range of 0.917 to 0.923 g/cm³, placing the grade below conventional high-density polyethylene and above plastomer sealant resins. The lower density relative to HDPE reduces seal initiation temperature and improves interlayer adhesion in extrusion lamination. Compared with unmodified low-density polyethylene film, the linear low-density polyethylene backbone requires less gauge to achieve equivalent dart impact and tear propagation resistance, but the film may exhibit lower clarity when blown-film processing is used.

    What Processing Boundaries Govern Laminating and Seal Integrity?

    Conversion of 76.2 µm LLDPE laminating film is governed by three coupled variables: interfacial wetting tension, web tension, and thermal input. When LX-1 is used as the sealant web in adhesive lamination, the corona-treated surface should be processed within 24 h to 72 h after surface oxidation because low-molecular-weight oxidation products migrate into the bulk, reducing surface energy and creating intermittent bond voids. On a narrow-web thermal laminator running at 50 to 150 m/min, web tension is typically set at 0.5 to 1.5 N/mm of web width. Tension above 2.0 N/mm has been observed on production-scale gravure coating lines to produce machine-direction chatter and gel streak, particularly on monolayer LLDPE webs with low stiffness after the drying tunnel.

    Heat-seal behavior is the critical property for packaging converters. For linear low-density polyethylene sealant layers of this gauge, heat seal initiation generally occurs between 95 °C and 110 °C on jaw sealers. Acceptable seal strength is normally reached at jaw temperatures of 120 °C to 150 °C with dwell times of 0.5 s to 1.5 s and jaw pressures of 275 kPa to 410 kPa. Above 160 °C, film distortion and edge thinning can occur, and the failure mode transitions from peel fracture to seal perimeter tear. Hot-tack strength follows a similar thermomechanical envelope; validation on vertical form-fill-seal equipment should follow ASTM F1921, while seal strength is measured per ASTM F88. Field data from pneumatic jaw sealers indicate that jaw pressures below 200 kPa create channel leaks at film fold-over points, while pressures above 600 kPa extrude the 76.2 µm web from the seal footprint.

    For adhesive lamination, the adhesive coating weight is influenced by the film’s surface roughness and wetting tension. A typical solventless polyurethane laminating adhesive is applied at 1.0 to 2.5 g/m²; on a 76.2 µm LLDPE web, dewetting is observed below 36 mN/m, so corona-treated film must be checked immediately before the coater. If the film is stored beyond the treatment window or exposed to high relative humidity, the coater may use an inline corona treater before the coating station. In extrusion lamination, the film is used as the secondary web and is not remelted; the molten low-density polyethylene or ethylene copolymer tie layer is extruded at melt temperatures of 300 °C to 320 °C and nip pressures of 30 to 60 N/cm. The chilled nip is maintained at 10 °C to 20 °C to prevent film relaxation and web bridging, because monolayer LLDPE has low melt strength above its softening point.

    When LX-1 Replaces Thinner LLDPE Sealant Layers in Flexible Packaging

    Replacing a 38.1 µm or 50.8 µm sealant web with 76.2 µm LX-1 changes heat transfer and seal-strength development. The thicker gauge requires approximately 40% to 60% longer dwell under constant jaw pressure to bring the seal interface to the same temperature. In practice, converters running vertical form-fill-seal equipment reduce line speed or increase jaw temperature within the validated range. The thicker gauge can absorb surface irregularities in board, textile, and foam laminates, reducing pinhole density, but it also increases stiffness and may change bag-handling characteristics on horizontal wrappers. Converters should re-run seal-strength curves per ASTM F88 after any gauge change, because the failure location can move from the seal interface to the film substrate. Published data for this specific configuration is limited; field verification on the actual packaging line is required.

    Compared with ethylene-vinyl acetate sealant webs, LX-1 provides a narrower heat-seal initiation plateau and lower clamp-temperature tolerance, but offers a lower water vapour transmission contribution and lower sealant extractables under FDA 21 CFR 177.1520(c). Compared with ionomer films, LX-1 does not provide the same scratch resistance or seal-through-contamination performance. Within the Sclairfilm product range, general-purpose films are specified for optical overwrap or surface protection; LX-1 is selected for laminating because the surface treatment and roll-profile characteristics are matched to adhesive coating equipment rather than shrink or display properties.

    For Tensile, Tear, and Barrier Testing, the Governing Methods Are...

    Tensile, tear, and barrier characterisation of 76.2 µm LLDPE laminating film is performed under controlled laboratory conditions. Machine-direction and transverse-direction tensile properties are measured per ASTM D882 with a jaw separation of 50 mm and crosshead speed of 500 mm/min. Elmendorf tear resistance is measured per ASTM D1922. Optical properties are measured using ASTM D1003 for haze and ASTM D2457 for 45° gloss. Coefficient of friction is determined by ASTM D1894 against stainless steel or against the treated film surface. Water vapour transmission is measured by ASTM F1249 or ASTM E96; for a 76.2 µm LLDPE film, the water vapour transmission rate is generally lower than for a 25.4 µm film of the same resin class. Oxygen and carbon dioxide permeability are not controlled for uncoated polyethylene because the film is a poor gas barrier; metallization or coating is required when gas barrier is specified.

    Representative LLDPE Laminating Film Class Values for 76.2 µm Gauge
    AttributeTest MethodTypical Range
    Nominal thicknessASTM D594776.2 µm ± 5%
    DensityASTM D15050.917–0.923 g/cm³
    Melt indexASTM D1238 at 190 °C/2.16 kg0.8–1.2 g/10 min
    Tensile strength at break MDASTM D88230–40 MPa
    Tensile strength at break TDASTM D88225–35 MPa
    Elongation at break MDASTM D882500–650%
    Elongation at break TDASTM D882600–750%
    Elmendorf tear MDASTM D1922200–500 gf
    Elmendorf tear TDASTM D1922300–600 gf
    HazeASTM D10033%–8%
    Gloss 45°ASTM D245770–90
    Kinetic coefficient of frictionASTM D18940.20–0.40
    Wetting tension treated surfaceASTM D257838–42 mN/m

    Elmendorf tear values in Table 1 are not directly scalable from thinner films because tear propagation in LLDPE involves yield-zone formation ahead of the crack tip; doubling the gauge may increase tear resistance by a factor of 1.4 to 1.8, not 2.0. This has implications for pouch drop resistance when replacing a 38.1 µm film with 76.2 µm LX-1. Water vapour transmission is roughly inversely proportional to gauge for uncoated polyethylene, so a 76.2 µm web transmits approximately one-third to one-half the moisture of a 25.4 µm web, depending on polymer density and temperature gradient. At 38 °C and 90% RH, a 76.2 µm LLDPE film can be expected to fall between 3 and 6 g/m²/day by ASTM F1249, but the exact value must be confirmed on the supplier’s certificate of analysis.

    Comparing LX-1 Against General-Purpose and Shrink-Film Sclairfilm Grades

    Compared with general-purpose Sclairfilm overwrap grades, LX-1 is not supplied with the same optical surface finish or display-window performance. The laminating-grade surface treatment is intended to receive adhesive or extrusion polymer, and its roll-profile characteristics are controlled for continuous web coating rather than for individual sheet separation. Compared with oriented shrink-film grades, LX-1 does not exhibit engineering shrink recovery in either machine or transverse direction, and it should not be used where oriented shrink force is required. In adhesive lamination, the main practical difference is the thickness of 76.2 µm: thinner sealant films such as 25.4 µm or 38.1 µm lower material cost but increase the risk of surface defect replication and pinholes; thicker films extend dwell time and reduce web temperature sensitivity.

    When compared with coextruded LLDPE films containing a metallocene-catalysed sealant core, LX-1 may have a broader melting peak and lower hot-tack peak strength. Converters should validate seal windows on high-speed packaging lines using ASTM F1921 or ASTM F88. If the laminating application requires low seal initiation below 90 °C, an ethylene-vinyl acetate or plastomer-based sealant web should be evaluated instead; LX-1 is not formulated as an ultra-low-initiation sealant grade.

    On Surface Treatment, Corona Decay, and Roll Inventory Conditions

    Corona-treated laminating film has a finite shelf life because surface oxidation products migrate into the bulk polymer. For LX-1 stored at 20 °C to 25 °C and 40% to 60% RH, surface treatment generally remains above 38 mN/m for 6 to 12 months, but converters should verify wetting tension at receipt and before each laminating run, because corona decay is faster in hot and humid environments. Storage above 35 °C or on sun-exposed loading docks accelerates antioxidant migration and blocking, especially at high reel hardness. Roll inventory should follow first-in, first-out discipline, and partial rolls should be rewound to uniform tension before return to storage. In high-humidity environments, moisture does not plasticize polyethylene, but condensation on the film surface can interfere with adhesive wetting and should be removed with an air-knife or surface dryer before coating.

    Compliance and Test Method Matrix
    RequirementReferenced StandardScope
    Food-contact olefin polymerFDA 21 CFR 177.1520(c)Permitted ethylene-alpha-olefin copolymers subject to extraction limits
    European food-contact packagingEU No 10/2011Overall migration and specific migration limits
    REACH SVHCEC 1907/2006Candidate list substances below 0.1% w/w
    RoHS heavy metalsDirective 2011/65/EULead, cadmium, mercury, hexavalent chromium, PBB, PBDE
    Seal strengthASTM F88Flexible packaging seal strength
    Hot tackASTM F1921Seal strength at elevated temperature
    Wetting tensionASTM D2578Surface treatment verification

    On high-speed lamination lines, the most common failure mode with monolayer 76.2 µm LLDPE webs is not bond strength loss but roll-hardness-induced web wander. If the incoming roll is wound at high tension or stored on end in a warm warehouse, internal blocking creates local slip-stick events that appear as alternating glossy and hazy bands on the coated laminate. Maintenance personnel can identify this by measuring web tension at the nip with a running tension meter and comparing the value to the 0.5 to 1.5 N/mm band. A second failure mode is post-lamination tunnelling when the film is bonded to a board substrate with water-borne adhesive and dried at insufficient airflow; the residual moisture is trapped by the LLDPE web, forming blisters that do not resolve upon rewinding. Specifying a drying tunnel air temperature of 70 °C to 90 °C and measuring web-out moisture with an infrared backscatter sensor can reduce this defect. Published data for this specific configuration is limited; the actual optimum setpoints must be established on the individual laminator, because air impingement and roll-contact geometry affect the result.

    Top